896 resultados para BORON


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Recently, partially ionic boron (γ-B28) has been predicted and observed in pure boron, in bulk phase and controlled by pressure [Nature, 457 (2009) 863]. By using ab initio evolutionary structure search, we report the prediction of ionic boron at a reduced dimension and ambient pressure, namely, the two-dimensional (2D) ionic boron. This 2D boron structure consists of graphene-like plane and B2 atom pairs, with the P6/mmm space group and 6 atoms in the unit cell, and has lower energy than the previously reported α-sheet structure and its analogues. Its dynamical and thermal stability are confirmed by the phonon-spectrum and ab initio molecular dynamics simulation. In addition, this phase exhibits double Dirac cones with massless Dirac fermions due to the significant charge transfer between the graphene-like plane and B2 pair that enhances the energetic stability of the P6/mmm boron. A Fermi velocity (vf) as high as 2.3 x 106 m/s, which is even higher than that of graphene (0.82 x 106 m/s), is predicted for the P6/mmm boron. The present work is the first report of the 2D ionic boron at atmospheric pressure. The unique electronic structure renders the 2D ionic boron a promising 2D material for applications in nanoelectronics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The ignition behaviour of boron powder, prepared through electrowinning process, was studied by using thermogravimetry coupled with simultaneous differential thermal analysis (TG-SDTA). The dependence of the inception of the ignition reaction on the partial pressure of oxygen, particle size of the boron powder and heating rate was investigated. It was observed that all these factors affect the ignition temperature. Boron powder with a mean particle size of about 10 mu m was found to be susceptible to ignition in oxygen even at 783K. In general, the susceptibility to ignition was found to vary inversely with the degree of crystallinity. Presence of carbon was found to retard the oxidation of boron and raise the ignition temperature. These results are useful in safe handling and storage of finely divided boron powder and in the subsequent production of boron carbide from it. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Theoretical studies using density functional theory are carried out to understand the electronic structure and bonding and electronic properties of elemental beta-rhombohedral boron. The calculated band structure of ideal beta-rhombohedral boron (B-105) shows valence electron deficiency and depicts metallic behavior. This is in contrast to the experimental result that it is a semiconductor. To understand this ambiguity we discuss the electronic structure and bonding of this allotrope with cluster fragment approach using our recently proposed mno rule. This helps us to comprehend in greater detail the structure of B-105 and materials which are closely related to beta-rhombohedral boron. The molecular structures B12H12-2, B28H21+1, BeB27H21, LiB27H21-1, CB27H21+2, B57H36+3, Be3B54H36, and Li2CB54H36, and corresponding solids Li8Be3B102 and Li10CB102 are arrived at using these ideas and studied using first principles density functional theory calculations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fugacity coefficients and isothermal changes of enthalpy have been calculated and reported. The calculations cover a temperature range of 0° to 75°C. up to gas densities of 1.0 gram per cc. The generalized Benedict-Webb-Rubin constants evaluated from generalized PVT relations is found to predict the experimental data with an over-all absolute deviation of 3.1%. Second virial coefficients and potential energy parameters for Lennard-Jones (12-6) potential energy function are reported also.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Reduction of smilagenin acetate (Va) using a boron trifluoride etherate-lithium aluminum hydride reagent, followed by hydrogen peroxide oxidation and acetylation, was found to yield: 3β-ethoxysmilagenin (Vb), 3β-ethoxydihydrosmilagenin acetate (VIa), dihydrosmilagenin diacetate (VIb), and a complex mixture of partially acetylated products. Similar reaction conditions were employed to convert dihydrodiosgenin (II) to dihydrochlorogenin (III). Boron trifluoride etherate-lithium aluminum hydride reduction of 3β-acetoxy-5α-cholestane and 3β-acetoxy-5α-lanostane (VIIIa) was shown to yield the corresponding 3β-ethoxy (e.g., VIIIb) derivatives.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This article describes successful incorporation of multiwalled boron nitride nanotubes (BNNTs) and various functionalized BNNTs by Lewis bases such as trioctylamine (TOA), tributylamine (TBA), and triphenylphosphine (TPP), etc., in organogels formed by triphenylenevinylene (TPV)-based low molecular weight gelator (LMWG) in toluene and consequent characterization of the resulting gel nanocomposites. Functionalized BNNTs were synthesized first,and the presence of tubular structures with high aspect ratio and increased diameter compared to the starting BNNTs was confirmed by SEM. TEM, and Raman spectroscopy. The micrographs of composites of I and BNNTs showed evidence of wrapping of the gelator molecules on to the BNNT surface presumably brought about by pi-pi stacking and van der Waals interactions, This leads to the formation of densely packed and directionally aligned fibrous networks. Such ``reinforced'' aggregation of the gelator molecules in presence of doped BNNTs led to an increase in the sot-to-gel transition temperature and the solidification temperature of the gel nanocomposites as revealed from differential scanning calorimetry. Rheological investigations of the gel nanocomposites indicate that the flow properties of the resulting materials become resistant to applied stress upon incorporation of even a very low wt % of BNNTs. Finally, the increase in thermal conductivity of the nanocomposite compared to the gelator alone was observed for the temperature range of 0-60 degrees C which may make these composites potentially useful in various applications depending on the choice and the amount of BNNT loading in the composite.