The effect of film orientation on piezoelectric and ferroelectric properties of bismuth layered compounds deposited on platinum coated silicon substrates was investigated. Piezo-force microscopy was used to probe the local piezoelectric properties of Bi(4)Ti(3)O(12), CaBi(4)Ti(4)O(15) and SrBi(4)Ti(4)O(15) films. Our measurements on individual grains clearly reveal that the local piezoelectric properties are determined by the polarization state of the grain. A piezoelectric coefficient of 65 pm/V was attained after poling in a grain with a polar axis very close to the normal direction. The piezoelectric coefficient and the remanent polarization were larger for a-b axes oriented than for c-axis-oriented films. (c) 2007 Elsevier B.V All rights reserved.
Resumo:
SrBi4Ti4O15 (SBTi) thin films were obtained by the polymeric precursor method and crystallized in a domestic microwave oven. For comparison, films were also crystallized in a conventional furnace at 700 degrees C for 2 h. Structural and morphological characterization of the SBTi thin films was investigated by X-ray diffraction (XRD) and atomic force microscopy (AFM), respectively. Using platinum coated silicon substrates configuration, ferroelectric properties of the films were determined with remanent\polarization P-r and a coercive field E-c of 5.1 mu C/cm(2) and 135 kV/cm for the film thermally treated in the microwave oven and 5.4 mu C/cm(2) and 85 kV/cm for the film thermally treated in conventional furnace, respectively. The films thermally treated in the conventional furnace exhibited excellent fatigue-free characteristics up to 10(10) switching cycles indicating that SBTi thin films can be a promise material for use in non-volatile memories. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Thin films of SrBi4Ti4O15 (SBTi), a prototype of the Bi-layered-ferroelectric oxide family, were obtained by a soft chemical method and crystallized in a domestic microwave oven. For comparison, films were also crystallized in a conventional method at 700 degrees C for 2 h. Structural and morphological characterization of the SBTi thin films were investigated by Xray diffraction (XRD) and atomic force microscopy (AFM), respectively. Using platinum coated silicon substrates, the ferroelectric properties of the films were determined. Remanent polarization P-r and a coercive field E-c values of 5.1 mu C/cm(2) and 135 kV/cm for the film thermally treated in the microwave oven and 5.4 mu C/cm(2) and 85 kv/cm for the film thermally treated in conventional furnace were found. The films thermally treated in the conventional furnace exhibited excellent fatigue-free characteristics up to 10(10) switching cycles indicating that SBTi thin films are a promising material for use in non-volatile memories. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Bi3.25La0.75Ti3O12 (BLT) thin films were grown on LaNiO3 (LNO), RuO2 (RuO2) and La0.5Sr0.5CoO3 (LSCO) bottom electrodes by using the polymeric precursor method and microwave furnace. The bottom electrode is found to be an important parameter which affects the crystallization, morphology and leakage current behaviors. The XRD results clearly show that film deposited on LSCO electrode favours the growth of (117) oriented grains whereas in films deposited on LNO and RuO2 the growth of (001) oriented grains dominated. The film deposited on LSCO has a plate-like grain structure, and its leakage current behavior is in agreement with the prediction of the space-charge-limited conduction model. on the other hand, the films deposited on RuO2 and LNO electrodes present a rounded grain shape with some porosity, and its high field conduction is well explained by the Schottky and Poole-Frenkel emission models. The remanent polarization (P-r) and the drive voltage (V-c) were in the range of 11-23 mu C cm(-2) and 0.86-1.56 V, respectively, and are better than the values found in the literature. (c) 2007 Published by Elsevier B.V.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
This paper presents a new family of pulsewidth-modulated (PWM) converters, featuring soft commutation of the semiconductors at zero current (ZC) in the transistors and zero voltage (ZV) in the rectifiers, Besides operating at constant frequency and with reduced commutation losses, these new converters have output characteristics similar to the hard-switching-PWM counterpart, which means that there is no circulating reactive energy that would cause large conduction losses, the new family of zero-current-switching (ZCS)-PWM converters is suitable for high-power applications using insulated gate bipolar transistors (IGBT's). The advantages of the new ZCS-PWM boast converter employing IGBT's, rated at 1.6 kW and operating at 20 kHz, are presented, This new ZCS operation can reduce the average total power dissipation in the semiconductors practically by half, when compared with the hard-switching method, This new ZCS-PWM boost converter is suitable for high-power applications using Ie;BT's in power-factor correction, the principle of operation, theoretical analysis, and experimental results of the new ZCS-PWM boost converter are provided in this paper to verify the performance of this new family of converters.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Flexible and free-standing films of piezoelectric composites made up of lead zirconate titanate (PZT) ceramic powder dispersed in a castor oil-based polyurethane (PU) matrix were obtained by spin coating and characterised as materials for sensor applications. The piezoelectric coefficients d(31) and d(33) were measured with the usual technique. The piezoelectric charge constant d(33) yields values up to less than or equal to 24 pC/N, even at lower PZT content (33 vol%). Some desirable properties like piezoelectricity, flexibility and good mechanical resistance show this new material to be a good alternative for use as sensors and actuators.
Resumo:
This paper reports studies on dielectric and ferroelectric properties of lead zirconate titanate (PZT) thin films crystallized by conventional thermal annealing (CTA) and rapid thermal annealing (RTA) in air, oxygen and nitrogen atmospheres to better understand, control and optimize these properties. The dielectric constant (epsilon) and dissipation factor (tan delta) values, at a frequency of 100 kHz; for film crystallized in air by CTA process, were 358 and 0.039, respectively. Considering the same frequency for film crystallized in air by RTA, these values were 611 and 0.026, respectively. The different dielectric values were justified by a space-charge or interfacial polarization in films, often characterized as Maxwell-Wagner type. This effect was also responsible to dispersion at frequencies above 1 MHz in film crystallized in air by CTA process and film crystallized by RTA in oxygen atmosphere. The film crystallized by RTA under nitrogen atmosphere presented an evident dispersion at frequencies around 100 Hz, characterized by an increase in both epsilon and tan delta. This dispersion was attributed to conductivity effects. The remanent polarization (P-r) and coercive field (E-c) were also obtained for all films. Films obtained from RTA in air presented higher P-r (17.8 muC cm(-2)) than film crystallized from CTA (7.8 muC cm(-2)). As a function of the crystallization atmospheres, films crystallized by RTA in air and nitrogen presented essentially the same P-r values (around 18 muC cm(-2)) but the P-r (3.9 muC cm(-2)) obtained from film crystallized under oxygen atmosphere was profoundly influenced.
Resumo:
Flexible piezo- and pyroelectric composite was made in the thin film form by spin coating. Lead Zirconate Titanate (PZT) ceramic powder was dispersed in a castor oil-based polyurethane (PU) matrix, providing a composite with 0-3 connectivity. The dielectric data, measured over a wide range of frequency (10(-5) Hz to 105 Hz), shows a loss peak around 100 Hz related with impurities in the polymer matrix. There is also an evidence of a peak in the range 10(-4) Hz, possibly originating from the glass transition temperature T of the polymer. The pyroelectric coefficient at 34 K is 7.0x10(-5) C(.)m(-2.)K(-1) which is higher than that of P-PVDF (1X10(-5) C(.)m(-2.)K(-1)).