Resumo:
基于热传导方程和高斯-赛德尔数值计算方法,对部分抽运板条激光器的温度分布、热应力和热致折射率变化等热效应进行了详细分析,并与单侧抽运及双侧抽运方式进行了比较。结果表明,设计合理的部分抽运板条激光器,可以获得较高的抽运效率,其热效应相比于均匀抽运的情况并没有显著劣化,不论是采用锯齿形传播方式还是直线传播方式的激光器都可以获得较好的光束质量,当一束高斯激光直线经过板条晶体中部时,光束质量因子为1.4,若采用锯齿形传播方式,则光束质量因子可提高到1.1。
Resumo:
利用自制高功率激光二极管(LD)列阵堆和波导整形抽运耦合系统,将抽运光耦合至Nd:YVO4板条晶体,平平腔运转得到了1.064μm的偏振激光输出。在最大抽运功率为84W时,透过率为10%的输出腔镜得到了31W的激光功率输出,光一光效率37%,斜效率45%,板条晶体两个方向的输出光束质量差别较大。为了进一步提高光束质量,使用柱面镜混合腔结构,在最大抽运功率为86W时,得到了19.3W的1064nm激光输出,测得的非稳腔和稳腔两个方向的M^2因子分别为1.4和1.7。
Resumo:
A planar waveguide laser operating in a negative branch unstable resonator is Q-switched by an acoustooptic mod latorin anew configuration, providing effective, high-speed switching. The laser using a 200-mu m Nd:YAG core, face pumped by 10 laser diode bars, has produced 100-W output in a good beam quality at 100-kHz pulse rate, and 4.5 mJ at lower frequency with 15-ns pulse duration.
Resumo:
实验研究了腔内位相锁定来至一LAD侧面抽运的Nd:YAG板条的两束激光,输出镜面出现干涉条纹,获得1.13W的相干光,其组束效率达到64.9%,相干度约60%。实验中发现只需要一根作为滤波的金属丝放在离输出镜合适的位置都就能有效稳定干涉条纹,金属丝引起的损耗低于8%。
Resumo:
寄生振荡的存在使得放大器在信号光到达之前消耗了大量的反转粒子数,降低了放大器的激光增益和储能效率,严重地影响了激光放大器的性能,尤其对高功率激光放大器。在理论分析和实验研究的基础上,以Nd∶YAG晶体板条为例,用8条半导体激光阵列对晶体进行双侧抽运,研究了高功率激光放大器的寄生振荡现象,分析了板条晶体寄生振荡产生的原因,并详细比较了晶体在不同的抽运功率和表面处理下的放大效果,得到了2倍的单程放大,当输入能量为140 mJ时,获得了278 mJ的激光输出。
Resumo:
开展了激光二极管(LD)抽运的全固态热容激光器的理论与实验研究, 数值模拟了在热容工作条件下侧面抽运的Nd:YAG板条激光器的热透镜效应, 分析了热透镜效应对激光输出的影响, 并进行了相应的实验论证。实验中采用的晶体尺寸为57 mm×40 mm×4 mm, 激光二极管阵列的抽运峰值功率为12 kW, 重复频率为1 kHz, 占空比为20%, 为了获得较高的增益, 将抽运光通过光学系统进行聚焦, 抽运光在晶体侧面的光斑大小为15 mm×57 mm。实验中观察了1 s内的脉冲能量输出的波动情况, 在开始工作的
Resumo:
An injection-locking excimer laser beam with a pulse duration of 25 ns is focused on the surface of a polymide film. The laser beam that passes through the etching film is shorter than the original one. By optimizing the thickness of the film and the beam power density, a pulse with a 3-ns pulse duration can be obtained using this switch technology.
Resumo:
In this letter, we present an all solid-state, injection-seeded Ti:sapphire laser. The laser is pumped by a laser diode pumped frequency-doubled Nd:YAG laser, and injection-seeded by an external cavity laser diode with the wavelength between 770 and 780 nm. The single longitude mode and the doubling efficiency of the laser are obtained after injection seeding. The experimental setup and relative results are reported. It is a good candidate laser source for mobile differential absorption lidar (DIAL) system.
Resumo:
By employing a continuous-wave (CW) Ti:sapphire tunable laser as a pumping source and a Cr4+:YAG single crystal as the saturable absorber (SA), a passively Q-switched Nd:YAG ceramic laser has been demonstrated at room temperature. With an absorbed pumping power of 541 mW at 808 nm, an average output power of 61 mW at 1064 nm has been obtained with 3.5 mu J pulse energy, 15 ns pulse width and 18.18 kHz repetition rate, and the corresponding slope-efficiency is 15%. The relationships between the pulse width, repetition rate, average output power, pulse energy, and peak power on the absorbed pumping power for different initial transmission of the Cr4+:YAG SA are discussed separately. The Nd:YAG ceramic is one of the most promising laser materials for compact, efficient, all-solid-state pulsed lasers.
Resumo:
A single-longitudinal-mode (SLM) laser-diode pumped Nd: YAG laser with adjustable pulse width is developed by using the techniques of pre-lasing and changing polarization of birefingent crystal. The Q-switching voltage is triggered by the peak of the pre-lasing pulse to achieve the higher stability of output pulse energy. The output energy of more than 1 mJ is obtained with output energy stability of 3% (rms) at 100 Hz. The pulse-width can be adjusted from 30 ns to 300 ns by changing the Q-switching voltage. The probability of putting out single-longitudinal-mode pulses is almost 100%. The laser can be run over four hours continually without mode hopping.