Resumo:
An evaluation was made of the influence of calcination temperatures on the structure, morphology and eletromagnetic properties of Ni-Zn ferrite powders. To this end, Ni(0.5)Zn(0.5)Fe(2)O(4) ferrite powders were prepared by combustion reaction and calcined at temperatures of 800, 1000 and 1200 degrees C/2 h. The resulting powders were characterized by XRD, SEM and reflectivity measurements in the frequency bands of 8-12 GHz. The results demonstrated that raising the calcination temperature increased the particle sizes of the powders of all the systems in question, improving the reflectivity of the materials. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
The disclosure of magnetic ionic liquids (MILs) as stable dispersions of surface modified gamma-Fe(2)O(3) or CoFe(2)O(4) nanoparticles (NPs) in the 1-n-butyl-3-methylimidazolium tetrafluoroborate (BMIBF(4)) ionic liquid is reported. The magnetic NPs were characterized by X-ray powder diffraction, transmission electron microscopy, and Raman spectroscopy. The surface modified NPs have proved to form stable dispersions in BMIBF(4) in the absence of water and behave like a magnetic ionic liquid. The MILs have been characterized by Raman spectroscopy, magnetic measurements, and DSC. The stability of the magnetic NPs in BMIBF(4) is consistently explained by assuming the formation of a semiorganized protective layer composed of supramolecular aggregates in the form of [(BMI)(2)(BF(4))(3)](-). A superparamagnetic behavior and saturation magnetization of ca. 18 emu/g for a sample containing 30% w/w maghemite NPs/BMIBF(4) have been inferred from static and dynamic magnetic measurements. DSC results have shown that the MIL composed of 30% w/w CoFe(2)O(4) NPs/BMIBF(4) remains a liquid phase down to -84 degrees C.
Resumo:
In this work we use magnetic resonant x-ray diffraction to study the magnetic properties of a 1.5 mu m EuTe film and an EuTe/PbTe superlattice (SL). The samples were grown by molecular beam epitaxy on (111) oriented BaF(2) substrates. The measurements were made at the Eu L(2) absorption edge, taking profit of the resonant enhancement of more than two orders in the magnetically diffracted intensity. At resonance, high counting rates above 11000 cps were obtained for the 1.5 gm EuTe film, allowing to check for the type II antiferromagnetic order of EuTe. An equal population of the three possible in-plane magnetic domains was found. The EuTe/PbTe SL magnetic peak showed a satellite structure, indicating the presence of magnetic correlations among the 5 ML (monolayers) EuTe layers across the 15 ML PbTe non-magnetic spacers. The temperature dependence of the integrated intensities of the film and the SL yielded different Neel temperatures T(N). The lower T(N) for the SL is explained considering the higher influence of the surface atoms, with partial bonds lost.
Resumo:
Magnetic M( T, H, P) and electrical transport.( T, H, P) measurements in a strong spin-lattice-charge coupled La(0.7)Ca(0.3)MnO(3) system have been conducted. The application of H and P leads to the formation of different magnetic domain structures in the vicinity and below the polaronic-to-ferromagnetic transition temperature. The charge mobility is more sensitive to the variation of the spatial wave function overlap between Mn(3+) eg and O(2-) 2p orbitals due to the applied compacting pressure rather than the relative spin orientation between neighbouring Mn ions when the magnetic field is applied. In spite of the presence of different magnetic domain structures due to the sample history, the effect of magnetic field and pressure is less pronounced at lower temperatures on electrical transport properties.
Resumo:
This work reports on magnetic measurements of the quasi-two-dimensional (quasi-2D) system Zn(1-x)Mn(x)In(2)Se(4), with 0.01 <= x <= 1.00. For x > 0.67, the quasi-2D system seems to develop a spin-glass behaviour. Evidence of a true phase transition phenomenon is provided by the steep increase of the nonlinear susceptibility chi(nl) when approaching T(C) from above. The static scaling of chi(nl) data yields critical exponents delta = 4.0 +/- 0.2, phi = 4.37 +/- 0.17 and TC = 3.4 +/- 0.1 K for the sample with x = 1.00 and similar values for the sample with x = 0.87. These critical exponents are in good agreement with values reported for other spin-glass systems with short-range interactions.
