982 resultados para Magnetic Properties
Resumo:
The crystal structure and magnetic properties of Sn1-xFexO2 nanograins synthesized by simple hydrothermal method using SnCl4 center dot 5H(2)O and FeCl3 center dot 6H(2)O as raw materials are studied. No secondary phase was found in the XRD spectrum. The linear change of lattice volume for different Fe content strongly supports that the Fe3+ substitutes Sn4+ in SnO2 lattice. A Raman and IR spectra study indicated that the Fe incorporates into the SnO2 lattice. Both ferromagnetic and paramagnetic signals are detected in the Mossbauer spectra. The Sn1-xFexO2 (x <= 0.10) samples show room-temperature ferromagnetism (RTFM) and the saturation magnetization increased with increasing Fe percent. Fe ions present three kinds of magnetic behaviors including paramagnetic, ferromagnetic, and antiferromagnetic in the samples observed by investigation of the M-H and M-T curves. The weak RTFM was due to only a fraction of Fe ions contributing to magnetic-order coupling mediated by oxygen vacancy.
Resumo:
The magnetic properties of naturally layered intermetallic compound SmMn2Si2 with textured structure have been studied. There exist a ferromagnetic transition at 35 K and two antiferromagnetic transitions at 120 and 230 K. The antiferromagnetic state below 230 K exhibits different magnetoresistance, with a negative magnetoresistance of 3%-4% for current I applied perpendicular to the c axis and with a positive magnetoresistance effect of about 4%-6% for current I parallel to the c axis. The observed magnetoresistance is likely to be related to magnetovolume effects. In the ferromagnetic state, a positive magnetoresistance with a maximum increase of 22% under an applied field of 5 T is observed at 4 K, and both H perpendicular to I and H parallel to I configurations show positive magnetoresistance. (C) 1997 American Institute of Physics.
Resumo:
Este trabalho centra-se na investigação da possibilidade de se conseguir um semicondutor magnético diluído (SMD) baseado em ZnO. Foi levado a cabo um estudo detalhado das propriedades magnéticas e estruturais de estruturas de ZnO, nomeadamente nanofios (NFs), nanocristais (NCs) e filmes finos, dopadas com metais de transição (MTs). Foram usadas várias técnicas experimentais para caracterizar estas estruturas, designadamente difracção de raios-X, microscopia electrónica de varrimento, ressonância magnética, SQUID, e medidas de transporte. Foram incorporados substitucionalmente nos sítios do Zn iões de Mn2+ e Co2+ em ambos os NFs e NCs de ZnO. Revelou-se para ambos os iões dopantes, que a incorporação é heterogénea, uma vez que parte do sinal de ressonância paramagnética electrónica (RPE) vem de iões de MTs em ambientes distorcidos ou enriquecidos com MTs. A partir das intensidades relativas dos espectros de RPE e de modificações da superfície, demonstra-se ainda que os NCs exibem uma estrutura core-shell. Os resultados, evidenciam que, com o aumento da concentração de MTs, a dimensão dos NCs diminui e aumentam as distorções da rede. Finalmente, no caso dos NCs dopados com Mn, obteve-se o resultado singular de que a espessura da shell é da ordem de 0.3 nm e de que existe uma acumulação de Mn na mesma. Com o objectivo de esclarecer o papel dos portadores de carga na medição das interacções ferromagnéticas, foram co-dopados filmes de ZnO com Mn e Al ou com Co e Al. Os filmes dopados com Mn, revelaram-se simplesmente paramagnéticos, com os iões de Mn substitucionais nos sítios do Zn. Por outro lado, os filmes dopados com Co exibem ferromagnetismo fraco não intrínseco, provavelmente devido a decomposição spinodal. Foram ainda efectuados estudos comparativos com filmes de ligas de Zn1-xFexO. Como era de esperar, detectaram-se segundas fases de espinela e de óxido de ferro nestas ligas; todas as amostras exibiam curvas de histerese a 300 K. Estes resultados suportam a hipótese de que as segundas fases são responsáveis pelo comportamento magnético observado em muitos sistemas baseados em ZnO. Não se observou nenhuma evidência de ferromagnetismo mediado por portadores de carga. As experiências mostram que a análise de RPE permite demonstrar directamente se e onde estão incorporados os iões de MTs e evidenciam a importância dos efeitos de superfície para dimensões menores que ~15 nm, para as quais se formam estruturas core-shell. As investigações realizadas no âmbito desta tese demonstram que nenhuma das amostras de ZnO estudadas exibiram propriedades de um SMD intrínseco e que, no futuro, são necessários estudos teóricos e experimentais detalhados das interacções de troca entre os iões de MTs e os átomos do ZnO para determinar a origem das propriedades magnéticas observadas.
