Nonlinear absorption and refraction phenomena in stoichiometric lithium niobate (SLN) pure and co-doped with Zn and Nd, and congruent lithium niobate (CLN) were investigated using Z-scan technique. Femtosecond laser pulses from Ti:Sapphire laser (800 nm, 110 fs pulse width and 1 kHz repetition rate) were utilized for the experiment. The process responsible for nonlinear behavior of the samples was identified to be three photon absorption (3PA). This is in agreement with the band gap energies of the samples obtained from the linear absorption cut off and the slope of the plot of Ln(1 − TOA) vs. Ln(I0) using Sutherland’s theory (s = 2.1, for 3PA). The nonlinear refractive index (n2) of Zn doped samples was found to be lower than that of pure samples. Our experiments show that there exists a correlation between the nonlinear properties and the stoichiometry of the samples. The values of n2 fall into the same range as those obtained for the materials of similar band gap.
Resumo:
A tunable DS-DBR laser is demonstrated for uncooled WDM C-band channel generation with tight spacing (SOGHz) and low thermal drift (±2.5GHz) up to 70°C. 2.5Gb/s direct modulation with transmission over a 75km link is achieved. © 2000 Optical Society of America.
Resumo:
研究在空气中使用1.06#mu#m YAG激光诱导放电打孔的方法。在不同的放电脉宽下进行激光诱导放电打孔的实验,比较了激光打孔和激光诱导放电打孔两种方法,指出了激光诱导放电打孔的优点。
Resumo:
实验研究了YAG激光诱导放电(LGD)表面离散强化形貌,包括强化点的表面形貌和横截面形貌.利用放电过程中的电弧压力,对强化点表面进行造型.大电流、倾斜放电容易将熔凝物吹起形成凹坑和突起,表面起伏更加明显,而小电流、垂直放电则能得到平坦的表面,有利于增大强化深度.随脉冲宽度的增加,强化点的径深比逐渐变小,在相同强化深度下,小电流、长脉冲宽度可以获得小径深比、厚深状的强化点,而大电流、短脉冲宽度可以获得大径深比、扁平状的强化点.在现有实验条件下,在电流150 A,脉冲宽度9.83 ms下得到最大强化深度为 0.479 mm,径深比为3.9
Resumo:
A Nd:glass regenerative amplifier has been set up to generate the pumping pulse with variable pulse width for an optical parametric chirped-pulse amplification (OPCPA) laser system. Each pulse of the pulse train from a cw self-mode-locking femtosecond Ti:sapphire oscillator is stretched to approximate to300 ps at 1062 nm to be split equally and injected into a nonlinear crystal and the Nd:glass regenerative amplifier, as the chirped signal pulse train and the seed pulse train of the pumping laser system, respectively. By adjusting the cavity length of the regenerative amplifier directly, the width of amplified pulse could be varied continuously from approximate to300 ps to approximate to3 ns. The chirped signal pulse for the OPCPA laser system and the seed pulse for the pumping laser system come from the same oscillator, so that the time jitter between the signal pulse and the pumping pulse in optical parametric amplification stages could be <10 ps. (C) 2003 Society of Photo-Optical Instrumentation Engineers.
Resumo:
We investigate the laser actions of 5at.% Yb:Gd2xY2(1-x)SiO5 (Yb:GYSO; x = 0.1) crystals with different cutting directions, parallel and vertical to the growth axis. Our results show that the cutting direction of the sample plays an astonished role in the laser operation. The sample cut vertically to the growth axis possesses the favourable lasing characteristics. Its output power reaches 3.13W at 1060nm with a slope efficiency of 44.68% when the absorbed pump power is 8.9 W. In contrast, the sample cut parallel reaches only 1.65 W at 1044 nm with a slope elLiciency of 33.76% with absorbed pump power of 7.99 W. The absorption and emission spectra of the two samples are examined and the merit factor M is calculated. Our analysis is in agreement well with the experimental results. The wavelength tuning range of the superior sample covers from 1013.68 nm to 1084.82 nm.
