Sapphire substrates patterned by a selective chemical wet and an inductively coupled plasma (ICP) etching technique was proposed to improve the performance of GaN-based light-emitting diodes (LEDs). GaN-based LEDs were fabricated on sapphire substrates through metal organic chemical vapor deposition (MOCVD). The LEDs fabricated on the patterned substrates exhibit improved device performance compared with the conventional LED fabricated on planar substrates when growth and device fabricating conditions were the same. The light output powers of the LEDs fabricated on wet-patterned and ICP-patterned substrates were about 37% and 17% higher than that of LEDs on planar substrates at an injection current of 20 mA, respectively. The enhancement is attributable to the combination of the improvement of GaN-based epilayers quality and the improvement of the light extraction efficiency. (c) 2008 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A 3-dB paired interference (PI) optical coupler in silicon-on-insulator (SOI) based on rib waveguides with trapezoidal cross section was designed with simulation by a modified finite-difference beam propagation method (FD-BPM) and fabricated by potassium hydroxide (KOH) anisotropic chemical wet etching. Theoretically, tolerances of width, length, and port distance are more than 1, 100, and 1 mu m, respectively. Smooth interface was obtained with the propagation loss of 1.1 dB/cm at the wavelength of 1.55 mu m. The coupler has a good uniformity of 0.2 dB and low excess loss of less than 2 dB.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Self-assembled InAs/AlAs quantum dots embedded in a resonant tunneling diode device structure are grown by molecular beam epitaxy. Through the selective etching in a C6H8O7 center dot H2O-K3C6H5O7 center dot H2O-H2O2 buffer solution, 310 nm GaAs capping layers are removed and the InAs/AlAs quantum dots are observed by field-emission scanning electron microscopy. It is shown that as-fabricated quantum dots have a diameter of several tens of nanometers and a density of 10(10) cm(-2) order. The images taken by this means are comparable or slightly better than those of transmission electron microscopy. The undercut of the InAs/AlAs layer near the edges of mesas is detected and that verifies the reliability of the quantum dot images. The inhomogeneous oxidation of the upper AlAs barrier in H2O2 is also observed. By comparing the morphologies of the mesa edge adjacent regions and the rest areas of the sample, it is concluded that the physicochemical reaction introduced in this letter is diffusion limited.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thick GaN films of high quality are directly grown on wet-etching patterned sapphire in a vertical hydride vapour phase epitaxy reactor. The optical and structural properties of GaN films are studied using scanning electronic microscopy and cathodoluminescence. Test results show that initial growth of hydride vapour phase epitaxy GaN occurs not only on the mesas but also on the two asymmetric sidewalls of the V-shaped grooves without selectivity. After the two-step coalescence near the interface, the GaN films near the surface keep on growing along the direction perpendicular to the long sidewall. Based on Raman results, GaN of the coalescence region in the grooves has the maximum residual stress and poor crystalline quality over the whole GaN film, and the coalescence process can release the stress. Therefore, stress-free thick GaN films are prepared with smooth and crack-free surfaces by this particular growth mode on wet-etching patterned sapphire substrates.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The choice of the etching depth for semiconductor microcavities is a compromise between a high Q factor and a difficult technique in a practical fabricating process. In this paper, the influences of the etching depth on mode Q factors for mid-infrared quantum cascade microcylinder and microsquare lasers around 4.8 and 7.8 mu m are simulated by three-dimensional (3D) finite-difference time-domain (FDTD) techniques. For the microcylinder and the microsquare resonators, the mode Q factors of the whispering-gallery modes (WGMs) increase exponentially and linearly with the increase in the etching depth, respectively Furthermore, the mode Q factors of some higher order transverse WGMs may be larger than that of the fundamental transverse WGM in 3D microsquares. Based on the field distribution of the vertical multilayer slab waveguide and the mode Q factors versus the etching depth, the necessary etching depth is chosen at the position where the field amplitude is 1% of the peak value of the slab waveguide. In addition, the influences of sidewall roughness on the mode Q factors are simulated for microsquare resonators by 2D FDTD simulation. (C) 2009 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The authors developed an inductively coupled plasma etching process for the fabrication of hole-type photonic crystals in InP. The etching was performed at 70 degrees C using BCl3/Cl-2 chemistries. A high etch rate of 1.4 mu m/min was obtained for 200 nm diameter holes. The process also yields nearly cylindrical hole shape with a 10.8 aspect ratio and more than 85 degrees straightness of the smooth sidewall. Surface-emitting photonic crystal laser and edge emitting one were demonstrated in the experiments.