980 resultados para METAL HEXACYANOMETALATE FILMS


Relevância:

20.00% 20.00%

Publicador:

Resumo:

WO3 nanoplate arrays with (002) oriented facets grown on fluorine doped SnO2 (FTO) glass substrates are tailored by tuning the precursor solution via a facile hydrothermal method. A 2-step hydrothermal method leads to the preferential growth of WO3 film with enriched (002) facets, which exhibits extraordinary photoelectrochemical (PEC) performance with a remarkable photocurrent density of 3.7 mA cm–2 at 1.23 V vs. revisable hydrogen electrode (RHE) under AM 1.5 G illumination without the use of any cocatalyst, corresponding to ~93% of the theoretical photocurrent of WO3. Density functional theory (DFT) calculations together with experimental studies reveal that the enhanced photocatalytic activity and better photo-stability of the WO3 films are attributed to the synergistic effect of highly reactive (002) facet and nanoplate structure which facilitates the photo–induced charge carrier separation and suppresses the formation of peroxo-species. Without the use of oxygen evolution cocatalysts, the excellent PEC performance, demonstrated in this work, by simply tuning crystal facets and nanostructure of pristine WO3 films may open up new opportunities in designing high performance photoanodes for PEC water splitting.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tin monosulfide (SnS) films with varying distance between the source and substrate (DSS) were prepared by the thermal evaporation technique at a temperature of 300 degrees C to investigate the effect of the DSS on the physical properties. The physical properties of the as-deposited films are strongly influenced by the variation of DSS. The thickness, Sn to S at.% ratio, grain size, and root mean square (rms) roughness of the films decreased with the increase of DSS. The films grown at DSS = 10 and 15 cm exhibited nearly single-crystalline nature with low electrical resistivity. From Hall-effect measurements, it is observed that the films grown at DSS <= 15 cm have p-type conduction and the films grown at higher distances have n-type conduction due to the variation of the Sn/S ratio. The films grown at DSS = 15 cm showed higher optical band gap of 1.36 eV as compared with the films grown at other distances. The effect of the DSS on the physical properties of SnS films is discussed and reported.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The treatment of [M(dppf)(H2O)2](OTf)2 (dppf =1,1′-bis(diphenylphosphino)ferrocene; M = Pd, Pt) with 1 equiv of disodium fumarate in methanol medium showed an unusual hydrogenation of the ethylenic bond followed by the formation of metallochelates linking M through one of the carboxylates and the β-carbon with respect to COO−. Despite the possibility of formation of a [2 + 2] or [4 + 4] self-assembled macrocycle, the reduction of fumarate to succinate, and in particular the linking through the β-carbon, is unique since a similar treatment using disodium succinate instead of disodium fumarate yielded an expected metallochelate where both the carboxylates were coordinated to the square-planar metal.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The optical properties of Bi(2)V(1-x)MnxO(5.5-x) (x=0.05, 0.1, 0.15 and 0.2 at.%) thin films fabricated by pulsed laser deposition on platinized Silicon Substrates were Studied in UV-visible spectral region (1.51-4.17 CV) using spectroscopic ellipsometry. The optical constants and thicknesses of these films have been obtained by fitting the ellipsometric data (Psi and Delta) using a multilayer four-phase model system and a relaxed Lorentz oscillator dispersion relation. The surface roughness and film thickness obtained by spectroscopic ellipsometry were found to be consistent with the results obtained by atomic force and scanning electron microscopy. The refractive index measured at 650 nm does not show any marginal increase with Mn content. Further, the extinction coefficient does not show much decrease with increasing Mn content. An increase in optical band gap energy from 2.52 to 2.77 eV with increasing Mn Content from x = 0.05 to 0.15 was attributed to the increase in oxygen ion vacancy disorder. (C) 2009 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fabrication of single-component multilayer thin films still remains a challenging task via the layer-by-layer (LbL) approach. In this communication, we report the self-assembly of single-component multilayer thin films on flat and colloidal substrates through glutaraldehyde mediated covalent bonding.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Studies of double-stranded-DNA binding have been performed with three isomeric bis)2-(n-pyridyl)-1H-benzimidazole)s (n = 2, 3, 4). Like the well-known Hoechst 33258, which is a bisbenzimidazole compound, these three isomers bind to the minor groove of duplex DNA. DNA binding by the three isomers was investigated in the presence of the divalent metal ions Mg2+, Co2+, Ni2+, Cu2+, and Zn2+. Ligand-DNA interactions were probed with fluorscence and circular dichroism spectroscopy. These studies revealed that the binding of the 2-pyridyl derivative to DNA is dramatically reduced in the presence of Co2+, Ni2+, and Cu2+ ions and is abolished completely at a ligand/metal-cation ratio of 1:1. Control experiments done with the isomeric 3- and 4-pyridyl derivatives showed that their binding to DNA is unaffected by the aforementioned transition-metal ions. The ability of 2-(2-pyridyl)benzimidazole changes of the ligand associated with ion chelation probably ledto such unusual binding results for the ortho isomer. The addition of ethylenediaminetetraacetic acid (EDTA) reversed the effects completely.