976 resultados para DOPED NANOPARTICLES
Resumo:
Manganese doped CdS nanoparticles were synthesized in basic aqueous solution by using mercapto acetate as capping reagents. The nanoparticles were characterized by HRTEM, EPR, photoluminescence and optical absorption measurements. Out of our expectation, doping of Mn2+ ions altered the recombination paths in CdS nanoparticles markedly. The surface stares facilitated PL from Mn2+ doped CdS nanoparticles is reported. A complete suppression of the emission from surface states at room temperature when doping with Mn2+ ions has been observed for the first time. (C) 2000 Elsevier Science Ltd. All rights reserved.
Resumo:
PL properties of Er3+ doped SiOx films containing Si nanoparticles have been studied. Er3+ emission intensity does not depend strongly upon crystallinity of Si clusters. The films can yield efficient Er3+ emission.
Resumo:
A series of Nd3+-doped LaF3 nanoparticles with Nd3+ concentrations from 0.5 to 10 mol% were synthesized. The fluorescence intensity and lifetime of the nanoparticles at various Nd3+ doping concentration were investigated. The nanoparticles displayed strongest fluorescence intensity at 3 mol% Nd3+ concentration. Eighty-eight percentage quantum efficiency was obtained when the Nd3+ concentration was 0.5 mol%. Optical properties of nanoparticles were studied according to Judd-Ofelt theory. A larger emission cross-section, sigma(em), for F-4(3/2) -> I-4(11/2) transition of the Nd3+ ion was obtained as 3.21 x 10(-20) cm(2), which was two times of the currently reported value. The larger emission cross-section and strong fluorescence intensity demonstrate that these nanoparticles are promising materials for laser applications. (C) 2010 Published by Elsevier B. V.
Resumo:
Magnetic nanoparticles of nickel substituted cobalt ferrite (NixCo1-xFe2O4:0 <= x <= 1) have been synthesized by co-precipitation route. Particles size as estimated by the full width half maximum (FWHM) of the strongest X-ray diffraction (XRD) peak and transmission electron microscopy (TEM) techniques was found in the range 18-28 +/- 4 nm. Energy dispersive X-ray (EDX) analysis confirms the presence of Co, Ni, Fe and oxygen as well as the desired phases in the prepared nanoparticles. The selective area electron diffraction (SAED) analysis confirms the crystalline nature of the prepared nanoparticles. Data collected from the magnetization hysteresis loops of the samples show that the prepared nanoparticles are highly magnetic at room temperature. Both coercivity and saturation magnetization of the samples were found to decrease linearly with increasing Ni-concentration in cobalt ferrite. Superparamagnetic blocking temperature as determined from the zero field cooled (ZFC) magnetization curve shows a decreasing trend with increasing Ni-concentration in cobalt ferrite nanoparticles. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
We show the potential application of Er3+-doped BaF2 nanoparticles prepared from microemulsion technology for 1.5 mu m amplification in telecommunication. Nanoparticles with different sizes of about 8, 10, and 20.5 nm were prepared. The XRD patterns showed the excursion of diffraction peaks. When the particle size is smaller or the diffraction angle is larger, this kind of excursion will be more serious.
Resumo:
[Ru(bpy)(3)](2+)-doped silica (RuSi) nanoparticles were synthesized by using a water/oil microemulsion method. Stable electrochemiluminescence (ECL) was obtained when the RuSi nanoparticles were immobilized on a glassy carbon electrode by using tripropylamine (TPA) as a coreactant. Furthermore, the ECL of the RuSi nanoparticles with layer-by-layer biomolecular coatings was investigated. Squential self-assembly of the polyelectrolytes and biomolecules on the RuSi nanoparticles gave nanocomposite suspensions, the ECL of which decreased on increasing the number of bilayers.
Resumo:
Spherical Ru(bpy)(3)(2+)-doped silica (RuSi) nanoparticles were prepared via a water-in-oil microemulsion approach. The electrochemical and electrochemiluminescent properties of the RuSi nanoparticles immobilized on an indium tin oxide (ITO) electrode were investigated. Further, electrochemiluminescence (ECL) of the RuSi nanoparticles with covalently coated biomacromolecules was studied. By covalent cross-linking with glutaraldehyde, gamma-(aminopropyl) triethoxysilane (APTES)-pretreated RuSi nanoparticles were coupled with different concentrations of bovine serum albumin (BSA), hemoglobin, and myoglobin, respectively.
