977 resultados para Ceramic material
Resumo:
Ceramic coatings are produced on aluminum alloy by autocontrol AC pulse Plasma Electrolytic Oxidation (PEO) with stabilized average current. Transient signal gathering system is used to study the current, voltage, and the transient wave during the PEO process. SEM, OM, XRD and EDS are used to study the coatings evolution of morphologies, composition and structure. TEM is used to study the micro profile of the outer looser layer and inner compact layer. Polarization test is used to study the corrosion property of PEO coatings in NaCl solution. According to the test results, AC pulse PEO process can be divided into four stages with different aspects of discharge phenomena, voltage and current. The growth mechanism of AC PEO coating is characterized as anodic reaction and discharge sintering effect. PEO coating can increase the corrosion resistance of aluminum alloy by one order or two; however, too long process time is not necessarily needed to increase the corrosion resistance. In condition of this paper, PEO coating at 60 min is the most protective coating for aluminum alloy substrate. (C) 2008 Elsevier B.V. All fights reserved.
Resumo:
The effect of a negative Poisson ratio is experimentally revealed in the tension deformation of a natural layered ceramic. This effect can increase the volume strain energy per unit volume by 1100% and, simultaneously, decrease the deformation strain energy per unit volume by about 44%, so that it effectively enhances the deformation capacity by about 1 order of magnitude in the tension of the material. The present study also shows that the physical mechanisms producing the effect are attributed to the climbing on one another of the nanostructures in the natural material, which provides a guide to the design of synthetic toughening composites.
Resumo:
This paper combines the four-point bending test, SEM and finite element method to study the interface fracture property of PEO coatings on aluminum alloy. The interface failure mode of the coating on the compression side is revealed. The ceramic coating crack firstly along the 45 degrees to the interface, then the micro crack in the coating deduces the interface crack. The plastic deformation observed by SEM shows excellent adhesion property between the coating and substrate. The plastic deformation in the substrate is due to the interfacial crack extension, so the interface crack mode of PEO coatings is ductile crack. The results of FEM show that the compression strength is about 600 MPa. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Two types of peeling experiments are performed in the present research. One is for the Al film/Al2O3 substrate system with an adhesive layer between the film and the substrate. The other one is for the Cu film/Al2O3 substrate system without adhesive layer between the film and the substrate, and the Cu films are electroplated onto the Al2O3 substrates. For the case with adhesive layer, two kinds of adhesives are selected, which are all the mixtures of epoxy and polyimide with mass ratios 1:1.5 and 1:1, respectively. The relationships between energy release rate, the film thickness and the adhesive layer thickness are measured during the steady-state peeling process. The effects of the adhesive layer on the energy release rate are analyzed. Using the experimental results, several analytical criteria for the steady-state peeling based on the bending model and on the two-dimensional finite element analysis model are critically assessed. Through assessment of analytical models, we find that the cohesive zone criterion based on the beam bend model is suitable for a weak interface strength case and it describes a macroscale fracture process zone case, while the two-dimensional finite element model is effective to both the strong interface and weak interface, and it describes a small-scale fracture process zone case. (C) 2007 Elsevier Ltd. All rights reserved.
Resumo:
In the present study, peel tests and inverse analysis were performed to determine the interfacial mechanical parameters for the metal film/ceramic system with an epoxy interface layer between film and ceramic. Al films with a series of thicknesses between 20 and 250 mu m and three peel angles of 90 degrees, 135 degrees and 180 degrees were considered. A finite element model with the cohesive zone elements was used to simulate the peeling process. The finite element results were taken as the training data of a neural network in the inverse analysis. The interfacial cohesive energy and the separation strength can be determined based on the inverse analysis and peel experimental result.
Resumo:
This paper studies the surface melting in the atmosphere by YAG laser-guided micro-arc discharge. In three kinds of surface conditions (free, oiled, and polyethylene covered), we try to control the diameter and the power density of discharge pit. It is found that the power density of 3 x 10(6) W/cm(2) of discharge pit on the oiled surface is moderate to form the melted layer thicker than that of the others, adapting to strengthen the surface of material, and the power density of 1.07 x 10(7) W/cm(2) of discharge pit on the polyethylene-covered surface is highest to form the deepest discharge pit among them, adapting to remove the material.
