938 resultados para Three-Phase Composites


Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Metal oxidenanocomposites were prepared by two different routes: polyol and sol-gel. Characterization by X ray diffraction showed that the first processproducesdirectly a two-phase material, while the sol-gelpowder never showed second phase below 600 degrees C. Light spectroscopy of the treated powders indicated similarities for the processed materials. Although the overall material compositions are about the same, different structural characteristics are found for each processing. With the exception of Ti-Zn materials, all the double metal oxide powders showed higher absorbance than either TiO2 powder.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Metal oxide nanocomposites were prepared by two different routes: polyol and sol-gel. Characterization by X ray diffraction showed that the first process produces directly a two-phase material, while the sol-gel powder never showed second phase below 600°C. Light spectroscopy of the treated powders indicated similarities for the processed materials. Although the overall material compositions are about the same, different structural characteristics are found for each processing. With the exception of Ti-Zn materials, all the double metal oxide powders showed higher absorbance than either TiO2 powder.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The objective of this paper is compare the common traffic lights (CTL) to three different types of traffic lights with countdown displays (SCD) and assess their effects on road safety and capacity. This comparison is required because the results found in the literature are divergent among countries and cities, and one of the SCD analyzed in our study is different from the SCD used worldwide. An observational before-after study was conducted to evaluate the safety and capacity in a period of one year before and one year after the implementation of the SCD in three Brazilian cities. The results indicate that the SCD models 1 and 3 had around 35%±14% reduction in the total number of accidents; the model 2, does not have significant reduction. In order to perform the capacity analysis a framework for data collection and an adaptation for estimation of initial lost time in each phase were developed. Considering the capacity analysis there was a reduction around 11% in the lost time in SCD model 1, 7% in SCD model 2 and 3% in SCD model 3. However the implications of this on capacity are trifle due to a small increase in the average headways for all SCD models compare to CTL.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Snake venom proteomes/peptidomes are highly complex and maintenance of their integrity within the gland lumen is crucial for the expression of toxin activities. There has been considerable progress in the field of venom proteomics, however, peptidomics does not progress as fast, because of the lack of comprehensive venom sequence databases for analysis of MS data. Therefore, in many cases venom peptides have to be sequenced manually by MS/MS analysis or Edman degradation. This is critical for rare snake species, as is the case of Bothrops cotiara (BC) and B. fonsecai (BF), which are regarded as near threatened with extinction. In this study we conducted a comprehensive analysis of the venom peptidomes of BC, BF, and B. jararaca (BJ) using a combination of solid-phase extraction and reversed-phase HPLC to fractionate the peptides, followed by nano-liquid chromatography-tandem MS (LC-MS/MS) or direct infusion electrospray ionization-(ESI)-MS/MS or MALDI-MS/MS analyses. We detected marked differences in the venom peptidomes and identified peptides ranging from 7 to 39 residues in length by de novo sequencing. Forty-four unique sequences were manually identified, out of which 30 are new peptides, including 17 bradykinin-potentiating peptides, three poly-histidine-poly-glycine peptides and interestingly, 10 L-amino acid oxidase fragments. Some of the new bradykinin-potentiating peptides display significant bradykinin potentiating activity. Automated database search revealed fragments from several toxins in the peptidomes, mainly from L-amino acid oxidase, and allowed the determination of the peptide bond specificity of proteinases and amino acid occurrences for the P4-P4' sites. We also demonstrate that the venom lyophilization/resolubilization process greatly increases the complexity of the peptidome because of the imbalance caused to the venom proteome and the consequent activity of proteinases on venom components. The use of proteinase inhibitors clearly showed different outcomes in the peptidome characterization and suggested that degradomic-peptidomic analysis of snake venoms is highly sensitive to the conditions of sampling procedures. Molecular & Cellular Proteomics 11: 10.1074/mcp.M112.019331, 1245-1262, 2012.