981 resultados para stress effects in superconducting thin films
Resumo:
Lead lanthanum zirconate titanate (PLZT) thin films with (9/65/35) stoichiometry were prepared by dip coating from polymeric precursor method. The films deposited on silicon (100) substrates, were thermally treated from 450° to 700°C for 6 hours in order to study the influence of thermal treatment on the crystallinity, microstructure, grain size and roughness of the final film. X-ray diffraction results showed that PLZT phase crystallizes at low temperature (500°C) and present preferential orientation. It was observed by scanning electron microscopy (SEM) that it is possible to obtain dense thin films at temperatures around 650°C. The atomic force microscopy (AFM) studies showed that the grain size and roughness are strongly influenced by the annealing temperature.
Resumo:
Ferroelectric SrBi2Nb2O9 (SBN) thin films were prepared by pulsed laser deposition (PLD) on Pt/Ti/SiO2/Si(100) using a sequential deposition process from two SBN and Bi2O3 targets. This route allows for bismuth enrichment of the film composition in order to improve the ferroelectric characteristics. Structural and microstructural characterizations were performed by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The composition of films and targets was determined by energy dispersive X-ray spectrometry (EDX). The deposition temperature, which provided well-crystallized layered perovskite SBN phase films in situ, was found to be 700°C. The results were compared with those obtained for SBN films deposited at 400°C and then crystallized ex situ. For an ex situ annealing temperature of 750°C, a remanent polarization value (Pr) of 23.2 μc/cm2 and a coercive field (Ec) of 112 kV/cm were measured. © 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
Strontium barium niobate (SBN) thin films were crystallized by conventional electric furnace annealing and by rapid-thermal annealing (RTA) at different temperatures. The average grain size of films was 70 nm and thickness around 500 nm. Using x-ray diffraction, we identified the presence of polycrystalline SBN phase for films annealed from 500 to 700 °C in both cases. Phases such as SrNb2O6 and BaNb2O6 were predominantly crystallized in films annealed at 500 °C, disappearing at higher temperatures. Dielectric and ferroelectric parameters obtained from films crystallized by conventional furnace and RTA presented essentially the same values.
Resumo:
Recently, was proposed a chemical method for preparation of ferroelectric thin films based on oxide precursors. In this work, PZT thin films were prepared to attest the viability of this method for cation-substitution. In this study, a small concentration of Nb (5 mol%) was selected as substitute of B-site in ABO 3 structure of PZT. Dielectric and ferroelectric properties of PZT films were studied as a function of cation-substitution. Results for Nb-PZT were compared with PZT films undoped. The values of dielectric constant, at typical 100 kHz frequency, were 358 and 137, for PZT and Nb-PZT films respectively. Remanent polarizations of these films were respectively 7.33 μ C/cm 2 and 13.3 μ C/cm 2 , while the measured coercive fields were 101 kV/cm and 93 kV/cm. As a result, changes on observed dielectric and ferroelectric values confirm the Nb substitution in PZT thin film produced by oxide precursor method. © 2002 Taylor & Francis.
Resumo:
The effect of magnesium addition on the phase formation, microstructure and electric and ferroelectric properties of LiNbO 3 thin films prepared through polymeric precursors was analyzed. By X ray diffraction no secondary phase was observed with the increase of magnesium concentration. Comparing to pure LiNbO 3, the addition of 0.5 and 1.0 mol% of Mg +2 increased of the dielectric constant, while 2.0 mol% decreased it. It was noticed that the increase in additive concentration decreases the ferroelectric remanent polarization and increases the coercive field. © 2002 Taylor & Francis.
Resumo:
Strontium-modified lead titanate thin films with composition Pb1-xSrxTiO3 were grown on Pt/Ti/SiO2/Si substrates using the polymeric precursor method. The structural phase evolution as a function of the Sr contents was studied using micro-Raman scattering, specular reflectance infrared Fourier transform spectroscopy, and x-ray diffraction. The results showed a gradual change from tetragonal to cubic structure, the transition occurring at about x = 0.58. The infrared reflectance spectra showed that the frequency of several peaks decreases as the strontium concentration increases. These features are correlated with a decrease in the tetragonal distortion of the TiO6 octahedra as the strontium concentration increases.
