Electrosynthesis methods using molten salts are suggested for obtaining a new catalytic system based on the Mo2C/Mo composition for the water gas shift reaction. The coatings obtained by the discharge of the carbonate ion on a molybdenum substrate and by the simultaneous reduction of the electroactive species MoO42 and CO32- are catalytically more active than bulk Mo2C or the commercial catalyst Cu-ZnO-Al2O3 by one and three orders of magnitude, respectively.
Resumo:
Highly crystalline zeolite Beta coatings in a range of Si/Al ratios of 12-23 were synthesized on a surface-modified molybdenum substrate by hydrothermal synthesis. The average thickness of the coatings was ca. 2 mu m corresponding to a coverage of 2.5 gm(-2). The coatings were obtained from a viscous Na, K, and TEAOH containing aluminosilicate precursor mixture with silica sol as reactive silicon source. A mechanism for the in situ growth of zeolite Beta coatings is proposed. According to this mechanism, the deposition of an amorphous gel layer on the substrate surface in the initial stage of the synthesis is an important step for the crystallization of continuous zeolite Beta coatings. The heating rate of the precursor mixture and the synthesis temperature were optimized to control the level of supersaturation and to stimulate the initial formation of a gel layer. At a Si/Al ratio of 23, fast heating and a temperature of 150 degrees C are required to obtain high coverage, while at a Si/Al ratio of 15, hydrothermal synthesis has to be performed with a slow initial heating rate at 140 degrees C. (c) 2007 Elsevier Inc. All rights reserved.
Resumo:
A method for the hydrothermal synthesis of a single layer of zeolite Beta crystals on a molybdenum substrate for microreactor applications has been developed. Before the hydrothermal synthesis, the surface of the substrate was modified by an etching procedure that increases the roughness at the nanoscale level without completely eliminating the surface lay structure. Then, thin films of Al2O3 (170 nm) and TiO2 (50 nm) were successively deposited by atomic layer deposition (ALD) on the substrate. The internal Al2O3 film protects the Mo substrate from oxidation up to 550 degrees C in an oxidative environment. The high wettability of the external TiO2 film after UV irradiation increases zeolite nucleation on its surface. The role of the metal precursor (TiCl4 vs TiI4), deposition temperature (300 vs 500 degrees C), and film thickness (50 vs 100 nm) was investigated to obtain titania films with the slowest decay in the superhydrophilic behavior after UV irradiation. Zeolite Beta coatings with a Si/Al ratio of 23 were grown at 140 degrees C for 48 It. After ion exchange with a 10(-4) M cobalt acetate solution, the activity of the coatings was determined in the ammoxidation of ethylene to acetonitrile in a microstructured reactor. A maximum reaction rate of 220 mu mol C2H3N g(-1) s(-1) was obtained at 500 degrees C, with 42% carbon selectivity to acetonitrile. (C) 2007 Elsevier Inc. All rights reserved.
Resumo:
A procedure has been developed to grow ZSM-5 crystals in situ on a molybdenum (Mo) support. The high heat conductivity (138 W/mK) and high mechanical stability at elevated temperatures of the Mo support allow the application of ZSM-5 coatings in micro reactors for high temperature processes involving large heat effects. The effect of the synthesis mixture composition on ZSM-5 coverage and on the uniformity of the ZSNI-5 coatings was investigated on plates of 10 X 10 mm(2). Ratios of H2O/Si = 50, SUAI = 25, and TPA/Al = 2.0 were found to be optimal for the formation of uniform coatings of 6 g/m(2) at a temperature of 150 degrees C and a synthesis time of 48 h. Scaling up of the synthesis procedure on 72 Mo plates of 40 x 9.8 x 0.1 mm 3 resulted in a uniform coverage of 14.8 +/- 0.4 g/m(2). The low deviation per individual plate (
Resumo:
The role of gaseous NO and C3H8 has been studied over low-exchanged Cu-ZSM-5 zeolite employing TPD, FTIR and pulse technique with the alternate introduction of NO or C3H8 onto the catalyst surface. The rate of the N-2 formation is directly proportional to the content of gaseous NO and the surface coverage with 2-nitrosopropane. There was no formation of N-2 during interaction of gaseous C3H8 with NO adsorbates. However, 2-nitrosopropane and its isomer acetone oxime were also formed in this reaction.