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Objectives. To verify the hypothesis that crack analysis and a mechanical test would rank a series of composites in a similar order with respect to polymerization stress. Also, both tests would show similar relationships between stress and composite elastic modulus and/or shrinkage. Methods. Soda-lime glass discs (2-mm thick) with a central perforation (3.5-mm diameter) received four Vickers indentations 500 mu m from the cavity margin. The indent cracks were measured (500x) prior and 10 min after the cavity was restored with one of six materials (Kalore/KL, Gradia/GR, Ice/IC, Wave/WV, Majesty Flow/MF, and Majesty Posterior/MP). Stresses at the indent site were calculated based on glass fracture toughness and increase in crack length. Stress at the bonded interface was calculated using the equation for an internally pressurized cylinder. The mechanical test used a universal testing machine and glass rods (5-mm diameter) as substrate. An extensometer monitored specimen height (2 mm). Nominal stress was calculated dividing the maximum shrinkage force by the specimen cross-sectional area. Composite elastic modulus was determined by nanoindentation and post-gel shrinkage was measured using strain gages. Data were subjected to one-way ANOVA/Tukey or Kruskal-Wallis/Mann-Whitney tests (alpha: 5%). Results. Both tests grouped the composites in three statistical subsets, with small differences in overlapping between the intermediate subset (MF, WV) and the highest (MP, IC) or the lowest stress materials (KL, GR). Higher stresses were developed by composites with high modulus and/or high shrinkage. Significance. Crack analysis demonstrated to be as effective as the mechanical test to rank composites regarding polymerization stress. (c) 2012 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The lyotropic liquid crystalline quaternary mixture made of potassium laurate (KL), potassium sulphate, 1-undecanol and water was investigated by experimental optical methods (optical microscopy and laser conoscopy). In a particular temperature and relative concentrations range, the three nematic phases (two uniaxial and one biaxial) were identified. The biaxial domain in the temperature/KL concentration surface is larger when compared to other lyotropic mixtures. Moreover, this new mixture gives nematic phases with higher birefringence than similar systems. The behavior of the symmetric tensor order parameter invariants sigma(3) and sigma(2) calculated from the measured optical birefringences supports that the uniaxial-to-biaxial transitions are of second order, described by a mean-field theory.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Purpose Cediranib is a highly potent inhibitor of vascular endothelial growth factor (VEGF) signaling with activity against all three VEGF receptors. HORIZON II [Cediranib (AZD2171, RECENTIN) in Addition to Chemotherapy Versus Placebo Plus Chemotherapy in Patients With Untreated Metastatic Colorectal Cancer] assessed infusional fluorouracil, leucovorin, and oxaliplatin/capecitabine and oxaliplatin (FOLFOX/CAPOX) with or without cediranib in patients with previously untreated metastatic colorectal cancer (mCRC). Patients and Methods Eligible patients were initially randomly assigned 1:1:1 to receive cediranib (20 or 30 mg per day) or placebo plus FOLFOX/CAPOX. In an early analysis of this and two other cediranib studies (HORIZON I [Cediranib Plus FOLFOX6 Versus Bevacizumab Plus FOLFOX6 in Patients With Previously Treated Metastatic Colorectal Cancer] and HORIZON III [Cediranib Plus FOLFOX6 Versus Bevacizumab Plus FOLFOX6 in Patients With Untreated Metastatic Colorectal Cancer]), the 20-mg dose met the predefined criteria for continuation. Subsequent patients were randomly assigned 2: 1 to the cediranib 20 mg or placebo arms. Progression-free survival (PFS) and overall survival (OS) were coprimary end points. Results In all, 860 patients received cediranib 20 mg (n = 502) or placebo (n = 358). The addition of cediranib to FOLFOX/CAPOX resulted in PFS prolongation (hazard ratio [HR], 0.84; 95% CI, 0.73 to 0.98; P = .0121; median PFS, 8.6 months for cediranib v 8.3 months for placebo) but had no impact on OS (HR, 0.94; 95% CI, 0.79 to 1.12; P = .5707; median OS, 19.7 months for cediranib v 18.9 months for placebo). There were no significant differences in the secondary end points of objective response rate, duration of response, or liver resection rate. Median chemotherapy dose-intensity was decreased by approximately 10% in patients treated with cediranib. Adverse events (AEs) associated with cediranib were manageable. Conclusion Addition of cediranib 20 mg to FOLFOX/CAPOX resulted in a modest PFS prolongation, but no significant difference in OS. The cediranib AE profile was consistent with those from previous studies. Because of the lack of improvement in OS, cediranib plus an oxaliplatin-based regimen cannot be recommended as a treatment for patients with mCRC. J Clin Oncol 30:3596-3603. (C) 2012 by American Society of Clinical Oncology

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study reports the performance of a combined anaerobic-aerobic packed-bed reactor that can be used to treat domestic sewage. Initially, a bench-scale reactor was operated in three experimental phases. In the first phase, the anaerobic reactor was operated with an average organic matter removal efficiency of 77% for a hydraulic retention time (HRT) of 10 h. In the second phase, the reactor was operated with an anaerobic stage followed by an aerobic zone, resulting in a mean value of 91% efficiency. In the third and final phase, the anaerobic-aerobic reactor was operated with recirculation of the effluent of the reactor through the anaerobic zone. The system yielded mean total nitrogen removal percentages of 65 and 75% for recycle ratios (r) of 0.5 and 1.5, respectively, and the chemical oxygen demand (COD) removal efficiencies were higher than 90%. When the pilot-scale reactor was operated with an HRT of 12 h and r values of 1.5 and 3.0, its performance was similar to that observed in the bench-scale unit (92% COD removal for r = 3.0). However, the nitrogen removal was lower (55% N removal for r = 3.0) due to problems with the hydrodynamics in the aerobic zone. The anaerobic-aerobic fixed-bed reactor with recirculation of the liquid phase allows for concomitant carbon and nitrogen removal without adding an exogenous source of electron donors and without requiring any additional alkalinity supplementation.