Grain growth kinetics was studied for commercially pure magnesium subjected to equal channel angular extrusion (ECAE). The specimens were ECAE processed upto 4 passes at 523 K following all the three important routes, namely A, 13, and C. Texture and microstructures of the samples were studied using Electron Back Scattered Diffraction (EBSD) technique in a Field Emission Gun Scanning Electron Microscope (FEG-SEM). It was observed that the grain size significantly reduces after ECAE. ECAE process produces a slightly rotated B and C-2 fiber. Static annealing leads to normal grain growth with unimodal distribution of grains through out the temperature range. Average activation energy for grain growth in the temperature range studied is found to be less than the activation energy for lattice diffusion and grain boundary diffusion of magnesium. No significant change in texture during isochronal annealing for 1 hour i.e., the predominant deformation texture remains same.
Resumo:
Paraserianthes falcataria is a very fast growing, light wood tree species, that has recently gained wide interest in Indonesia for industrial wood processing. At the moment the P. falcataria plantations managed by smallholders are lacking predefined management programmes for commercial wood production. The general objective of this study was to model the growth and yield of Paraserianthes falcataria stands managed by smallholders in Ciamis, West Java, Indonesia and to develop management scenarios for different production objectives. In total 106 circular sample plots with over 2300 P. falcataria trees were assessed on smallholder plantation inventory. In addition, information on market prices of P. falcataria wood was collected through rapid appraisals among industries. A tree growth model based on Chapman-Richards function was developed on three different site qualities and the stand management scenarios were developed under three management objectives: (1) low initial stand density with low intensity stand management, (2) high initial stand density with medium intensity of intervention, (3) high initial stand density and strong intensity of silvicultural interventions, repeated more than once. In general, the 9 recommended scenarios have rotation ages varying from 4 to 12 years, planting densities from 4x4 meters (625 trees ha-1) to 3x2 meters (1666 trees ha-1) and thinnings at intensities of removing 30 to 60 % of the standing trees. The highest annual income would be generated on high-quality with a scenario with initial planting density 3x2 m (1666 trees ha-1) one thinning at intensity of removing 55 % of the standing trees at the age of 2 years and clear cut at the age of 4 years.
Resumo:
A sensitive framework has been developed for modelling young radiata pine survival, its growth and its size class distribution, from time of planting to age 5 or 6 years. The data and analysis refer to the Central North Island region of New Zealand. The survival function is derived from a Weibull probability density function, to reflect diminishing mortality with the passage of time in young stands. An anamorphic family of trends was used, as very little between-tree competition can be expected in young stands. An exponential height function was found to fit best the lower portion of its sigmoid form. The most appropriate basal area/ha exponential function included an allometric adjustment which resulted in compatible mean height and basal area/ha models. Each of these equations successfully represented the effects of several establishment practices by making coefficients linear functions of site factors, management activities and their interactions. Height and diameter distribution modelling techniques that ensured compatibility with stand values were employed to represent the effects of management practices on crop variation. Model parameters for this research were estimated using data from site preparation experiments in the region and were tested with some independent data sets.
Resumo:
The oxidation of liquid Al–Mg–Si alloys at 900–1400 °C was studied by thermogravimetric analysis (TGA). The development of a semi-protective surface layer of MgO/MgAl2O4 allows the continuous formation of an Al2O3-matrix composite containing an interpenetrating network of metal microchannels at 1000–1350 °C. An initial incubation period precedes bulk oxidation, wherein Al2O3 grows from a near-surface alloy layer by reaction of oxygen supplied by the dissolution of the surface oxides and Al supplied from a bulk alloy reservoir through the microchannel network. The typical oxidation rate during bulk growth displays an initial acceleration followed by a parabolic deceleration in a regime apparently limited by Al transport to the near-surface layer. Both regimes may be influenced by the Si content in this layer, which rises due to preferential Al and Mg oxidation. The growth rates increase with temperature to a maximum at ~1300 °C, with a nominal activation energy of 270 kJ/mole for an Al-2.85 wt. % Mg-5.4 wt. % Si alloy in O2 at furnace temperatures of 1000–1300 °C. An oscillatory rate regime observed at 1000–1075 °C resulted in a banded structure of varying Al2O3-to-metal volume fraction.