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A variety of ketoxime ethyl carbonates-easily prepared from the oximes and ethyl chloroformate-undergo the Beckmann rearrangement upon treatment with 1 equivalent of boron trifluoride etherate, in dichloromethane solution at room temperature in excellent yields (generally 75-99%). (C) 2000 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A variety of ketoxime ethyl carbonates-easily prepared from the oximes and ethyl chloroformate-undergo the Beckmann rearrangement upon treatment with 1 equivalent of boron trifluoride etherate, in dichloromethane solution at room temperature in excellent yields (generally 75-99%). (C) 2000 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The electrochemical reduction of oxygen has been studied on gold, boron-doped diamond (BDD) and glassy carbon (GC) electrodes in a ternary eutectic mixture of acetamide (CH3CONH2), urea (NH2CONH2) and ammonium nitrate (NH4NO3). Cyclic voltammetry (CV), differential pulse voltammetry (DPV), chronoamperometry and rotating disk electrode (RDE) voltammetry techniques have been employed to follow oxygen reduction reaction (ORR). The mechanism for the electrochemical reduction of oxygen on polycrystalline gold involves 2-step. 2-electron pathways of O-2 to H2O2 and further reduction of H2O2 to H2O. The first 2-electron reduction of O-2 to H2O2 passes through superoxide intermediate by 1-electron reduction of oxygen. Kinetic results suggest that the initial 1-electron reduction of oxygen to HO2 is the rate-determining step of ORR on gold surfaces. The chronoamperometric and ROE studies show a potential dependent change in the number of electrons on gold electrode. The oxygen reduction reaction on boron-doped diamond (BOO) seems to proceed via a direct 4-electron process. The reduction of oxygen on the glassy carbon (GC) electrode is a single step, irreversible, diffusion limited 2-electron reduction process to peroxide. (C) 2010 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The alloy, Ti-6Al-4V is an alpha + beta Ti alloy that has large prior beta grain size (similar to 2 mm) in the as cast state. Minor addition of B (about 0.1 wt.%) to it refines the grain size significantly as well as produces in-situ TiB needles. The role played by these microstructural modifications on high temperature deformation processing maps of B-modified Ti64 alloys is examined in this paper.Power dissipation efficiency and instability maps have been generated within the temperature range of 750-1000 degrees C and strain rate range of 10(-3)-10(+1) s(-1). Various deformation mechanisms, which operate in different temperature-strain rate regimes, were identified with the aid of the maps and complementary microstructural analysis of the deformed specimens. Results indicate four distinct deformation domains within the range of experimental conditions examined, with the combination of 900-1000 degrees C and 10(-3)-10(-2) s(-1) being the optimum for hot working. In that zone, dynamic globularization of alpha laths is the principle deformation mechanism. The marked reduction in the prior beta grain size, achieved with the addition of B, does not appear to alter this domain markedly. The other domains, with negative values of instability parameter, show undesirable microstructural features such as extensive kinking/bending of alpha laths and breaking of beta laths for Ti64-0.0B as well as generation of voids and cracks in the matrix and TiB needles in the B-modified alloys. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Addition of boron in small quantities to various titanium alloys have shown significant improvement in mechanical behavior of materials. In the present study, electron back-scatter diffraction (EBSD) techniques have been applied to investigate the deformation microstructure evolution in boron modified two-phase titanium alloy Ti-6Al-4V. The alloy was hot compressed at 750 degrees C up to 50% height reduction at two different strain rates (10(-3) s(-1) and 1 s(-1)). The EBSD analyses indicated significant differences in deformed microstructure of the base alloy and the alloy containing boron. A strong subgrain formation tendency was observed along with inhomogeneous distribution of dislocations inside large a colonies of Ti64. In contrast, a colonies were relatively strain free for Ti64 + B, with more uniform dislocation density distribution. The observed difference is attributed to microstructural modifications viz, grain size refinement and presence of TiB particles at grain boundary produced due to boron addition. (C) 2010 Elsevier B.V. All rights reserved.