1000 resultados para Horizontal bone augmentation
Resumo:
PURPOSE To analyze the indications and frequency for three-dimensional (3D) imaging for implant treatment planning in a pool of patients referred to a specialty clinic over a 3-year period. MATERIALS AND METHODS All patients who received dental implants between 2008 and 2010 at the Department of Oral Surgery and Stomatology at the University of Bern were included in the study. The influence of age, gender, and time of treatment (2008 to 2010) on the frequency of use of two-dimensional (2D) radiographic imaging modalities alone or in combination with 3D cone beam computed tomography (CBCT) scans was analyzed. Furthermore, the influence of the indication, location, and need for bone augmentation on the frequency of use of 2D imaging modalities alone or in combination with CBCT was evaluated. RESULTS In all, 1,568 patients (792 women and 776 men) received 2,279 implants. Overall, 633 patients (40.4%) were analyzed with 2D imaging procedures alone. CBCT was performed in 935 patients (59.6%). There was a statistically significant increase in CBCT between 2008 and 2010. Patients older than 55 years received a CBCT scan in addition to 2D radiographic imaging statistically significantly more often. Additional 3D imaging was most frequently performed in the posterior maxilla, whereas 2D radiographs alone exhibited the highest frequency in the anterior mandible. The combination of 2D with CBCT was used predominantly for implant placement with simultaneous or staged guided bone regeneration or sinus elevation. CONCLUSION Based on these findings from a specialty clinic, the use of additional CBCT imaging for implant treatment planning is influenced by the indication, location, local anatomy (including the need for bone augmentation), and the age of the patient.
Resumo:
Purpose: The purpose of this work was to evaluate the potential of substituting autogenous bone (AB) by bone marrow aspirate concentrate (BMAC). Both AB and BMAC were tested in combination with a bovine bone mineral (BBM) for their ability of new bone formation (NBF) in a multicentric, randomized, controlled, clinical and histological noninferiority trial. Materials and Methods: Forty-five severely atrophied maxillary sinus from 26 patients were evaluated in a partial cross-over design. As test arm, 34 sinus of 25 patients were augmented with BBM and BMAC containing mesenchymal stem cells. Eleven control sinus from 11 patients were augmented with a mixture of 70% BBM and 30% AB. Biopsies were obtained after a 3-4-month healing period at time of implant placement and histomorphometrically analyzed for NBF. Results: NBF was 14.3%+/- 1.8% for the control and nonsignificantly lower (12.6%+/- 1.7%) for the test (90% confidence interval: -4.6 to 1.2). Values for BBM (31.3%+/- 2.7%) were significantly higher for the test compared with control (19.3%+/- 2.5%) (p < 0.0001). Nonmineralized tissue was lower by 3.3% in the test compared with control (57.6%; p = 0.137). Conclusions: NBF after 3-4 months is equivalent in sinus, augmented with BMAC and BBM or a mixture of AB and BBM. This technique could be an alternative for using autografts to stimulate bone formation.
Resumo:
Previous studies support resorbable biocomposites made of poly(L-lactic acid) (PLA) and beta-tricalcium phosphate (TCP) produced by supercritical gas foaming as a suitable scaffold for tissue engineering. The present study was undertaken to demonstrate the biocompatibility and osteoconductive properties of such a scaffold in a large animal cancellous bone model. The biocomposite (PLA/TCP) was compared with a currently used beta-TCP bone substitute (ChronOS, Dr. Robert Mathys Foundation), representing a positive control, and empty defects, representing a negative control. Ten defects were created in sheep cancellous bone, three in the distal femur and two in the proximal tibia of each hind limb, with diameters of 5 mm and depths of 15 mm. New bone in-growth (osteoconductivity) and biocompatibility were evaluated using microcomputed tomography and histology at 2, 4 and 12 months after surgery. The in vivo study was validated by the positive control (good bone formation with ChronOS) and the negative control (no healing with the empty defect). A major finding of this study was incorporation of the biocomposite in bone after 12 months. Bone in-growth was observed in the biocomposite scaffold, including its central part. Despite initial fibrous tissue formation observed at 2 and 4 months, but not at 12 months, this initial fibrous tissue does not preclude long-term application of the biocomposite, as demonstrated by its osteointegration after 12 months, as well as the absence of chronic or long-term inflammation at this time point.
