Resumo:
The wetting behavior of rhamnolipids produced by Pseudomonas aeruginosa LBI strain grown on waste oil substrate and sodium dodecyl sulfate (SDS) on glass, polyethylene terephthalate (PET), poly(vinyl chloride) (PVC), poly(epsilon-caprolactone) (PCL) and polymer blend (PVC-PCL) was investigated by the measuring contact angle of sessile drops, to determine the wetting characteristics of rhamnolipids. The comparison of the wetting profiles showed that at low SDS and rhamnolipid concentrations, the contact angle increased and when the concentration of the surfactant increased further, the contact angle decreased. The blend surface (PVC-PCL) showed better wettability than the homopolymers themselves and the blend changed the surface hydrophobicity of the polymer, making it more hydrophilic. The rhamnolipids produced by the LBI strain exhibited superior wetting abilities than the chemical surfactant SDS one. This is the first work that evaluates the wetting properties of rhamnolipids on polymer blends.
Resumo:
It is analyzed through the concepts of tribology and mechanical contact and damage the suggestion of implementing a backup system for traction and passage of Pipeline Inspection Gauge (Pig) from the inside of pipelines. In order to verify the integrity of the pipelines, it is suggested the possibility of displacement of such equipment by pulling wires with steel wires. The physical and mechanical characteristics of this method were verified by accelerated tests in the laboratory in a tribological pair, wire versus a curve 90. It also considered the main mechanisms of wear of a sliding system with and without lubricant, in the absence and presence of contaminants. To try this, It was constructed a test bench able to reproduce a slip system, work on mode back-and-forth ("reciprocation"). It was used two kinds of wires, a galvanized steel and other stainless steel and the results achieved using the two kinds of steel cables were compared. For result comparative means, it was used steel cables with and without coating of Poly Vinyl Chloride (PVC). The wires and the curves of the products were characterized using metallographic analysis, microhardness Vickers tests, X-ray diffraction (XRD), X-Ray Refraction (XRF) and tensile tests. After the experiments were analyzed some parameters that have been measurable, it demonstrates to the impracticality of this proposed method, since the friction force and the concept of alternating request at the contact between the strands of wire and the inner curves that are part ducts caused severe wear. These types of wear are likely to cause possible failures in future products and cause fluid leaks
Resumo:
The underground natural gas found associated or not with oil is characterized by a mixture of hydrocarbons and residual components such as carbon dioxide (CO2), nitrogen gas (N2) and hydrogen sulfide (H2S), called contaminants. The H2S especially promotes itself as a contaminant of natural gas to be associated with corrosion of pipelines, to human toxicity and final applications of Natural Gas (NG). The sulfur present in the GN must be fully or partially removed in order to meet the market specifications, security, transport or further processing. There are distinct and varied methods of desulfurization of natural gas processing units used in Natural Gas (UPGN). In order to solve these problems have for example the caustic washing, absorption, the use of membranes and adsorption processes is costly and great expenditure of energy. Arises on such findings, the need for research to active processes of economic feasibility and efficiency. This work promoted the study of the adsorption of sulfide gas in polymer matrices hydrogen pure and modified. The substrates of Poly(vinyl chloride) (PVC), poly(methyl methacrylate) (PMMA) and sodium alginate (NaALG) were coated with vanadyl phosphate compounds (VOPO4.2H2O), vanadium pentoxide (V2O5), rhodamine B (C28H31N2O3Cl) and ions Co2+ and Cu2+, aiming to the adsorption of hydrogen sulfide gas (H2S). The adsorption tests were through a continuous flow of H2S in a column system (fixed bed reactor) adsorption on a laboratory scale. The techniques used to characterize the adsorbents were Infrared spectroscopy (FTIR), thermogravimetry analysis (TGA), X-ray fluorescence (XRF), the X-ray diffraction (XRD) electron microscopy (SEM). Such work indicates, the results obtained, the adsorbents modified PMMA, PVC and NaALG have a significant adsorptive capacity. The matrix that stood out and had the best adsorption capacity, was to ALG modified Co2+ with a score of 12.79 mg H2S / g matrix
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
HDPE and PVC geomembranes are sensitive to changes in their properties when in contact with high temperatures. The effects of hot temperature on polymeric geomembranes are assessed by the ASTM D794 and ASTM D5721.This paper brings an analysis of degradation of the Poly Vinyl Chloride (PVC) and High Density Poly Ethylene (HDPE) geomembranes when exposed to conventional and air oven after specific periods.. Mechanical and physical properties were evaluated. OIT tests were also performanced to evaluate the level of oxidation degradation occurred on the HDPE geomembranes. Geomembranes of two thicknesses were tested: 1.0, 2.0 nun (PVC) and 0.8, 2.5 mm, (HDPE). The results obtained show, for example, that after the last period of exposure, the PVC geomembranes (1.0, 2.0 mm) were more rigid and stiffer than fresh samples. The HDPE geomembranes, on the other hand, when exposed to heat presented increases in deformation. OIT tests showed efficient to detect some level of degradation on the HDPE geomembranes.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
