The ZnO luminescent properties are strongly influenced by the preparation method and they are principally related to electronic and crystalline structures. This work reports about the correlation among luminescence properties of ZnO, obtained from zinc hydroxycarbonate, and crystalline lattice defects, microstrain, as function of thermal treatment. The crystallite size increase and the qualitative microstrain, obtained by Williamson-Hall plots, decrease as function of temperature. The evolution of electronic defects is analyzed by luminescence spectroscopy based on energy of the electronic transitions. From excitation spectrum, it is verified two bands around 377 nm and 405 nm attributed to the transitions between valence-conduction bands and valence band to interstitial zinc level, respectively. The emission spectra of sample treated at 600 degreesC shows large band at 670 nm. However, the green emission around 530 nm is observed for samples treated at 900 degreesC. The intensities of excitation and emission bands are associated with the increase of the electronic defects that depend on the strain lattice decrease. The lowest strain lattice results on the best green luminescent properties of zinc oxide. (C) 2001 Elsevier B.V. Ltd. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pure yttrium oxide or mixed with europium oxide (3 at%) were treated in supercritical isopropanolic suspension at 500degreesC for 20 It and filling degree of 50%. Products were supercritically dried and characterized by scanning electron microscopy (SEM), X-ray powder diffraction (XRD), infrared spectroscopy (IR) and luminescence spectroscopy (LS). Particle shape is irregular with an equivalent diameter of ca. 5 mum. Cubic crystalline phase is mainly obtained and hydroxide ion in low concentration is detected by IR vibrational spectrum. Europium in this concentration does not extensively change such observed characteristics from the pure yttrium oxide. Luminescence spectra show that the doped product is a mixture of the two oxides added by oxyhydroxide impurities. Nevertheless, this precursor sample, after being heated at 900degreesC during 1 h, has all characteristics, especially luminescent ones, of the P22 commercial phosphor. (C) 2003 Elsevier B.V. (USA). All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Erbium-activated silica-based planar waveguides were prepared by three different technological routes: RF-sputtering, sol-gel and ion exchange. Various parameters of preparation were varied in order to optimize the waveguides for operation in the NIR region. Particular attention was devoted to the minimization of the losses and the increase of the luminescence efficiency of the metastable I-4(13/2) state of the Er3+ ion. Waveguide properties were determined by m-line spectroscopy and loss measurements. Waveguide Raman and luminescence spectroscopy were used to obtain information about the structure of the prepared films and about the dynamical processes related to the luminescence of the Er3+ ions.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This work reports on the luminescence spectroscopy sensitivity in the determination of the phase purity in gadolinium compounds using Eu3+ as a probe. Cubic Gd2O3 and hexagonal Gd2O2S doped with Eu3+ spherical fine particles were obtained from doped gadolinium basic carbonates with morphological control and were also characterized by IR and XRD. Doped samples present Eu3+ characteristic transitions, with specific energy positions related to each phase. Emission and excitation spectra patterns were established for oxide and oxysulfide compounds, then oxysulfate and oxide impurities generated during oxysulfide preparation were monitored. From emission spectra some experimental intensity parameters were also calculated. All spectroscopic results reflect the presence or not of impurities in all compounds. (C) 2001 Elsevier B.V. Ltd. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This work reports on the preparation of Gd2O3, cubic system, with spherical particles, narrow size distribution, whether or not doped with 1-5 at.% of Eu3+ and the influence of Eu3+ concentration on optical and morphological properties. Average diameter and size distribution particle analyses were performed for all samples from SEM results. Doped samples were also investigated by luminescence spectroscopy and emission kinetic measurements. All oxide samples present a particle average diameter distribution range from 110 to 150 nm and a decrease of particle average diameter with the presence of Eu3+. The particle size decrease is almost the same for all samples with different doping ion concentration. Therefore, the presence of doping ion may be inhibiting particle growth after the nucleation process. From spectroscopic studies, the doping ion distribution in the surface of oxide samples can be considered homogeneous because concentration quenching is not observed, as well as a significant difference among the calculated lifetime for each sample. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

