The restoration and recovery of the alveolar healing process are a challenge to dental surgeons to achieve satisfactory results at the osseointegration of implants and implant rehabilitation. Different operative technique and biomaterials are being used to reconstruct the framework of the alveolar process. One of the biomaterials used for this purpose is the bioactive glass. The aim of this study was to report clinical and histologic final results of 7 clinical reports of alveolar ridge augmentation using bioactive glass. Clinically, bioglass was able to maintain bone architecture of the alveolar bone and repaired satisfactory. Biopsy was performed on the histologic samples and showed bone formation in intimate contact to the particles of the biomaterial.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The present study compares the biologic behavior of BioGran and Calcitite as fillers for surgical cavities in the mandibles of 4 adult monkeys (Cebus apella). The surgical cavities were prepared through both mandibular cortices, with a diameter of 5 mm, in the angle region. Two cavities were prepared on the right side and 1 on the left and divided into 3 groups: R-1 sites were filled with bioglass (BioGran), R, sites were not filled, and L sites were filled with hydroxyapatite (Calcitite). After 180 days the animals were sacrificed and the specimens were removed for histologic processing. Results showed no bone formation in group R, (empty cavities). BioGran-treated sites showed bone formation and total repair of the bone defect, and the bioglass particles were almost totally resorbed and substituted by bone. The few remaining crystals were in intimate contact with newly formed bone. Calcitite did not allow bone formation, and granules inside the cavities were involved by connective tissue. Based upon those results, the authors concluded that bioglass resulted in total obliteration of the surgical cavity with bone and hydroxyapatite was present in a large amount and involved by connective tissue, without bone formation.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This study investigated, both histologically and histometrically, the efficacy of enamel matrix derived proteins (EMD) associated with bioactive glass (BG) and an absorbable membrane in the treatment of class III furcation defects in mongrel dogs. After surgical defect creation and chronification, the lesions were randomly divided into three groups according to the treatment employed: Test Group 1 - EMD + BG + membrane, Test Group 2 - EMD + membrane and Control Group - BG + membrane. After a 90-day healing period, the dogs were sacrificed. The descriptive analysis and the histometric data showed similar results for the experimental groups in all studied parameters (MANOVA, p > 0.05). The association of Emdogain® with bioglass and GTR, or with GTR only, showed similar results when compared with the ones obtained with bioglass associated with membrane in the treatment of class III furcation defects in dogs. The three modalities of treatment showed partial filling of the furcations, with bone and cementum regeneration limited to the apical portion of the defects.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Objective: The purpose of this study was to histologically analyze the influence of bioactive glass and/or a calcium sulfate barrier on bone healing in surgically created defects in rat tibias. Material and methods: Sixty-four rats were divided into 4 groups: C (control), CS (calcium sulfate), BG (bioactive glass), and BG/CS (bioactive glass/calcium sulfate). A surgical defect was created in the tibia of each animal. In Group CS, a calcium sulfate barrier was placed to cover the defect. In Group BG the defect was filled with bioactive glass. In Group BG/CS, it was filled with bioactive glass and protected by a barrier of calcium sulfate. Animals were sacrificed at 10 or 30 days post-operative. The formation of new bone in the cortical area of the defect was evaluated histomorphometrically. Results: At 10 days post-operative, Group C presented significantly more bone formation than Groups CS, BG, or BG/CS. No statistically significant differences were found between the experimental groups. At 30 days post-operative, Group C demonstrated significantly more bone formation than the experimental groups. Groups CS and BG/CS showed significantly more bone formation than Group BG. No statistically significant differences were found between Group CS and BG/CS. Conclusions: (a) the control groups had significantly more bone formation than the experimental groups; (b) at 10 days post-operative, no significant differences were found between any of the experimental groups; and (c) at 30 days post-operative, the groups with a calcium sulfate barrier had significantly more bone formation than the group that used bioactive glass only. Copyright © Blackwell Munksgaard 2005.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Modified fluorcanasite glasses were fabricated by either altering the molar ratios of Na 2O and CaO or by adding P 2O 5 to the parent stoichiometric glass compositions. Glasses were converted to glass-ceramics by a controlled two-stage heat treatment process. Rods (2 mm x 4 mm) were produced using the conventional lost-wax casting technique. Osteoconductive 45S5 bioglass was used as a reference material. Biocompatibility and osteoconductivity were investigated by implantation into healing defects (2 mm) in the midshaft of rabbit femora. Tissue response was investigated using conventional histology and scanning electron microscopy. Histological and histomorphometric evaluation of specimens after 12 weeks implantation showed significantly more bone contact with the surface of 45S5 bioglass implants when compared with other test materials. When the bone contact for each material was compared between experimental time points, the Glass-Ceramic 2 (CaO rich) group showed significant difference (p = 0.027) at 4 weeks, but no direct contact at 12 weeks. Histology and backscattered electron photomicrographs showed that modified fluorcanasite glass-ceramic implants had greater osteoconductivity than the parent stoichiometric composition. Of the new materials, fluorcanasite glass-ceramic implants modified by the addition of P 2O 5 showed the greatest stimulation of new mineralized bone tissue formation adjacent to the implants after 4 and 12 weeks implantation. © 2010 Wiley Periodicals, Inc.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The aim of this study was to evaluate the effect of platelet rich plasma (PRP) associated to bovine inorganic bone (Bio-Oss®; Geistlich) or bioactive glass (Bio-Gran®; Orthovita, Implant Innovations) on bone healing. Bone cavities were prepared in both sides of the mandible of 4 adult male dogs. The cavities were divided into 4 groups according to the filling material as follows: control, PRP, PRP/Bio-Oss, PRP/Bio-Gran. The animals were sacrificed after 120 days and histological and histomorphometrical analysis was performed. The control group showed 80.6% of bone formation in the longitudinal sections at 6 mm depth and 83.7% at 13 mm depth. The transverse sections displayed 74.2% at both 6 and 13 mm depths. The PRP group showed 21.1% of bone formation in the longitudinal sections at 6 mm depth, and 23.1% at 13 mm depth. The transverse sections presented 28.98% of bone formation at 6 mm depth and 41.2% at 13 mm depth. The PRP/Bio-Gran group showed 25.1% of bone formation in the longitudinal sections at 6 mm depth and 30.4% at 13 mm depth. In the transverse sections, the bone formation was 43.0% at 6 mm depth and 39.7% at 13 mm depth. The PRP/Bio-Oss group showed 35.5% of bone formation in the longitudinal sections at 6 mm depth and 42% at 13 mm depth. In the transversal sections, the bone formation was 26.8% and 31.2% at the depths of 6 and 13 mm, respectively. PRP alone or associated with bovine inorganic bone or bioglass had no significant effect in bone healing.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Pós-graduação em Ciências Odontológicas - FOAR