Resumo:
A surface intermediate with a C/N ratio close to 3 has been shown by TPD to form at co-adsorption of NO and propane as well as NO, propane and O-2 On low-exchanged Cu-ZSM-5. The adsorption of NO, propane and oxygen has been studied to evaluate their effect on the formation of this complex. Its formation is accompanied by a decrease in the concentration of surface nitrite-nitrate. The kinetics of nitrite-nitrate adspecies formation as a function of the reagents concentration and temperature has been investigated. Some NO adspecies have been found to decompose yielding N2O.
Resumo:
A simple UV-activated, TiO2-based film or ink for removing thin oxide or sulfide layers from metal surfaces by reductive photocatalysis is described.
Resumo:
The preparation and characterisation of a novel, UV-activated solvent-based, colourimetric indicator for O-2 is described, comprising a redox dye (methylene blue, MB), semiconductor photocatalyst (TiO2), and a sacrificial electron donor (SED), all dispersed/dissolved in a polymer medium (sulfonated polystyrene, SPS). Upon exposure, the indicator is readily photobleached as the MB is converted into its oxygen-sensitive, leuco form, LMB. Unlike its water-based counterpart, the recovery of the original colour is very slow (ca. 5 days cf. 6 min), probably due to the largely hydrophobic nature of the polymer encapsulation medium. The kinetics of film photobleaching appear to fit very well, in terms of: irradiance, [TiO2] and [MB], to the usual Langmuir-Hinshelwood type equation associated with a photocatalytic process. The glycerol appears not only to function as a SED, but also a plasticizer and medium for dye dissolution. The kinetics of colour recovery of the photobleached film appear directly dependent upon the ambient level of O-2 but shows a more complex dependence upon the relative humidity, RH. The photobleached film does not recover any of its colour over a 24 h period if the RH
Resumo:
The continuing interest in semiconductor photochemistry, SPC, and the emergence of commercial products that utilise films of photocatalyst materials, has created an urgent need to agree a set of methods for assessing photocatalytic activity and international committees are now meeting to address this issue. This article provides a brief overview of two of the most popular current methods employed by researchers for assessing SPC activity. and one which has been published just recently and might gain popularity in the future, given its ease of use. These tests are: the stearic acid (SA) test, the methylene blue (MB) test and the resazurin (Rz) ink test, respectively. The basic photochemical and chemical processes that underpin each of these tests are described, along with typical results for laboratory made sol-gel titania films and a commercial form of self-cleaning glass, Activ (TM). The pros and cons of their future use as possible standard assessment techniques are considered. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
The initial kinetics of the oxidation of 4-chlorophenol, 4-CP, photocatalyzed by titania films and aqueous dispersions were studied as a function of oxygen partial pressure, P-O2, and incident light intensity, I. The reaction conditions were such that the kinetics were independent of [4-CP] but strongly dependent on PO2-a situation that allowed investigation of the less-often studied kinetics of oxygen reduction. The observed kinetics fit a pseudo-steady-state model in which the oxygen is Langmuir-adsorbed on the titania photocatalyst particles before being reduced by photogenerated electrons. The maximum rate of photocatalysis depends directly on I-beta, where, beta = 1 for films and 0.7 for dispersions of titania, indicating that the kinetics are dominated by the surface reactions of the photogenerated electrons and holes for the films and by direct recombination for the powder dispersions. Using the pseudo-first-order model, for both titania films and dispersions, the apparent Langmuir adsorption constant, K-LH, derived from a Langmuir-Hinshelwood analysis of the kinetics, appears to be largely independent of incident light intensity, unlike KLH for 4-CP Consequently, similar values are obtained for the Langmuir adsorption constant, K-ads, extracted from a pseudosteady-state analysis of the kinetics for oxygen on TiO2 dispersions and films in aqueous solution (i.e., ca. 0.0265 +/- 0.005 kPa(-1)), and for both films and dispersions, oxygen appears to be weakly adsorbed on TiO2 compared with 4-CP, at a rate that would take many minutes to reach equilibrium. The value of Kads for oxygen on titania particles dispersed in solution is ca. 4.7 times lower than that reported for the dark Langmuir adsorption isotherm; possible causes for this difference are discussed. (c) 2006 Elsevier Inc. All rights reserved.
