956 resultados para Found Footage Films
Resumo:
Iron encapsulated carbon nanoparticle polyvinyl chloride composite films have been prepared by solvent mixing and drying method. The films were characterized by scanning electron microscope (SEM) and high resolution transmission electron microscope (HRTEM). A 5 nm thin graphitic carbon coating is observed on cubic Fe nanoparticles. The microwave absorption studies by wave guide technique in the Ka band range showed highest electromagnetic interference shielding efficiency of 18dB on a 300 micron thick film. The shielding efficiency depends on weight % of the filler in the composite. The data obtained for different films indicate that these lightweight materials are good candidates for potential electromagnetic interference shielding applications.
Resumo:
The greatest effect on reducing mortality in breast cancer comes from the detection and treatment of invasive cancer when it is as small as possible. Although mammography screening is known to be effective, observer errors are frequent and false-negative cancers can be found in retrospective studies of prior mammograms. In the year 2001, 67 women with 69 surgically proven cancers detected at screening in the Mammography Centre of Helsinki University Hospital had previous mammograms as well. These mammograms were analyzed by an experienced screening radiologist, who found that 36 lesions were already visible in previous screening rounds. CAD (Second Look v. 4.01) detected 23 of these missed lesions. Eight readers with different kinds of experience with mammography screening read the films of 200 women with and without CAD. These films included 35 of those missed lesions and 16 screen-detected cancers. CAD sensitivity was 70.6% and specificity 15.8%. Use of CAD lengthened the mean time spent for readings but did not significantly affect readers sensitivities or specificities. Therefore the use of applied version of CAD (Second Look v. 4.01) is questionable. Because none of those eight readers found exactly same cancers, two reading methods were compared: summarized independent reading (at least a single cancer-positive opinion within the group considered decisive) and conference consensus reading (the cancer-positive opinion of the reader majority was considered decisive). The greatest sensitivity of 74.5% was achieved when the independent readings of 4 best-performing readers were summarized. Overall the summarized independent readings were more sensitive than conference consensus readings (64.7% vs. 43.1%) while there was far less difference in mean specificities (92.4% vs. 97.7%). After detecting suspicious lesion, the radiologist has to decide what is the most accurate, fast, and cost-effective means of further work-up. The feasibility of FNAC and CNB in the diagnosis of breast lesions was compared in non-randomised, retrospective study of 580 (503 malignant) breast lesions of 572 patients. The absolute sensitivity for CNB was better than for FNAC, 96% (206/214) vs. 67% (194/289) (p < 0.0001). An additional needle biopsy or surgical biopsy was performed for 93 and 62 patients with FNAC, but for only 2 and 33 patients with CNB. The frequent need of supplement biopsies and unnecessary axillary operations due to false-positive findings made FNAC (294 ) more expensive than CNB (223 ), and because the advantage of quick analysis vanishes during the overall diagnostic and referral process, it is recommendable to use CNB as initial biopsy method.
Resumo:
The blue emission of ethyl-hexyl substituted polyfluorene (PF2/6) films is accompanied by a low energy green emission peak around 500 nm in inert atmosphere. The intensity of this 500 nm peak is large in electroluminescence (EL) compared to photoluminescence (PL)measurements. Furthermore, the green emission intensity reduces dramatically in the presence of molecular oxygen. To understand this, we have modeled various nonradiative processes by time dependent quantum many body methods. These are (i) intersystem crossing to study conversion of excited singlets to triplets leading to a phosphorescence emission, (ii) electron-hole recombination (e-hR) process in the presence of a paramagnetic impurity to follow the yield of triplets in a polyene system doped with paramagnetic metal atom, and (iii) quenching of excited triplet states in the presence of oxygen molecules to understand the low intensity of EL emission in ambient atmosphere, when compared with that in nitrogen atmosphere. We have employed the Pariser-Parr-Pople Hamiltonian to model the molecules and have invoked electron-electron repulsions beyond zero differential approximation while treating interactions between the organic molecule and the rest of the system. Our time evolution methods show that there is a large cross section for triplet formation in the e-hR process in the presence of paramagnetic impurity with degenerate orbitals. The triplet yield through e-hR process far exceeds that in the intersystem crossing pathway, clearly pointing to the large intensity of the 500 nm peak in EL compared to PL measurements. We have also modeled the triplet quenching process by a paramagnetic oxygen molecule which shows a sizable quenching cross section especially for systems with large sizes. These studies show that the most probable origin of the experimentally observed low energy EL emission is the triplets.
