Resumo

The purpose of the study was to evaluate the influence of the biomimetic surface treatment in osseointegration of experimental alloy Ti30Ta for dentistry applications. Methods and materials: Experimental alloy with Ta concentration of 30 wt% was produced from sheets of commercially pure titanium (99.9%) and tantalum (99.9%). Ingots were melted in an arc furnace under an argon atmosphere and re-melted ten times at least. They were homogenized under vacuum at 1100 °C for 86.4 ks to eliminate chemical segregation and cold-worked by swaging. Implants with 2.5 mm diameter and 2.0 mm of height were machined (Fig. 1a), treated and inserted in animals for in vivo study. The implants were submitted surface treatment according methodology development for our group. Analyzes were performed by Scanning Electron microscopy (SEM), Atomic Force Microscopy (AFM). Osteoblast morphology on Ti-30Ta alloys was examined after 4 and 7 days of incubation with MSCs using SEM imaging.

Formato

e95-e96

Identificador

http://dx.doi.org/10.1016/j.dental.2013.08.197

Dental Materials, v. 29, n. 12, p. e95-e96, 2013.

0109-5641

http://hdl.handle.net/11449/135386

10.1016/j.dental.2013.08.197

9184489134524097

Idioma(s)

eng

Relação

Dental Materials

Direitos

closedAccess

Palavras-Chave #Titanium #Dental alloy #Surface treatment
Tipo

info:eu-repo/semantics/conferenceObject