Resumo:
Modified fluorcanasite glasses were fabricated by either altering the molar ratios of Na(2)O and CaO or by adding P(2)O(5) to the parent stoichiometric glass compositions. Glasses were converted to glass-ceramics by a controlled two-stage heat treatment process. Rods (2 mm x 4 mm) were produced using the conventional lost-wax casting technique. Osteoconductive 45S5 bioglass was used as a reference material. Biocompatibility and osteoconductivity were investigated by implantation into healing defects (2 mm) in the midshaft of rabbit femora. Tissue response was investigated using conventional histology and scanning electron microscopy. Histological and histomorphometric evaluation of specimens after 12 weeks implantation showed significantly more bone contact with the surface of 45S5 bioglass implants when compared with other test materials. When the bone contact for each material was compared between experimental time points, the Glass-Ceramic 2 (CaO rich) group showed significant difference (p = 0.027) at 4 weeks, but no direct contact at 12 weeks. Histology and backscattered electron photomicrographs showed that modified fluorcanasite glass-ceramic implants had greater osteoconductivity than the parent stoichiometric composition. Of the new materials, fluorcanasite glass-ceramic implants modified by the addition of P(2)O(5) showed the greatest stimulation of new mineralized bone tissue formation adjacent to the implants after 4 and 12 weeks implantation. (C) 2010 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 94A: 760-768, 2010
Resumo:
Our aim was to compare the osteogenic potential of mononuclear cells harvested from the iliac crest combined with bovine bone mineral (BBM) (experimental group) with that of autogenous cancellous bone alone (control group). We studied bilateral augmentations of the sinus floor in 6 adult sheep. BBM and mononuclear cells (MNC) were mixed and placed into one side and autogenous bone in the other side. Animals were killed after 8 and 16 weeks. Sites of augmentation were analysed radiographically and histologically. The mean (SD) augmentation volume was 3.0 (1.0) cm(3) and 2.7 (0.3) cm(3) after 8 and 16 weeks in the test group, and 2.8 (0.3) cm(3) (8 weeks) and 2.8 (1.2) cm(3) (16 weeks) in the control group, respectively. After 8 weeks, histomorphometric analysis showed 24 (3)% BBM, and 19 (11)% of newly formed bone in the test group. The control group had 20 (13%) of newly formed bone. Specimens after 16 weeks showed 29 (12%) of newly formed bone and 19 (3%) BBM in the test group. The amount of newly formed bone in the control group was 16 (6%). The results show that mononuclear cells, including mesenchymal stem cells, in combination with BBM as the biomaterial, have the potential to form bone. (C) 2009 The British Association of Oral and Maxillofacial Surgeons. Published by Elsevier Ltd. All rights reserved.
Resumo:
Background: Preventing ridge collapse with the extraction of maxillary anterior teeth is vital to an esthetic restorative result. Several regenerative techniques are available and are used for socket preservation. The aim of this study is to analyze by clinical parameters the use of acellular dermal matrix (ADM) and anorganic bovine bone matrix (ABM) with synthetic cell-binding peptide P-15 to preserve alveolar bone after tooth extraction. Methods: Eighteen patients in need of extraction of maxillary anterior teeth were selected and randomly assigned to the test group (ADM plus ABM/P-15) or the control group (ADM only). Clinical measurements were recorded initially and at 6 months after ridge-preservation procedures. Results: In the clinical measurements (external vertical palatal measurement [EVPM], external vertical buccal measurement [EVBM], and alveolar horizontal measurement [AHM]) the statistical analysis showed no difference between test and control groups initially and at 6 months. The intragroup analysis, after 6 months, showed a statistically significant reduction in the measurements for both groups. In the comparison between the two groups, the differences in the test group were as follows: EVPM = 0.83 +/- 1.53 mm; EVBM = 1.20 +/- 2.02 mm; and AHM = 2.53 +/- 1.81 mm. The differences in the control group were as follows: EVPM = 0.87 +/- 1.13 mm; EVBM = 1.50 +/- 1.15 mm; and AHM = 3.40 +/- 1.39 mm. The differences in EVPM and EVBM were not statistically significant; however, in horizontal measurement (AHM), there was a statistically significant difference (P<0.05). Conclusion: The results of this study show that ADM used as membrane associated with ABM/P-15 can be used to reduce buccal-palatal dimensions compared to ADM alone for preservation of the alveolar ridge after extraction of anterior maxillary teeth. J Periodontol 2011;82:72-79.