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The tie-lines representing the inter-crystalline ion exchange equilibria between the NiCr2O4-NiAl2O4 spinet solid solution and Cr2O3-Al2O3 corundum solid solution are determined by electron microprobe andEDAX pointcountanalysis of the oxide phases equilibrated with metallic Ni at 1373 K. The component activities in the spinet solid solution are derived from the tie-lines and thermodynamic data for Cr2O3-Al2O3 solid solution available in the literature. The Gibbs energy of mixing of the spinet solid solution calculated from the experimental data is discussed in relation to the values derived from the cation distribution models which assume random mixing of cations on both tetrahedral and octahedral sites. Positive deviation from the models is observed indicating significant positive enthalpy contribution arising form the size mismatch between Al+3 and Ni+2 ions on the tetrahedral site and Al+3, Ni+2 and Cr+3 on the octahedral site. Variation of the oxygen potential for threephase equilibrium involving metallic nickel, spinet solid solution and corundum solid solution is computed as a function of composition of the solid solutions at 1373 K. The oxygen potential exhibits a minimum at aluminum cationic fraction eta(Al)/(eta(Al) + eta(Cr)) = 0.524 in the oxide solid solutions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The ferroelectric Pb(Zr0.48Ti0.52)O-3 (PZT) thin films prepared by the pulsed laser deposition technique were studied for their response to high energy lithium ion irradiation through impedance spectroscopy. The Debye peaks, observed in the impedance and modulus plots of irradiatedfilms, shifts towards higher frequencies compared to those of unirradiated films. This is equivalent to the trend observed with increase in temperature in the unirradiated films due to the dielectric relaxation. The irradiated films showed a decrease in the grain resistance compared to the unirradiated films. The activation energy of dielectric relaxation increases from 1.25 eV of unirradiated film to 1.62 eV of irradiated film. The observed modifications in the irradiated film were ascribed to the modifications in the grain structure due to the high value of electronic energy loss.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two new alkali metal borophosphates, K-3[BP(3)o(9)(OH)(3)] and Rb-3[B2P3O11(OH)(2)], were synthesized by applying solvothermal techniques using ethanol as solvent. The crystal structures were solved by means of single-crystal X-ray diffraction (K-3[BP3O9(OH)(3)], monoclinic, C2/c (No. 15), a = 2454.6(8) pm, b = 736.3(2) pm, c = 1406.2(4) pm, beta = 118.35(2)degrees, Z = 8; Rb-3[B2P3O11(OH)(2)], monoclinic, P2(1)/c (No. 14), a = 781.6(2) pm, b:= 667.3(2) pm, c = 2424.8(5) pm, beta = 92.88(1)degrees, Z = 4). Both crystal structures comprise borophosphate chain anions. While for the rubidium compound a loop-branched chain motif is found as common for most of the chain anions in alkali metal borophosphates, the crystal structure of the potassium phase comprises the first open-branched chain with the highest phosphate content found so far in this group of compounds. Both chain anions are Closely related to known anhydrous or hydrated phases, and the structural relations are discussed in terms of how the presence of OH groups and hydrogen bonds as well as number, charge, and size of charge balancing cations influence the 3D structural arrangement. The anionic entities are classified in terms of general principles of structural systematics for borophosphates.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thin films of antimony-doped tin oxide (SnO2:Sb) were prepared by spray pyrolysis using stannous chloride (SnCl2) and antimony trichloride (SbCl3) as precursors. The antimony doping was varied from 0 to 4 wt%. Scanning electron microscopy (SEM) revealed the surface morphology to be very smooth, yet grainy in nature. X-ray diffraction (XRD) shows films to have preferred orientation, which varies with the extent of antimony doping: undoped films prefer the (2 1 1) orientation, while the (3 0 1) orientation is preferred for doping levels of 0.5 and 1.0 wt%. For higher doping levels, the (2 0 0) orientation is preferred. This difference in preferred orientations is reflected in the SEM of the films. Atomic force microscopy (AFM) reveals that film roughness is not affected by antimony doping. The minimum sheet resistance (2.17 ohm/square) achieved in the present study is lower than values reported to date in SnO2:Sb films prepared from SnCl2 precursor. The Hall mobility of undoped SnO2 films was found to be 109.52 cm(2)/V s, which reduces to 2.55 cm(2)/ Vs for the films doped with 4 wt% of Sb. On the other hand, the carrier concentration, which is 1.23 x 10(19) cm(-3) in undoped films, increases to 2.89 x 10(21) cm(-3) for the films doped with 4 wt% of Sb. (c) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Films of CuInSe2 were deposited onto glass substrates by a