Resumo:
Fluorescence spectra of Nd: YVO4 under excitation of a continuous wave (CW) diode laser and a femtosecond laser at 800nm were investigated. It was found that Nd: YVO4 shows different upconversion and downconversion luminescencent behaviors when excited by the diode laser and the femtosecond laser. The dependence of the upconversion luminescence intensity on the pump power of the femtosecond laser was discussed. The populations of the upper energy levels for upconversion and downconversion luminescence were calculated based on the Bloch equations. The calculations agree well with the experimental results. (c) 2007 Optical Society of America.
Resumo:
20 at.% Yb:YAG single crystals have been grown by the CZ method and gamma-ray irradiation induced color centers and valence change of Fe3+ and Yb3+ ions in Yb:YAG have been studied. One significant 255 nm absorption band was observed in as-grown crystals and was attributed to Fe3+ ions. Two additional absorption (AA) bands located at 255 nm and 345 nm, respectively, were produced after gamma irradiation. The changes in the AA spectra after gamma irradiation and air annealing are mainly related to the charge exchange of the Fe3+, Fe2+, oxygen vacancies and F-type color centers. Analysis shows that the broad AA band is associated with Fe2+ ions and F-type color centers. The transition Yb3+ Yb2+ takes place as an effect of recharging of one of the Yb3+ ions from a pair in the process of gamma irradiation. (C) 2006 Elsevier Ltd. All rights reserved.
Resumo:
设计并实现了一种放大纳秒激光脉冲的高稳定的激光二极管(LD)抽运Nd∶YLF再生放大器。为了获得高稳定的输出,再生放大器工作在饱和状态。此时,再生放大器输出稳定性最好,而且注入激光脉冲能量波动引起的输出激光脉冲波动被抑制。由于增益饱和效应,再生放大器输出脉冲出现时域波形失真,附加后缀脉冲能够减弱时域波形失真。放大器工作波长1053nm,工作频率1Hz。输入240pJ的3ns方波激光脉冲,输出激光脉冲能量4.2mJ,总增益大于107,不稳定度小于1%(均方根),方波扭曲1.33。为3ns方波激光脉冲引入其本身幅度0.75倍的后缀脉冲,输出激光脉冲方波扭曲由1.33降至1.17。
Resumo:
We present the design and experimental results for a diode pumped Nd:YLF regenerative amplifier applied to amplify a nanosecond laser pulse. Numerical simulation shows that the maximum output energy and the best stability can be obtained when the regenerative amplifier operates in a saturated mode for all pulse duration and temporal profiles. Using extra post-pulse is a good method to decrease the square-pulse distortion caused by gain saturation effect. The amplifier shows output energy of 4.2mJ with a total energy gain of more than 107 and output energy stability of better than 1% rms. When extra post-pulse is added, square-pulse distortion is decreased from 1.33 to 1.17 for the amplifier that is seeded with an optical pulse of 3 ns.
Resumo:
We present a destructive method for detecting and measuring subsurface damage of Nd-doped phosphate glasses. An instrument based on the dimple method - a destructive method - was developed. Subsurface damage depth produced in each fabrication procedure was obtained. We extend the surface roughness-subsurface damage relation to Nd-doped phosphate glasses. The constant ratio of subsurface damage and surface roughness was obtained as well. We also analyse the relation of abrasive size and subsurface damage experimentally. From a measurement of the surface roughness or abrasive size, one can obtain an accurate estimate of the damage layer thickness that must be eliminated by polishing or subsequent grinding operations. (C) 2007 Elsevier GmbH. All rights reserved.
Resumo:
采用面泵浦的CAMIL结构,我们研究了970 nm泵浦的Yb:YAG/YAG复合陶瓷薄片激光器,获得了连续和调Q的激光输出。在连续运转情况下,获得了最高1.05 W的激光输出,中心波长为1031 nm,后腔输出镜透射率为2%。我们同时获得了声光调Q的脉冲输出,重复频率从1 kHz到30 kHz,脉宽分别从166 ns到700 ns。