1000 resultados para sulphur deposition
Resumo:
Titanium dioxide thin films with a rutile crystallinite size around 20 nm were fabricated by pulsed laser deposition (PLD) aided with an electron cyclotron resonance (ECR) plasma. With annealing treatment, the crystal size of the rutile crystallinite increased to 100 nm. The apatite-forming ability of the films as deposited and after annealing was investigated in a kind of simulated body fluid with ion concentrations nearly equal to those of human blood plasma. The results indicate that ECR aided PLD is an effective way both to fabricate bioactive titanium dioxide thin films and to optimize the bioactivity of titanium dioxide, with both crystal size and defects of the film taken into account.
Resumo:
Carbon nanotips have been synthesized from a thin carbon film deposited on silicon by bias-enhanced hot filament chemical vapor deposition under different process parameters. The results of scanning electron microscopy indicate that high-quality carbon nanotips can only be obtained under conditions when the ion flux is effectively drawn from the plasma sustained in a CH4 + NH3 + H2 gas mixture. It is shown that the morphology of the carbon nanotips can be controlled by varying the process parameters such as the applied bias, gas pressure, and the NH3 / H2 mass flow ratios. The nanotip formation process is examined through a model that accounts for surface diffusion, in addition to sputtering and deposition processes included in the existing models. This model makes it possible to explain the major difference in the morphologies of the carbon nanotips formed without and with the aid of the plasma as well as to interpret the changes of their aspect ratio caused by the variation in the ion/gas fluxes. Viable ways to optimize the plasma-based process parameters to synthesize high-quality carbon nanotips are suggested. The results are relevant to the development of advanced plasma-/ion-assisted methods of nanoscale synthesis and processing.
Resumo:
Carbon nanotips with different structures were synthesized by plasma-enhanced hot filament chemical vapor deposition and plasma-enhanced chemical vapor deposition using different deposition conditions, and they were investigated by scanning electron microscopy and Raman spectroscopy. The results indicate that the photoluminescence background of the Raman spectra is different for different carbon nanotips. Additionally, the Raman spectra of the carbon nanotips synthesized using nitrogen-containing gas precursors show a peak located at about 2120 cm-1 besides the common D and G peaks. The observed difference in the photoluminescence background is related to the growth mechanisms, structural properties, and surface morphology of a-C:H and a-C:H:N nanotips, in particular, the sizes of the emissive tips.
Resumo:
Graphitization, a common process involving the transformation of metastable nongraphitic carbon into graphite is one of the major present-day challenges for micro- and nanocarbons due to their unique structural character and highly unusual thermal activation. Here we report on the successful graphitization of nanocrystalline carbon microcoils prepared by catalytic chemical vapor deposition and post-treated in argon atmosphere at temperatures ∼2500 °C for 2 h. The morphology, microstructure, and thermal properties of the carbon microcoils are examined in detail. The graphitization mechanism is discussed by invoking a model of structural transformation of the carbon microcoils. The results reveal that after graphitization the carbon microcoils are prominently purified and feature a clear helical morphology, as well as a more regular and ordered microstructure. The interlayer spacing of the carbon microcoils decreases from 0.36 to 0.34 nm, whereas the mean crystal sizes in the c - and a -directions increase from 1.64 to 2.04 nm and from 3.86 to 7.21 nm, respectively. Thermal treatment also substantially improves the antioxidation properties of the microcoils by lifting the oxidation onset temperature from 550 to 672 °C. This process may be suitable for other nongraphitic micro- and nanomaterials.
Resumo:
A theoretical model to describe the plasma-assisted growth of carbon nanofibers (CNFs) is proposed. Using the model, the plasma-related effects on the nanofiber growth parameters, such as the growth rate due to surface and bulk diffusion, the effective carbon flux to the catalyst surface, the characteristic residence time and diffusion length of carbon atoms on the catalyst surface, and the surface coverages, have been studied. The dependence of these parameters on the catalyst surface temperature and ion and etching gas fluxes to the catalyst surface is quantified. The optimum conditions under which a low-temperature plasma environment can benefit the CNF growth are formulated. These results are in good agreement with the available experimental data on CNF growth and can be used for optimizing synthesis of related nanoassemblies in low-temperature plasma-assisted nanofabrication. © 2008 American Institute of Physics.