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Composites formed of a polymer-embedded layer of sub-10 nm gold nanoclusters were fabricated by very low energy (49 eV) gold ion implantation into polymethylmethacrylate. We used small angle x-ray scattering to investigate the structural properties of these metal-polymer composite layers that were fabricated at three different ion doses, both in their original form (as-implanted) and after annealing for 6 h well above the polymer glass transition temperature (150 degrees C). We show that annealing provides a simple means for modification of the structure of the composite by coarsening mechanisms, and thereby changes its properties. (C) 2012 American Institute of Physics. [http://dx.doi.org/10.1063/1.4720464]

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The aim of this research was to characterize emulsion systems (ES) containing nonionic ethoxylated surfactants by using rheological, microscopic, and thermogravimetric assays. Three formulations were developed: ES-1: 8.0% (w/w) oleth-20; ES-2: 4.0% (w/w) oleth-20/4.0% (w/w) steareth-21; and ES-3: 8.0% (w/w) steareth-21. The systems showed typical non-Newtonian pseudo-plastic behavior. The presence of a lamellar gel phase was observed for all systems, with ES-2 being more pronounced. Through thermogravimetry, the profiles of the three systems were found to be similar, consisting of two main events, the first one being characterized by loss of water and, beyond 110 degrees C, by loss of the oil phase.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The deep bedding is a swine alternative production, especially in the finishing phase, whose byproduct can be recycled, reducing the environmental impact. The objectives of this study were to characterize the ash coming from the controlled burning of the swine deep bedding (SDBA) based on rice husk, and to evaluate their performance in composites as a partial substitute for Portland cement (PC). To measure the differences between SDBA and rice husk ash (RHA) as a reference, we have characterized: particle size distribution, real specific density, x-ray diffraction, electrical conductivity, scanning electron microscopy, chemical analysis and loss on ignition. Samples were prepared for two experimental series: control, and another one with the partial replacement of 30% of SDBA in relation to the mass of the Portland cement. According to the results obtained for physical and mechanical characterization, the composites with SDBA can be used as a constructive element in the rural construction.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The purpose of the present study was to evaluate in vivo the failure rate of metallic brackets bonded with two orthodontic composites. Nineteen patients with ages ranging from 10.5 to 38.7 years needing corrective orthodontic treatment were selected for study. The enamel surfaces from second premolars to second premolars were treated with Transbond Plus-Self Etching Primer (3M Unitek). Next, 380 orthodontic brackets were bonded on maxillary and mandibular teeth, as follows: 190 with Transbond XT composite (3M Unitek) (control) and 190 with Transbond Plus Color Change (3M Unitek) (experimental) in contralateral quadrants. The bonded brackets were light cured for 40 s, and initial alignment archwires were inserted. Bond failure rates were recorded over a six-month period. At the end of the evaluation, six bond failures occurred, three for each composite. Kaplan-Meyer method and log-rank test (Mantel-Cox) was used for statistical analysis, and no statistically significant difference was found between the materials (p=0.999). Both Transbond XT and Transbond Plus Color Change composites had low debonding rates over the study period.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study evaluated the effect of artificially accelerated aging (AAA) on the surface hardness of eight composite resins: Filtek Z250, Filtek Supreme, 4 Seasons, Herculite, P60, Tetric Ceram, Charisma, and Filtek Z100. Sixteen specimens were made from the test piece of each material, using an 8.0 × 2.0 mm teflon matrix. After 24 hours, eight specimens from each material were submitted to three surface hardness readings using a Shimadzu Microhardness Tester for 5 seconds at a load of 50 gf. The other eight specimens remained in the artificially accelerated aging machine for 382 hours and were submitted to the same surface hardness analysis. The means of each test specimen were submitted to the Kolmogorov-Smirnov test (p > 0.05), ANOVA and Tukey test (p < 0.05). With regard to hardness (F = 86.74, p < 0.0001) the analysis showed significant differences among the resin composite brands. But aging did not influence the hardness of any of the resin composites (F = 0.39, p = 0.53). In this study, there was interaction between the resin composite brand and the aging factors (F = 4.51, p < 0.0002). It was concluded that notwithstanding the type of resin, AAA did not influence surface hardness. However, with regard to hardness there was a significant difference among the resin brands.