961 resultados para Beckman Coulter Laser diffraction particle size analyzer LS 200


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Formation of bumps in chalcogenide phase change thin films during the laser writing process is theoretically and experimentally investigated. The process involves basically fast heating and quenching stages. Circular bumps are formed after cooling, and the shape and size of the bumps depend on various parameters such as temperatures, laser power, beam size, laser pulse duration, etc. In extreme cases, holes are formed at the apex of the bumps. To understand the bumps and their formation is of great interest for data storage. In the present work, a theoretical model is established for the formation process, and the geometric characters of the formed bumps can be analytically and quantitatively evaluated from various parameters involved in the formation. Simulations based on the analytic solution are carried out taking Ag8In14Sb55Te23 as an example. The results are verified with experimental observations of the bumps. (C) 2008 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

研制成功便携式激光尘埃粒子计数器的核心部件——微型光学传感器。该传感器采用直角散射光收集形式。以高功率半导体激光器作为光源,同时采用高性能的PIN型光电二极管作为光电探测器。散射光收集系统为单一大数值孔径的球面反射镜,其对粒子散射光的收集角范围从20°到160°。粒子散射光信号是脉冲信号,其频谱成份主要在高频段,所以在PIN型光电二极管后用一个带通式前置放大器来消除外界的低频噪声.根据米氏散射理论计算了该光学传感器的光散射响应特性,并用聚苯乙烯标准粒子实测了该光学传感器的性能。结果表明,该系统具有高的信噪

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Esta Dissertação discorre sobre a pesquisa de caracterização de palha de milho e a sua utilização como matéria prima para a obtenção de nanocelulose. Segundo o IBGE, este resíduo agrícola foi produzido no Brasil, no ano de 2013, em cerca de seis milhões de toneladas. As amostras deste resíduo lignocelulósico utilizadas neste trabalho foram coletadas na forma cotidiana de descarte mais frequentemente encontrada em supermercados e feiras livres. Procedeu-se, então, ao beneficiamento mecânico, beneficiamento químico (mercerização e branqueamento) e hidrólise ácida dessas amostras, o que produziu os seguintes materiais: palha de milho beneficiada mecanicamente, palha de milho beneficiada quimicamente e nanocelulose. Cada um destes materiais foi caracterizado, conforme o tipo, por menos ou mais dos seguintes ensaios: determinação de densidade, determinação de umidade, determinação do teor de cinzas, resistência à tração, determinação do teor de extraíveis, determinação do teor de holocelulose, determinação do teor de hemicelulose, determinação do teor de alfacelulose, determinação do teor de lignina, análise termogravimétrica (TGA), espectroscopia por infravermelho por transformada de Fourier (FTIR), índice de cristalinidade por difração de raios-x (CrI), medição do tamanho de partícula por espalhamento de luz dinâmico (DLS), morfologia por microscopia eletrônica de varredura (SEM) e determinação do rendimento dos produtos de hidrólise. Nesta pesquisa também se estudou, empregando a técnica de planejamento de experimento fatorial com ponto central, a influência dos fatores razão fibra/ácido e tempo da reação na obtenção da nanocelulose, conseguida com êxito em todos os experimentos executados com a palha de milho que foi branqueada de forma efetiva neste trabalho