Resumo:
An analysis on crack creep propagation problem of power-law nonlinear viscoelastic materials is presented. The creep incompressilility assumption is used. To simulate fracture behavior of craze region, it is assumed that in the fracture process zone near the crack tip, the cohesive stress sigma(f) acts upon the crack surfaces and resists crack opening. Through a perturbation method, i. e., by superposing the Mode-I applied force onto a referential uniform stress state, which has a trivial solution and gives no effect on the solution of the original problem, the nonlinear viscoelastic problem is reduced to linear problem. For weak nonlinear materials, for which the power-law index n similar or equal to 1, the expressions of stress and crack surface displacement are derived. Then, the fracture process zone local energy criterion is proposed and based on which the formulas of cracking incubation time t
Resumo:
In this paper, the dynamic response of a penny-shaped interface crack in bonded dissimilar homogeneous half-spaces is studied. It is assumed that the two materials are bonded together with such a inhomogeneous interlayer that makes the elastic modulus in the direction perpendicular to the crack surface is continuous throughout the space. The crack surfaces art assumed to be subjected to torsional impact loading. Laplace and Hankel integral transforms are applied combining with a dislocation density,function to reduce the mixed boundary value problem into a singular integral equation with a generalized Cauchy kernel in Laplace domain. By solving the singular integral equation numerically, and using a numerical Laplace inversion technique, the dynamic stress intensity factors art obtained. The influences of material properties and interlayer thickness on the dynamic stress intensity factor are investigated.
Resumo:
Abstract: During extensive salvage excavations carried out during the years 2004-2008 in a large Early Islamic industrial area at the vicinities of Ramla, in Central Israel, an unparalleled industrial device was unearthed. The star-shaped, soil embedded installation, whose lower part was preserved, consisted of a central pottery jar surrounded by five minor jars, linked by ceramic pipes. Evidence of heat was observed mainly around the central vessel, and metal hollow cones perforated in the tip were found inside the surrounding jars. Although the manufacturing procedures and operation techniques of the installation are not completely clear, it is proposed that the installation is part of an industrial workshop or an alchemy laboratory. Both industry and alchemy were well-developed during the Early Islamic period and very often closely related, to the point that sometimes it is difficult to distinguish between them. The identification proposed is based on comparisons with tools described in literary sources, and somewhat later drawings and etchings. Circumstantial ceramic evidence was found, as well as the proximity of a bathhouse whose guests could have been the consumers of perfumes and unguents seem to reinforce this possibility. Due to the poor state of preservation of the device and the lack of available comparisons, the identification proposed here is tentative, and future research coupled with eventual new discoveries is needed in order to clarify this matter.
Resumo:
Multilayer ceramic coatings were fabricated on steel substrate using a combined technique of hot dipping aluminum(HDA) and plasma electrolytic oxidation(PEO). A triangle of normalized layer thickness was created for describing thickness ratios of HDA/PEO coatings. Then, the effect of thickness ratio on stresses field of HDA/PEO coatings subjected to uniform normal contact load was investigated by finite element method. Results show that the surface tensile stress is mainly affected by the thickness ratio of Al layer when the total thickness of coating is unchanged. With the increase of A] layer thickness, the surface tensile stress rises quickly. When Al2O3 layer thickness increases, surface tensile stress is diminished. 'Meanwhile, the maximum shear stress moves rapidly towards internal part of HDA/PEO coatings. Shear stress at the Al2O3/Al interface is minimal when Al2O3 layer and Al layer have the same thickness.
Resumo:
Many physical experiments have shown that the domain switching in a ferroelectric material is a complicated evolution process of the domain wall with the variation of stress and electric field. According to this mechanism, the volume fraction of the domain switching is introduced in the constitutive law of ferroelectric ceramic and used to study the nonlinear constitutive behavior of ferroelectric body in this paper. The principle of stationary total energy is put forward in which the basic unknown quantities are the displacement u (i) , electric displacement D (i) and volume fraction rho (I) of the domain switching for the variant I. Mechanical field equation and a new domain switching criterion are obtained from the principle of stationary total energy. The domain switching criterion proposed in this paper is an expansion and development of the energy criterion. On the basis of the domain switching criterion, a set of linear algebraic equations for the volume fraction rho (I) of domain switching is obtained, in which the coefficients of the linear algebraic equations only contain the unknown strain and electric fields. Then a single domain mechanical model is proposed in this paper. The poled ferroelectric specimen is considered as a transversely isotropic single domain. By using the partial experimental results, the hardening relation between the driving force of domain switching and the volume fraction of domain switching can be calibrated. Then the electromechanical response can be calculated on the basis of the calibrated hardening relation. The results involve the electric butterfly shaped curves of axial strain versus axial electric field, the hysteresis loops of electric displacement versus electric filed and the evolution process of the domain switching in the ferroelectric specimens under uniaxial coupled stress and electric field loading. The present theoretic prediction agrees reasonably with the experimental results given by Lynch.
