Plasmas generated in de discharges in aromatic compounds have been used for several years in polymerization processes. The chemical kinetics developed in such a plasma environment are extremely complicated. Therefore it is extremely important to set up optical and electrical diagnostics in order to establish the kinetics of the film growth, In this work we studied de plasmas generated ill low-pressure atmospheres of benzene for different values of gas pressure and power coupled to the discharge. The pressure range varied from 0.2 to 1.0 mbar for electric power running from 4 to 25 W, the main chemical species observed within the discharge were CH, H and C. It was observed that the CH relative concentration increases continuously with the power in the range investigated. The electron temperature varied from 0.5 to 2.0 eV with the increase of the power, for a fixed value of gas pressure. The relative dielectric constant of the plasma polymerized benzene was kept around 4.8 from 100 Hz to 10 kHz, presenting a resonance near 25 kHz. This electric behaviour of the film was the same fur different conditions of polymeric film deposition, (C) 1997 Elsevier B.V. S.A.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Thin films of SrBi4Ti4O15 (SBTi), a prototype of the Bi-layered-ferroelectric oxide family, were obtained by a soft chemical method and crystallized in a domestic microwave oven. For comparison, films were also crystallized in a conventional method at 700 degrees C for 2 h. Structural and morphological characterization of the SBTi thin films were investigated by Xray diffraction (XRD) and atomic force microscopy (AFM), respectively. Using platinum coated silicon substrates, the ferroelectric properties of the films were determined. Remanent polarization P-r and a coercive field E-c values of 5.1 mu C/cm(2) and 135 kV/cm for the film thermally treated in the microwave oven and 5.4 mu C/cm(2) and 85 kv/cm for the film thermally treated in conventional furnace were found. The films thermally treated in the conventional furnace exhibited excellent fatigue-free characteristics up to 10(10) switching cycles indicating that SBTi thin films are a promising material for use in non-volatile memories. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Molecular mobility in castor oil based polyurethane was investigated with thermally stimulated depolarization current (TSDC) measurements and alternating-current (ac) dielectric relaxation spectroscopy. Three peaks could be observed in TSDC thermograms from 173 to 373 K. The relaxation located at 213 K could be attributed to the change in the molecular chain due to the interaction between the isocyanate and the solvent, and it was well fitted with the Vogel-Fulcher-Tammann equation. The other two peaks were located at 274 and 365 K and could be attributed to interfacial polarization and space charge, respectively. (c) 2005 Wiley Periodicals, Inc.
Resumo:
The aim of this work was the preparation of polyols from reactions between castor oil and dietanolamine to increase the hydroxyl content and the network degree in the products to application in electronic devices. The polyols and the mixtures obtained were characterized by nuclear magnetic ressonance. Castor oil (CO) is a natural triglyceride - based polyol possessing hydroxyl groups, which allow several reactions that produce many different products. Among them are the polyurethanes (PU), which have been considered an ideal product for the covering of electricelectronic circuits, due to their excellent electrical, shock-absorbing, solvents resistance and hydrolytic stability properties. About 90% of the fatty acids present in the castor oil are ricinoleic acid (12-hydroxyoleic acid), while the remaining 10% correspond to non-hydroxylated fatty acids, mainly linoleic and oleic acids. The chemical analysis of castor oil indicates a hydroxyl number of 2.7. In this work, a polyol was obtained by the reaction of the CO with diethanolamine (DEA), in order to elevate the hydroxyl value from 160 to 230 or to 280 mgKOH/g, and characterized by nuclear magnetic resonance (NMR) 1H and 13C (Mercury 200). The polyadition of the resulting polyol with isophorone diisocianate (IPDI) was carried out at 60°C, and the reaction kinetics was followed by rheological measurements in a Haake RS150 rheometer. The electrical