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The influence of particle shape on the stress-strain response of fine silica sand is investigated experimentally. Two sands from the same source and with the same particle size distribution were examined using Fourier descriptor analysis for particle shape. Their grains were, on average, found to have similar angularity but different elongation. During triaxial stress path testing, the stress-strain behavior of the sands for both loading and creep stages were found to be influenced by particle elongation. In particular, the behavior of the sand with less elongated grains was more like that of rounded glass beads during creep. The results highlight the role of particle shape in stress transmission in granular packings and suggest that shape should be taken more rigorously into consideration in characterizing geomaterials. © 2005 Taylor & Francis Group.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Granular reactive materials have higher permeability and are therefore desirable for in situ groundwater pollution control. Three granular bentonites were prepared: an Al-pillared bentonite (PBg), an organo-bentonite (OBg) using a quaternary ammonium cation (QAC), and an inorgano-organo-bentonite (IOBg), using both the pillaring agent and the QAC. Powdered IOB (IOBp) was also prepared to test the effect of particle size. The modified bentonites were characterised with X-ray diffraction (XRD), Fourier transform infrared spectrometry (FT-IR), thermal gravimetric analysis (TGA) and uniaxial compression tests. The d-spacing increased only with QAC intercalation. The Young's modulus of IOBg was twice as high as OBg. Batch adsorption tests were performed with aqueous multimetal solutions of Pb2+, Cu2+, Cd2+, Zn2+ and Ni2+ ions, with liquid dodecane and with aqueous dodecane solutions. Metal adsorption fit the Langmuir isotherm. Adsorption occurred within 30min for PBg, while the granular organo-bentonite needed at least 12h to reach equilibrium. IOBp had the maximum adsorption capacity at higher metal concentration and lower adsorbent content (Cu2+: 2.2, Ni2+: 1.7, Zn2+: 1.4, Cd2+: 0.9 and Pb2+: 0.7 all in mmolg-1). The dual pillaring of the QAC and Al hydroxide increased the adsorption. The adsorption of liquid dodecane was in the order IOBg>OBg>PBg (3.2>2.7>1.7mmolg-1). Therefore IOBg has potential for the removal of toxic compounds found in soil, groundwater, storm water and wastewater. © 2012 Elsevier B.V.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

© 2014 AIP Publishing LLC. Superparamagnetic nanoparticles are employed in a broad range of applications that demand detailed magnetic characterization for superior performance, e.g., in drug delivery or cancer treatment. Magnetic hysteresis measurements provide information on saturation magnetization and coercive force for bulk material but can be equivocal for particles having a broad size distribution. Here, first-order reversal curves (FORCs) are used to evaluate the effective magnetic particle size and interaction between equally sized magnetic iron oxide (Fe2O3) nanoparticles with three different morphologies: (i) pure Fe2O3, (ii) Janus-like, and (iii) core/shell Fe2O3/SiO2synthesized using flame technology. By characterizing the distribution in coercive force and interaction field from the FORC diagrams, we find that the presence of SiO2in the core/shell structures significantly reduces the average coercive force in comparison to the Janus-like Fe2O3/SiO2and pure Fe2O3particles. This is attributed to the reduction in the dipolar interaction between particles, which in turn reduces the effective magnetic particle size. Hence, FORC analysis allows for a finer distinction between equally sized Fe2O3particles with similar magnetic hysteresis curves that can significantly influence the final nanoparticle performance.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Large-scale synthesis of high-quality GaN nano-crystallites has been achieved by direct reaction of a 4:1 molar Ga/Ga2O3 mixture with ammonia at 950degreesC. X-ray diffraction, transmission electron microscopy, selected-area electron diffraction and high-resolution transmission electron microscopy revealed that the produced GaN nanocrystallites were single hexagonal wurtzite structure with an average particle size around 45 nm. A sharp near band edge emission peak and a blue light emission peak were observed in photoluminescence spectroscopy. The synthesis approach is simple and easy to be commercialized.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Structural and magnetic characteristics of Fe3-xSnxO4 (x < 0.3) nanoparticles synthesized using the precipitation exchange method have been investigated by X-ray diffraction, transmission electron microscope, Mossbauer spectra, X-ray photoelectron spectroscopy and magnetization measurement. The mean particle dimension decreases from 8 to 6 nm, the lattice parameters enlarge, the saturation magnetization decreases, as well as the magnetization and the coercive field increase, with increasing tin-content. The paramagnetic property of the specimens indicates that the replacement of Fe3+ by Sn4+ on the octahedral sites of Fe3O4 causes a progressive lowering of the Curie temperature and the Curie temperatures of the materials are all lower than that of crystallite tin-doped magnetite. This striking debasing is due to the lessening of the grain size. This is the smallest size reported thus far for paramagnetic tin-doped magnetite particles. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnO nanoparticles were synthesized in ethanolic solution using a sol-gel method. The structural and optical properties were investigated by X-ray diffraction, transmission electron microscopy, UV absorption, and photoluminescence. After annealing at 200 degrees C, the particle size is increased and the peak of defect luminescence in the visible region is changed. A yellow emission was observed in the as-prepared sample and a green emission in the annealed sample. The change of the visible emission is related to oxygen defects. Annealing in the absence of oxygen would increase oxygen vacancies. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnO nanoparticles were synthesized in ethanolic solution using a sol-gel method. The structural and optical properties were investigated by X-ray diffraction, transmission electron microscopy, UV absorption, and photoluminescence. After annealing at 200 degrees C, the particle size is increased and the peak of defect luminescence in the visible region is changed. A yellow emission was observed in the as-prepared sample and a green emission in the annealed sample. The change of the visible emission is related to oxygen defects. Annealing in the absence of oxygen would increase oxygen vacancies. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

