992 resultados para PHOTOLUMINESCENCE
Resumo:
We investigate theoretically the electron-hole pair states in CdTe quantum dot (QD) containing a single Mn2+ ion by the magneto-optical spectrum tuned by the electric field. It is shown that the electric field does not only tune the spin splitting via the sp-d exchange interaction but also affect significantly the anticrossing behavior in the photoluminescence spectrum. This anticrossing is caused by the s-d exchange interaction and/or the hole mixing effect, which depends sensitively on the shape of the QD. (C) 2008 American Institute of Physics.
Resumo:
Excitation power-dependent micro-photoluminescence spectra and photon-correlation measurement are used to study the optical properties and photon statistics of single InAs quantum dots. Exciton and biexciton emissions, whose photoluminescence intensities have linear and quadratic excitation power dependences, respectively, are identified. Under pulsed laser excitation, the zero time delay peak of second order correlation function corresponding to exciton emission is well suppressed, which is a clear evidence of single photon emission.
Resumo:
ZnO nanoflowers are synthesized on AIN films by solution method. The synthesized nanoflowers are composed of nanorods, which are pyramidal and grow from a central point, thus forming structures that are flower-shaped as a whole. The nanoflowers have two typical morphologies: plate-like and bush-like. The XRD spectrum corresponds to the side planes of the ZnO nanorods made up of the nanoflowers. The micro-Raman spectrum of the ZnO nanoflowers exhibits the E-2 (high) mode and the second order multiple-phonon mode. The photoluminescence spectrum of the ZnO nanoflowers exhibits ultraviolet emission centred at 375 nm and a broad green emission centred at 526 nm.
Resumo:
The properties of the wetting layer (WL) of InAs nanorings grown by droplet epitaxy have been studied. The heavy-hole (HH) and light-hole (LH) related transitions of the In(Ga)As WL were observed by reflectance difference spectroscopy. From the temperature dependent photoluminescence behavior of InAs rings, the channel for carriers to redistribute was found to be the compressed GaAs instead of the In(Ga)As layer, which strongly indicated that the wetting layer was depleted around the rings. Futhermore, a complex evolution of the WL with In deposition amount has been observed. (c) 2008 American Institute of Physics.
Resumo:
We grow In-GaAs quantum dot (QD) at low growth rate with 70 times insertion of growth interruption in MBE system. It is found that because of the extreme growth condition, QDs exhibit a thick wetting layer, large QD height value and special surface morphology which is attributed to the In segregation effect. Temperature dependence of photoluminescence measurement shows that this kind of QDs has a good thermal stability which is explained in terms of a "group coupling" model put forward by us. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Strongly vertically coupled InAs/GaAs quantum dots (QDs) with modulation doping are investigated, and polarization dependence of two-color absorptions was observed. Analysis of photoluminescence (PL) and absorption spectra shows that s-polarized absorptions at. 10.0 and 13.4 mu m, stem from the first excited state E-1 and the second excited state E-2 in the QDs to the bound state E-InGaAs in the InGaAs spacer, respectively, whereas p-polarized absorptions at 10.0 and 8.2 mu m stem from the first excited state E-1 and the ground E-g in the QDs to the bound state E-InGaAs in the InGaAs spacer, respectively. These measurements illustrate that transitions from excited states are more sensitive to normal incidence, which are very important in designing QD infrared detector. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Hall effect, Raman scattering, photoluminescence spectroscopy (PL), optical absorption (OA), mass spectroscopy, and X-ray diffraction have been used to study bulk ZnO single crystal grown by a closed chemical vapor transport method. The results indicate that shallow donor impurities (Ga and Al) are the dominant native defects responsible for n-type conduction of the ZnO single crystal. PL and OA results suggest that the as-grown and annealed ZnO samples with poor lattice perfection exhibit strong deep level green photoluminescence and weak ultraviolet luminescence. The deep level defect in as-grown ZnO is identified to be oxygen vacancy. After high-temperature annealing, the deep level photoluminescence is suppressed in ZnO crystal with good lattice perfection. In contrast, the photoluminescence is nearly unchanged or even enhanced in ZnO crystal with grain boundary or mosaic structure. This result indicates that a trapping effect of the defect exists at the grain boundary in ZnO single crystal. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
We have investigated the exciton spin relaxation in a GaInNAs/GaAs quantum well. The recombination from free and localized excitons is resolved on the basis of an analysis of the photoluminescence characteristics. The free exciton spin relaxation time is measured to be 192 ps at 10 K, while the localized exciton spin relaxation time is one order of magnitude longer than that of the free exciton. The dependence of the free exciton spin relaxation time on the temperature above 50 K suggests that both the D'yakonov-Perel' and the Elliot-Yafet effects dominate the spin relaxation process. The temperature independence below 50 K is considered to be due to the spin exchange interaction. The ultralong spin relaxation time of the localized excitons is explained to be due to the influence of nonradiative deep centers. (c) 2008 American Institute of Physics.