Resumo:
Electrochemical quartz crystal microbalance (EQCM) has been used to study the electrochemical precipitation of Mn(OH)(2) on a Au crystal and its capacitance properties. From the EQCM data, it is inferred that NO3- ions get adsorbed on the Au crystal and then undergo reduction, resulting in an increase in pH near the electrode surface. Precipitation of Mn2+ occurs as Mn(OH)(2), with an increase in mass of the Au crystal. Mn(OH)(2) undergoes oxidation to MnO2, which exhibits electrochemical supercapacitor behavior on subjecting to electrochemical cycling in a Na2SO4 electrolyte. EQCM data indicate mass variations corresponding to surface insertion/extraction of Na+ ions during discharge/charge cycling. (C) 2010 The Electrochemical Society. DOI: 10.1149/1.3479665] All rights reserved.
Resumo:
L-arginine phosphate monohydrate (LAP) is a relatively new organic nonlinear optical material. In this paper, the results of our recent investigations on the growth of this crystal are presented. The growth of the undesirable micro-organisms was prevented by protecting the solution surface by placing a thick layer of n-hexane over it. Colouration of the solution could be avoided by keeping the growth temperature low and by protecting it from light. The effect of pH value of the solution on the solubility and habit was analysed. The grown crystals were characterized by means of X-ray topography.
Resumo:
This working paper reports the ongoing research conducted in the research project, The Quest for Well-being in Growth Industries: A Collaborative Study in Finland and Scotland, under the auspices of Academy of Finland research programme, The Future of Work and Well-being. The research project examines the contradictory pressures for policies and practices towards both the inhibition and the enhancement of work-related well-being that are likely in growth industries. The overall aim is to evaluate the development, implementation and use of work-related well-being policies in four selected growth industries. These – electronics, care, finance and accounting, and tourism – have been selected on the basis of EU and national forecasts, and demographic and socio-economic trends in standard and non-standard employment. In this paper we aim to review the survey that constitutes the second main phase of this research.
Resumo:
An attempt to systematically investigate the effects of microstructural parameters in influencing the resistance to fatigue crack growth (FCG) in the near-threshold region under three different temper levels has been made for a high strength low alloy steel to observe in general, widely different trends in the dependence of both the total threshold stress intensity range, DELTA-K(th) and the intrinsic or effective threshold stress intensity range, DELTA-K(eff-th) on the prior austenitic grain size (PAGS). While a low strain hardening microstructure obtained by tempering at high temperatures exhibited strong dependence of DELTA-K(th) on the PAGS by virtue of strong interactions of crack tip slip with the grain boundary, a high strength, high strain hardening microstructure as a result of tempering at low temperature exhibited a weak dependence. The lack of a systematic variation of the near-threshold parameters with respect to grain size in temper embrittled structures appears to be related to the wide variations in the amount of intergranular fracture near threshold. Crack closure, to some extent provides a basis on which the increases in DELTA-K(th) at larger grain sizes can be rationalised. This study, in addition, provides a wide perspective on the relative roles of slip behaviour embrittlement and environment that result in the different trends observed in the grain size dependence of near-threshold fatigue parameters, based on which the inconsistency in the results reported in the literature can be clearly understood. Assessment of fracture modes through extensive fractography revealed that prior austenitic grain boundaries are effective barriers to cyclic crack growth compared to martensitic packet boundaries, especially at low stress intensities. Fracture morphologies comprising of low energy flat transgranular fracture can occur close to threshold depending on the combinations of strain hardening behaviour, yield strength and embrittlement effects. A detailed consideration is given to the discussion of cyclic stress strain behaviour, embrittlement and environmental effects and the implications of these phenomena on the crack growth behaviour near threshold.
