997 resultados para PL spectra
Resumo:
In this paper we demonstrate that the structural and optical properties of Si nanoclusters (Si ncs) formed by thermal annealing of SiOx films prepared by plasma enhanced chemical vapor deposition (PECVD) and magnetron sputtering are very different. In fact, at a fixed Si excess and annealing temperature, photoluminescence (PL) spectra of sputtered samples are redshifted with respect to PECVD samples, denoting a larger Si ncs size. In addition, PL intensity reaches a maximum in sputtered films at annealing temperatures much lower than those needed in PECVD films. These data are correlated with structural properties obtained by energy filtered transmission electron microscopy and electron energy loss spectroscopy. It is shown that in PECVD films only around 30% of the Si excess agglomerates in clusters while an almost complete agglomeration occurs in sputtered films. These data are explained on the basis of the different initial structural properties of the as-deposited films that become crucial for the subsequent evolution. © 2008 American Institute of Physics.
Resumo:
A spin-injection/-detection device has been fabricated based on the multiple quantum well light emitting diode (LED) structure. It is found that only a broad electroluminescence (EL) peak of a full width at half maximum of 8.6 nm appears at the wavelength of 801 nm in EL spectra with a circular luminescence polarization degree of 18%, despite PL spectra always show three well resolved peaks. The kinetic energy gained by injected electrons and holes in their drift along opposite directions broadens the EL peak, and makes three EL peaks converge together. The same process also destroys the injected spin polarization of electrons mainly dominated by the Bir-Aronov-Pikus spin relaxing mechanism.
Resumo:
Five-micron thick freestanding Si cantilevers were fabricated on bulk Si (1 1 1) substrates with surface/bulk micromachining (SBM) process. Then 1-mu m thick GaN layers were deposited on the Si cantilevers by metal-organic chemical vapor deposition (MOCVD). Epilayers on cantilever areas were obtained crack-free, and the photoluminescence (PL) spectra verified the stress reduction and better material quality in these suspended parts of GaN. Back sides of the cantilevers were also covered with GaN layers, which prevented the composite beams from bending dramatically. This paper had proved the feasibility of integrating high-quality GaN epilayers with Si micromechanical structures to realize GaN-based micro electro-mechanical system (MEMS). (C) 2009 Elsevier Ltd. All rights reserved.
Resumo:
By using photoluminescence (PL) and time-resolved PL spectra, the optical properties of single InAs quantum dot (QD) embedded in the p-1-n structure have been studied under an applied electric field With the increasing of electric field, the exciton lifetime increases due to the Stark effect. We noticed that the decrease or quenching of PL intensity with increasing the electric field is mainly due to the decrease of the carriers captured by QD.
Resumo:
Si-doped ZnO can be synthesized on the surface of the early grown Zn2SiO4 nanostructures and form core/ shell coaxial heterostructure nanobelts with an epitaxial orientation relationship. A parallel interface with a periodicity array of edge dislocations and an inclined interface without dislocations can be formed. The visible green emission is predominant in PL spectra due to carrier localization by high density of deep traps from complexes of impurities and defects. Due to band tail localization induced by composition and defect fluctuation, and high density of free-carriers donated by doping, especially the further dissociation of excitons into free-carriers at high excitation intensity, the near-band-edge emission is dominated by the transition of free-electrons to free-holes, and furthermore, exhibits a significant excitation power-dependent red-shift characteristic. Due to the structure relaxation and the thermalization effects, carrier delocalization takes place in deep traps with increasing excitation density. As a result, the green emission passes through a maximum at 0.25I(0) excitation intensity, and the ratio of the violet to green emission increases monotonously as the excitation laser power density increases. The violet and green emission of ZnO nanostructures can be well tuned by a moderate doping and a variation in the excitation density.