Inductively coupled Ar/CH₄/H₂plasmas for low-temperature deposition of ordered carbon nanostructures
Resumo:
The study of inductively coupled Ar/CH 4/H 2 plasmas in the plasma enhanced chemical vapor deposition (PECVD) of self-assembled carbon nanostructures (CN) was presented. A spatially averaged (global) discharge model was developed to study the densities and fluxes of the radical neutrals and charged species, the effective electron temperature, and methane conversion factors under various conditions. It was found that the deposited cation fluxes in the PECVD of CNs generally exceed those of the radical neutrals. The agreement with the optical emission spectroscopy (OES) and quadrupole mass spectrometry (QMS) was also derived through numerical results.
Resumo:
The role of the plasma-grown nanoparticles in the plasma-enhanced chemical vapor deposition (PECVD) of the nanostructured carbon-based films was investigated. The samples were grown in the low-pressure rf plasmas of CH 4+H2+Ar gas mixtures. The enhanced deposition of the building units from the gas phase was found to support the formation of polymorphous nanostructured carbon films. The results reveal the crucial role played by the thermophoretic force in controlling the deposition of the plasma-grown fine particles.
Resumo:
A custom-designed inductively coupled plasma (ICP)-assisted radio-frequency magnetron sputtering deposition system has been employed to synthesize aluminium-doped zinc oxide (ZnO:Al) nanofilms on glass substrates at room temperature. The effects of film thickness and ZnO target (partially covered by Al chips) power on the structural, electrical and optical properties of the ZnO:Al nanofilms are studied. A high growth rate (∼41 nm/min), low electrical sheet resistance (as low as 30 Ω/□) and high optical transparency (>80%) over the visible spectrum has been achieved at a film thickness of ∼615 nm and ZnO target power of 150 W. The synthesis of ZnO:Al nanofilms at room temperature and with high growth rates is attributed to the unique features of the ICP-assisted radio-frequency magnetron sputtering deposition approach. The results are relevant to the development of photovoltaic thin-film solar cells and flat panel displays.
Resumo:
Plasma-assisted reactive rf magnetron sputtering deposition is used to fabricate vanadium oxide films on glass, silica and silicon substrates. The process conditions are optimized to synthesize phase-pure vanadium pentoxide (V2O5) featuring a nanocrystalline structure with the predominant (0 0 1) crystallographic orientation, surface morphology with rod-like nanosized grains and very uniform (the non-uniformity does not exceed 4%) coating thickness over large surface areas. The V2O5 films also show excellent and temperature-independent optical transmittance in a broad temperature range (20-95 °C). The results are relevant to the development of smart functional coatings with temperature-tunable properties. © 2007 IOP Publishing Ltd.
Resumo:
Nanocrystalline silicon carbide (nc-SiC) films are prepared by low-frequency inductively coupled plasma chemical vapor deposition from feedstock gases silane and methane diluted with hydrogen at a substrate temperature of 500 °C. The effect of different hydrogen dilution ratios X [hydrogen flow (sccm) / silane + methane flow (sccm)] on the growth of nc-SiC films is investigated by X-ray diffraction, scanning electron microscopy, Fourier transform infrared (FTIR) spectroscopy, and X-ray photoelectron spectroscopy (XPS). At a low hydrogen dilution ratio X, cubic silicon carbide is the main crystal phase; whereas at a high hydrogen dilution ratio X, hexagonal silicon carbide is the main crystal phase. The SiC crystal phase transformation may be explained by the different surface mobility of reactive Si-based and C-based radicals deposited at different hydrogen dilution ratios X. The FTIR and XPS analyses show that the Si-C bonds are the main bonds in the films and elemental composition of SiC is nearly stoichiometric with almost equal share of silicon and carbon atoms.
Resumo:
The results of 1D simulation of nanoparticle dynamics in the areas adjacent to nanostructured carbon-based films exposed to chemically active complex plasma of CH4 + H2 + Ar gas mixtures are presented. The nanoparticle-loaded near-substrate (including sheath and presheath) areas of a low-frequency (0.5 MHz) inductively coupled plasma facility for the PECVD growth of the ordered carbon-based nanotip structures are considered. The conditions allowing one to predict the size of particles that can pass through the plasma sheath and softly land onto the surface are formulated. The possibility of soft nano-cluster deposition without any additional acceleration common for some existing nano-cluster deposition schemes is demonstrated. The effect of the substrate heating power and the average atomic mass of neutral species is studied numerically and verified experimentally.