Resumo:
Lead zirconate titanate (PZT) solutions were prepared using a polymeric precursor method, Zr n-propoxide and Ti i-propoxide were used as starting materials with ethylene glycol and water as solvents. The PZT solution was spin-coated on Pt/Ti/SiO2/Si substrates, baked on a hot plate, and finally heat-treated in a tube furnace between 400 and 800°C. The surface morphology and grain size of the films were characterized by atomic force microscopy (AFM), using a tapping mode with amplitude modulation. The films, thermal annealed at temperatures higher than 500°C, exhibited a dense microstructure, without noticeable cracks or voids. Electrical properties were investigated as a function of composition and annealing temperature.
Resumo:
Thin films of lithium niobate were deposited on the Pt/Ti/SiO2 (111) substrates by the polymeric precursor method (Pechini process). Annealing in static air and oxygen atmosphere was performed at 500°C for 3 hours. The films obtained were characterized by X-ray diffraction, scanning electron microscopy and transmission electron microscopy. The dielectric constant, dissipation factor and resistance were measured in frequency region from 10 Hz to 10 MHz. Electrical characterizations of the films pointed to ferroelectricity via hysteresis loop. The influence of oxygen atmosphere on crystallization and properties of LiNbO3 thin films is discussed.
Resumo:
It is very important for the building of the SAW devices to study dielectric and ferroelectrics properties because every SAW device is based in piezoelectric effect that it is made up to transform an electric sign in the mechanical or acoustic sign and a mechanical or acoustic sign in an electric sign. Thus, the purpose of the present work is to prepare PbZr 0,53Ti0.47O3 (PZT) and PbTiO3 (PT) thin films on the Si (100) substrates across spin-coating using a chemical method based in polymeric precursors. After conventional treatment in the furnace, the films were characterized by impedance spectroscopy and hysteresis loops to know its dielectric and ferroelectric properties.
Resumo:
Since the discovery of the high Tc superconductors, several works have been made about the different properties of these materials. Anelastic spectroscopy experiments are sensitive tools to the study of defects in solids and phase transitions. By this technique, we can distinguish the different types of atomic jumps that happen to different temperatures. The intensity of the peaks in the anelastic spectrum and the step in the torsional modulus are related with the concentration of the relaxing entities, and the position of the peaks is determined by its mobility. In this paper, the study on Bi and Sm based superconducting oxides was made by anelastic relaxation measurements using a torsion pendulum. The samples were submitted to successive thermal treatments in high vacuum, in the temperature range between 100 K and 650 K, heating rate about 1 K/min. For Bi based superconducting oxides the results shown two peaks, that were associated to interstitial oxygen mobility and to orthorhombic to monoclinic phase transition. For Sm based superconducting oxides the results shown a relaxation peak that was attributed to the jumps of the oxygen atoms in the inter-chains O1 and 05 of the lattice.
Resumo:
This study verified the effects of CaSO4 on physiological responses of the tropical fish matrinxãBrycon amazonicus(200.2 ± 51.1 g) in water containing CaSO4 after a 4-h transportation at concentrations of: 0, 75, 150, and 300 mg L-1. Blood samples were collected prior to transportation (initial levels), immediately after packaging, at arrival, and 24 h and 96 h after transportation (recovery). Cortisol levels increased after ackaging (118.2 ± 14.2 ng ml-1), and decreased slightly after transportation in water containing CaSO4 (106.8 ± 14.1), but remained higher than initial levels (21.0 ± 2.6 ng ml)1). Fish kept at 150 mg L-1 CaSO4 reached the pre-transportation levels at 24 h of recovery. Blood glucose increased after transportation in all treatments (8.2 ± 0.2 mmol L-1) and declined after full recovery to values below initial levels (4.8 ± 0.1 mmol L-1). Chloride levels did not change in CaSO4 treatments; serum sodium concentrations decreased after packaging and after transportation. Serum calcium levels did not differ among treatments, but decreased after packaging and increased at 96 h of recovery. Hematocrit and the number of red blood cells were higher in all treatments after packaging and arrival, except in fish exposed to 300 mg L-1 CaSO4. Mean corpuscular volume increased in 75 mg L-1 CaSO4, which reached the higher VCM after transportation. Hemoglobin levels increased only after transportation, regardless of calcium sulfate levels. Handling before transportation and transportation itself were both stressful to fish; calcium sulfate at concentrations tested in the present work had a moderate influence in the reduction of stress responses. © 2009 Blackwell Verlag, Berlin.