Resumo:
Background: Prosthetic rehabilitation of the posterior maxilla with dental implants is often difficult because of proximity to the maxillary sinus and insufficient bone height. Maxillary sinus floor augmentation procedures aim to obtain enough bone with an association between biomaterials and autogenous bone.Purpose: the purpose of this study was to evaluate histomorphometrically two grafting materials (calcium phosphate and Ricinus communis polymer) used in maxillary sinus floor augmentation associated with autogenous bone.Materials and Methods: Biopsies were taken from 10 consecutive subjects (mean age 45 years) 10 months after maxillary sinus floor augmentation. The sinus lift was performed with a mixture of autogenous bone and R. communis polymer or calcium phosphate in a 1:2 proportion. Routine histologic processing and staining with hernatoxylin and eosin were performed.Results: the histomorphometric analysis indicated satisfactory regenerative results in both groups for a mean of bone tissue in the grafted area (44.24 +/- 13.79% for the calcium phosphate group and 38.77 +/- 12.85% for the polymer group). Histologic evaluation revealed the presence of an inflammatory infiltrate of mononuclear prevalence that, on average, was nonsignificant. The histologic sections depicted mature bone with compact and cancellous areas in both groups.Conclusion: the results indicated that both graft materials associated with the autogenous bone were biocompatible, although both were still present after 10 months.
Resumo:
The aim of this study was to assess vascular endothelial growth factor (VEGF) expression and microvessel density (MVD) in maxillary sinus augmentation with autogenous bone and different graft materials for evaluating their angiogenic potential.Biopsies were harvested 10 months after sinus augmentation with a combination of autogenous bone and different graft materials: hydroxyapatite (HA, n = 6 patients), demineralized freeze-dried bone allograft (DFDBA, n = 5 patients), calcium phosphate (CP, n = 5 patients), Ricinus communis polymer (n = 5 patients) and control group - autogenous bone only (n = 13 patients).In all the samples, higher intensities of VEGF expression were prevalent in the newly formed bone, while lower intensities of VEGF expression were predominant in the areas of mature bone. The highest intensity of VEGF expression in the newly formed bone was expressed by HA (P < 0.001) and CP in relation to control (P < 0.01) groups. The lowest intensities of VEGF expression in newly formed bone were shown by DFDBA and polymer groups (P < 0.05). When comparing the different grafting materials, higher MVD were found in the newly formed bone around control, HA and CP (P < 0.001).Various graft materials could be successfully used for sinus floor augmentation; however, the interactions between bone formation and angiogenesis remain to be fully characterized.
Resumo:
The aim of the current study is to evaluate fresh-frozen human bone allografts (FHBAs) used in vertical ridge augmentation clinically and by computed tomography, and to analyze the resulting bone formation and graft resorption. Sixteen FHBAs were grafted in the maxillae and mandibles of 9 patients. The FHBAs, which were provided by the Musculoskeletal Tissue Bank of Marilia Hospital (Unioss), were frozen at -80A degrees C. After 7 months, dental implants were placed and bone parameters were evaluated. Vertical bone formation was measured by computerized tomography before (T0) and at 7 months (T1) after the surgical procedure. Bone graft resorption was measured clinically from a landmark screw head using a periodontal probe. The results were analyzed by Student's t-test. Significant differences existed in the bone formation values at T0 and T1, with an average change of 4.03 +/- A 1.69 mm. Bone graft resorption values were 1.0 +/- A 0.82 mm (20%). Implants were placed with varying insertion torque values (35-45 Ncm), and achieved primary stability. This study demonstrates that FHBAs promote satisfactory vertical bone formation with a low resorption rates, good density, and primary implant stability.
Resumo:
Background: Maxillary sinus floor augmentation procedures are currently the treatment of choice when the alveolar crest of the posterior maxilla is insufficient for dental implant anchorage. This procedure aims to obtain enough bone with biomaterial association with the autogenous bone graft to create volume and allow osteo conduction. The objective of this study was to histologically and histometrically evaluate the bone formed after maxillary sinus floor augmentation by grafting with a combination of autogenous bone, from the symphyseal area mixed with DFDBA or hydroxyapatite.Methods: Ten biopsies were taken from 10 patients 10 months after sinus floor augmentation using a combination of 50% autogenous bone plus 50% dernineralized freeze-dried bone allograft (DFDBA group) or 50% autogenous bone plus 50% hydroxyapatite (HA group). Routine histological processing and staining with hernatoxylin and eosin and Masson's trichrome were performed.Results: the histomorphometrical analysis indicated good regenerative results in both groups for the bone tissue mean in the grafted area (50.46 +/- 16.29% for the DFDBA group and 46.79 +/- 8.56% for the HA group). Histological evaluation revealed the presence of mature bone with compact and cancellous areas in both groups. The inflammatory infiltrate was on average nonsignificant and of mononuclear prevalence. Some biopsies showed blocks of the biomaterial in the medullary spaces close to the bone wall, with absence of osteogenic activity.Conclusions: the results indicated that both DFDBA and HA associated with an autogenous bone graft were biocompatible and promoted osteoconduction, acting as a matrix for bone formation. However, both materials were still present after 10 months.
