978 resultados para HO-YAG


Relevância:

20.00% 20.00%

Publicador:

Resumo:

研究了国产Yb:YAG陶瓷的激光输出特性。激光器采用激光二极管(LD)纵向同轴抽运Yb:YAG陶瓷样品,样品的掺杂原子数分数为1%,一端面镀940 nm和1030 nm双增透膜,另一端面镀1030 nm增透膜,激光器在1031 nm处获得了近红外激光输出。实验中分别测试了Yb:YAG陶瓷在不同输出透射率(T=4%,8%,10%)条件下的激光输出特性。整个实验过程中,激光器维持基横模运转。当输出透射率为10%,吸收的抽运功率为9 W时,激光器获得最大的激光输出功率为1.63 W,相应的斜率效率为23.2%。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Damage threshold of crystals SiO2 and YAG against 60-900 fs, 800 nm laser pulses are reported. The breakdown mechanisms were discussed based on the double-flux model and Keldysh theory. We found that impact ionization plays the important role in the femtosecond laser-induced damage in crystalline SiO2, while the roles of photoionization and impact ionization in YAG crystals depend on the laser pulse durations. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

20 at.% Yb:YAG single crystals have been grown by the CZ method and gamma-ray irradiation induced color centers and valence change of Fe3+ and Yb3+ ions in Yb:YAG have been studied. One significant 255 nm absorption band was observed in as-grown crystals and was attributed to Fe3+ ions. Two additional absorption (AA) bands located at 255 nm and 345 nm, respectively, were produced after gamma irradiation. The changes in the AA spectra after gamma irradiation and air annealing are mainly related to the charge exchange of the Fe3+, Fe2+, oxygen vacancies and F-type color centers. Analysis shows that the broad AA band is associated with Fe2+ ions and F-type color centers. The transition Yb3+ Yb2+ takes place as an effect of recharging of one of the Yb3+ ions from a pair in the process of gamma irradiation. (C) 2006 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A laser-diode array (LDA) side-pumped Nd:YAG slab ring laser is described that incorporates a prism-shaped acousto-optic modulator to enforce unidirectional operation and Q-switching. When pumped by the maximum power of 50 W, Q-switched energies of 3.6 mJ and 50 ns duration, corresponding to a peak power of 72 kW, are obtained. (C) 1999 Society of Photo-Optical Instrumentation Engineers. [S0091-3286(99)01306-9].

Relevância:

20.00% 20.00%

Publicador:

Resumo:

考虑固体热容激光器对工作介质的要求,对比分析了掺钕的玻璃、YAG和GGG的多种材料性能。并对三者在激光工作周期内的瞬态温度场及热应力进行了数值模拟。结果表明:在给定的边界及工作条件下,当钕玻璃激光器以热容方式工作,时间为5S时,介质最高升温超过400K,最大热致应力为25MPa,接近其断裂极限的50%。在此条件下进行冷却,当水温为283K时,需经过约120S才基本恢复到初始工作状态。而Nd:YAG和Nd:GGG两种介质在相同输入工作条件下,工作时间可达10S,且温度分布相对平坦,温差和热应力较小,经水冷约