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A thermo-optic Mach-Zehnder (MZ) variable optical attenuator based on silicon waveguides with a large cross section was designed and fabricated on silicon-on-insulator (SOI) wafer. Multimode interferometers were used as power splitters and combiners in the MZ structure. In order to achieve a smooth interface, anisotropic chemical etching of silicon was used to fabricate the waveguides. Isolating grooves were introduced to reduce power consumption and device length. The device has a low power consumption of 210 mW and a response time of 50 mus. (C) 2004 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A 2 x 2 thermo-optic (TO) Mach-Zehnder (MZ) switch based on silicon waveguides with large cross section was designed and fabricated on silicon-on-insulator (SOI) wafer. The multi-mode interferometers (MMI) were used as power splitter and combiner in MZ structure. In order to get smooth interface, anisotropy chemical wet-etching of silicon was used to fabricate the waveguides instead of dry-etching. Additional grooves were introduced to reduce power consumption. The device has a low switching power of 235 mW and a switching speed of 60 mus. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A folding nonblocking 4 X 4 optical matrix switch in simplified-tree architecture was designed and fabricated on a silicon-on-insulator wafer. To compress chip size, switch elements (SEs) were connected by total internal reflection mirrors instead of conventional S-bends. For obtaining smooth interfaces, potassium hydroxide (KOH) anisotropic chemical etching of silicon was employed. The device has a compact size of 20 X 3.2 mm(2) and a fast response of 8 +/- 1 mu s. Power consumption of 2 x 2 SE and excess loss per mirror were 145 mW and -1.1 dB, respectively. (c) 2005 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A folding rearrangeable nonblocking 4 x 4 optical matrix switch was designed and fabricated on silicon-on-insulator wafer. To compress chip size, switch elements (SEs) were interconnected by total internal reflection (TIR) mirrors instead of conventional S-bends. For obtaining smooth interfaces, potassium hydroxide anisotropic chemical etching of silicon was utilized to make the matrix switch for the first time. The device has a compact size of 20 x 1.6 mm(2) and a fast response of 7.5 mu s. The power consumption of each 2 x 2 SE and the average excess loss per mirror were 145 mW and -1.1 dB, respectively. Low path dependence of +/- 0.7 dB in total excess loss was obtained because of the symmetry of propagation paths in this novel matrix switch.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An optimal concentration of the etching solution for deep etching of silicon, including 3% tetramethyl ammonium hydroxide and 0.3% (NH4)(2)S2O8, was achieved in this paper. For this etching solution, the etching rates of silicon and silicon dioxide were about 1.1 mu m(.)min(-1) and 0.5 nm(.)min(-1), respectively. The etching ratio between (100) and (111) planes was about 34:1, and the etched surface was very smooth.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A low power consumption 2 x 2 thermo-optic switch with fast response was fabricated on silicon-on-insulator by anisotropy chemical etching. Blocking trenches were etched on both sides of the phase-shifting arms to shorten device length and reduce power consumption. Thin top cladding layer was grown to reduce power consumption and switching time. The device showed good characteristics, including a low switching power of 145 mW and a fast switching speed of 8 +/- 1 mus, respectively. Two-dimensional finite element method was applied to simulate temperature field in the phase-shifting arm instead of conventional one-dimensional method. According to the simulated result, a new two-dimensional index distribution of phase-shifting arm was determined. Consequently finite-difference beam propagation method was employed to simulate the light propagation in the switch, and calculate the power consumption as well as the switching speed. The experimental results were in good agreement with the theoretical estimations. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A compact optical switch matrix was designed, in which light circuits were folded by total internal reflective (TIR) mirrors. Two key elements, 2 x 2 switch and TIR mirror, have been fabricated on silicon-on-insulator wafer by anisotropy chemical etching. The 2 x 2 switch showed very low power consumption of 140 mW and a very high speed of 8 +/- 1 mus. An improved design for the TIR mirror was developed, and the fabricated mirror with smooth and vertical reflective facet showed low excess loss of 0.7 +/- 0.3 dB at 1.55 mum.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The three-dimensional morphology of In(Ga)As nanostructures embedded in a GaAs matrix is investigated by combining atomic force microscopy and removal of the GaAs cap layer by selective wet etching. This method is used to investigate how the morphology of In(Ga)As quantum dots changes upon GaAs capping and subsequent in situ etching with AsBr3. A wave function calculation based on the experimentally determined morphologies suggests that quantum dots transform into quantum rings during in situ etching. (c) 2007 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Inductively coupled plasma (ICP) etching of InP in Cl-2/BCl3 gas mixtures is studied in order to achieve low-damage and high-anisotropy etching of two-dimensional InP/InGaAsP photonic crystal. The etching mechanisms are discussed and the effect of plasma heating on wafer during etching is analyzed. It is shown that the balance between the undercut originating from plasma heating and the redeposition of sputtering on the side-wall is crucial for highly anisotropic etching, and the balance point moves toward lower bias when the ICP power is increased. High aspect-ratio etching at the DC bias of 203 V is obtained. Eventually, photonic crystal structure with nearly 90 degrees side-wall is achieved at low DC bias after optimization of the gas mixture.