Resumo:
Thermally stable mesoporous TiO2/SiO2 hybrid films with pore size of 50 nm have been synthesized by adopting the polymeric micelle-assembly method. A triblock copolymer, poly(styrene-b-2-vinyl pyridine-b-ethylene oxide), which serves as a template for the mesopores, was utilized to form polymeric micelles. The effective interaction of titanium tetraisopropoxide (TTIP) and tetraethyl orthosilicate (TEOS) with the polymeric micelles enabled us to fabricate stable mesoporous films. By changing the molar ratio of TEOS and TTIP, several mesoporous TiO2/SiO2 hybrid films with different compositions can be synthesized. The presence of amorphous SiO2 phase effectively retards the growth of anatase TiO2 crystal in the pore walls and retains the original mesoporous structure, even at higher temperature (650 °C). These TiO2/SiO2 hybrid films are of very high quality, without any cracks or voids. The addition of SiO2 phase to mesoporous TiO2 films not only adsorbs more organic dyes, but also significantly enhances the photocatalytic activity compared to mesoporous pure TiO2 film without SiO2 phase.
Resumo:
A stable Y-doped BaZrO3 electrolyte film, which showed a good performance in proton-conducting SOFCs, was successfully fabricated using a novel ionic diffusion strategy.
Resumo:
The difficult sintering of BaZr0.8Y0.2O 3-δ (BZY20) powders makes the fabrication of anode-supported BZY20 electrolyte films complex. Dense BZY20 membranes were successfully fabricated on anode substrates made of sinteractive NiO-BZY20 powders, prepared by a combustion method. With respect to traditional anode substrates made of powders prepared by mechanical mixing, the anode substrates made of the wet-chemically synthesized composite NiO-BZY20 powders significantly promoted the densification of BZY20 membranes: dense BZY20 films were obtained after co-pressing and co-firing at 1300 °C, a much lower temperature than those usually needed for densifying BZY20 membranes. Improved electrochemical performance was also observed: the supported BZY20 films maintained a high proton conductivity, up to 5.4 × 10-3 S cm-1 at 700 °C. Moreover, an anode-supported fuel cell with a 30 m thick BZY20 electrolyte film fabricated at 1400 °C on the anode made of the wet-chemically synthesized NiO-BZY20 powder showed a peak power density of 172 mW cm-2 at 700 °C, using La0.6Sr0.4Co 0.2Fe0.8O3-δ-BaZr0.7Y 0.2Pr0.1O3-δ as the cathode material, with a remarkable performance for proton-conducting solid oxide fuel cell (SOFC) applications.
Resumo:
Electrical Switching Studies on bulk Ge10Se90-xTlx ( 15 <= x <= 34) glasses have been undertaken to examine the type of switching, composition and thickness dependence of switching voltages. Unlike Ge-Se-Tl thin films which exhibit memory switching, the bulk Ge10Se90-xTlx glasses are found to exhibit threshold type switching with fluctuations seen in their current-voltage (I-V) characteristics. Further, it is observed that the switching voltages (V-T) of Ge10Se90-xTlx glasses decrease with the increase in the Tl concentration. An effort has been made to understand the observed composition dependence on the basis of nature of bonding of Tl atoms and a decrease in the chemical disorder with composition. In addition. the network connectivity and metallicity factors also contribute for the observed decrease in the switching voltages of Ge10Se90-xTlx glasses with Tl addition. It is also interesting to note that the composition dependence of switching voltages of Ge10Se90-xTlx glasses exhibit a small Cusp around the composition x = 22. which is understood on the basis of a thermally reversing window in this system in the composition range 22 <= x <= 30. The thickness dependence of switching voltages has been found to provide an insight about the type of switching mechanism involved in these samples. (C) 2009 Elsevier B.V. All rights reserved
Resumo:
Formation of nanocrystalline TiN at low temperatures was demonstrated by combining Pulsed Laser Deposition (PLD) and ion implantation techniques. The Ti films of nominal thickness similar to 250 nm were deposited at a substrate temperature of 200 degrees C by ablating a high pure titanium target in UHV conditions using a nanosecond pulsed Nd:YAG laser operating at 1064 nm. These films were implanted with 100 keV N+ ions with fluence ranging from 1.0 x 10(16) ions/cm(2) to 1.0 x 10(17) ions/cm(2). The structural, compositional and morphological evolutions were tracked using Transmission Electron Microscopy (TEM), Secondary Ion Mass Spectrometry (SIMS) and Atomic Force Microscopy (AFM), respectively. TEM analysis revealed that the as-deposited titanium film is an fcc phase. With increasing ion fluence, its structure becomes amorphous phase before precipitation of nanocrystalline fcc TiN phase. Compositional depth profiles obtained from SIMS have shown the extent of nitrogen concentration gradient in the implantation zone. Both as-deposited and ion implanted films showed much higher hardness as compared to the bulk titanium. AFM studies revealed a gradual increase in surface roughness leading to surface patterning with increase in ion fluence.