Resumo:
Random multimode lasers are achieved in 4-(dicyanomethylene)-2-tert-butyl-6(1,1,7,7-tetramethyljulolidyl-9-enyl)-4H-pyran (DCJTB) doped polystyrene thin films by introducing silicon dioxide (SiO2) nanoparticles as scatterers. The devices emit a resonance multimode peak at a center wavelength of 640 nm with a mode linewidth less than 0.87 nm. The threshold excitation intensity is as low as 0.25 mJ pulse(-1) cm(-2). It can be seen that the microscopic random resonance cavities can be formed by multiple scattering of SiO2 nanoparticles.
Resumo:
A large-scale process combined sonication with self-assembly techniques for the preparation of high-density gold nanoparticles supported on a [Ru(bpy)(3)](2+)-doped silica/Fe3O4 nanocomposite (GNRSF) is provided. The obtained hybrid nanomaterials containing Fe3O4 spheres have high saturation magnetization, which leads to their effective immobilization on the surface of an ITO electrode through simple manipulation by an external magnetic field (without the need of a special immobilization apparatus). Furthermore, this hybrid nanomaterial film exhibits a good and very stable electrochemiluminescence (ECL) behavior, which gives a linear response for tripropylamine (TPA) concentrations between 5 mu m and 0.21 mM, with a detection limit in the micromolar range. The sensitivity of this ECL sensor can be easily controlled by the amount of [Ru(bpy)(3)](2+) immobilized on the hybrid nanomaterials (that is, varying the amount of [Ru(bpy)(3)](2+) during GNRSF synthesis).
Resumo:
A Ru(bpy)(3)(2+)-doped silica nanoparticle-[Ru@Silica] modified indium tin oxide electrode was prepared by simple electrostatic self-assembly technique, and one-electron catalytic oxidation of guanine bases in double-strand and denatured DNA was realized using the electrochemiluminescence detection means.
Resumo:
The authors report a random lasing emission from 4-(dicy-anomethylene)-2-t-butyl-6(1,1,7,7-tetramethyljulolidyl-9-enyl)-4H-pyran doped polystyrene thin films by introducing polystyrene nanoparticles. The aspects of concentration and diameter of polystyrene nanoparticles have been intensively investigated and found that the lasing occurs due to the scattering role of polystyrene nanoparticles. The devices emit a resonance multimode peak centered at a wavelength of 630 nm with a mode linewidth of less than 0.35 nm and exhibit threshold excitation intensity of as low as 0.06 mJ pulse(-1) cm(-2). The microscopic laser cavities formed by multiple scattering have been captured. The demonstration of random laser opens up the possibility of using organic scattering as alternative sources of coherent light emission.
Resumo:
Erbium-doped BaF2 nanoparticles were prepared from the microemulsion of cetyl trimethyl ammonium bromide (CTAB), n-butanol, n-octane and water. The X-ray diffraction (XRD) patterns were indexed to a pure BaF2 cubic phase. Transmission electron microscopy (TEM) images showed that BaF2 products were monodispersed with 15-20 nm in size at the dopant concentration of 0.06 mol%. At higher dopant concentration, there was no significant increase in particle size, but more polydispersed. Photoluminescence (PL) properties of the final products were examined. We can observe fluorescence of Er3+ around 1540 nm and with the increase of dopant concentration, the fluorescent intensity increases.
Resumo:
CeF3 and lutetium-doped CeF3 nanoparticles with the dopant concentration of 17, 25, 30, 42 and 50 mol% (molar ratio, Lu/Ce) were synthesized. XRD patterns were indexed to a pure CeF3 hexagonal phase even under the dopant concentration of 50 mol%. Environmental scanning electron microscopy-field emission gun (ESEM-FEG) was used to characterize the morphology of the final products. From the luminescence spectra of the products, we can get a broad emission ranging from 290 to 400 nm with peak at 325 nm. Lutetium-doping increases the luminescence intensity. We got. the most intense luminescence at the dopant concentration of 30 mol%.