981 resultados para Upconversion luminescence (UCL)
Resumo:
Here, we report for the first time a simple thermal oxidation strategy for the large area synthesis of Ge/GeO2 nanoholes from Ge and studied the luminescence of Ge/GeO2 and hole formation mechanism through phase and luminescence mapping. Photoluminescence mapping reveals that the emission in the visible range is only from the hole region, which provokes the necessity of the nanoholes. Such materials can also be used to convert ultraviolet to visible radiation for detection by conventional phototubes and to coat blue or ultraviolet diodes to obtain white light.
Resumo:
Wafer/microcrystallites of oxidized Ge with holes/nanoholes synthesized by thermal oxidation strategy from Ge wafer/microcrystallites can convert one wavelength to another. Both oxidized Ge wafer and microcrystallites shows excitation- and power-dependent luminescence. Red-shift is observed as the excitation wavelength is increased, while blue-shift is observed as power density is increased. Over all, blue-green-yellow-orange luminescence is observed depending on the excitation wavelength and the morphology of oxidized Ge. The various defects level associated with germanium-oxygen vacancies in GeO2 and Ge/GeO2 interface are responsible for the excitation-dependent luminescence. Being a light-conversion material, oxidized Ge is expected to find potential applications in solid-state lighting, photovoltaic devices and photocatalysis.
Comparison of ZnO films deposited on indium tin oxide and soda lime glass under identical conditions
Resumo:
ZnO films have been grown via a vapour phase transport (VPT) on soda lime glass (SLG) and indium-tin oxide (ITO) coated glass. ZnO film on ITO had traces of Zn and C which gives them a dark appearance while that appears yellowish-white on SLG. X-ray photoelectron spectroscopy studies confirm the traces of C in the form of C-O. The photoluminescence studies reveal a prominent green luminescence band for ZnO film on ITO. (C) 2013 Author(s).
Resumo:
Structural, iono (IL) and thermoluminescence (TL) studies of Zn2SiO4:Sm3+ (1-5 mol%) nanophosphor bombarded with swift heavy ions in the fluence range 3.91 x 10(12)-21.48 x 10(12) cm(-2) have been carried out. The average crystallite sizes for pristine and ion irradiated for 3.91 x 10(12) ions cm(-2) and 21.48 x 10(12) ions cm(-2) were found to be 34, 26 and 20 nm. With increase of ion fluence, the intensity of XRD peaks decreases and FWHM increases. The peak broadening indicates the stress induced point/clusters defects produced due to heavy ion irradiation. IL studies were carried out for different Sm3+ concentrations in Zn2SiO4 by irradiating with ion fluence of 15.62 x 10(12) ions cm(-2). The characteristic emission peaks at similar to 562, 599, 646 and 701 nm were recorded by exciting Si7+ ions in the fluence range 3.91 x 10(12)-21.48 x 10(12) ions cm(-2). These peaks were attributed to (4)G(5/2)-> H-6(5/2) (562 nm), (4)G(5/2)-> H-6(7/2) (599 nm), (4)G(5/2)-> H-6(9/2) (646 nm), and (4)G(5/2)-> H-6(5/2) (701 nm) transitions of Sm3+. The highest emission was recorded at 3 mol% of Sm3+ doped Zn2SiO4. TL studies were carried out for 3 mol% Sm3+ concentration in the fluence range 3.91 x 10(12)-21.48 x 10(12) ions cm(-2). Two U glow peaks at 152 and 223 degrees C were recorded. The kinetic parameters (E, b, and s), were estimated using Chen's peak shape method. Simple glow curve structure (223 degrees C), highly resistive, increase in TL. intensity up to 19.53 x 10(12) ions cm(-2), simple trap distribution makes Zn2SiO4:Sm3+ (3 mol%) phosphor highly useful in radiation dosimetry.
Resumo:
Studies were carried on the growth behavior of InN nanodots by plasma assisted molecular beam epitaxy on bare Si(100) substrates and their structural, optical, electrical properties. The growth was carried out by two different methods such as, (i) mono-step growth process at a low temperature and a (ii) bi-step growth process with the combination of low and high temperatures for the formation of single crystalline nanodots with well defined crystallographic facets due to cluster migration. Low temperature photoluminescence shows a free excitonic (FE) luminescence at 0.80 eV. The Raman spectroscopy and X-ray diffraction studies reveal that the nanodots as well as the film were of wurtzite structure and strain free.