Resumo:
Tensile-strained GaAsP/GaInP single quantum well (QW) laser diode (I-D) structures have been grown by low-pressure metal organic chemical vapor deposition (LP-MOCVD) and related photoluminescence (PL) properties have been investigated in detail. The samples have the same well thickness of 16 nm but different P compositions in a GaAsP QW. Two peaks in room temperature (RT) PL spectra are observed for samples with a composition larger than 0.10. Temperature and excitation-power-dependent PL spectra have been measured for a sample with it P composition of 0.15. It is found that the two peaks have a 35 meV energy separation independent of temperature and only the low-energy peak exists below 85 K. Additionally, both peak intensities exhibit a monotonous increase as excitation power increases. Analyses indicate that the two peaks arise from the intrinsic-exciton recombination mechanisms of electron-heavy hole (e-hh) and electron-light hole (e-hh). A theoretical calculation based oil model-solid theory, taking, into account the spin-orbit splitting energy, shows good agreement with our experimental results. The temperature dependence of PL intensity ratio is well explained using the spontaneous emission theory for e-hh and e-hh transitions. front which the ratio can be characterized mainly by the energy separation between the fill and Ill states.
Resumo:
10 mu m-thick ultra-thin Si (111) membranes for GaN epi-layers growth were successfully fabricated on silicon-on-insulator (SOI) substrate by backside etching the handle Si and buried oxide (BOX) layer. Then 1 mu m-thick GaN layers were deposited on these Si membranes by metal-organic chemical vapor deposition (MOCVD). The crack-free areas of 250 mu m, x 250 mu m were obtained on the GaN layers due to the reduction of thermal stress by using these ultra-thin Si membranes, which was further confirmed by the photoluminescence (PL) spectra and the simulation results from the finite element method calculation by using the software of ANSYS. In this paper, a newly developed approach was demonstrated to utilize micromechanical structures for GaN growth, which would improve the material quality of the epi-layers and facilitate GaN-based micro electro-mechanical system (MEMS) fabrication, especially the pressure sensor, in the future applications. (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
ZnO films are prepared on glass substrates by pulsed laser deposition (PLD) at different oxygen pressures, and the effects of oxygen pressure on the structure and optoelectrical properties of as-grown ZnO films are investigated. The results show that the crystallite size and surface roughness of the films increase, but the carrier concentration and optical energy gap E-g decrease with increasing oxygen pressure. Only UV emission is found in the photoluminescence (PL) spectra of all the samples, and its intensity increases with oxygen pressure. Furthermore, there are marked differences in structure and properties between the films grown at low oxygen pressures (0.003 and 0.2 Pa) and the films grown at high oxygen pressures (24 and 150 Pa), which is confirmed by the fact that the crystallite size and UV emission intensity markedly increase, but the carrier concentration markedly decreases as oxygen pressure increases from 0.2 to 24 Pa. These results show that the crystal quality, including the microstructural quality and stoichiometry proportion, of the prepared ZnO films improves as oxygen pressure increases, particularly from 0.2 to 24 Pa.
Resumo:
The effect of thermal annealing on the luminescence properties of neon implanted GaN thin films was studied. Low temperature photoluminescence (PL) measurements were carried out on the samples implanted with different doses ranging from 10(14) to 9 x 10(15) cm(-2) and annealed isochronally at 800 and 900 degrees C. We observed a new peak appearing at 3.44 eV in the low temperative PL spectra of all the implanted samples after annealing at 900 degrees C. This peak has not been observed in the PL spectra of implanted samples annealed at 800 degrees C except for the samples implanted with the highest dose. The intensity of the yellow luminescence (YL) band noticed in the PL spectra measured after annealing was observed to decrease with the increase in dose until it was completely suppressed at a dose of 5 x 10(15) cm(-2). The appearance of a new peak at 3.44 eV and dose dependent suppression of the YL band are attributed to the dissociation of VGaON complexes caused by high energy ion implantation.