properties were determined in a HP LCR Meter 4262A, at 1.0 Hz and 10.0 KHz. The chemical analysis showed that the polyols obtained presented hydroxyl number from 230 to 280 mgKOH/g. The polyadition reaction with IPDI produced polyurethane resins with the following properties: hardness in the range from 45 shore A to 65 shore D (ASTM D2240); a dielectric constant of 3.0, at 25°C (ASTM D150). Those results indicate that the obtained resins present compatible properties to the similar products of fossil origin, which are used nowadays for covering electric-electronic circuits. Therefore, the PUs from castor oil can be considered as alternative materials of renewable source, free from the highly harmful petroleum - derived solvents
Resumo:
Composite made of Lead Zirconate Titranate (PZT) ceramic powder and castor oil based polyurethane (PU) were prepared in the thin film form with 0-3 connectivity by spin coating. The composite films were obtained in the thickness range of 100 mum to 300 mum using 33-vol.% of ceramic. The samples mechanical resistance. The material was characterised by dielectric spectroscopy, thermally stimulated discharge current (TSDC), hysteresis measurements and laser-intensity-modulation method (LIMM). The pyroelectric coefficient at 343 K was 7x10(-5) C.m(-2) K-1 for the sample poled with 10 MV/m at 373 K for Ih. The results show that this new composite can be used as suitable piezo and pyroelectric sensors.
Resumo:
Slightly < 111 >-oriented 0.65Pb(Mg1/3Nb2/3)03-0.35PbTiO(3) ceramic was prepared using fine powders obtained by means of an alternative and promising chemical oxide precursor method. High quality samples with improved structural, microstructural, dielectric and ferroelectric properties were obtained. The dielectric constant value (epsilon similar to 2577) measured at 1 kHz is compared to unpoled < 112 > grain-oriented ceramics while the remanent polarization (P-r similar to 19-1 mu cm(-2)) is compared with random grain-oriented ceramics. These results point out the viability to produce ferroelectric PMN-PT ceramics of very good quality using powder precursors prepared from this chemical method. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Low-density polyethylene (LDPE) was characterised for its dielectric and electrical properties before and after chemical treatment. A reduction in the permittivity and dielectric loss was observed in the polymer after treatment with hexane. The intensity in the Raman Spectrum in the disordered longitudinal acoustic mode region (DLAM) also was reduced due to a hexane treatment. Using thermally stimulated discharge current (TSDC) and laser-intensity-modulated method (LIMM) techniques it was observed that charge injection can be enhanced in the polymer matrix in the empty sites, created by the removal of the low molecular weight impurities with chemical treatment. (C) 2002 Kluwer Academic Publishers.
Resumo:
Thin films of blend made up of castor oil-based polyurethane (PU) and polyaniline (PANI) were obtained by casting. The molecular mobility was studied using dielectric spectroscopy and thermally stimulated depolarization current (TSDC) for blends with two different compositions (90/10, 80/20) and the results were compared with PU pure. The peak located around -60 degrees C in TSDC thermograms of PU/PANI blend has dipolar behavior and might be attributed to the change in the molecular chain due to the interaction between isocyanate and the solvent. Vogel-Fulcher Tammann fits was performed on the observed relaxation and the result shows a alpha-relaxation-like. (c) 2005 Springer Science + Business Media, Inc.
Resumo:
Non-isothermal dielectric analysis (DEA) and differential scanning calorimetry (DSC) techniques were used to study the epoxy nanocomposites prepared by reacting 1,3,5,7,9,11,13,15-octa[dimethylsiloxypropylglycidylether] pentaciclo [9.5.1.1(3,9).1(5,15).1(7,13)] octasilsesquioxane (ODPG) with methylenedianiline (MDA). Loss factor (epsilon) and activation energy were calculated by DEA. The relationships between the loss factor, the activation energy, the structure of the network, and the mechanical properties were investigated. Activation energies determined by DEA and DSC, heat of polymerization, fracture toughness and tensile modulus show the same profile for mechanical properties with respect to ODPG content.