Resumo:
Although weak interactions, such as C-H center dot center dot center dot O and pi-stacking, are generally considered to be insignificant, it is their reorganization that holds the key for many a solid-state phenomenon, such as phase transitions, plastic deformation, elastic flexibility, and mechanochromic luminescence in solid-state fluorophores. Despite this, the role of weak interactions in these dynamic phenomena is poorly understood. In this study, we investigate two co-crystal polymorphs of caffeine:4-chloro-3-nitrobenzoic acid, which have close structural similarity (2D layered structures), but surprisingly show distinct mechanical behavior. Form I is brittle, but shows shear-induced phase instability and, upon grinding, converts to Form II, which is soft and plastically shearable. This observation is in contrast to those reported in earlier studies on aspirin, wherein the metastable drug forms are softer and convert to stable and harder forms upon stressing To establish a molecular level understanding, have investigated the two co-crystal polymorphs I and II by single crystal X-ray diffraction, nanoindentation to quantify mechanical properties, and theoretical calculations. The lower hardness (from nanoindentation) and smooth potential surfaces (from theoretical studies) for shearing of layers in Form II allowed us to rationalize the role of stronger intralayer (sp(2))C-H center dot center dot center dot O and nonspecific interlayer pi-stacking interactions in the structure of II. Although the Form I also possesses the same type of interactions, its strength is clearly opposite, that is, weaker intralayer (sp(3))C-H center dot center dot center dot O and specific interlayer pi-stacking interactions. Hence, Form I is harder than Form IL Theoretical calculations and indentation on (111) of Form I suggested the low resistance of this face to mechanical stress; thus, Form I converts to II upon mechanical action. Hence, our approach demonstrates the usefulness of multiple techniques for establishing the role of weak noncovalent interactions in solid-state dynamic phenomena, such as stress induced phase transformation, and hence is important in the context of solid-state pharmaceutical chemistry and crystal engineering.
Resumo:
This article presents the investigation of the coordination behavior of a newly synthesized tricarboxylate ligand, obtained by joining imidazole dicarboxylic acid and 4-carboxybenzyl moieties cbimdaH(3), 1-(4-carboxybenzyl)-1H-imidazole-4,5-dicarboxylic acid]. Two novel coordination polymers were obtained through solvothermal reactions under similar conditions namely Sr(cbimdaH)(H2O)](n) (1) and Cd-2(cbimdaH)(2)(H2O)(6)](n)center dot(DMF)(3n)(H2O)(3n) (2), with the ligand behaving as a dianionic tricarboxylate linker. The single crystal X-ray structures show that while 1 forms a 3D coordination polymer, 2 forms a 1D polymer which is further assembled in three dimensions through supramolecular interactions (H-bonding). Complex 1 consists of Sr2+ ions in a distorted dodecahedral coordination geometry, while 2 consists of Cd2+ ions in distorted pentagonal bipyramidal geometries. A topology study reveals that 1 has a new topology based on the 5,6-coordinated 3D net architecture. The luminescence properties of the complexes in the solid state and their thermal stabilities were studied.
Resumo:
We report the synthesis of Pr6O11 microspheres self-assembled from ultra-small nanocrystals formed by the microwave irradiation of a solution of a salt of Pr in ethylene glycol (EG). The as-prepared product consists of microspheres measuring 200 to 500 nm in diameter and made of <5 nm nano-crystallites. The surface of these microspheres/nanocrystals is covered/capped with an organic layer of ethylene glycol as shown by TEM analysis and confirmed by IR spectroscopy measurements. The as-prepared product shows blue-green emission under excitation, which changes to orange-red when the product is annealed in air at 600 degrees C for 2 h. This change in luminescence behaviour can be attributed to presence of ethylene glycol layer in the as-prepared product. The samples were characterized by X-ray powder diffraction (XRD), field emission scanning electron microscopy (FE-SEM), IR Spectroscopy (IR), transmission electron microscopy (TEM), and thermogravimetric analysis (TGA). (C) 2013 Elsevier B.V. All rights reserved.
Resumo:
Despite being a particularly good emitter, use of divalent Eu has been seriously limited. This is because severe reducing environments or special hosts are needed during synthesis of divalent Eu containing phosphors. In this work we stabilize Eu in its 2+ state (in CaAl2O4) using an open-air solution combustion reaction. The impact of fuel (F) to oxidizer (O) molar ratios (F/O = 0.5-2.0) on luminescence properties is explored. Chromaticity of Eu:CaAl2O4 depends sensitively on the F/O ratio. In general, higher F/O inhibits Eu3+ and promotes Eu2+ formation, which in turn improves the quality of the blue phosphor. EPR spectra show inhomogeneous broadening effects with the increase in F/O ratio, which suggests that disorder creation is promoted when F/O is increase. This is also confirmed by an increase in emission line width in PL spectra, when F/O is increased. (C) 2013 Elsevier B.V. All rights reserved.