This paper shows in detail the modelling of anisotropic polymeric foam under compression and tension loadings, including discussions on isotropic material models and the entire procedure to calibrate the parameters involved. First, specimens of poly(vinyl chloride) (PVC) foam were investigated through experimental analyses in order to understand the mechanical behavior of this anisotropic material. Then, isotropic material models available in the commercial software Abaqus (TM) were investigated in order to verify their ability to model anisotropic foams and how the parameters involved can influence the results. Due to anisotropy, it is possible to obtain different values for the same parameter in the calibration process. The obtained set of parameters are used to calibrate the model according to the application of the structure. The models investigated showed minor and major limitations to simulate the mechanical behavior of anisotropic PVC foams under compression, tension and multi-axial loadings. Results show that the calibration process and the choice of the material model applied to the polymeric foam can provide good quantitative results and save project time. Results also indicate what kind and order of error one will get if certain choices are made throughout the modelling process. Finally, even though the developed calibration procedure is applied to specific PVC foam, it still outlines a very broad drill to analyze other anisotropic cellular materials.
Resumo:
This paper emphasizes the influence of micro mechanisms of failure of a cellular material on its phenomenological response. Most of the applications of cellular materials comprise a compression loading. Thus, the study focuses on the influence of the anisotropy in the mechanical behavior of cellular material under cyclic compression loadings. For this study, a Digital Image Correlation (DIC) technique (named Correli) was applied, as well as SEM (Scanning Electron Microscopy) images were analyzed. The experimental results are discussed in detail for a closed-cell rigid poly (vinyl chloride) (PVC) foam, showing stress-strain curves in different directions and why the material can be assumed as transversely isotropic. Besides, the present paper shows elastic and plastic Poisson's ratios measured in different planes, explaining why the plastic Poisson's ratios approach to zero. Yield fronts created by the compression loadings in different directions and the influence of spring-back phenomenon on hardening curves are commented, also.
Resumo:
Óleo de soja epoxidado (OSE) é um produto químico há muito tempo utilizado como co-estabilizante e plastificante secundário do poli (cloreto de vinila) (PVC), ou seja, como um material que tem limitações na quantidade máxima que pode ser usada no composto de PVC. A sua aplicação como plastificante primário, ou seja, como o principal elemento plastificante no composto de PVC, e como base para outros plastificantes de fontes renováveis, tem aumentado nos últimos anos, principalmente devido a melhorias de desempenho e à redução do custo do OSE em comparação com plastificantes tradicionais. A reação de epoxidação do óleo de soja é bem conhecida e ocorre em duas fases líquidas, com reações em ambas as fases, e transferência de massa entre as fases. O processo industrial mais utilizado conta com formação in-situ do ácido perfórmico, através da adição gradativa do principal reagente, o peróxido de hidrogênio a uma mistura agitada de ácido fórmico e óleo de soja refinado. Industrialmente, o processo é realizado em batelada, controlando a adição do reagente peróxido de hidrogênio de forma que a geração de calor não ultrapasse a capacidade de resfriamento do sistema. O processo tem um ciclo que pode variar entre 8 e 12 horas para atingir a conversão desejada, fazendo com que a capacidade de produção seja dependente de investimentos relativamente pesados em reatores agitados mecanicamente, que apresentam diversos riscos de segurança. Estudos anteriores não exploram em profundidade algumas potenciais áreas de otimização e redução das limitações dos processos, como a intensificação da transferência de calor, que permite a redução do tempo total de reação. Este trabalho avalia experimentalmente e propõe uma modelagem para a reação de epoxidação do óleo de soja em condições de remoção de calor máxima, o que permite que os reagentes sejam adicionados em sua totalidade no início da reação, simplificando o processo. Um modelo foi ajustado aos dados experimentais. O coeficiente de troca térmica, cuja estimativa teórica pode incorrer em erros significativos, foi calculado a partir de dados empíricos e incluído na modelagem, acrescentando um fator de variabilidade importante em relação aos modelos anteriores. O estudo propõe uma base teórica para potenciais alternativas aos processos adotados atualmente, buscando entender as condições necessárias e viáveis em escala industrial para redução do ciclo da reação, podendo inclusive apoiar potenciais estudos de implementação de um reator contínuo, mais eficiente e seguro, para esse processo.