Resumo:
The lead based ferroelectric PbZr0.53Ti0.47O3 (PZT), (Pb0.90La0.10)TiO3 (PLT10) and (Pb0.80La0.20)TiO3 (PLT20) thin films, prepared by pulsed laser ablation technique, were studied for their response to the 70 MeV oxygen ion irradiation. The dielectric analysis, capacitance-voltage (C- V) and DC leakage current measurements were performed before and after the irradiation to high-energy oxygen ions. The irradiation produced considerable changes in the dielectric, C-V, leakage characteristics and induced some amount of amorphization. The PZT films showed partial recrystallization after a thermal annealing at 400 degrees C for 10 min. The phase transition temperature [T-c] of PLT20 increased from 115 degrees C to 120 degrees C. The DC conductivity measurements showed a shift in the onset of non-linear conduction region. The current density decreased by two orders of magnitude after irradiation. After annealing the irradiated films at a temperature of 400 degrees C for 10 min, the films partially regained the dielectric and electrical properties. The results are discussed in terms of the irradiation-induced amorphization, the pinning of the ferroelectric domains by trapped charges and the thermal annealing of the defects generated during the irradiation. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Thin films of Cd1−xMnxS (0<=x<=0.5) were deposited on glass substrates by thermal evaporation. All the films were deposited at 300 K and annealed at 373, 473, and 573 K for 1 h in a high vacuum in the range 10−4 Pa. The as-deposited and the annealed films were characterized for composition, structure, and microstructure by using energy-dispersive X-ray, X-ray diffraction, scanning electron microscopy, and atomic force microscopy (AFM). The electrical properties were studied by Hall effect measurement. Electrical conductivity was studied in the temperature range 190–450 K. AFM studies showed that all the films were in nanocrystalline form with grain size varying in the range between 36 and 82 nm. Grain size studies showed a definite increase with annealing temperature. All the films exhibited wurtzite structure of the host material. The lattice parameter varied linearly with composition, following Vegard's law in the entire composition range. Grain size, electrical conductivity, Hall mobility, carrier concentration, and activation energy varied, exhibiting either maxima or minima at x=0.3.
Resumo:
In1-xMnxSb films have been grown with different Mn doping concentrations (x = 0.0085, 0.018, 0.029 and 0.04) beyond the equilibrium 14 solubility limit by liquid phase epitaxy. We have studied temperature dependent resistivity, the Hall effect, magnetoresistance and magnetization for all compositions. Saturation in magnetization observed even at room temperature suggests the existence of ferromagnetic clusters in the film which has been verified by scanning electron microscopy studies. The anomalous Hall coefficient is found to be negative. Remnant field present on the surface of the clusters seems to affect the anomalous Hall effect at very low fields (below 350 Gauss). In the zero field resistivity, a variable-range hopping conduction mechanism dominates below 3.5 K for all samples above which activated behavior is predominant. The temperature dependence of the magnetization measurement shows a magnetic ordering below 10 K which is consistent with electrical measurements. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Thin films of ZrO2 were prepared by reactive magnetron sputtering. Annealing of the films exhibited a drastic change in the properties due to improved crystallinity and packing density. The root mean square roughness of the sample observed from atomic force microscope is about 5.75 nm which is comparable to the average grain size of the thin film which is about 6 nm obtained from X-ray diffraction. The film annealed at 873 K exhibits an optical band gap of around 4.83 eV and shows +4 oxidation state of zirconium indicating fully oxidized zirconium, whereas higher annealing temperatures lead to oxygen deficiency in the films and this is reflected in their properties. A discontinuity in the imaginary part of the AC conductivity was observed in the frequency range of tens of thousands of Hz, where as, the real part does not show such behavior.
Resumo:
A novel synthesis of inorganic-organic hybrid films containing well dispersed and almost uniform size Ag nanoparticles in agar-agar matrix has been reported. The films are found to be highly stable for more than a year. The colloidal particles of Ag can be obtained in large quantities in the form of a film or in the gel form when dispersed in agar-agar or by dissolving in a suitable solvent as solution. Characterization has been done by UV-visible spectroscopy and TEM. The hybrid may be of interest to study third-order non-linear susceptibility.
Resumo:
In this paper, we report a systematic study of low frequency 1∕fα resistance fluctuation in thin metal films (Ag on Si) at different stages of damage process when the film is subjected to high current stressing. The resistance fluctuation (noise) measurement was carried out in situ using a small ac bias that has been mixed with the dc stressing current. The experiment has been carried out as a function of temperature in the range of 150–350 K. The experiment establishes that the current stressed film, as it undergoes damage due to various migration forces, develops an additional low-frequency noise spectral power that does not have the usual 1∕f spectral shape. The magnitude of extra term has an activated temperature dependence (activation energy of ≈0.1 eV) and has a 1∕f1.5 spectral dependence. The activation energy is the same as seen from the temperature dependence of the lifetime of the film. The extra 1∕f1.5 spectral power changes the spectral shape of the noise power as the damage process progress. The extra term likely arising from diffusion starts in the early stage of the migration process during current stressing and is noticeable much before any change can be detected in simultaneous resistance measurements. The experiment carried out over a large temperature range establish a strong correlation between the evolution of the migration process in a current stressed film and the low-frequency noise component that is not a 1∕f noise.