Resumo:
We report interparticle interactions effects on the magnetic structure of the surface region in Fe(3)O(4) nanoparticles. For that, we have studied a desirable system composed by Fe(3)O(4) nanoparticles with (d) = 9.3 nm and a narrow size distribution. These particles present an interesting morphology constituted by a crystalline core and a broad (similar to 50% vol.) disordered superficial shell. Two samples were prepared with distinct concentrations of the particles: weakly-interacting particles dispersed in a polymer and strongly-dipolar-interacting particles in a powder sample. M(H, T) measurements clearly show that strong dipolar interparticle interaction modifies the magnetic structure of the structurally disordered superficial shell. Consequently, we have observed drastically distinct thermal behaviours of magnetization and susceptibility comparing weakly- and strongly-interacting samples for the temperature range 2 K < T < 300 K. We have also observed a temperature-field dependence of the hysteresis loops of the dispersed sample that is not observed in the hysteresis loops of the powder one.
Resumo:
The addition of both Ti-C and Cr as grain refiners in Nd-Fe-B nanocomposites substantially increases the coercive field Hc. This motived our investigation of the effect of Ti-C and Cr on Pr-Fe-B nanocomposites. Melt-spun ribbons of composition (Pr(9.5)Fe(84.5)B(6))(0.97-x)Cr(x)(TiC)(0.03)(x = 0; 0.25; 0.5; 0.75; 1) and (Nd(9.5)Fe(84.5)B(6))(0.97-x)Cr(x)(TiC)(0.03)(x = 0.5 and 1) were produced for study. For a Pr nanocomposite with 1% Cr, Hc = 12.5 kOe. However, the energy product was limited to 13.6 MGOe by the remanence value. Rietveld analysis of X-ray spectra showed the ribbons to consist of predominantly hard (similar to 70 wt%) R(2)Fe(14)B, the soft phase being (similar to 30 wt%) alpha-Fe. Mossbauer measurements at 300 K are consistent with a reduced hyperfine field for the hard magnetic phase due to the Cr addition. Analysis of transmission electron microscopy images showed the Pr nanocomposite with 1% Cr to have an increased average grain size.
Resumo:
Structural, magnetic and hyperfine interaction measurements have been carried out on the novel compound La(3.5)Ru(4)O(13) prepared under two different atmospheres (air and oxygen flow). This compound is formed in the orthorhombic structure (space group Pmmm, # 47). The coexistence of the triple-layered perovskite-type planes (quasi-2D structure) and the rutile-like slabs (1D structure) leads to interesting magnetic and electronic properties in this compound. The magnetic susceptibility of this system shows a peak at T similar to 47 K associated with antiferromagnetic interactions. The Curie-Weiss behaviour of the susceptibility provides an effective magnetic moment consistent with Ru ions in low-spin state. Perturbed angular correlation measurements carried out with (111)Cd probe in the temperature range 10-60 K reveal only quadrupole interactions and indicate the occurrence of structural distortions for T<40K. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Measurements of H-1 and C-13 Nuclear Magnetic Resonance (NMR) for the nano-composite materials formed by the intercalation of hexadecylamine (HDA) in metal oxides (TiO2, V2O5 and MoO3), are reported. The H-1 NMR spin-lattice relaxation in the rotating frame was described by using the spectral density due to Davidson and Cole, which incorporates a distribution of correlation times characterized by a width parameter epsilon. The fitting of the data was obtained for epsilon = 0.74, indicating that the correlation times are distributed over a narrow range in this system. High-resolution C-13 NMR techniques were used to resolve the NMR lines of middle-chain methylene groups in the spectra and variable contact time cross-polarization {H-1-}C-13 experiments were employed to analyze the reorientation dynamics of the CH3 and CH2 groups in the HDA chains.
