A series of hydrogenated amorphous silicon carbide (a-Si1-xCx:H) films were prepared by plasma-enhanced chemical vapour deposition (PECVD) using a gas mixture of silane, methane, and hydrogen as the reactive source. The previous results show that a high excitation frequency, together with a high hydrogen dilution ratio of the reactive gases, allow an easier incorporation of the carbon atoms into the silicon-rich a-Si1-xCx:H film, widen the valence controllability. The data show that films with optical gaps ranging from about 1.9 to 3.6 eV could be produced. In this work the influence of the hydrogen dilution ratio of the reactive gases on the a-Si1-xCx:H film properties was investigated. The microstuctural and photoelectronic properties of the silicon carbide films were characterized by Rutherford backscattering spectrometry (RBS), elastic recoil detection analysis (ERDA), and FT-IR spectrometry. The results show that a higher hydrogen dilution ratio enhances the incorporation of silicon atoms in the amorphous carbon matrix for carbon-rich a-Si1-xCx:H films. One pin structure was prepared by using the a-Si1-xCx:H film as the intrinsic layer. The light spectral response shows that this structure fits the requirement for the top junction of colour sensor. (c) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The microstructures of hydrogenated microcrystalline silicon (tic-Si: H) thin films, prepared by plasma-enhanced chemical vapor deposition (PECVD), hot wire CVD(HWCVD) and plasma assisted HWCVD (PE-HWCVD), have been analyzed by the small angle x-ray scattering(SAXS) measurement. The SAXS data show that the microstructures of the μ c-Si: H films display different characteristics for different deposition techniques. For films deposited by PECVD, the volume fraction of micro-voids and mean size are smaller than those in HWCVD sample. Aided by suitable ion-bombardment, PE-HWCVD samples show a more compact structure than the HWCVD sample. The microstructure parameters of the μ c-Si: H thin films deposited by two-steps HWCVD and PE-HWCVD with Ar ions are evidently improved. The result of 45° tilting SAXS measurement indicates that the distribution of micro-voids in the film is anisotropic. The Fouriertransform infrared spectra confirm the SAXS data.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A thermo-optical waveguide switch matrix is designed and fabricated on silicon-on-insulator wafer. Multi-mode interferometers are used as power splitters and combiners in a Mach-Zehnder structure. Inductively coupled plasma reactive ion etching is used to fabricate the waveguides. The rise and fall times of the switch matrix are 13 mu s and 7 mu s, respectively. Switch cells have an average switching power consumption of 340 mW.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We model the recent experimental results and demonstrate that the internal shrinkage of nanocavities in silicon is intrinsically associated with preferential amorphization as induced by self-ion irradiation. The results reveal novel thermodynamic nonequilibrium properties of such an open-volume nanostructure in condensed matter and also of covalently bound amorphous materials both at nanosize scale and during ultrafast interaction with energetic beam.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new type of photovoltaic system with higher generation power density has been studied in detail. The feature of the system is a V-shaped module (VSM) with two tilted monocrystalline solar cells. Compared to solar cells in a flat orientation, the VSM enhances external quantum efficiency and leads to an increase of 31% in power conversion efficiency. Due to the VSM technique, short-circuit current density was raised from 24.94 to 33.7mA/cm(2), but both fill factor and open-circuit voltage were approximately unchanged. For the VSM similar results (about 30% increase) were obtained for solar cells fabricated by using mono-crystal line silicon wafers with only conventional background impurities. (c) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Improved methods of reduction of bend loss of silicon-on-insulator waveguides were simulated and analyzed by means of effective index method (EIM) and two dimensional beam propagation method (2D-BPM). The simulation results indicate that two different methods, one of which are introducing an offset at the junction of two waveguides and the other is etching groove at the outside of bend waveguide, can decrease bend loss. And the later one is more effective. Meanwhile, experiments validate them. By etching groove, the insertion loss of bend waveguide of R = 16mm, transverse displacement 70mum was decreased 5dB. And its bend loss was almost eliminated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel method to fabricate a thermally tunable filter with a tuning range of 26 nm from 1.504 to 1.530 mum is reported. The high-reffectivity bottom mirror is deposited in the hole formed by anisotropically etching in the basic solution from the backside of the slice with the buried SiO2 layer in silicon-on-insulator substrate as the etching-stop layer. Because of the formation of the mesa and the removing of the substrate of the hole, the power from the metal heater can be more effectively consumed in the crystalline silicon cavity. So it lowers the power consumption and the filter has a higher tuning range. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new type of photovoltaic system with higher generation power density has been studied in detail. The feature of the proposed system is a V-shaped structure with two polycrystalline solar cells. Compared to solar cells in a conventional approach, the V-shaped structure enhances external quantum efficiency and leads to an increase of 24% in power conversion efficiency.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An electro-optic variable optical attenuator in silicon-on-insulator is designed and fabricated. A series Structure is used to improve the device efficiency Compared to the attenuator in the single p-i-n diode Structure in the same modulating length, the attenuation range of the device in the series structure improves 2-3 times in the same injecting current density, while the insertion loss is not affected. The maximum dynamic attenuation of the device is greater than 30 dB. The response frequency is obtained to be about 2 MHz.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Based on thermo-optical effect of silicon, a 2 x 2 switch is fabricated in silicon-on-insulator by chemical etching. The switch presents an extinction ratio of 26 dB and a power consumption of 169 mW. The response time F similar to 10.5 mus.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A compact optical switch matrix was designed, in which light circuits were folded by total internal reflective (TIR) mirrors. Two key elements, 2 x 2 switch and TIR mirror, have been fabricated on silicon-on-insulator wafer by anisotropy chemical etching. The 2 x 2 switch showed very low power consumption of 140 mW and a very high speed of 8 +/- 1 mus. An improved design for the TIR mirror was developed, and the fabricated mirror with smooth and vertical reflective facet showed low excess loss of 0.7 +/- 0.3 dB at 1.55 mum.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Boron-doped ( B-doped) silicon nanowires have been successfully synthesized by plasma-enhanced chemical vapor deposition (PECVD) at 440degreesC using silane as the Si source, diborane( B2H6) as the dopant gas and An as the catalyst. It is desirable to extend this technique to the growth of silicon nanowire pn junctions because PECVD enables immense chemical reactivity.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The GaN film was grown on the (111) silicon-on-insulator (SOI) substrate by metal-organic chemical vapor deposition and then annealed in the deposition chamber. A multiple beam optical stress sensor was used for the in-situ stress measurement, and X-ray diffraction (XRD) and Raman spectroscopy were used for the characterization of GaN film. Comparing the characterization results of the GaN films on the bulk silicon and SOI substrates, we can see that the Raman spectra show the 3.0 cm(-1) frequency shift of E-2(TO), and the full width at half maximum of XRD rocking curves for GaN (0002) decrease from 954 arc see to 472 are sec. The results show that the SOI substrates can reduce the tensile stress in the GaN film and improve the crystalline quality. The annealing process is helpful for the stress reduction of the GaN film. The SOI substrate with the thin top silicon film is more effective than the thick top silicon film SOI substrate for the stress reduction. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

GaN epilayers have been deposited on silicon-on-insulator (SOI) and bulk silicon substrates. The stress transition thickness and the initial compressive stress of a GaN epilayer on the SOI substrate are larger than those on the bulk silicon substrate, as shown in in situ stress measurement results. It is mainly due to the difference of the three-dimensional island density and the threading dislocation density in the GaN layer. It can increase the compressive stress in the initial stage of growth of the GaN layer, and helps to offset the tensile stress generated by the lattice mismatch.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A two-dimensional (2D) photonic crystal waveguide in the Gamma-K direction with triangular lattice on a silicon-on insulator (SOI) substrate in the near-infrared band is fabricated by the combination of electron beam lithography and inductively coupled plasma etching. Its transmission characteristics are analysed from the stimulated band diagram by the effective index and the 2D plane wave expansion (PWE) methods. In the experiment, the transmission band edge in a longer wavelength of the photonic crystal waveguide is about 1590 nm, which is in good qualitative agreement with the simulated value. However, there is a disagreement between the experimental and the simulated results when the wavelength ranges from 1607 to 1630 nm, which can be considered as due to the unpolarized source used in the transmission measurement.