996 resultados para Silicon wafer


Relevância:

20.00% 20.00%

Publicador:

Resumo:

地址: Chinese Acad Sci, Inst Semicond, State Key Lab Integrated Optoelect, Beijing 100083, Peoples R China

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Enhanced near-infrared photoluminescence (PL) from sulfur-related isoelectronic luminescent centers in silicon was observed from thermally quenched sulfur-implanted silicon in which additional copper or silver ions had been coimplanted. The PL from the sulfur and copper coimplanted silicon peaked between 70 and 100 K and persisted to 260 K. This result strongly supports the original conjecture from the optical detection of magnetic resonance studies that the strong PL from sulfur-doped silicon comes from S-Cu isoelectronic complexes [Frens , Phys. Rev. B 46, 12316 (1992); Mason , ibid. 58, 7007 (1998).]. (c) 2007 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The temperature dependence of silicon-on-insulator thermo-optic attenuators is analysed, which originates from the temperature dependence of characteristics of multimode interference. The attenuator depth and power consumption are independent of temperature while the insertion loss depends on the temperature heavily. The variation of the insertion loss decreases from 4.3 dB to 1 dB as the temperature increases from 273 K to 343 K.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Novel folding 8 x 8 matrix switches based on silicon on insulator were demonstrated. In the design, single-mode rib waveguides and multimode interferences are connected by optimized tapered waveguides to reduce the mode coupling loss between the two types of waveguides. The self-aligned method was applied to the key integrated turning mirrors for perfect positions and low loss of them. A mixed etching process including inductively coupled plasma and chemical etching was employed to etch waveguides and mirrors, respectively. The compact size of the device is only 20 x 3.2 mm(2). The switch element with high switching speed and low power consumption is presented in the matrix. The average insertion loss of the matrix is about -21 dB, and the excess loss of one mirror is measured of -1.4 dB. The worst crosstalk is larger than 21 dB. Experimental results illuminate that some of the main characteristics of optical matrix switches are. developed in the modified design, which is in accord with theoretic analyses.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two silicon light emitting devices with different structures are realized in standard 0.35 mu m complementary metal-oxide-semiconductor (CMOS) technology. They operate in reverse breakdown mode and can be turned on at 8.3 V. Output optical powers of 13.6 nW and 12.1 nW are measured at 10 V and 100 mA, respectively, and both the calculated light emission intensities are more than 1 mW/Cm-2. The optical spectra of the two devices are between 600-790 nm with a clear peak near 760 nm..

Relevância:

20.00% 20.00%

Publicador:

Resumo:

By vertical sedimentation and oblique titration, silica microspheres were grown in different shapes of concave microzones that were etched on a (100) p-silicon substrate. Through scanning electron microscope observation and optical reflective spectra measurement, sedimentation of microspheres in those microzones was compared. An index was introduced to judge the efficiency of sedimentation. The comparison demonstrates that regular hexagons and triangles facilitate the growth of photonic crystals the most. (c) 2006 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

