669 resultados para Aluminum alloy 2524
Resumo:
Plates of NbTi (50:50, by weight) were nitrided in a nitrogen atmosphere in the temperature range 800-1000 °C for 15, 30, 60, 120 and 180 min. X-Ray diffraction and optical and electronic microscopy were used to characterize the samples. Two nitride layers were identified on the substrate: an external and continuous phase of TiN, named δ, and a deeper and discontinuous phase of Ti 2N, named ε{lunate}. The electron micrographs reveal the presence of paths rich in Nb which may be responsible for the diffusion of nitrogen into the matrix. © 1993.
Resumo:
Recasting process influence upon corrosion behavior of Co-Cr-Mo dental alloy in simulated physiological serum has been investigated using chemical and electrochemical techniques. Recast Co-Cr-Mo alloy by induction (IND) or by blowtorch (FLAME) has exhibited similar dendritic structures. Both IND and FLAME alloys have presented good corrosion resistance in physiological serum. Passivation process provides this corrosion resistance. Codissolution makes this process difficult. Passive films, formed on these alloys, have been analyzed as a dual layer consisting of an inner barrier and an outer porous layer. Passive film protective characteristics are higher in FLAME than in IND alloy. On this last alloy, the passive film is more porous due to a higher Codissolution. ©Carl Hanser Verlag, München.
Resumo:
The mechanism of electrochemical oxidation of surface reformed CuA1Ag alloys having different composition of heat treatment, in 0.5 M NaOH was studied by means of cyclic polarization, constant potential electrolysis, ICP, AA, SEM and EDX. The surface reformation consisted of a repetitive triangular potential sweep (RTPS) between H 2 and O 2 evolution at 100 mV s -1 in the working solution itself, performed in order to increase the electrode roughness and obtain a quasi-stationary I/E profile in which the potentiodynamic behaviour of copper and silver was clearly revealed. The alloys suffer aluminum dealloying after such an RTPS. The quasi-stationary cyclic polarization curve exhibits a multiplicity of current peaks which have been related to the electrochemical reactions involving the pure alloying elements. Complex potential perturbation programmes in regions having different anodic and cathodic limits allowed the study of the mechanism of the electrochemical oxidation of the surface reformed alloys and the compare with that corresponding to the pure metals. The basic differences between the electro-oxidation processes of the surface reformed CuA1Ag alloys with respect to those established for the high purity alloying metals are the splitting of the peaks corresponding to the formation of the Cu(I) and Ag(I) species. © 1991.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Purpose: In the present work, a susceptibility and efficacy of the Ti–7.5Mo alloy and Ti alloy to bacterial biofilm formation after surface treatment was evaluated. Methods and materials: The alloy Ti–7.5Mo was obtained in arc furnace under an argon atmosphere. Ingots were then homogenized under vacuum at 1100 °C for 86.4 ks to eliminate chemical segregation and after cold worked discs were cutting. Samples were immersed in NaOH aqueous solution (5 M) and treated at 450 °C. Biofilms were grown in Ti–7.5Mo discs immersed in sterile brain heart infusion broth (BHI)containing 5% sucrose, inoculated with microbial suspension (106 cells/ml) and incubated for 5 days. Next, the discs were placed in tubes with sterile physiological solution 0.9% sodium chloride (NaCl) and sonicated for to disperse the biofilms. Tenfold serial dilutions were carried and aliquots seeded in selective agar, which were then incubated for 48 h. Then, the numbers CFU/ml (log 10) were counted and analyzed statistically. Scanning electron microscopy (SEM) on discs with biofilms groups was performed, atomic force microscope (AFM) and contact angle. Results: The results show that there is a 5% difference in bacterial adhesion between pure titanium and Ti–7.5Mo alloy. Conclusion: It was concluded that the greater the roughness, the greater the hydrophilic effect.
Resumo:
The purpose of the study was to evaluate the influence of the biomimetic surface treatment in osseointegration of experimental alloy Ti30Ta for dentistry applications. Methods and materials: Experimental alloy with Ta concentration of 30 wt% was produced from sheets of commercially pure titanium (99.9%) and tantalum (99.9%). Ingots were melted in an arc furnace under an argon atmosphere and re-melted ten times at least. They were homogenized under vacuum at 1100 °C for 86.4 ks to eliminate chemical segregation and cold-worked by swaging. Implants with 2.5 mm diameter and 2.0 mm of height were machined (Fig. 1a), treated and inserted in animals for in vivo study. The implants were submitted surface treatment according methodology development for our group. Analyzes were performed by Scanning Electron microscopy (SEM), Atomic Force Microscopy (AFM). Osteoblast morphology on Ti-30Ta alloys was examined after 4 and 7 days of incubation with MSCs using SEM imaging.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pós-graduação em Ciência e Tecnologia de Materiais - FC
Resumo:
O principal objetivo desse trabalho é investigar a influência dos parâmetros térmicos velocidade de solidificação (VL) e taxa de resfriamento (TR), nos espaçamentos dendríticos primários (λ1) da liga hipoeutética Al-7%Si, durante a solidificação direcional horizontal, em regime transiente. Os valores de λ1 foram medidos ao longo do comprimento do lingote e correlacionados com esses parâmetros. A variação dos espaçamentos dendríticos estudados é expressa por meio de funções na forma de potência de VLe TRdadas, respectivamente, por λ1= 55(VL)-1.1e λ1= 212 (TR)-0.55. Um estudo comparativo é realizado entre os resultados encontrados nesse trabalho e aqueles obtidos para a mesma liga quando solidificada direcionalmente nos sistemas verticais ascendente e descendente, sob as mesmas condições assumidas. Finalmente, os resultados experimentais obtidos são comparados com valores fornecidos por alguns modelos teóricos propostos na literatura para analisar espaçamentos dendríticos primários.