hot wall deposition method using bulk CuInSe2 as a source material. All the deposited CuInSe2 films were found to be polycrystalline in nature exhibiting the chalcopyrite structure with the crystallite orientation along (101),(112),(103),(211),(220),(312) and (400) directions. The photocurrent was found to increase with increase in film thickness and also with increase of light intensity. Photocurrent spectra show a peak related to the band-to-band transition. The spectral response of CuInSe2 thin films was studied by allowing the radiation to pass through a series of interference filters in the wavelength range 700-1200 rim. Films of higher thickness exhibited higher photosensitivity while low thickness films exhibited moderate photosensitivity. CuInSe2-based Solar cells with different types of buffer layers such as US, Cdse, CuInSe2 and CdSe0.7Te0.3 were fabricated. The current and voltage were measured using an optical power meter and an electrometer respectively. The fabricated solar cells were illuminated using 100 mW/cm(2) white light under AM1 conditions. (C) 2006 Elsevier Inc. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This thesis comprises four intercomplementary parts that introduce new approaches to brittle reaction layers and mechanical compatibility of metalloceramic joints created when fusing dental ceramics to titanium. Several different methods including atomic layer deposition (ALD), sessile drop contact angle measurements, scanning acoustic microscopy (SAM), three-point bending (TPB, DIN 13 927 / ISO 9693), cross-section microscopy, scanning electron microscopy (SEM), and energy dispersive X-ray spectroscopy (EDS) were employed. The first part investigates the effects of TiO2 layer structure and thickness on the joint strength of the titanium-metalloceramic system. Samples with all tested TiO2 thicknesses displayed good ceramics adhesion to Ti, and uniform TPB results. The fracture mode was independent of oxide layer thickness and structure. Cracking occurred deeper inside titanium, in the oxygen-rich Ti[O]x solid solution surface layer. During dental ceramics firing TiO2 layers dissociate and joints become brittle with increased dissolution of oxygen into metallic Ti and consequent reduction in the metal plasticity. To accomplish an ideal metalloceramic joint this needs to be resolved. The second part introduces photoinduced superhydrophilicity of TiO2. Test samples with ALD deposited anatase TiO2 films were produced. Samples were irradiated with UV light to induce superhydrophilicity of the surfaces through a cascade leading to increased amount of surface hydroxyl groups. Superhydrophilicity (contact angle ~0˚) was achieved within 2 minutes of UV radiation. Partial recovery of the contact angle was observed during the first 10 minutes after UV exposure. Total recovery was not observed within 24h storage. Photoinduced ultrahydrophilicity can be used to enhance wettability of titanium surfaces, an important factor in dental ceramics veneering processes. The third part addresses interlayers designed to restrain oxygen dissolution into Ti during dental ceramics fusing. The main requirements for an ideal interlayer material are proposed. Based on these criteria and systematic exclusion of possible interlayer materials silver (Ag) interlayers were chosen. TPB results were significantly better in when 5 μm Ag interlayers were used compared to only Al2O3-blasted samples. In samples with these Ag interlayers multiple cracks occurred inside dental ceramics, none inside Ti structure. Ag interlayers of 5 μm on Al2O3-blasted samples can be efficiently used to retard formation of the brittle oxygen-rich Ti[O]x layer, thus enhancing metalloceramic joint integrity. The most brittle component in metalloceramic joints with 5 μm Ag interlayers was bulk dental ceramics instead of Ti[O]x. The fourth part investigates the importance of mechanical interlocking. According to the results, the significance of mechanical interlocking achieved by conventional surface treatments can be questioned as long as the formation of the brittle layers (mainly oxygen-rich Ti[O]x) cannot be sufficiently controlled. In summary in contrast to former impressions of thick titanium oxide layers this thesis clearly demonstrates diffusion of oxygen from sintering atmosphere and SiO2 to Ti structures during dental ceramics firing and the following formation of brittle Ti[O]x solid solution as the most important factors predisposing joints between Ti and SiO2-based dental ceramics to low strength. This among other predisposing factors such as residual stresses created by the coefficient of thermal expansion mismatch between dental ceramics and Ti frameworks can be avoided with Ag interlayers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Metal nanoparticles (NPs) of Cu(air-stable),Ag,and Au have been prepared using an atom-economy green approach Simple mechanical stirring of solid mixtures (no solvent) of a metal salt and ammonia borane at 60 degrees C resulted in the formation of metal NPs. In this reaction, ammonia borane is transformed into a BNHx polymer, which protects the NPs formed and halts their growth. This results in the formation of the BNHx polymer protected monodisperse NPs Thus, ammonia borane used in these reactions plays a dual role (reducing agent andprecursor for the stabilizing agent).