Resumo:
Impedance spectroscopy and nuclear magnetic resonance (NMR) were used to investigate the mobility of water molecules located in the interlayer space of H(+) - exchanged bentonite clay. The conductivity obtained by ac measurements was 1.25 x 10(-4) S/cm at 298 K. Proton ((1)H) lineshapes and spin-lattice relaxation times were measured as a function of temperature over the temperature range 130-320 K. The NMR experiments exhibit the qualitative features associated with the proton motion, namely the presence of a (1)H NMR line narrowing and a well-defined spin-lattice relaxation rate maximum. The temperature dependence of the proton spin-lattice relaxation rates was analyzed with the spectral density function appropriate for proton dynamics in a two-dimensional system. The self-diffusion coefficient estimated from our NMR data, D similar to 2 x 10(-7) cm(2)/s at 300 K, is consistent with those reported for exchanged montmorillonite clay hydrates studied by NMR and quasi-elastic neutron scattering (QNS).
Resumo:
Magnetic fabric and rock magnetism studies were performed on 25 unmetamorphosed mafic dikes of the Meso-Late Proterozoic (similar to 1.02 Ga) dike swarm from Salvador (Bahia State, NE Brazil). This area lies in the north-eastern part of the Sao Francisco Craton, which was dominantly formed/reworked during the Transamazonian orogeny (2.14-1.94 Ga). The dikes crop out along the beaches and in quarries around Salvador city, and cut across both amphibolite dikes and granulites. Their widths range from a few centimeters up to 30 m with an average of similar to 4 m, and show two main trends N 140-190 and N 100-120 with vertical dips. Magnetic fabrics were determined using both anisotropy of low-field magnetic susceptibility (AMS) and anisotropy of anhysteretic remanent magnetization (AARM). The magnetic mineralogy was investigated by many experiments including remanent magnetization measurements at variable low temperatures (10-300 K), Mossbauer spectroscopy, high temperature magnetization curves (25-700 degrees C) and scanning electron microscopy (SEM). The rock magnetism study suggests pseudo-single-domain magnetite grains carrying the bulk magnetic susceptibility and AARM fabrics. The magnetite grains found in these dikes are large and we discard the presence of single-domain grains. Its composition is close to stoichiometric with low Ti substitution, and its Verwey transition occurs around 120 K. The main AMS fabric recognized in the swarm is so-called normal, in which the K(max)-K(int) plane is parallel to the dike plane and the magnetic foliation pole K(min)) is perpendicular to it. This fabric is interpreted as due to magma flow, and analysis of the K m inclination permitted to infer that approximately 80% of the dikes were fed by horizontal or sub-horizontal flows (K(max) < 30 degrees). This interpretation is supported by structural field evidence found in five dikes. In addition, based on the plunge of K(max), two mantle sources could be inferred; one of them which fed about 80% of the swarm would be located in the southern part of the region, and the other underlied the Valeria quarry. However, for all dikes the AARM tensors are not coaxial with AMS fabrics and show a magnetic lineation (AARM(max)) oriented to N30-60E, suggesting that magnetite grains were rotated clockwise from dike plane. The orientation of AARM lineation is similar to the orientation of a system of faults in which the Salvador normal fault is the most important. These faults were formed during Cretaceous rifting in the Reconcavo-Tucano-jatoba assemblage that corresponds to an aborted intra-continental rift formed during the opening of the South Atlantic. Therefore, the AARM fabric found for the Salvador dikes is probably tectonic in origin and suggests that the dike swarm was affected by the important tectonic event responsible for the break-up of the Gondwanaland. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
CoFe(2)O(4) nanoparticles were obtained by the co-precipitation method. They were further modified by the adsorption of ricinoleic acid (RA). The non-modified and modified CoFe(2)O(4)/RA nanoparticles were characterized by transmission electron microscopy (TEM), atomic force microscopy (AFM), Raman, and Fourier transform infrared (FTIR) spectroscopy. The modified particles present a mean diameter < 20 nm. The adsorption of RA on the CoFe(2)O(4) surface is characterized by the IR absorptions of the RA while in the Raman spectrum the predominant signals are those from the CoFe(2)O(4). The cis-polyisoprene (PI) composite was prepared by dissolving PI in cyclohexane followed by the addition of a magnetic fluid based on CoFe(2)O(4)/RA nanoparticles dispersed in cyclohexane. After solvent evaporation a magnetic composite was obtained and characterized by AFM, Raman, and FTIR measurements. AFM images show uniformly CoFe(2)O(4)/RA particles distributed in the PI matrix. Raman spectra obtained for the composites reveal the characteristic Raman peaks of PI and CoFe(2)O(4) nanoparticles.
