939 resultados para laser ion source
Resumo:
In this paper, we demonstrated a dual-wavelength competitive output in Nd:Y3SC1.5Al3.5O12 ceramic disk laser. Different dual-wavelength output behaviors for Nd:YSAG and Nd:YAG ceramic disk laser were investigated and discussed. By applying the energy transfer model, we suggested the reasonable explanation for this new phenomenon as the disordered replacing of Al3+ ions by Sc3+ ions. The main advantage of the dual-wavelength ceramic laser is the possibility to serve as the seed source to generate Terahertz radiation. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
A novel Vb(3+)-Er-(3+) codoped phosphate glass for high power flashlamp pumping and high repetition rate laser at 1.54 mu m, designated EAT5-2, is developed. The weight-loss rate of is 1.3 x 10(-5) gcm(-2) h(-1) in boiling water, which is comparable to Kigre's QX-Er glass. Some spectroscopic parameters are analysed by Judd-Ofelt theory and McCumber theory The emission cross section is calculated to be 0.73 x 10(-20) cm(2). The thermo-mechanical properties of EAT5-2 are modified after an ion-exchange chemical strengthening process in a KNO3/NaNO3 molten salt bath. The thresholds for optical damage from the flashlamp pumping are tested on glass rods. A repetition rate of 15 Hz is achieved for chemically strengthened glass. The laser experimental results at. 1.54 mu m from flashlamp pumping are also reported.
Resumo:
We report on the fabrication and characterization of low-loss planar and stripe waveguides in a Nd3+-doped glass by 6 MeV oxygen-ion implantation at a dose of 1x10(15) ions/cm(2). The dark mode spectroscopy of the planar waveguide was measured using a prism coupling arrangement. The refractive index profile of the planar waveguide was reconstructed from a code based on the reflectivity calculation method. The results indicate that a refractive index enhanced region as well as an optical barrier have been created after the ion beam processing. The near-field mode profiles of the stripe waveguide were obtained by an end-fire coupling arrangement, by which three quasitransverse electric modes were observed. After annealing, the propagation losses of the planar and stripe waveguides were reduced to be similar to 0.5 and similar to 1.8 dB/cm, respectively. (c) 2007 American Institute of Physics.
Resumo:
Broadband infrared luminescence centred at around 1300 nm with full-width at half maximum of about 342 nm was observed from transparent Ni2+-doped lithium-alumino-silicate glass-ceramics embedded with beta-eucryptite crystallines. The room temperature fluorescent lifetime was 98 mu s. The transparent glass-ceramics may have potential applications in a widely tunable laser and a super-broadband optical amplifier for optical communications.
Resumo:
The spectral properties in different concentration of Yb ions (0.5-5 mol%)-doped silica glasses are explored in this paper. The glasses are prepared by traditional melting method. The absorption spectra and the fluorescent lifetime (tau(f)) are measured at room temperature and low temperature (18 K). The stimulated cross-section (sigma(emi)) and potential laser properties (beta(min), I-sat, I-min) are calculated based on the absorption spectra. The absorption cross-section (sigma(abs)) are in the range 1.08 x 10(-20) - 1.18 x 10(-20) cm(2) in different glasses, the fluorescence lifetime (tau(f)) change from 1.9 to 1.2 ms with the increase of Yb3+ concentration. The potential laser properties indicate that lead silica glass is a good host for highly Yb ion doping glass. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Nd:silicate glass was implanted at room temperature by 6.0 MeV C3+ ions with a dose of 2.0 x 10(15) ions cm(-2). A waveguide with thickness of about 6.3 mu m was formed. The prism-coupling method was used to observe the dark modes of the waveguide at 633 nm and 1539 nm, respectively. There are three dark modes at 633 nm, of which one is the enhanced-index mode. The propagation loss of the enhanced-index mode in the waveguide measured at 633 nm is 0.42 dB cm(-1) after annealing at 217 degrees C for 35 min. The reflectivity calculation method was applied to simulate the refractive index profiles in the waveguide. The mode optical near-field output at 633 nm was presented.
Resumo:
We demonstrate, for the first time as far as Re known, a passively Q-switched operation of a Nd:YVO4 laser in which a Cr4+:YAG crystal and a laser-diode bar are used as the saturable absorber and the pump source, respectively. Stable laser pulses as short as 28 ns with 20-mu J energy can be generated with this laser, which has the advantages of simplicity, high efficiency, and good long-term stability. (C) 1997 Optical Society of America.
Resumo:
By using a continuous-wave Ti:sapphire laser as a pumping source, we demonstrated a passively Q-switched Yb:YAG laser at room temperature with Cr4+:YAG as the saturable absorber. We achieved an average output power of as much as 55 mW at 1.03 mum with a pulse width (FWHM) as short as 350 ns. The initial transmission of the Cr4+:YAG has an effect on the pulse duration (FWHM) and the repetition rate of the Yb:YAG passively Q-switched laser. The Yb:YAG crystal can be a most promising passively Q-switched laser crystal for compact, efficient, solid-state lasers. (C) 2001 Optical Society of America.
Resumo:
By use of a laser diode as a pump source, a self-Q-switched laser from a Cr,Nd:YAG crystal is demonstrated. The output Q-switched traces are very stable, the threshold pump power is 3.5 W, the pulse duration is 50 ns, and the slope efficiency is as high as 20%. In addition, the pulse width remains constant while the pulse repetition rate Varies with pump power. (C) 2000 Optical Society of America OCIS codes: 140.0140, 140.2020, 140.3380, 140.3480, 140.3540, 140.3580.