Resumo:
This study deals with the rheological aspects of poly-vinyl chloride (PVC) plastisol gelation and fusion processes in foamable formulations. Here, such processes are simulated by temperature-programmed experiment (5 K min−1) in which complex viscosity components are continuously recorded. Nineteen samples based on a PVC-VAC (vinyl acetate 95/5) copolymer with 100 phr plasticizer have been studied, differing only by the plasticizer structure. The sample shear modulus increases continuously with temperature until a maximum, long time after the end of the dissolution process as characterized by DSC. The temperature at the maximum varies between 345 and 428 K with a clear tendency to increase almost linearly with the plasticizer molar mass, and to vary with the flexibility and the degree of branching of the plasticizer molecule. The shear modulus increase is interpreted in terms of progressive “welding” of swelled particles by polymer chain reptation. The plasticizer nature would mainly affect the friction parameter of chain diffusion.
Resumo:
This project is concerned with the deterioration of surface coatings as a result of weathering and exposure to a pollutant gas (in this case nitric oxide). Poly(vinyl chloride) (PVC) plastisol surface coatings have been exposed to natural and artificial weathering and a comparison of the effects of these two types of weathering has been made by use of various analytical techniques. These techniques have each been assessed as to their value in providing information regarding changes taking place in the coatings during ageing, and include, goniophotometry, micro-penetrometry, surface energy measurements, weight loss measurements, thermal analysis and scanning electron microscopy. The results of each of these studies have then been combined to show the changes undergone by PVC plastisol surface coatings during ageing and to show the effects which additives to the coatings have on their behaviour and in particular the effects of plasticiser, pigment and uv and thermal stabilisers. Finally a preliminary study of the interaction between five commercial polymers and nitric oxide has been carried out, the polymers being polypropylene, cellulose acetate butyrate, polystyrene, polyethylene terephthalate and polycarbonate. Each of the samples was examined using infra-red spectroscopy in the transmission mode.
Resumo:
Flexible poly(vinylidene chloride-co-vinyl chloride)/TiO2 nanocomposite films were fabricated and their dielectric properties were studied. The structural characterization of the composites was carried out using various spectroscopic and electron microscopic techniques. From the thermal analysis of the composites, an improvement in the thermal properties was observed for the composites, as compared to the neat polymer. An increase in the DC conductivity was also observed in the composites, which was due to the tunneling of charge carriers. Furthermore, it was observed that the optimal loading of titania in the matrix was required, above which the properties of the composites showed deterioration. The study of the dielectric properties of the composites supports their use in microelectronic devices as separator in charge storage devices and in transistors.
Resumo:
Copper doped methylene blue sensitized poly(vinyl alcohol) (MBPVA)–acrylamide films were fabricated to improve the storage life of recorded gratings. The films were fabricated using gravity settling method and the copper chloride concentration was optimized as 3:18 10 3 mol/l for a dye concentration of 6:2 10 4 mol/l. The gratings recorded on the optimized film constitution could be stored for months with stable diffraction efficiency (24%) without any chemical or thermal fixing techniques. The resolution of the material is found to be unaffected with the addition of copper chloride.
Resumo:
Copper doped methylene blue sensitized poly(vinyl alcohol) (MBPVA)–acrylamide films were fabricated to improve the storage life of recorded gratings. The films were fabricated using gravity settling method and the copper chloride concentration was optimized as 3:18 10 3 mol/l for a dye concentration of 6:2 10 4 mol/l. The gratings recorded on the optimized film constitution could be stored for months with stable diffraction efficiency (24%) without any chemical or thermal fixing techniques. The resolution of the material is found to be unaffected with the addition of copper chloride.