Resumo:
ZnO thin films were prepared by pulsed laser deposition (PLD) on glass substrates with growth temperature from room temperature (RT) to 500 degrees C. The effects of substrate temperature on the structural and optical properties of ZnO films have been investigated by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission spectra, and RT photoluminescence (PL) measurements. The results showed that crystalline and (0 0 2)-oriented ZnO films were obtained at all substrate temperatures. As the substrate temperature increased from RT to 500 degrees C, the ratio of grain size in height direction to that in the lateral direction gradually decreased. The same grain size in two directions was obtained at 200 degrees C, and the size was smallest in all samples, which may result in maximum E, and E-0 of the films. UV emission was observed only in the films grown at 200 degrees C, which is probably because the stoichiometry of ZnO films was improved at a suitable substrate temperature. It was suggested that the UV emission might be related to the stoichiometry in the ZnO film rather than the grain size of the thin film. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
It is studied whether there is any regular relationship between the yellow luminescence band and electron mobility of n-type GaN. For a series of GaN samples grown with the same Si doping, it is found that the electron mobility decreases with an increase of relative intensity of yellow luminescence, accompanied by an increase of edge dislocation density. Further research indicates that it is acceptors introduced by edge dislocations which lead to the concomitant changes of yellow luminescence and electron mobility. Similar changes are induced by Si doping in the n-type GaN samples with relatively low edge dislocation density. However, the relationship between the yellow luminescence and electron mobility of n-type GaN is not a simple one. A light Si doping may simultaneously increase yellow luminescence and electron mobility when Si doping plays a dominant role in reducing the carrier scattering. This means that even the intensity of yellow luminescence is often used as an indicator of material quality for GaN, it does not have any monotonous correlation with the electron mobility of GaN. (c) 2007 American Institute of Physics.
Resumo:
This letter reports on the Raman, optical and magnetic properties of FeNi co-doped ZnO nanowires prepared via a soft chemical solution method. The microstructural investigations show that the NiFe co-dopants are substituted into wurtzite ZnO nanostructure without forming any secondary phase. The co-doped nanowires show a remarkable reduction of 34 nm (267.9 meV) in the optical band gap, while suppression in the deep-level defect transition in visible luminescence. Furthermore, these nanowires exhibit ferromagnetism and an interesting low-temperature spin glass behavior, which may arise due to the presence of disorder and strong interactions of frustrated spin moments of Ni and Fe co-dopants on the ZnO lattice sites. Copyright (C) EPLA, 2009
Resumo:
The Pt nanoparticles (NPs), which posses the wider tunable localized-surface-plasmon (LSP) energy varying from deep ultraviolet to visible region depending on their morphology, were prepared by annealing Pt thin films with different initial mass-thicknesses. A sixfold enhancement of the 357 nm forward emission of ZnMgO was observed after capping with Pt NPs, which is due to the resonance coupling between the LSP of Pt NPs and the band-gap emission of ZnMgO. The other factors affecting the ultraviolet emission of ZnMgO, such as emission from Pt itself and light multi-scattering at the interface, were also discussed. These results indicate that Pt NPs can be used to enhance the ultraviolet emission through the LSP coupling for various wide band-gap semiconductors.
Resumo:
The first report of a short wavelength infrared detector based on type II InAs/GaSb superlattices is presented. Very short period superlattices containing InAs (2ML)/GaSb (8ML) superlattices (SLs) were grown by molecular-beam epitaxy on GaSb substrates. The photoluminescence showed a cut-off wavelength at 2.1 mu m at 10 K and 2.6 mu m at 300 K. Room-temperature optical transmittance spectra shows obvious absorption in InAs (2ML)/GaSb (8ML) SL in the range of 450-680 meV, i.e. 1.8-2.7 mu m. The cut-off wavelength moved from 2.3 mu m to 2.6 mu m with temperature rising from 77 K to 300 K in photoresponse spectra. The blackbody response R-v exponentially decreased as a function of 1/T in two temperature sections (130-200 K and 230-300 K). The blackbody detectivity D-bb(center dot) was beyond 1 x 10(8) cmHz(1/2)/W at room temperature. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
A two dimensional silicon-on-insulator based photonic crystal structure is used to enhance the emission from colloidal HgTe nanocrystal quantum dots embedded in a thin polymer film. The enhancement is resonant to the leaky eigenmodes of the photonic crystals due to coherent scattering effects. Transmittance and photoluminescence experiments are presented to map the leaky mode dispersion and the angle dependence of the emission enhancement factor, which reaches values up to 80 (650) for vertical (oblique) emission in the telecommunication wavelength range.
Resumo:
Nanostructured hexagonal InN overlayers were heteroepitaxially deposited on vertically oriented c-axis GaN nanorods by metal-organic chemical vapor deposition. InN overlayers grown in radial directions are featured by a nonpolar heteroepitaxial growth mode on GaN nanorods, showing a great difference from the conventional InN growth on (0001) c-plane GaN template. The surface of InN overlayers is mainly composed of several specific facets with lower crystallographic indices. The orientation relationship between InN and GaN lattices is found to be [0001](InN) parallel to [0001](GaN) and [1100](InN)parallel to[1100](GaN). A strong photoluminescence of InN nanostructures is observed. (C) 2009 American Institute of Physics. [DOI 10.1063/1.3177347]