Three-photon-excited upconversion luminescence of Ce3+: YAP crystal by femtosecond laser irradiation
Resumo:
Infrared to ultraviolet and visible upconversion luminescence was demonstrated in trivalent cerium doped YAlO3 crystal (Ce3+: YAP) under focused infrared femtosecond laser irradiation. The fluorescence spectra show that the upconverted luminescence comes from the 5d-4f transitions of trivalent cerium ions. The dependence of luminescence intensity of trivalent cerium on infrared pumping power reveals that the conversion of infrared radiation is dominated by three-photon excitation process. It is suggested that the simultaneous absorption of three infrared photons pumps the Ce3+ ion into upper 5d level, which quickly nonradiatively relax to lowest 5d level. Thereafter, the ions radiatively return to the ground states, leading to the characteristic emission of Ce3+. (c) 2005 Optical Society of America.
Resumo:
By using a pump recycling configuration, the maximum power of 8.1 W in the wavelength range 1.935-1.938 mu m is generated by a 5-mm long Tm:YAlO3 (4 at. %) laser operating at 18 degrees C with a pump power of 24 W. The highest slope efficiency of 42% is attained, and the pump quantum efficiency is up to 100%. The Tm:YAlO3 laser is employed as a pumping source of singly-doped Ho(l%):GdVO4 laser operating at room temperature, in which continuous wave output power of greater than 0.2 W at 2.05 mu m is achieved with a slope efficiency of 9%.
Resumo:
ZrO2, films were deposited by electron-beam evaporation with the oxygen partial pressure varying from 3 X 10(-3) Pa to I I X 10(-3) Pa. The phase structure of the samples was characterized by x-ray diffraction (XRD). The thermal absorption of the films was measured by the surface thermal lensing technique. A spectrophotometer was employed to measure the refractive indices of the samples. The laser-induced damage threshold (LIDT) was assessed using a 1064, nm Nd: yttritium-aluminium-garnet pulsed laser at pulse width of 12 ns. The influence of oxygen partial pressure on the microstructure and LIDT of ZrO2 films was investigated. XRD data revealed that the films changed from polycrystalline to amorphous as the oxygen partial pressure increased. The variation of refractive index at 550 nm wavelength indicated that the packing density of the films decreased gradually with increasing oxygen partial pressure. The absorptance of the samples decreased monotonically from 125.2 to 84.5 ppm with increasing oxygen partial pressure. The damage threshold, values increased from 18.5 to 26.7 J/cm(2) for oxygen partial pressures varying from 3 X 10(-3) Pa to 9 X 10(-3) Pa, but decreased to 17.3 J/cm(2) in the case of I I X 10(-3) Pa. (C) 2005 American Vacuum Society.
Resumo:
ZrO2, films were deposited by electron-beam evaporation with the oxygen partial pressure varying from 3 X 10(-3) Pa to I I X 10(-3) Pa. The phase structure of the samples was characterized by x-ray diffraction (XRD). The thermal absorption of the films was measured by the surface thermal lensing technique. A spectrophotometer was employed to measure the refractive indices of the samples. The laser-induced damage threshold (LIDT) was assessed using a 1064, nm Nd: yttritium-aluminium-garnet pulsed laser at pulse width of 12 ns. The influence of oxygen partial pressure on the microstructure and LIDT of ZrO2 films was investigated. XRD data revealed that the films changed from polycrystalline to amorphous as the oxygen partial pressure increased. The variation of refractive index at 550 nm wavelength indicated that the packing density of the films decreased gradually with increasing oxygen partial pressure. The absorptance of the samples decreased monotonically from 125.2 to 84.5 ppm with increasing oxygen partial pressure. The damage threshold, values increased from 18.5 to 26.7 J/cm(2) for oxygen partial pressures varying from 3 X 10(-3) Pa to 9 X 10(-3) Pa, but decreased to 17.3 J/cm(2) in the case of I I X 10(-3) Pa. (C) 2005 American Vacuum Society.
Resumo:
探讨了HfO2薄膜中负离子元素杂质破坏模型,并得出薄膜中的杂质主要来源于镀膜材料。用电子束蒸发方法沉积两种不同Cl元素古量的HfO2薄膜,测定薄膜弱吸收和损伤阈值来验证负离子元素破坏模型。结果表明,随着Cl元素含量的增加薄膜的弱吸收增加损伤阈值减小。这主要是因为负离子元素在蒸发过程中形成挥发性的气源中心而产生缺陷,缺陷在激光辐照过程中又形成吸收中心.因此负离子元素的存在将加速薄膜的破坏。
Resumo:
The single-sided and dual-sided high reflective mirrors were deposited with ion-beam sputtering (IBS). When the incident light entered with 45 degrees, the reflectance of p-polarized light at 1064 nm exceeded 99.5%. Spectrum was gained by spectrometer and weak absorption of coatings was measured by surface thermal lensing (STL) technique. Laser-induced damage threshold (LIDT) was determined and the damage morphology was observed with Lecia-DMRXE microscope simultaneously. The profile of coatings was measured with Mark III-GPI digital interferometer. It was found that the reflectivity of mirror exceeded 99.9% and its absorption was as low as 14 ppm. The reflective bandwidth of the dual-sided sample was about 43 nm wider than that of single-sided sample, and its LIDT was as high as 28 J/cm2, which was 5 J/cm2 higher than that of single-sided sample. Moreover, the profile of dual-sided sample was better than that of substrate without coatings.