Resumo:
INVESTIGATION INTO CURRENT EFFICIENCY FOR PULSE ELECTROCHEMICAL MACHINING OF NICKEL ALLOY Yu Zhang, M.S. University of Nebraska, 2010 Adviser: Kamlakar P. Rajurkar Electrochemical machining (ECM) is a nontraditional manufacturing process that can machine difficult-to-cut materials. In ECM, material is removed by controlled electrochemical dissolution of an anodic workpiece in an electrochemical cell. ECM has extensive applications in automotive, petroleum, aerospace, textile, medical, and electronics industries. Improving current efficiency is a challenging task for any electro-physical or electrochemical machining processes. The current efficiency is defined as the ratio of the observed amount of metal dissolved to the theoretical amount predicted from Faraday’s law, for the same specified conditions of electrochemical equivalent, current, etc [1]. In macro ECM, electrolyte conductivity greatly influences the current efficiency of the process. Since there is a certain limit to enhance the conductivity of the electrolyte, a process innovation is needed for further improvement in current efficiency in ECM. Pulse electrochemical machining (PECM) is one such approach in which the electrolyte conductivity is improved by electrolyte flushing in pulse off-time. The aim of this research is to study the influence of major factors on current efficiency in a pulse electrochemical machining process in macro scale and to develop a linear regression model for predicting current efficiency of the process. An in-house designed electrochemical cell was used for machining nickel alloy (ASTM B435) by PECM. The effects of current density, type of electrolyte, and electrolyte flow rate, on current efficiency under different experimental conditions were studied. Results indicated that current efficiency is dependent on electrolyte, electrolyte flow rate, and current density. Linear regression models of current efficiency were compared with twenty new data points graphically and quantitatively. Models developed were close enough to the actual results to be reliable. In addition, an attempt has been made in this work to consider those factors in PECM that have not been investigated in earlier works. This was done by simulating the process by using COMSOL software. However, it was found that the results from this attempt were not substantially different from the earlier reported studies.
Resumo:
Research has provided no definitive answers on whether PET plastic bottles or aluminum cans are a more environmentally sustainable choice as soda containers. This paper researches the fuel used in recycling each of these materials from Yellowstone National Park to processing locations. The data is used to determine which of these alternatives use less fuel in this process. It was found that plastics use more fuel when transported from Yellowstone National Park to the processing center. Aluminum uses less fuel per ton to transport from Yellowstone to the processing center. The conclusions from this research may have implications on which material would be advised to use in selling soda in Yellowstone National Park.
Resumo:
The corrosion protection of AA6063 aluminium alloy by cerium conversion, polyaniline conducting polymer and by duplex coatings has been investigated. The electrochemical behaviour was evaluated in aerated 3.5 wt.% NaCl. All coatings tested shifted the corrosion and pitting potentials to more positive values, indicating protection against corrosion. The duplex coatings are significantly more effective than each coating alone: corrosion and pitting potentials were shifted by +183 and +417 mV(SCE), respectively, by duplex coatings in relation to the untreated aluminium alloy. Optical microscopy and scanning electron microscopy are in agreement with the electrochemical results, reinforcing the superior performance of duplex coatings. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
Dental implants have increased the use of titanium and titanium alloys in prosthetic applications. Whitening toothpastes with peroxides are available for patients with high aesthetic requirements, but the effect of whitening toothpastes on titanium surfaces is not yet known, although titanium is prone to fluoride ion attack. Thus, the aim of the present study was to compare Ti-5Ta alloy to cp Ti after toothbrushing with whitening and conventional toothpastes. Ti-5Ta (%wt) alloy was melted in an arc melting furnace and compared with cp Ti. Disks and toothbrush heads were embedded in PVC rings to be mounted onto a toothbrushing test apparatus. A total of 260,000 cycles were carried out at 250 cycles/minute under a load of 5 N on samples immersed in toothpaste slurries. Surface roughness and Vickers microhardness were evaluated before and after toothbrushing. One sample of each material/toothpaste was analyzed by Scanning Electron Microscopy (SEM) and compared with a sample that had not been submitted to toothbrushing. Surface roughness increased significantly after toothbrushing, but no differences were noted after toothbrushing with different toothpastes. Toothbrushing did not significantly affect sample microhardness. The results suggest that toothpastes that contain and those that do not contain peroxides in their composition have different effects on cp Ti and Ti-5Ta surfaces. Although no significant difference was noted in the microhardness and roughness of the surfaces brushed with different toothpastes, both toothpastes increased roughness after toothbrushing.