In this work particles of ZnO of size range 33-56 Angstrom were prepared by a sol-gel method. The effect of reaction time on the particle size of ZnO or ZnO:Ce was investigated by transmission electron microscopy measurements, UV-vis absorption and luminescence spectroscopy. A linear increase of the mean particle size is observed as a function of reaction time. The cerium-doped particles are bigger than the pure ZnO ones obtained at the same reaction time. A shift to lower energy at the maximum of the bands is observed in all absorption, emission and excitation spectra as a function of particle growth. From the absorption spectra the optical energy gap values (Eg) for these particles were determined. In the quantum size regime, Eg was found to decrease with particle growth.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The effect of doping by europium triflate on the nanoscopic structure of organic-inorganic hybrid formed by a siliceous network containing pendant amine-terminated propyl chains, called aminosils, was investigated by Small-Angle X-ray Scattering (SAXS). It appears that the composites exhibit a two-level structure. The first level consists of well-condensed cubic-like siloxane octamers, with a radius of gyration around 2 angstrom. The second level is formed by the aggregation of these siloxane nanodomains to form larger structures, in which the nanodomains are spatially correlated and separated by the organic pendant chains. Europium doping inhibits the aggregation between siloxane octamers, leading to a less compact second-level structure. This can be explained by the Eu3+ stop coordination close to the external surface of the siloxane nanodomains, as detected by luminescence spectroscopy.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The synthesis and spectroscopic characterization of yttrium diphenylphosphinates doped with europium are reported. The purity of all samples was confirmed by carbon and hydrogen micro analysis, thermal analysis, IR vibrational spectroscopy, and X-ray diffraction. Luminescence spectra indicated the presence of two or more symmetry centers. The dynamic luminescence measurements suggested that one symmetry site presented an inversion center, while the others had lower symmetry. The average quantum yield of Eu3+ emission in the yttrium, matrices was 60%. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Gallium-doped zinc oxide (ZnO:Ga 1, 2 3, 4 and 5 at%) samples were prepared in powder form by modifying the Pechini method. The formation of zinc gallate (ZnGa2O4) With the spinel crystal structure was observed even in ZnO:Ga 1 at% by X-ray diffraction. The presence of ZnGa2O4 in ZnO:Ga samples was also evidenced by luminescence spectroscopy through its blue emission at 430 nm, assigned to charge transfer between Ga3+ at regular octahedral symmetry and its surrounding O2- ions. The amount of ZnGa2O4 increases as the dopant concentration increases, as observed by the quantitative phase analysis by the Rietveld method. (C) 2006 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The oxysulfide compounds La2O2S:Eu and Y2O2S were obtained directly from thermodecomposition of the respective oxalate compounds under argon and sulfur vapor, the obtained compounds were analyzed by infrared spectroscopy, X ray diffraction and luminescence spectroscopy. The particle size distribution and crystalline habit of the compounds were observed by scanning electron microscopy. Although the particle size of the oxysulfide was found to be 30%-40% smaller than the precursor oxalates, the initial morphology was completely maintained, which indicates the occurrence of a topochemical reaction from oxalates to oxysulfides. © Gauthier-Villars.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The preparation of spherical Y2O2S and Y2O2S:Eu particles using a solid-gas reaction of monodispersed precursors with elemental sulfur vapor under an argon atmosphere has been investigated. The precursors, undoped and doped yttrium basic carbonates, are synthesized by aging a stock solution containing the respective cation chloride and urea at 82-84 °C. Y2O2S and Y2O2S:Eu were characterized in terms of their composition, crystallinity and morphology by chemical analysis, X-ray powder diffraction (XRD), IR spectroscopy, and scanning electron microscopy (SEM). The Eu-doped oxysulfide was also characterized by atomic absorption spectrophotometry and luminescence spectroscopy. The spherical morphology of oxysulfide products and of basic carbonate precursors suggests a topotatic inter-relationship between both compounds.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A series of insoluble, chemically inert and thermally stable compounds La1-xEux(DPP)3 (x = 0.50, 0.20, 0.10, and 0.050; DPP = diphenylphosphinate) was synthesized and characterized by elemental and thermogravimetric analysis, FT Infrared spectroscopy and X-ray powder diffraction. Luminescence spectroscopy at both 77 and 298 K showed changes in the intensity of the hypersensitive transition 5D 0 → 7F2 of Eu3+ which are dependent of the excitation wavelength, suggesting that the europium occupies two different sites in the compounds. The large quantum efficiency and quantum yield, as well as the long radiative lifetime of the 5D0 Eu3+ level of the series of compounds, which are desirable qualities for light-conversion molecular devices, are discussed in terms of the interactions and the energy transfer process between the ligands and the metal ion. © 2012 Elsevier B.V. All rights reserved.