Resumo:
Ceramic coatings were formed by plasma electrolytic oxidation (PEO) on aluminized steel. Characteristics of the average anodic voltages versus treatment time were observed during the PEO process. The micrographs, compositions and mechanical properties of ceramic coatings were investigated. The results show that the anodic voltage profile for processing of aluminized steel is similar to that for processing bulk Al alloy during early PEO stages and that the thickness of ceramic coating increases approximately linearly with the Al layer consumption. Once the Al layer is completely transformed, the FeAl intermetallic layer begins to participate in the PEO process. At this point, the anodic voltage of aluminized steel descends, and the thickness of ceramic coating grows more slowly. At the same time, some micro-cracks are observed at the Al2O3/FeAl interface. The final ceramic coating mainly consists of gamma-Al2O3, mullite, and alpha-Al2O3 phases. PEO ceramic coatings have excellent elastic recovery and high load supporting performance. Nanohardness of ceramic coating reaches about 19.6 GPa. (c) 2007 Elsevier B. V. All rights reserved.
Resumo:
Peel test measurements have been performed to estimate both the interface toughness and the separation strength between copper thin film and Al2O3 substrate with film thicknesses ranging between 1 and 15 mu m. An inverse analysis based on the artificial neural network method is adopted to determine the interface parameters. The interface parameters are characterized by the cohesive zone (CZ) model. The results of finite element simulations based on the strain gradient plasticity theory are used to train the artificial neural network. Using both the trained neural network and the experimental measurements for one test result, both the interface toughness and the separation strength are determined. Finally, the finite element predictions adopting the determined interface parameters are performed for the other film thickness cases, and are in agreement with the experimental results.
Resumo:
El presente trabajo de investigación se estableció entre los meses de Abril- Junio, 2013, en el vivero de la Facultad de Recursos Naturales de la Universidad Nacional Agraria, con la finalidad de evaluar germinación y sobrevivencia de las plántulas, afectaciones por plagas y enfermedades, altura de la planta, diámetro basal del tallo, número de hojas, tasa de crecimiento en función de la altura, longitud de la raíz principal, numero de raíces, diámetro de la raíz principal, peso fresco y seco de la parte aérea de la planta y su raíz de dos poblaciones de Moringa oleifera: acriollada y mejorada PKM1. Se utilizó un Diseño Completamente Aleatorizado con 20 repeticiones para las primeras 8 variables y 8 repeticiones para las 5 últimas variables en ambos tratamientos. Durante el periodo experimental, M. oleifera acriollada presentó un porcentaje de germinación de 98.33% mientras que PKM1 de 78.30%, en cuanto a la sobrevivencia para acriollada fue de 99.43% y la PKM1 de 97.16%. Las dos poblaciones fueron afectadas por Zompopo (Atta. spp) siendo la más afectada PKM1 con él 90% consideradas como susceptibles. Al final de la evaluación se observaron diferencias estadísticas (P <0.05) a favor de Moringa acriollada en: altura de la planta, diámetro basal del tallo, numero de hojas, tasa de crecimiento en función de la altura, longitud de la raíz principal, número de raíces, diámetro de la raíz principal, peso seco de la raíz. El peso seco de la parte aérea no mostró diferencias estadísticas (P <0.05) entre tratamientos. Mediante el análisis se demostró que existe comportamiento diferente de crecimiento entre los tratamientos evaluados, aun cuando el material acriollado exhibió mejores resultados en la mayoría de las variables medidas ambos presentaron un buen comportamiento en la fase de vivero.