Relevância:

10.00% 10.00%

Publicador:

Resumo:

PURPOSE: To evaluate the effects of copaiba oil on jaw defects repair in Wistar rats treated with bioglass or adipose tissue. METHODS: A jaw defect was randomly created in forty-two rats and filled with bioglass or adipose tissue. The two groups (Gbio and Gcell) were subdivided in three subgroups with seven animals each according to gavage administration: control (distillated water), oil (copaiba oil) and melox (meloxicam). Euthanasia was performed after forty post-operative days. The bone formation was analyzed regarding the histological aspects. RESULTS: The osteoclasts activity was observed only in four subgroups (p=0.78). Regarding the osteoblasts presence, it was very similar between the subgroups, the difference was due to Gcell-melox (p=0.009) that presented less osteoblastic activity. The inflammatory cells were more evident in Gcell-melox subgroup, however, there was no difference in comparison with the other subgroups (p=0.52). Bone formation was observed in all subgroups, just two animals showed no bone formation even after 40 days. More than 50% of bone matrix mineralization was observed in 56% (23 animals) of the analyzed areas. The bone matrix mineralization was not different between subgroups (p=0.60). CONCLUSIONS: The subgroups that received copaiba oil showed bone repair, although not statistically significant in comparison to subgroups treated whit meloxicam or controls. Copaiba oil administered by gavage had no effect on bone repair in this experimental model.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)