Resumo:
The nucleation and growth mechanisms during high temperature oxidation of liquid Al-3% Mg and Al-3% Mg-3% Si alloys were studied with the aim of enhancing our understanding of a new composite fabrication process. The typical oxidation sequence consists of an initial event of rapid but brief oxidation, followed by an incubation period of limited oxide growth after which bulk Al2O3/Al composite forms. A duplex oxide layer, MgO (upper) and MgAl2O4 (lower), forms on the alloy surface during initial oxidation and incubation. The spinel layer remains next to the liquid alloy during bulk oxide growth and is the eventual repository for most of the magnesium in the original alloy. Metal microchannels developed during incubation continuously supply alloy through the composite to the reaction interface. During the growth process, a layered structure exists at the upper extremity of the composite, consisting of MgO at the top surface, MgAl2O4 (probably discontinuous), Al alloy, and finally the bulk Al2O3 composite containing microchannels of the alloy. The bulk oxide growth mechanism appears to involve continuous formation and dissolution of the Mg-rich oxides at the surface, diffusion of oxygen through the underlying liquid metal, and epitaxial growth of Al2O3 on the existing composite body. The roles of Mg and Si in the composite growth process are discussed.
Resumo:
The diruthenium(III) complex [Ru2O(O2CAr)2(MeCN)4(PPh3)2](ClO4)2 (1), on reaction with 1,2-diaminoethane (en) in MeOH at 25-degrees-C, undergoes nucleophilic attacks at the carbon of two facial MeCN ligands to form [(Ru2O)-O-III(O2CAr)2-{NH2CH2CH2NHC(Me)NH}2(PPh3)2](ClO4)2 (2) (Ar = C6H4-p-X, X = H, Me, OMe, Cl) containing two seven-membered amino-amidine chelating ligands. The molecular structure of 2 with Ar = C6H4-p-OMe was determined by X-ray crystallography. Crystal data are as follows: triclinic, P1BAR, a = 13.942 (5) angstrom, b = 14.528 (2) angstrom, c = 21.758 (6) angstrom, alpha = 109.50 (2)-degrees, beta = 92.52 (3)-degrees, gamma = 112.61 (2)-degrees, V = 3759 (2) angstrom 3, and Z = 2. The complex has an {Ru2(mu-O)(mu-O2CAr2)2(2+)} core. The Ru-Ru and average Ru-O(oxo) distances and the Ru-O-Ru angle are 3.280 (2) angstrom, 1.887 [8] angstrom, and 120.7 (4)-degrees, respectively. The amino group of the chelating ligand is trans to the mu-oxo ligand. The nucleophilic attacks take place on the MeCN ligands cis to the mu-oxo ligand. The visible spectra of 2 in CHCl3 display an absorption band at 565 nm. The H-1 NMR spectra of 2 in CDCl3 are indicative of the formation of an amino-amidine ligand. Complex 2 exhibits metal-centered quasireversible one-electron oxidation and reduction processes in the potential ranges +0.9 to +1.0 V and -0.3 to -0.5 V (vs SCE), respectively, involving the Ru(III)2/Ru(III)Ru(IV) and Ru(III)2/Ru(II)Ru(III) redox couples in CH2Cl2 containing 0.1 M TBAP. The mechanistic aspects of the nucleophilic reaction are discussed.
Resumo:
The free-base octabromotetraphenylporphyrin (H2OBP) has been prepared by a novel bromination reaction of (meso-tetraphenylporphyrinato)copper(II). The metal [V(IV)O, Co(II), Ni(II), Cu(II), Zn(II), Pd(II), Ag(II), Pt(II)] derivatives exhibit interesting electronic spectral features and electrochemical redox properties. The electron-withdrawing bromine substituents at the pyrrole carbons in H2OBP and M(OBP) derivatives produce remarkable red shifts in the Soret (50 nm) and visible bands (100 nm) of the porphyrin. The low magnitude of protonation constants (pK3 = 2.6 and pK4 = 1.75) and the large red-shifted Soret and visible absorption bands make the octabromoporphyrin unique. The effect of electronegative bromine substituents at the peripheral positions of the porphyrin has been quantitatively analyzed by using the four-orbital approach of Gouterman. A comparison of MO parameters of MOBP derivatives with those of the meso-substituted tetraphenylporphyrin (M(TPP)) and unsubstituted porphine (M(P)) derivatives provides an explanation for the unusual spectral features. The configuration interaction matrix element of the M(OBP) derivatives is found to be the lowest among the known substituted porphyrins, indicating delocalization of ring charge caused by the increase in conjugation of p orbitals of the bromine onto the ring orbitals. The electron-transfer reactivities of the porphyrins have been dramatically altered by the peripheral bromine substituents, producing large anodic shifts in the ring and metal-centered redox potentials. The increase in anodic shift in the reduction potential of M(OBP)s relative to M(TPP)s is found to be large (550 mV) compared to the shift in the oxidation potential (300 mV). These shifts are interpreted in terms of the resonance and inductive interactions of the bromine substituents.
