Ti45Zr35Ni17Cu3 amorphous and single icosahedral quasicrystalline powders were synthesized by mechanical alloying and subsequent annealing at 855 K. Microstructure and electrochemical properties of two alloy electrodes were characterized. When the temperature was enhanced from 303 to 343 K, the maximum discharge capacities increased from 86 to 329 mAh g(-1) and 76 to 312 mAh g(-1) for the amorphous and quasicrystalline alloy electrodes, respectively. Discharge capacities of two electrodes decrease distinctly with increasing cycle number. The I-phase is stable during charge/discharge cycles, and the main factors for its discharge capacity loss are the increase of the charge-transfer resistance and the pulverization of alloy particles. Besides the factors mentioned above, the formation of TiH2 and ZrH2 hydrides is another primary reason for the discharge capacity loss of the amorphous alloy electrode.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Nano/microstructure of bis(propyl)triethoxysilane substituted perylenediimide (1) with nanoparticle and twisted microrod morphologies were obtained by reprecipitation method induced by water and petroleum ether, respectively. It is believed that the different nucleation and growth processes involved are responsible for the formation of the nano/micro-structure With different morphologies of 1. UV-vis absorption and photoluminescence measurements show that their UV-vis absorption and photoluminescence properties are different from each other as well as their monomer mid bulk materials due to the different effects on the change transfer (CT) transition energy levels caused by their different aggregation behaviors.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The effects of crystallization temperature (T,), glass bead content and its size on the, formation of beta-crystal and structural stability of originally formed beta-crystal in glass bead filled polypropylene (PP) were examined. The differential scanning calorimetry (DSC) measurements indicated that the amount of beta-phase in PP crystals was a function of the crystallization temperature and glass bead content. For a constant crystallization temperature, it was observed that the amount of beta-crystal initially increased with increase in glass bead content up to 30 wt.%, and then decreased slightly with further increase in the filler content. From the DSC data, a disorder parameter (S) was derived to define the structural stability of originally formed beta-crystals. The structural stability of originally formed beta-crystals was enhanced with increase in either the crystallization temperature or the glass bead content. Also, the influence of glass bead size (4-66 mu m) on the formation and stability of beta-crystals in PP/glass bead blends was studied. Large glass bead particles suppressed the formation and decreased the stability of beta-crystals.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The electrochemical properties of the Ti0.17Zr0.08V0.35Cr0.10Ni0.30 alloy electrode were investigated. This alloy has good cycle life at 303 K, 313 K, and even at 323 K, but the discharge capacity decreases gradually at 333 K with increasing cycle number. Both the charge-discharge efficiency and the charge-discharge voltage reduce. The electrochemical impendence spectra indicate that the charge-transfer resistance decreases while the exchange current density increases as temperature increases. The apparent activation energy of the charge-transfer reaction is about 50 kJ mol(-1), which is higher than that on the AB(5) type alloy electrode.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

采用XRD、FESEM-EDS、ICP及EIS等方法研究了Ti0.17Zr0.08V0.34Nb0.01Cr0.1Ni0.3氢化物电极合金微观结构和电化学性能。X射线衍射分析表明:该合金由体心立方结构(bcc)的V基固溶体主相和少量六方结构的C14型Laves相组成;FESEM及EDS分析表明:V基固溶体主相形成树枝晶,C14型Laves相呈网格状围绕着树枝晶的晶界,元素在两相中的分布呈现镜像关系。电化学性能测试结果表明:该合金的氢化物电极在303 ̄343K较宽的温度区间内,表现出较高的电化学容量,在303K和343K时,电化学容量分别为337.0mAh·g-1和327.9mAh·g-1。在303K循环100周后,容量为282.7mAh·g-1。ICP分析结果表明,氢化物电极在充放电循环过程中,V及Zr元素向KOH电解质中的溶出较为严重。EIS研究表明,金属氢化物电极表面电化学反应的电荷转移电阻(RT)随循环次数的增加而增加,相应的交换电流密度则随循环次数的增加而降低。氢化物电极循环过程中RT的增大以及V和Zr元素的溶解,可能是导致电极容量衰减的主要原因。

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Excess intercalation of cationic surfactants into Na-montmorillonites (MMTs) was investigated in organically modified silicates (OMSs), synthesized with MMTs and octadecylammonium chloride (OAC) by systematically varying the surfactant loading level from 0.625 to 1, 1.25, 1.56, 2, and 2.5 with respect to the cation exchange capacity (CEC) of MMTs. Wide-angle X-ray diffraction and thermogravimetric analysis results indicated that the continuous increase of interlayer distances came from the entering of surfactants into the interlayer of MMTs. Excess surfactants were extracted with a Soxhlet apparatus, which showed two kinds of intercalation states of surfactants in the interlayer when the surfactant loading level was beyond the CEC. Fourier transform infrared spectroscopy and differential scanning calorimetry were used to explore the microstructures of OMSs. It was found that the surfactants arranged more orderly as the loading level increased and the excess surfactants piled up in the interlayer together with counterions, forming a sandwiched surfactant layer. On the basis of the results, the layer structures of OMSs and the mechanism by which the surfactants entered the interlayer were expounded: surfactant cations entered the interlayer through cation exchange reactions and were tightly attracted to the silicate platelet surfaces when the surfactant loading level was below the CEC;