Resumo:
Ferrites of the type M(II)Fe(2)O(4) (M = Fe and Co) have been prepared by the traditional coprecipitation method. These ferrites were modified by the adsorption of fatty acids derived from soybean and castor oil and were then dispersed in cyclohexane, providing very stable magnetic fluids, readily usable in nonpolar media. The structural properties of the ferrites and modified ferrites as well as the magnetic fluids were characterized by XRD (X-ray powder diffraction), TEM (transmission electron microscopy), DRIFTS (diffusion reflectance infrared Fourier transform spectroscopy), FTMR (Fourier transform near-infrared), UV-vis, normal Raman spectroscopy, and surface-enhanced Raman scattering (SERS). XRD and TEM analysis have shown that the magnetic nanoparticles (nonmodified and modified) present diameters in the range of 10-15 nm. DRIFTS measurements have shown that the carboxylate groups of soybean and castor oil fatty acids adsorb on the ferrite surface, forming three different structures: a bridging bidentate, a bridging monodentate, and a bidentate chelate structure. The FTIR and Raman spectra of nonmodified Fe(3)O(4) and CoFe(2)O(4) nanoparticles have shown that the number of observed phonons is not compatible with the expected O(h)(7) symmetry, since IR-only active phonons were observed. in the Raman spectra and vice versa. SERS measurements of a CoFe(2)O(4) thin film on a SERS-active gold electrode at different applied potentials made possible the assignment of the signals near 550 and 630 cm(-1) to Co-O motions and the signals near 470 and 680 cm(-1) to Fe-O motions.
Resumo:
A erosão é a forma de degradação do solo com efeitos na produtividade das culturas e na poluição do meio ambiente. Para compreender a variabilidade espacial desse fenômeno, técnicas geoestatísticas e conceitos da relação solo-paisagem podem ser utilizados para identificar compartimentos da paisagem com diferentes potenciais de erosão. O objetivo deste trabalho foi estabelecer elementos para a compreensão dos fatores de erosão em compartimentos da paisagem e das relações com a suscetibilidade magnética (SM) dos solos de uma vertente no município de Gilbués -PI. Foram montadas malhas de amostragem nos compartimentos I e II, com 121 pontos, e compartimento III, com 99 pontos, espaçados a cada 10 m. Houve diferença significativa para erodibilidade (K) e risco de erosão (RE); a variabilidade espacial da SM foi menor do que a dos fatores de erosão do solo. As perdas de solo (A), potencial natural de erosão (PNE), RE e SM tiveram relação espacial com o fator topográfico, indicando dependência da erosão ao relevo. Concluiu-se que as perdas de solo, o potencial natural de erosão e o risco de erosão apresentaram relação espacial com o fator topográfico, comprovando a dependência dos fatores de erosão ao relevo. A suscetibilidade magnética do solo pode ser utilizada como variável auxiliar na quantificação indireta do fator erodibilidade e do risco de erosão do solo.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)