While the thermodynamic nonequilibrium properties of nanoparticles are being extensively studied, the thermodynamic nonequilibrium properties of their counterpart: nanocavities, however, are less noticed. Here, we systematically review and comprehensively model the recently published results on the newly-found thermodynamic nonequilibriurn properties of nanocavities in covalently bound materials during energetic beam irradiation. We also review and model the thermodynamic nonequilibrium properties of nanoparticles. The review and modelling not only demonstrates the novel nonequilibriurn properties of such an open-volume nanostructure during external excitation but also gives a deep insight into the nonequilibrium thermodynamics of amorphous structures and the difference in the behaviours of defects in crystalline and in amorphous silicon. Especially, the review and modelling leads to two new concepts:anti-symmetry relation between a nanoparticle and a nanocavity;energetic beam induced-soft mode and lattice instability in condensed matter;which reveals that structure of a condensed matter would be unstable not only at nanosize scale but also at a nanotime scale in general. It is also reveals that such nanoinstabilities would be more pronounced in an amorphous structure than in a crystalline structure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Detailed X-ray photoelectron spectroscopy (XPS) depth profiling measurements were performed across the back n-layer/transparent conducting oxide (n/TCO) inter-faces for superstrate p-i-n solar cells to examine differences between amorphous silicon (a-Si:H) and microcrystalline silicon (mu c-Si:H) n-layer materials as well as TCO materials ZnO and ITO in the chemical, microstructural and diffusion properties of the back interfaces. No chemical reduction of TCO was found for all variations of n-layer/TCO interfaces. We found that n-a-Si:H interfaces better with ITO, while n-mu c-Si:H, with ZnO. A cross-comparison shows that the n-a-Si:H/ITO interface is superior to the n-mu c-Si:H/ZnO interface, as evidenced by the absence of oxygen segregation and less oxidized Si atoms observed near the interface together with much less diffusion of TCO into the n-layer. The results suggest that the n/TCO interface properties are correlated with the characteristics of both the n-layer and the TCO layer. Combined with the results reported on the device performance using similar back n/TCO contacts, we found the overall device performance may depend on both interface and bulk effects related to the back n/TCO contacts. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The mode edges of photonic crystal waveguide with triangular lattice based on a silicon-on-insulator slab are investigated by combination of the effective index method and two-dimensional plane wave expansion method. The variations of waveguide-mode edges with structure parameters of photonic crystal are deduced. When the ratio of the radius of air holes to the lattice constrant, r/Lambda, is fixed and the lattice constant of photonic crystal, Lambda, increases, the waveguide-mode edges shift to longer wavelengths. When Lambda is fixed and r/Lambda increases, the waveguide-mode edges shift to shorter wavelengths. Additionally, when r/Lambda and Lambda are both fixed, the radius of the two-row air holes adjacent to the waveguide increases, the waveguide-mode edges shift to shorter wavelengths.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A concrete two-dimensional photonic crystal slab with triangular lattice used as a mirror for the light at wavelength 1.3 mu m with a silicon-on-insulator (Sol) substrate is designed by the three-dimensional plane wave expansion method. For TE-like modes, the bandgap in the F-K direction is from 1087nm to 1559nm. The central wavelength in the bandgap is about 1.3 mu m, hence the incident light at wavelength 1.3 mu m will be strongly reflected. Experimentally, such a photonic crystal slab is fabricated on an SOI substrate by the combination of EBL and ICP etching. The measurement of its transmission characteristics shows the bandgap edge in a longer wavelength is about 1540mn. The little discrepancy between the experimental data and the theoretical values is mainly due to the size discrepancy of the fabricated air holes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Diphasic silicon films (nc-Si/a-Si:H) have been prepared by a new regime of plasma enhanced chemical vapour deposition in the region adjacent of phase transition from amorphous to microcrystalline state. Comparing to the conventional amorphous silicon (a-Si:H), the nc-Si/a-Si:H has higher photoconductivity (sigma(ph)), better stability, and a broader light spectral response range in the longer wavelength range. It can be found from Raman spectra that there is a notable improvement in the medium range order. The blue shift for the stretching mode and red shift for the wagging mode in the IR spectra also show the variation of the microstructure. By using this kind of film as intrinsic layer, a p-i-n junction solar cell was prepared with the initial efficiency of 8.51 % and a stabilized efficiency of 8.01% (AM 1.5, 100 mw/cm(2)) at room temperature. (c) 2006 Published by Elsevier B.V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Wafer bonding between p-Si and an n-InP-based InGaAsP multiple quantum well (MQW) wafer was achieved by a direct wafer bonding method. In order to investigate the strain at different annealing temperatures, four pre-bonded pairs were selected, and pair one was annealed at 150 degrees C, pair two at 250 degrees C, pair three at 350 degrees C, and pair four at 450 degrees C, respectively. The macroscopical strains on the bonded epitaxial layer include two parts, namely the internal strain and the strain caused by the mismatching of the crystalline orientation between InP (100) and Si (100). These strains were measured by the X-ray double crystalline diffraction, and theoretical calculations of the longitudinal and perpendicular thermal strains at different annealing temperatures were calculated using the bi-metal thermostats model, both the internal strain and the thermal strain increase with the annealing temperature. Normal thermal stress and the elastic biaxial thermal strain energy were also calculated using this model. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Intrinsic nanocrystalline silicon films (nc-Si:H) were prepared by plasma enhanced chemical vapor deposition (PECVD) method. Films' microstructures and characteristics were studied with Raman spectroscopy and Atom Force Microscope (AFM). The electronic conductivity of nc-Si:H films was found to be 4.9 x 10(0)Omega(-1) cm(-1), which was one order of magnitude higher than the reported 10(-3)-10(-1)Omega(-1)cm(-1). And PIN solar cells with nc-Si:H film as intrinsic thin-layer (ITO/n(+)-nc-Si:H/i-nc-Si:H/p-c-Si/Ag) were researched. The cell's performances were measured, the open-circuit voltage V-oc was 534.7 mV, short-circuit current I-sc was 49.24 mA (3 cm(2)) and fill factor FF was 0.4228. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Straight single-line defect optical waveguides in photonic crystal slabs are designed by the plane wave expansion method and fabricated into silicon-on-insulator (SOI) wafer by 248-nm deep UV lithography. We present an efficient way to measure the light transmission spectrum of the photonic crystal waveguide (PhC WG) at given polarization states. By employing the Mueller/Stokes method, we measure and analyse the light propagation properties of the PhC WG at different polarized states. It is shown that experimental results are in agreement with the simulation results of the three-dimensional finite-difference-time-domain method.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Arrays of vertically well-aligned ZnO nanorod-nanowall junctions have been synthesized on an undoped ZnO-coated silicon substrate by a carbothermal reduction and vapour phase transport method. X-ray diffraction (XRD) and scanning electron microscopy (SEM) show that the nanostructures are well-oriented with the c-axis perpendicular to the substrate. The room temperature photoluminescence (PL) spectrum of the as-prepared ZnO nanostructure reveals a dominant near-band-edge (NBE) emission peak and a weak deep level (DL) emission, which demonstrates its good optical properties. Temperature-dependent PL spectra show that both the intensity of NBE and DL emissions increased with decreasing temperature. The NBE emission at 3.27 eV is identified to originate from the radiative free exciton recombination. The possible growth mechanism of ZnO nanorod-nanowall junctions is also proposed.