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A series of organically modified clays (OMCs) with a surfactant loading range from 0.625 to 2.5 times the cation exchange capacity (CEC) were melt-mixed with maleated polypropylene (PPMA). Wide-angle X-ray diffraction and transmission electron microscopy results of these narrocomposites show that dispersion of clays becomes unfavorable in the PPMA matrix during melt intercalation as the surfactant loading increases in the process of modifying clays, though larger interlayer distances are obtained in their corresponding OMCs. It is even important that clays uniformly disperse at the nanoscale level in the PPMA matrix when the surfactant loadings are below the CEC, which implies that incomplete exchange of inorganic cations in the process of modifying clay benefits the dispersion of clays in the PPMA matrix.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

By using the average band-gap model, the chemical bond properties of (La1-x, M-x)(2)CuO4(M=Ba, Sr) were calculated. The calculated covalencies for Cu-O and La-O bond in the compounds are 0.3 and 0.03 respectively. Mossbauer isomer shifts of Fe-57 doped in La2CuO4 and Sn-119 doped in La2CuO4 were calculated by using the chemical surrounding factor defined by covalency and electronic polarizability. Four valence state tin and three valence iron sites were identified in Fe-57 and Sn-119 doped La2CuO4.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The kinetics of RE (La, Gd, Er, Yb and Y) extraction with sec-octylphenoxy acetic acid was investigated using a constant interfacial area cell with laminar flow at 303 K. The natures of the extracted complexes have some effect on the extraction rate which is controlled by the reaction rate of M(III) and extractant molecules at two-phase interface for Er(III), Yb(III) and Y(III), by a mixed chemical reaction-diffusion for Gd(III) and a diffusion for La( III). The extractant molecules tend to adsorb at the interface. So an interfacial extraction reaction model was derived.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A novel amperometric biosensor for the detection of hydrogen peroxide is described. The biosensor was constructed by electrodepositing HRP/PPy membrane on the surface of ferrocenecarboxylic acid mediated sol-gel derived composite carbon electrode. The biosensor gives response to hydrogen peroxide in a few seconds with detection limit of 5x10(-7) mol (.) L-1 (based on signal : noise=3). Linear range is up to 0.2 mmol (.) L-1.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A method for the determiantion of rare earth elements in biological sampels by inductively coupled plasma mass spectrometry was developed. Oxide ion yield of the rare earth elements (RFE) decreased with the increasing of RF power and the sampling depth, or with the decreasing of carrier gas flow rate. The spectral interference arising from (PrO)-Pr-141-O-16 on Gd-157 must be corrected. if the concentration of Ba was high enough, it was necessary to correct the spectral interference arising from (BO)-B-135-O-16 on Eu-151, and it was not necessary to correct spectral interference arising from (NdO)-Nd-143-O-16 on Tb-159 etc. in the biological samples under the selected operation parameters. In the biological sample, the major matrix elements, such as K, Na and Ca, result in the suppression of REEs signals and the suppression degree of the Ca is grezter than that of the K and Na. The mussel sample was digested by thd dry ashing, wet digestion with HNO3 + H2O2 and HNO3 + HClO4, respectively. The analytical results of REEs were consistent with each other. Detection limits for REEs are 0.001 similar to 0.013 mu g/L. Recoveries of standard addition are 91.7% similar to 125%. REEs in biological samples were determined directly without separation and preconcentration procedure.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The ion pair between the dianion of 7,7,8, 8-tetracyanoquinodimethane(TCNQ) and Li+ were investigated by in - situ microscopic Fourier transform infrared( FTIR) spectroelectrochemical technique. The effect of ion pair increases with increasing the concentration of cation. We observed a new band at 2130 cm(-1).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

用现场显微红外光谱电化学技术研究了聚电解质中TCNQ在电化学还原过程中二价阴离子与Li~+离子之间形成的离子对.离子对效应随阳离子浓度增加而增大.观察到一个文献中未曾报道的谱带位于2130cm~(-1)附近.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

采用电感耦合等离子体质谱法测定了生物样品中的稀土元素.稀土元素的氧化物离子产率随入射功率和采样深度增加,载气流速减小而降低.在选择的测量条件下,~(141)Pr~(16)O对~(157)Gd的测定可产生严重干扰,必须校正,当样品中钡含量较高时,应考虑校正~(135)Ba对~(151)Eu的干扰.生物样品的主要基体元素K、Na和Ca在浓度较高时,对稀土元素的信号强度均表现出抑制效应,且Ca的抑制程度大于K和Na.比较了干灰化、HNO_3+H_2O_2和HNO_3+HClO_4 3种样品消解方法,结果表明,3种消解方法可得到一致的结果.稀土元素的检出限为0.001~0.013μg/L,标准加入回收率为91.7%~125%,不经分离富集可直接测定生物样品中的超痕量稀土元素.