Resumo:
Bone spreading technique (BST) is a horizontal augmentation with minimal trauma for simultaneous implant placement and an alternative to Summer's osteotome technique both for its clinical use and for the armamentarium. The foremost advantage of the crest dilation technique is a substantially less invasive method; the buccal wall expands after the medullary bone is compressed against the cortical bone. The lateral dilation and compaction of medullary bone improved primary stability. The vital difference is that the BST used in this case report avoided discomfort of the patient, thus eliminating the need for malleting.
Resumo:
Modified fluorcanasite glasses were fabricated by either altering the molar ratios of Na 2O and CaO or by adding P 2O 5 to the parent stoichiometric glass compositions. Glasses were converted to glass-ceramics by a controlled two-stage heat treatment process. Rods (2 mm x 4 mm) were produced using the conventional lost-wax casting technique. Osteoconductive 45S5 bioglass was used as a reference material. Biocompatibility and osteoconductivity were investigated by implantation into healing defects (2 mm) in the midshaft of rabbit femora. Tissue response was investigated using conventional histology and scanning electron microscopy. Histological and histomorphometric evaluation of specimens after 12 weeks implantation showed significantly more bone contact with the surface of 45S5 bioglass implants when compared with other test materials. When the bone contact for each material was compared between experimental time points, the Glass-Ceramic 2 (CaO rich) group showed significant difference (p = 0.027) at 4 weeks, but no direct contact at 12 weeks. Histology and backscattered electron photomicrographs showed that modified fluorcanasite glass-ceramic implants had greater osteoconductivity than the parent stoichiometric composition. Of the new materials, fluorcanasite glass-ceramic implants modified by the addition of P 2O 5 showed the greatest stimulation of new mineralized bone tissue formation adjacent to the implants after 4 and 12 weeks implantation. © 2010 Wiley Periodicals, Inc.
Resumo:
Objectives: This study aimed to comparatively evaluate the in vitro osteogenic potential of cells obtained from the mandibular ramus (MR, autogenous bone donor site) and from the maxillary sinus (MS) bone grafted with a mixture of anorganic bovine bone (ABB) and MR prior to titanium implant placement (MS, grafted implant site). Material and methods: Cells were obtained from three patients subjected to MS floor augmentation with a 1: 1 mixture of ABB (GenOx Inorg®) and MR. At the time of the sinus lift procedure and after 8 months, prior to implant placement, bone fragments were taken from MR and MS, respectively, and subjected to trypsin-collagenase digestion for primary cell culturing. Subcultured cells were grown under osteogenic condition for up to 21 days and assayed for proliferation/viability, osteoblast marker mRNA levels, alkaline phosphatase (ALP) activity and calcium content/Alizarin red staining. ALP activity was also determined in primary explant cultures exposed to GenOx Inorg® (1: 1 with MR) for 7 days. Data were compared using either the Mann-Whitney U-test or the Kruskal-Wallis test. Results: MS cultures exhibited a significantly lower osteogenic potential compared with MR cultures, with a progressive increase in cell proliferation together with a decrease in osteoblast markers, reduced ALP activity and calcium content. Exposure of MR-derived primary cultures to GenOx Inorg® inhibited ALP activity. Conclusion: These results suggest that the use of GenOx Inorg® in combination with MR fragments for MS floor augmentation inhibits the osteoblast cell differentiation at the implant site in the long term. © 2013 John Wiley & Sons A/S.
Resumo:
Objectives: To evaluate dimensional changes in autologous (AT) and fresh-frozen allogeneic (AL) block bone grafts 6 months after alveolar ridge augmentation. Material and methods: Twenty-six partially or totally edentulous patients treated either with fresh-frozen AL bone or AT bone onlay block grafts prior to implant placement (13 patients in each group), were included in this analysis. Patients received CBCT (i-CAT Classic) examinations prior to surgery and 14 days and 6 months after grafting. Differences in alveolar ridge area among the various observation times were evaluated by planimetric measurements on two-dimensional CBCT images of the grafted regions. Nineteen grafted blocks from each group were evaluated. Results: Significant increase in alveolar ridge dimensions, allowing implant placement, was obtained with both types of grafts 6 months after grafting; no significant differences in alveolar ridge area were observed between the groups at the various observation times. However, graft resorption in the AL group was significantly larger compared to that in the AT group at 6 months. Conclusions: Larger bone graft resorption was seen in patients treated with fresh-frozen AL bone than in those treated with AT bone 6 months following alveolar ridge augmentation. © 2011 John Wiley & Sons A/S.