Resumo:
Single crystals of (Bal - xKx)Fe2As2 were prepared using the Sn flux method. Two heating methods were used to prepare the single crystals: the slow heating and rapid heating methods. It was found that the single crystals grown using the slow heating method were not superconducting due to a significant loss of potassium. When the rapid heating method was used, the single crystals were observed to be superconducting with the desired potassium concentration. The energy dispersive X-ray spectroscopy analysis indicated the presence of multiple phases in the single crystals. Using single crystal X-ray diffraction, the crystal structure of the single crystals was found to be 14/mmm tetragonal at room temperature. The magnetic measurements on the single crystals indicated the presence of multiple phases and magnetic impurities.
Resumo:
In the present study the preparation and characterisation of rubber ferrite composites (RFC) containing barium ferrite (BaF) and strontium ferrite (SrF) have been dealt with. The incorporation of the hard ferrites into natural and nitrile rubber was carried out according to a specific recipe for various loadings of magnetic fillers. For this, the ferrite materials namely barium ferrite and strontium ferrite having the general formula MO6Fe2O3 have been prepared by the conventional ceramic techniques. After characterisation they were incorporated into the natural and nitrile rubber matrix by mechanical method. Carbon black was also incorporated at different loading into the rubber ferrite composites to study its effect on various properties. The cure characteristics, mechanical, dielectric and magnetic properties of these composites were evaluated. The ac electrical conductivity of both the ceramic ferrites and rubber ferrite composites were also calculated using a simple relation. The investigations revealed that the rubber ferrite composites with the required dielectric and magnetic properties can be obtained by the incorporation of ferrite fillers into the rubber matrix, without compromising much on the processability and mechanical properties.
Resumo:
This thesis lays importance in the preparation and characterization of a few selected representatives of the ferrite family in the nanoregime. The candidates being manganese zinc ferrite and cobalt ferrite prepared by coprecipitation and sol-gel combustion techniques respectively. The thesis not only stresses importance on the preparation techniques and optimization of the reaction conditions, but emphasizes in investigating the various properties namely structural, magnetic and electrical. Passivated nickel nanocomposites are synthesized using polystyrene beads and adopting a novel route of ion exchange reduction. The structural and magnetic properties of these magnetic nanocomposites are correlated. The magnetocaloric effect (MCE) exhibited by these materials are also investigated with a view to finding out the potential of these materials as magnetic refrigerants. Calculations using numerical methods are employed to evaluate the entropy change on selected samples.
Resumo:
Department of Physics, Cochin University of Science & Technology
Resumo:
Department of Physics, Cochin University of Science & Technology
Resumo:
Fine particles of lithium ferrite were synthesized by the sol-gel method. By subsequent heat treatment at different temperatures, lithium ferrites of different grain sizes were prepared. A structural characterization of all the samples was conducted by the x-ray diffraction technique. A grain size of around 12 nm was observed for Li0.5Fe2.5O4 obtained through the sol-gel method. Magnetic properties of lithium ferrite nanoparticles with grain size ranging from 12 to 32 nm were studied. Magnetization measurements showed that Li0.5Fe2.5O4 fine particles exhibit a deviation from the predicted magnetic behaviour. The as-prepared sample of lithium ferrite showed a maximum saturation magnetization of 75 emu g−1. Variation of coercivity is attributed to the transition from multi-domain to single domain nature. Dielectric permittivity and ac conductivity of all the samples were evaluated as a function of frequency, temperature and grain size. Variation of permittivity and ac conductivity with frequency reveals that the dispersion is due to the Maxwell–Wagner type interfacial polarization
Resumo:
Rubber–nickel nanocomposites were synthesized by incorporating freshly prepared nanometric nickel particles in two different matrices namely natural rubber and neoprene rubber according to specific recipes for various loadings of nano nickel and the cure characteristics of these composites were evaluated. The maximum torque values register an increase with the increase in loading of nickel in both composites and this is attributed to the non-interacting nature of nickel nanoparticles with rubber matrices. The cure time of natural rubber composites decreases with increase in the content of nickel, and in neoprene rubber cure, time increases with increase in filler content. In natural rubber, the curing reaction seems to be activated by the presence of nickel particles. The magnetization studies of the composites reveal that the magnetic properties of nickel are retained in the composite samples. The elastic modulus of natural rubber and neoprene rubber are largely improved by the incorporation of nickel particles