Resumo:
We present a study on the thin film morphology and the optical properties of eumelanin resulting from different synthesis routes: the oxidation of tyrosine with hydrogen peroxide, the auto-oxidation of dihydroxyphenylanaline in water and its auto-oxidation in dimethyl sulfoxid. Atomic Force Microscopy images indicate that the presence of holes and particles depends on the eumelanin synthesis route and the substrate employed. Smooth films with very few defects could be obtained with eumelanin synthesized in dimethyl sulfoxide deposited on glass substrates. Our study shows that all eumelanin preparations are comparable in terms of thin film morphology on the submicrometer scale and UV-visible transmission properties. ©The Electrochemical Society.
Resumo:
Lead zirconate titanate Pb(Zr 0.50Ti 0.50)O 3 (PZT) thin films were deposited by a polymeric chemical method on Pt(111)/Ti/SiO2/Si substrates to understand the mechanisms of phase transformations and the effect of film thickness on the structure, dielectric and piezoelectric properties in these films. PZT films pyrolyzed at temperatures higher than 350 °C present a coexistence of pyrochlore and perovskite phases, while only perovskite phase grows in films pyrolyzed at temperatures lower than 300 °C. For pyrochlore-free PZT thin films, a small (100) orientation tendency near the film-substrate interface was observed. Finally, we demonstrate the existence of a self-polarization effect in the studied PZT thin films. Results suggest that Schottky barriers and/or mechanical coupling near the filmsubstrate interface are not primarily responsible for the observed self-polarization effect in our films. © 2012 IEEE.
Resumo:
The influence of benzoyl peroxide (BPO) on the synthesis of polysiloxane thin films doped with Ce(III) deposited onto Sn coated steel as well as their anticorrosion properties are reported. The addition of BPO, whose role is polymerize the film, showed an increase in |Z| values due to the fact that augments the crossed link bonds and therefore improves the protective feature of the film. Ce(III) does not act in the polymerization process and thus is essential the addition of BPO to obtain more resistant polysiloxane films. ©The Electrochemical Society.
Resumo:
Fabrication and optical characterization of Tm3+/Yb3+ codoped PbO-GeO2 (PGO) pedestal-type waveguides are investigated in this work. It is important to mention that, to the best of authors' knowledge, the use of PGO pedestal-type waveguide has not been studied before. PGO thin films codoped with Tm3+ and Yb3+ were obtained through RF magnetron sputtering technique. The pedestal profile was obtained using conventional optical lithography procedures, followed by plasma etching and sputtering deposition. The profile of Tm3+/Yb3+ codoped PGO waveguides was observed by means of Scanning Electron Microscopy (SEM) measurements. Also the infrared and infrared-to-visible frequency upconversion luminescences of Tm3+ ions were measured exciting the samples with a cw 980 nm diode laser. Propagation losses around 11 dB/cm and 9 dB/cm were obtained at 630 and 1050 nm, respectively, for waveguides in the 20-100 μm width range. Single-mode propagation was observed for waveguides width up to 12 μm and 7 μm, at 1050 nm and 630 nm, respectively; larger waveguides width provided multi-mode propagation. The present results corroborate the possibility of using Tm3+/Yb3+ codoped PGO thin films as active waveguide for photonic applications. © 2013 Elsevier B.V. All rights reserved.