Resumo:
The plasma-assisted RF sputtering deposition of a biocompatible, functionally graded calcium phosphate bioceramic on a Ti6A14 V orthopedic alloy is reported. The chemical composition and presence of hydroxyapatite (HA), CaTiO3, and CaO mineral phases can be effectively controlled by the process parameters. At higher DC biases, the ratio [Ca]/[P] and the amount of CaO increase, whereas the HA content decreases. Optical emission spectroscopy suggests that CaO+ is the dominant species that responds to negative DC bias and controls calcium content. Biocompatibility tests in simulated body fluid confirm a positive biomimetic response evidenced by in-growth of an apatite layer after 24 h of immersion.
Resumo:
Selective and controlled deposition of plasma-grown nanoparticles is one of the pressing problems of plasma-aided nanofabrication. The results of advanced numerical simulations of motion of charge-variable nanoparticles in the plasma presheath and sheath areas and in localized microscopic electric fields created by surface microstructures are reported. Conditions for site-selective deposition of such nanoparticles onto individual microstructures and open surface areas within a periodic micropattern are formulated. The effects of plasma parameters, surface potential, and micropattern features on nanoparticle deposition are investigated and explained using particle charging and plasma force arguments. The results are generic and applicable to a broad range of nanoparticle-generating plasmas and practical problems ranging from management of nanoparticle contamination in microelectronics to site-selective nanoparticle deposition into specified device locations, and synthesis of advanced microporous materials and nanoparticle superlattices. © 2007 American Institute of Physics.
Resumo:
Hydroxyapatite (HA) coatings have numerous applications in orthopedics and dentistry, owing to their excellent ability to promote stronger implant fixation and faster bone tissue ingrowth and remodeling. Thermal plasma spray and other plasma-assisted techniques have recently been used to synthesize various calcium phosphate-based bioceramics. Despite notable recent achievements in the desired stoichiometry, phase composition, mechanical, structural, and bio-compatible properties, it is rather difficult to combine all of the above features in a single coating. For example, many existing plasma-sprayed HA coatings fall short in meeting the requirements of grain size and crystallinity, and as such are subject to enhanced resorption in body fluid. On the other hand, relatively poor interfacial bonding and stability is an obstacle to the application of the HA coatings in high load bearing Ti6Al4V knee joint implants. Here, we report on an alternative: a plasma-assisted, concurrent, sputtering deposition technique for high performance biocompatible HA coatings on Ti6Al4V implant alloy. The plasma-assisted RF magnetron co-sputtering deposition method allows one to simultaneously achieve most of the desired attributes of the biomimetic material and overcome the aforementioned problems. This article details the film synthesis process specifications, extensive analytical characterization of the material's properties, mechanical testing, simulated body fluid assessments, biocompatibility and cytocompatibility of the HA-coated Ti6Al4V orthopedic alloy. The means of optimization of the plasma and deposition process parameters to achieve the desired attributes and performance of the HA coating, as well as future challenges in clinical applications are also discussed.
Resumo:
This paper reports on the efficient deposition of hydrogenated diamond-like carbon (DLC) film in a plasma reactor that features both the capacitively and inductively coupled operation regimes. The hydrogenated DLC films have been prepared on silicon wafers using a low-frequency (500 kHz) inductively coupled plasma (ICP) chemical vapor deposition (CVD) system. At low RF powers, the system operates as an asymmetric capacitively coupled plasma source, and the film deposition process is undertaken in the electrostatic (E) discharge regime. Above the mode transition threshold, the high-density inductively coupled plasma is produced in the electromagnetic (H) discharge regime. It has been shown that the deposition rate and hardness of the DLC film are much higher in the H-mode deposition regime. For a 2.66-Pa H-mode CH4 + Ar gas mixture discharge, the deposited DLC film exhibits a mechanical hardness of 18 GPa, Young's modulus of 170 GPa, and compressive stress of 1.3 GPa.