Resumo:
Nickel nanocomposites were prepared by incorporating nickel nanoparticles in a neoprene matrix according to a specific recipe for various loadings of nickel particles. The dielectric properties of these composites were evaluated for different frequencies ranging from 100 kHz to 8MHz at different temperatures from 30 ◦C to 120 ◦C. The dielectric permittivity increases with increase of nickel concentration. Increase in temperature enhances the permittivity initially, till 40 ◦C and thereafter the permittivity decreases. The dielectric loss exhibits relaxation peaks and the peaks shift to lower frequencies with increase in volume fraction of the nickel nanoparticles in the matrix. The evaluation of magnetic and dielectric properties of these composites suggests that the dielectric permittivity can be tailored by an appropriate loading of the filler using semi-empirical equations and the magnetic properties vary according to simple mixture equations
Resumo:
The results of the investigation of the magnetic and structural properties of the alloy system Fe0.75–xSi0.25Sbx, where x = 0, 0.05, 0.1, 0.15, 0.2, and 0.25 synthesized by mechanical alloying followed by heat treatment are described. The x-ray diffraction reveals that all samples crystallize in the DO3-type cubic phase structure. Substituting Fe by Sb led to a de-crease in the lattice constant and the unit cell volume. The magnetic properties are investigated by vibrating sample magnetometer and show that all the samples are ferromagnetically ordered at room temperature. The Curie temperature is found to decrease linearly from (850 ± 5) K for the parent alloy to (620 ± 5) K for the alloyith x = 0.25. The satura-tion magnetizations at room temperature and at 100 K are found to decrease with increasing the antimony concentration. The above results indicate that Sb dissolves in the cubic structure of this alloy system.
Resumo:
A new family of vanadium-substituted chromium sulfides (VxCr2-xS3, 0 < x < 2) has been prepared and characterized by powder X-ray and neutron diffraction, SQUID magnetometry, electrical resistivity, and Seebeck coefficient measurements. Vanadium substitution leads to a single-phase region with a rhombohedral Cr2S3 structure over the composition range 0.0 < x e 0.75, while at higher vanadium contents (1.6 e x < 2.0) a second single-phase region, in which materials adopt a cation-deficient Cr3S4 structure, is observed. Materials with the Cr2S3 structure all exhibit semiconducting behavior. However, both transport and magnetic properties indicate an increasing degree of electron delocalization with increasing vanadium content in this compositional region. Materials that adopt a Cr3S4-type structure exhibit metallic behavior. Magnetic susceptibility data reveal that all materials undergo a magnetic ordering transition at temperatures in the range 90–118 K. Low-temperature magnetization data suggest that this involves a transition to a ferrimagnetic state.
Resumo:
This work involved an investigation to ascertain how the substitution of nickel ions for zinc ions affects the structural, morphological and magnetic properties of NiFe(2)O(4) ferrite samples. Ni(1-x)Zn(x)Fe(2)O(4) (x = 0.0, 0.3 0.5, 0.7) powders were prepared by combustion reaction and characterized structurally by X-ray diffraction. The specific surface area of the powders was determined by the nitrogen adsorption method (BET). Magnetization measurements were taken using an alternative gradient magnetometer (AGM), which revealed that the powders prepared by combustion reaction resulted in nanosized particles with a particle size of 18-27 nm. The crystallite size and lattice parameter increased as the concentration of Zn increased. Moreover, augmenting the Zn content in the NiFe(2)O(4) ferrite increased the saturation magnetization and coercive field. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
High-energy ball milling was employed to produce small particles of Gd5Si2Ge2. Magnetic and magnetocaloric properties of the ball-milled and bulk Gd5Si2Ge2 samples were investigated through the magnetization measurements. When compared to the bulk material, a significant decrease in saturation magnetization and magnetocaloric effect (-Delta S-max = 4 vs. 20 J/kgK for Delta H = 0-5 T) is observed even after the relatively short ball milling time of 4 h which produced particles with an average size of ca. 0.5 mu m. The ball-milled samples appear to loose a first-order structural transition, present in bulk Gd5Si2Ge2, and display a superparamagnetic behaviour below the corresponding Curie temperatures. (C) 2010 Elsevier Masson SAS. All rights reserved.