An experimental study on ignition and combustion of single particles was conducted at normal gravity (1-g) and microgravity (l-g) for three high volatile coals with initial diameter of 1.5 and 2.0 mm, respectively. The non-intrusive twin-color pyrometry method was used to retrieve the surface temperature of the coal particle through processing the images taken by a color CCD camera. At the same time, a mathematical model considering thermal conduction inside the coal particle was developed to simulate the ignition process. Both experiments and modeling found that ignition occurred homogeneously at the beginning and then heterogeneously for the testing coal particles burning at l-g. Experimental results confirmed that ignition temperature decreased with increasing volatile content and increasing particle size. However, contradicted to previous studies, this study found that for a given coal with certain particle size, ignition temperature was about 50–80 K lower at l-g than that at 1-g. The model predictions agreed well with the l-g experimental data on ignition temperature. The criterion that the temperature gradient in the space away from the particle surface equaled to zero was validated to determine the commence of homogeneous ignition. Thermal conduction inside the particle could have a noticeable effect for determining the ignition temperature. With the consideration of thermal conduction, the critical size for the phase transient from homogeneous to heterogeneous is about 700 lm at ambient temperature 1500 K and oxygen concentration 0.23. 2009 The Combustion Institute. Published by Elsevier Inc. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Magnetic nanoparticles of nickel ferrite (NiFe2O4) have been synthesized by co-precipitation route using stable ferric and nickel salts with sodium hydroxide as the precipitating agent and oleic acid as the surfactant. X-ray diffraction (XRD) and transmission electron microscope (TEM) analyses confirmed the formation of single-phase nickel ferrite nanoparticles in the range 8-28 nm depending upon the annealing temperature of the samples during the synthesis. The size of the particles (d) was observed to be increasing linearly with annealing temperature of the sample while the coercivity with particle size goes through a maximum, peaking at similar to 11 nm and then decreases for larger particles. Typical blocking effects were observed below similar to 225 K for all the prepared samples. The superparamagnetic blocking temperature (T-B) was found to be increasing with increasing particle size that has been attributed to the increased effective anisotropy energy of the nanoparticles. The saturation moment of all the samples was found much below the bulk value of nickel ferrite that has been attributed to the disordered surface spins or dead/inert layer in these nanoparticles. (c) 2008 Elsevier B. V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The electrocatalysts of Pt/C, PtRu/C and Ru/C were prepared by the impregnation method. The facet characterization, the dispersion and the particle size for the catalysts were determined by means of X-ray diffraction and transmission electron microscopy. X-ray photoelectron spectroscopy was also used to analyze the state and the valency of the noble metals. The results show that the particle size was in nanometer range and the binary metals have come into being an alloy. The platinum in the catalysts existed in zero valency. The valency of the ruthenium on the surface is different from that in the body, while the ruthenium on the surface existed in oxide-form. PtRu/C and Pt/C are of good activity to the electrooxidation of hydrogen except Ru/C. PtRu/C is more tolerant of CO than Pt/C, and CO is only adsorbed on Pt.