965 resultados para density distribution


Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the first estimate of jaguar density in the semi-arid caatinga biome of north-eastern Brazil. During August-October 2007, in the Serra da Capivara National Park, we used camera traps to identify and count jaguars. Jaguar abundance and density were calculated using mark-recapture models. In a sampling effort of 1,249 camera-trap-nights we identified 12 adult jaguars and estimated an 2 abundance of 14 +/- 3.6 jaguars in an area of 524 km(2), i.e. a density of 2.67 +/- 1.00 jaguars per 100 km(2). This estimate is higher than in most other Brazilian biomes and indicates Serra da Capivara National Park as an important reserve for protecting jaguars in north-eastern Brazil.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this work was to determine the effect of temperature and heating rate on the densification of four leucite-based dental porcelains: two low-fusion (Dentsply Ceramco and Ivoclar) and two high-fusion commercial porcelains (Dentsply Ceramco). Porcelain powders were characterized by differential thermal analysis (DTA), X-ray diffraction (XRD), particle size distribution, helium picnometry, and by scanning electron microscopy. Test specimens were sintered from 600 to 1050 degrees C, with heating rates of 55 degrees C/min and 10 degrees C/min. The bulk density of the specimens was measured by the Archimedes method in water, and microstructures of fracture surfaces were analyzed by scanning electron microscopy (SEM). The results showed that densification of specimens increased with the increase in temperature. The increase in the heating rate had no effect on the densification of the porcelains studied. Both high-fusion materials and one of the low-fusing porcelains reached the maximum densification at a temperature that was 50 degrees C lower than that recommended by the manufactures. (C) 2011 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives. To assess the elastic modulus (EM), volumetric shrinkage (VS), and polymerization shrinkage stress (PSS) of experimental highly filled nanohybrid composites as a function of matrix composition, filler distribution, and density. Methods. One regular viscosity nanohybrid composite (Grandio, VOCO, Germany) and one flowable nanohybrid composite (Grandio Flow, VOCO) were tested as references along with six highly filled experimental nanohybrid composites (four Bis-GMA-based, one UDMA-based, and one Ormocer (R) -based). The experimental composites varied in filler size and density. EM values were obtained from the ""three-point bending"" load-displacement curve. VS was calculated with Archimedes` buoyancy principle. PSS was determined in 1-mm thick specimens placed between two (poly) methyl methacrylate rods (empty set = 6 mm) attached to an universal testing machine. Data were analyzed using oneway ANOVA, Tukey`s test (alpha = 0.05), and linear regression analyses. Results. The flowable composite exhibited the highest VS and PSS but lowest EM. The PSS was significantly lower with Ormocer. The EM was significantly higher among experimental composites with highest filler levels. No significant differences were found between all other experimental composites regarding VS and PSS. Filler density and size did not influence EM, VS, or PSS. Significance. Neither the filler configuration nor matrix composition in the investigated materials significantly influenced composite shrinkage and mechanical properties. The highest filled experimental composite seemed to increase EM by keeping VS and PSS low; however, matrix composition seemed to be the determinant factor for shrinkage and stress development. The Ormocer, with reduced PSS, deserves further investigation. Filler size and density did not influence the tested parameters. (C) 2011 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The objective of this study was to evaluate the long-term influence of xenogenic grafts on bone crestal height and radiographic density following extraction of teeth. The right and left third lower molars of 22 patients were surgically extracted, and one randomly chosen socket was filled with a xenogenic graft (Gent-Tech). The contralateral molar was left to heal naturally, serving as a paired control. Digital intraoral radiographies were taken at surgery and 2, 6, and 24 months after, to evaluate bone density (BD) and alveolar bone crest to cementoenamel junction distance. The data obtained were subjected to two-way analysis of variance and Tukey`s test (alpha = 0.05). The significant decrease in cementoenamel junction distance observed for both groups was limited to the first 6 months. BD values increased significantly in the first 6 months, with no alterations observed up to 24 months for both groups. BD was higher for the experimental group at all time points (p < 0.05). Socket grafting with the xenogenic materials tested did not changed bone crestal height and bone radiographic density in the long term.