Resumo:
By the reaction of Ru2Cl(O2CAr)4 (1) and PPh3 in MeCN-H2O the diruthenium(II,III) and diruthenium(II) compounds of the type Ru2(OH2)Cl(MeCN)(O2CAr)4(PPh3)2 (2) and Ru2(OH2)(MeCN)2(O2CAr)4(PPh3)2 (3) were prepared and characterized by analytical, spectral, and electrochemical data (Ar is an aryl group, C6H4-p-X; X = H, OMe, Me, Cl, NO2). The molecular structure of Ru2(OH2)Cl(MeCN)(O2CC6H4-p-OMe)4(PPh3)2 was determined by X-ray crystallography. Crystal data are as follows: triclinic, P1BAR, a = 13.538 (5) angstrom, b = 15.650 (4) angstrom, c = 18.287 (7) angstrom, alpha = 101.39 (3)-degrees, beta = 105.99 (4)-degrees, gamma = 97.94 (3)-degrees, V = 3574 angstrom 3, Z = 2. The molecule is asymmetric, and the two ruthenium centers are clearly distinguishable. The Ru(III)-Ru(II), Ru(III)-(mu-OH2), and Ru(II)-(mu-OH2) distances and the Ru-(mu-OH2)-Ru angle in [{Ru(III)Cl(eta-1-O2CC6H4-p-OMe)(PPh3)}(mu-OH2)(mu-O2CC6H4-p-OMe)2{Ru(II)(MeCN)(eta-1-O2CC6H4-p-OMe)(PPh3)}] are 3.604 (1), 2.127 (8), and 2.141 (10) angstrom and 115.2 (5)-degrees, respectively. The compounds are paramagnetic and exhibit axial EPR spectra in the polycrystalline form. An intervalence transfer (IT) transition is observed in the range 900-960 nm in chloroform in these class II type trapped mixed-valence species 2. Compound 2 displays metal-centered one-electron reduction and oxidation processes near -0.4 and +0.6 V (vs SCE), respectively in CH2Cl2-TBAP. Compound 2 is unstable in solution phase and disproportionates to (mu-aquo)diruthenium(II) and (mu-oxo)diruthenium(III) complexes. The mechanistic aspects of the core conversion are discussed. The molecular structure of a diruthenium(II) compound, Ru2(OH2)(MeCN)2(O2CC6H4-p-NO2)4(PPh3)2.1.5CH2Cl2, was obtained by X-ray crystallography. The compound crystallizes in the space group P2(1)/c with a = 23.472 (6) angstrom, b = 14.303 (3) angstrom, c = 23.256 (7) angstrom, beta = 101.69 (2)-degrees, V = 7645 angstrom 3, and Z = 4. The Ru(II)-Ru(II) and two Ru(II)-(mu-OH2) distances and the Ru(II)-(mu-OH2)-Ru(II) angle in [{(PPh3)-(MeCN)(eta-1-O2CC6H4-p-NO2)Ru}2(mu-OH2)(mu-O2CC6H4-p-NO2)2] are 3.712 (1), 2.173 (9), and 2.162 (9) angstrom and 117.8 (4)-degrees, respectively. In both diruthenium(II,III) and diruthenium(II) compounds, each metal center has three facial ligands of varying pi-acidity and the aquo bridges are strongly hydrogen bonded with the eta-1-carboxylato facial ligands. The diruthenium(II) compounds are diamagnetic and exhibit characteristic H-1 NMR spectra in CDCl3. These compounds display two metal-centered one-electron oxidations near +0.3 and +1.0 V (vs SCE) in CH2Cl2-TBAP. The overall reaction between 1 and PPh3 in MeCN-H2O through the intermediacy of 2 is of the disproportionation type. The significant role of facial as well as bridging ligands in stabilizing the core structures is observed from electrochemical studies.