Photoluminescence study of AlGaInP/GaInP quantum well intermixing induced by zinc impurity diffusion
Resumo:
AlGaInP/GaInP quantum well intermixing phenomena induced by Zn impurity diffusion at 540 degrees C were studied using room-temperature photo luminescence (PL) spectroscopy. As the diffusion time increased from 40 to 120 min, PL blue shift taken on the AlGaInP/GaInP quantum well regions increased from 36.3 to 171.6 meV. Moreover, when the diffusion time was equal to or above 60 min, it was observed firstly that a PL red shift occurred with a PL blue shift on the samples. After detailed analysis, it was found that the red-shift PL spectra were measured on the Ga0.51In0.49P buffer layer of the samples, and the mechanism of the PL red shift and the PL blue shift were studied qualitatively. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
The crystalline, surface, and optical properties of the (10 (1) over bar(3) over bar) semipolar GaN directly grown on m-plane sapphire substrates by hydride vapor phase epitaxy (HVPE) were investigated. It was found that the increase of V/III ratio led to high quality (10 (1) over bar(3) over bar) oriented GaN epilayers with a morphology that may have been produced by step-flow growth and with minor evidence of anisotropic crystalline structure. After etching in the mixed acids, the inclined pyramids dominated the GaN surface with a density of 2 X 10(5) cm(-2), revealing the N-polarity characteristic. In the low-temperature PL spectra, weak BSF-related emission at 3.44eV could be observed as a shoulder of donor-bound exciton lines for the epilayer at high V/III ratio, which was indicative of obvious reduction of BSFs density. In comparison with other defect related emissions, a different quenching behavior was found for the 3.29 eV emission, characterized by the temperature-dependent PL measurement. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Short period InAs(4 ML)/GaSb(8 ML) superlattices (SLs) with InSb- and mixed-like (or Ga(1-x)In(x)As(1-)ySb(y)-like) interfaces (IFs) are grown by molecular-beam epitaxy (MBE) on (001) GaSb substrates at optimized growth temperature. Raman scattering reveals that two kinds of IFs can be formed by controlling shutter sequences. X-ray diffraction (XRD) and atomic force microscopy (AFM) demonstrate that SLs with mixed-like IFs are more sensitive to growth temperature than that with InSb-like IFs. The photoluminescence (PL) spectra of SLs with mixed-like IFs show a stronger intensity and narrower line width than with InSb-like IFs. It is concluded that InAs/GaSb SLs with mixed-like IFs have better crystalline and optical properties.
Resumo:
The GaN-rich side of GaNP ternary alloys has been successfully synthesized by light-radiation heating and low-pressure metal-organic chemical vapor deposition. X-ray diffraction (XRD) rocking curves show that the ( 0002) peak of GaNP shifts to a smaller angle with increasing P content. From the GaNP photoluminescence (PL) spectra, the red shifts from the band-edge emission of GaN are determined to be 73, 78 and 100 meV, respectively, in the GaNP alloys with the P contents of 1.5%, 5.5% and 7.5%. No PL peak or XRD peak related to GaP is observed, indicating that phase separation induced by the short-range distribution of GaP-rich regions in the GaNP layer has been effectively suppressed. The phase-separation suppression in the GaNP layer is associated with the high growth rate and the quick cooling rate under the given growth conditions, which can efficiently restrain the accumulation of P atoms in the GaNP layer.
Resumo:
We report a systematical study on the molecular beam epitaxy growth and optical property of (GaAs1-xSbx/In-y Ga1-yAs)/GaAs bilayer quantum well (BQW) structures. It is shown that the growth temperature of the wells and the sequence of layer growth have significant influence on the interface quality and the subsequent photoluminescence (PL) spectra. Under optimized growth conditions, three high-quality (GaAsSb0.29/In0.4GaAs)/GaAs BQWs are successfully fabricated and a room temperature PL at 1314 nm is observed. The transition mechanism in the BQW is also discussed by photoluminescence and photoreflectance measurements. The results confirm experimentally a type-II band alignment of the interface between the GaAsSb and InGaAs layers.
Resumo:
Triple-axis x-ray diffraction (TXRD) and photoluminescence (PL) spectra are used to assess the influence of the ratio of TMIn flow to group III flow on structural defects, such as dislocations and interface roughness, and optical properties of multiple quantum wells(MQWs). In this paper the mean densities of edge and screw dislocations in InGaN/GaN MQWs are obtained by W scan of every satellite peak of (0002) symmetric and (1012) asymmetric diffractions. At the same time, the interface roughness is measured by the radio of the full width at half maximum of satellite peaks to the peak orders. The experimental results showed that the density of dislocation, especially of edge dislocation, and interface roughness increase with the increase of the ratio, which leads to the decrease of PL properties. It also can be concluded that the edge dislocation acts as nonradiative recombination centers in InGaN/GaN MQWs. Also noticed is that the variation of the ratio has more influence on edge dislocation than on screw dislocation.