Correlations between mechanical and photoluminescence properties in Eu doped sodium bismuth titanate
Resumo:
Nanoindentation technique is utilized to examine mechanical property variation in Eu doped Na0.5Bi0.5 TiO3 (NBT). Doping levels of Eu in NBT is systematically varied. Dilute doping results in a linear reduction in both modulus and hardness. At higher concentrations, a recovery of the mechanical properties (to undoped NBT values) is observed. These experimental trends mirror variations in the optical emission intensities with Eu concentration. Observed trends are rationalized on the basis of a model, which hypothesizes phase segregation beyond a critical Eu doping level. Such segregation leads to the formation of pure NBT, nano-Eu saturated NBT, and nano-mixed Eu oxides in the microstructure. Pure NBT is optically inactive, while saturated Eu:NBT is a much better emitter when compared to europium oxide. Hence beyond the critical concentration, luminescence signal comes primarily from the saturated Eu:NBT phase. The model presented is supported by nanoindentation, and spectroscopic results. (C) 2013 Elsevier Ltd. All rights reserved.
Resumo:
A new technique based on luminescent molecular sensors is utilized in these series of experiments for measurement of temperatures in material removal processes. 2-Dimensional machining of metals at low speeds and surface grinding configurations are used as the model experimental systems to understand the efficacy of this experimental technique. The experiments were conducted with a series of luminescent sensors and binder combinations for the temperature measurement. The luminescence of the sensor was measured through a charge-coupled device imaging camera, and intensive calibration exercises were performed on these sensors. Excellent agreement in the temperature fields measured through this new experimental approach and traditional infrared thermography is seen here. This technique offers the unique capability of allowing measurement of temperatures in the presence of a lubricant, akin to manufacturing conditions in situ. Extension of the technique to measure the temperature field at the tool-chip contact is described.
Resumo:
We report a novel, rapid, and low-temperature method for the synthesis of undoped and Eu-doped GdOOH spherical hierarchical structures, without using any structure-directing agents, through the microwave irradiation route. The as-prepared product consists of nearly monodisperse microspheres measuring about 1.3 mu m in diameter. Electron microscopy reveals that each microsphere is an assembly of two-dimensional nanoflakes (about 30 nm thin) which, in turn, result from the assembly of crystallites measuring about 9 nm in diameter. Thus, a three-level hierarchy can be seen in the formation of the GdOOH microspheres: from nanoparticles to 2D nanoflakes to 3D spherical structures. When doped with Eu3+ ions, the GdOOH microspheres show a strong red emission, making them promising candidates as phosphors. Finally, thermal conversion at modest temperatures leads to the formation of corresponding oxide structures with enhanced luminescence, while retaining the spherical morphology of their oxyhydroxide precursor.
Resumo:
Two new dicyanovinyl (DCV) functionalized triarylboranes (Mes(2)B-pi-spacer-DCV, for 1: pi-spacer = C6H4, for 2: pi-spacer = 2,3,5,6-tetramethyl-phenyl) are reported. The molecular structures of 1 and 2 are similar except for the spacer which connects the boryl and DCV units. This small structural perturbation induces drastic changes in the optical properties of 1 and 2. Compound 2 shows weak dual fluorescence emission in nonpolar solvents and a stronger emission in polar solvents. Compound 1 is weakly fluorescent in polar environments but shows an intense single luminescence peak in less polar environments. Compound 1 exhibits a turn-off fluorescence response for both fluoride and cyanide: in contrast, 2 shows a turn on fluorescence response for both anions with different fluorescence signatures. The NMR titration studies reveal that for compound 2, fluoride binds to the boron centre and cyanide binds to the DCV unit. For compound 1, the fluoride ion binds to the boron center, whereas the CN- binds to both the Ar3B and DCV units.
Resumo:
Dy-doped GdOOH microspherical structures were prepared in minutes without using any structure-directing agents, through the microwave irradiation route. The as-prepared product consists of nearly monodisperse sphere-like entities with each one representing a three-level hierarchy in its formation. Dy:GdOOH powder samples show a bright blue-green luminescence under UV excitation, making these structures potentially important in the field of optical and luminescent devices. Finally, thermal conversion to the corresponding oxide structures occurs at modest temperatures, spherical morphology intact and with enhanced luminescence behaviour. (C) 2014 Elsevier B.V. All rights reserved.
Resumo:
Systematic structural perturbation has been used to fine-tune and understand the luminescence properties of three new 1,8-naphthalimides (NPIs) in solution and aggregates. The NPIs show blue emission in the solution state and their fluorescence quantum yields are dependent upon their molecular rigidity. In concentrated solutions of the NPIs, intermolecular interactions were found to quench the fluorescence due to the formation of excimers. In contrast, upon aggregation (in THF/H2O mixtures), the NPIs show aggregation-induced emission enhancement (AIEE). The NPIs also show moderately high solid-state emission quantum yields (ca. 10-12.7 %). The AIEE behaviour of the NPIs depends on their molecular rigidity and the nature of their intermolecular interactions. The NPIs 1-3 show different extents of intermolecular (pi-pi and C-H center dot center dot center dot O) interactions in their solid-state crystal structures depending on their substituents. Detailed photophysical, computational and structural investigations suggest that an optimal balance of structural flexibility and intermolecular communication is necessary for achieving AIEE characteristics in these NPIs.