Resumo:
When TiO2 powder was irradiated with a laser light (>0.8 MW peak pulse power (PPP) at 355 nm) a visible change in its colour from white to dark blue was observed. The initial rate of change of the total colour difference was related to the laser light intensity and the longer the irradiation time the more substantial the colour change. The result of X-ray diffraction (XRD) studies showed that the crystal structure of the TiO2 developed a more rutile form after laser exposure. ESR studies indicated that the colour change was associated with the generation of Ti(III) species in the photocatalyst. Electron microscopic studies showed that more spherical shaped particles of TiO2 were observed after laser treatment although the average particle size remained largely unchanged. No significant changes in the band gap or the surface area of the laser modified TiO2 were observed. The laser modified photocatalyst showed no enhancement in activity for the destruction of methylene blue, rhodamine B and stearic acids, indicating that the rutile/anatase ratio is unimportant in the destruction of the test pollutants used in this work, via TiO2 photocatalysis
Resumo:
Selected Bronsted acidic ionic liquids were tested as homogeneous catalysts for the dehydration of methanol to dimethyl ether. Ionic liquids incorporating an alkanesulfonic acid as a part of the cation, a complex acidic anion, [A(2)H](-), or both, proved to be good catalysts for this process, providing high conversions and selectivities. Homogeneous catalysis in the liquid state represents a novel approach to dimethyl ether synthesis.
Resumo:
Usage of anticoagulant rodenticides (ARs) is an integral component of modern agriculture and is essential for the control of commensal rodent populations. However, the extensive deployment of ARs has led to widespread exposure of a range of non-target predatory birds and mammals to some compounds, in particular the second-generation anticoagulant rodenticides (SCARS). As a result, there has been considerable effort placed into devising voluntary best practice guidelines that increase the efficacy of rodent control and reduce the risk of non-target exposure. Currently, there is limited published information on actual practice amongst users or implementation of best practice. We assessed the behaviour of a typical group of users using an on-farm questionnaire survey. Most baited for rodents every year using SGARs. Most respondents were apparently aware of the risks of non-target exposure and adhered to some of the best practice recommendations but total compliance was rare. Our questionnaire revealed that users of first generation anticoagulant rodenticides rarely protected or checked bait stations, and so took little effort to prevent primary exposure of non-targets. Users almost never searched for and removed poisoned carcasses and many baited for prolonged periods or permanently. These factors are all likely to enhance the likelihood of primary and secondary exposure of non-target species. (C) 2010 Published by Elsevier Ltd.
Resumo:
In this article, we describe general trends to be expected at short times when an excess electron is generated or injected in different room-temperature ionic liquids (RTILs). Perhaps surprisingly, the excess electron does not localize systematically on the positively charged cations. Rather, the excess charge localization pattern is determined by the cation and anion HOMO/LUMO gaps and, more importantly, by their relative LUMO alignments. As revealed by experiments, the short-time (ps/ns) transient UV spectrum of excess electrons in RTILs is often characterized by two bands, a broad band at low energies (above 1000 nm) and another weaker band at higher energies (around 400 nm). Our calculations show that the dry or presolvated electron spectrum (fs) also has two similar features. The broad band at low energies is due to transitions between electronic states with similar character on ions of the same class but in different locations of the liquid. The lower-intensity band at higher energies is due to transitions in which the electron is promoted to electronic states of different character, in some cases on counterions. Depending on the chemical nature of the RTIL, and especially on the anions, excess electrons can localize on cations or anions. Our findings hint at possible design strategies for controlling electron localization, where electron transfer or transport across species can be facilitated or blocked depending on the alignment of the electronic levels of the individual species.