967 resultados para Cladding of laser glass
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Objective: To evaluate the impact of the type of root canal preparation, intraradicular post and mechanical cycling on the fracture strength of roots. Material and Methods: Eighty human single rooted teeth were divided into 8 groups according to the instruments used for root canal preparation (manual or rotary instruments), the type of intraradicular post (fiber posts-FRC and cast post and core-CPC) and the use of mechanical cycling (MC) as follows: Manual and FRC; Manual, FRC and MC; Manual and CPC; Manual, CPC and MC; Rotary and FRC; Rotary, FRC and MC; Rotary and CPC; Rotary, CPC and MC. The filling was performed by lateral compactation. All root canals were prepared for a post with a 10 mm length, using the custom # 2 bur of the glass fiber post system. For mechanical cycling, the protocol was applied as follows: an angle of incidence of 45 degrees, 37 degrees C, 88 N, 4 Hz, 2 million pulses. All groups were submitted to fracture strength test in a 45 degrees device with 1 mm/min cross-head speed until failure occurred. Results: The 3-way ANOVA showed that the root canal preparation strategy (p<0.03) and post type (p<0.0001) affected the fracture strength results, while mechanical cycling (p=0.29) did not. Conclusion: The root canal preparation strategy only influenced the root fracture strength when restoring with a fiber post and mechanical cycling, so it does not seem to be an important factor in this scenario.
Resumo:
Pós-graduação em Engenharia Mecânica - FEIS
Resumo:
Pós-graduação em Odontologia Restauradora - ICT
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Candida albicans is classified into different serotypes according to cell wall mannan composition and cell surface hydrophobicity. Since the effectiveness of photodynamic therapy (PDT) depends on the cell wall structure of microorganisms, the objective of this study was to compare the sensitivity of in vitro biofilms of C. albicans serotypes A and B to antimicrobial PDT. Reference strains of C. albicans serotype A (ATCC 36801) and serotype B (ATCC 36802) were used for the assays. A gallium-aluminum-arsenide laser (660 nm) was used as the light source and methylene blue (300 mu M) as the photosensitizer. After biofilm formation on the bottom of a 96-well microplate for 48 h, each Candida strain was submitted to assays: PDT consisting of laser and photosensitizer application (L + P+), laser application alone (L + P-), photosensitizer application alone (L-P+), and application of saline as control (L-P-). After treatment, biofilm cells were scraped off and transferred to tubes containing PBS. The content of the tubes was homogenized, diluted, and seeded onto Sabouraud agar plates to determine the number of colony-forming units (CFU/mL). The results were compared by analysis of variance and Tukey test (p < 0.05). The two strains studied were sensitive to PDT (L + P+), with a log reduction of 0.49 for serotype A and of 2.34 for serotype B. Laser application alone only reduced serotype B cells (0.53 log), and the use of the photosensitizer alone had no effect on the strains tested. It can be concluded that in vitro biofilms of C. albicans serotype B were more sensitive to PDT.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Thin films of GeAsS glass are prepared by e-beam evaporation technique. Photoinduced birefringence (PIB) is studied as function of the As content with concentrations ranging from 10% to 40%. Raman spectroscopy is used as additional tool to explain the corresponding changes undergone by the material system. The breakdown of homopolar bonds is suggested as a possible mechanism of photo induced structural changes leading to the creation of the PIB.
Resumo:
Ideally projected to be applied on soft tissues, infrared lasers were improved by restorative dentistry to be used in hard dental tissues cavity preparations-namely enamel and dentin. This paper evidentiates the relevant aspects of infrared Erbium laser's action mechanism and its effects, and characterizes the different effects deriving from the laser's beams emission. The criteria for use and selection of optimal parameters for the correct application of laser systems and infuence of supporting factors on the process, such as water amount and its presence in the ablation process, protection exerted by the plasma shielding and structural factors, which are indispensable in dental tissues cavity preparation related to restorative technique, are subordinated to optical modifcations caused by the interaction of the energy dissipated by these laser light emission systems in the targeted tissue substrate. Clinical relevance: Differences in the action of infrared Erbium laser system in regard to the nature of the ablation process and variations on the morphological aspects observed in the super-fcial structure of the target tissue irradiated, may be correlated to the structural optical modifcations of the substrate produced by an interaction of the energy propagated by laser systems.
Resumo:
The present study evaluated the radiopacity and flow of different endodontic sealers: AH Plus, Endo CPM, MTA Fillapex, Sealapex, Epiphany, and Epiphany SE. For the radiopacity test, six specimens measuring 10mm in diameter and 1mm in thickness were fabricated from each material. They were radiographed on an occlusal film alongside an aluminum step wedge. Radiographs were digitized to determine the radiopacity equivalence in millimeters of aluminum. To evaluate the flow, a 120 g load was placed on top of a glass slab containing 0.05 } 0.005ml of sealer. The diameters of each material were measured (mm) with a caliper and samples were photographed. Digitized images were analyzed using the UTHSCSA Image Tool for Windows software, to determine the sealer area (mm2). Data were submitted to ANOVA and Tukey's test at 5% significance. AH Plus and Epiphany SE presented the greatest radiopacity (12.5 mm Al and 12.0 mm Al, respectively) (p>0.05), followed by Epiphany (9.6 mm Al) and Fillapex (8.9 mm Al). Endo CPM (5.46 mm Al) and Sealapex (5.51 mm Al) presented lower radiopacity. MTA Fillapex presented significantly higher values of flow than other sealers (33.11 mm and 844.9 mm2). AH Plus, Epiphany, and Epiphany SE had similar values. Endo CPM (21.05 mm and 342.8 mm2) and Sealapex (19.98 mm and 352.5 mm2) presented the lowest flow values (p>0.05). All sealers presented radiopacity and flow values according to ISO and ANSI/ADA recommendations.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)