993 resultados para Photoluminescence emission


Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

CaMoO4 (CMO) disordered and ordered thin films were prepared by the complex polymerization method (CPM). The films were annealed at different temperatures and time in a conventional resistive furnace (RF) and in a microwave (MW) oven. The microstructure and surface morphology of the structure were monitored by atomic force microscopy (AFM) and high-resolution scanning electron microscopy (HRSEM). Order and disorder were characterized by X-ray diffraction (XRD) and optical reflectance. A strong photoluminescence (PL) emission was observed in the disordered thin films and was attributed to complex cluster vacancies. The experimental results were compared with density functional and Hartree-Fock calculations. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Intense and broad photoluminescence (PL) emission at room temperature was observed on structurally disordered Ba[Zr0.25Ti0.75]O-3 (BZT) powders synthesized by the polymeric precursor method. BZT powders were annealed at 573 K for different times and at 973 K for 2 h in oxygen atmosphere. The single-phase cubic perovskite structure of the powder annealed at 973 K for 2 It was identified by X-ray diffraction and Fourier transform Raman techniques. PL emission increased with the increase of annealing time, which reached its maximum value in the powder annealed at 573 K for 192 h. First principles quantum mechanical calculations based on density functional theory (B3LYP level) were employed to study the electronic structure of ordered and disordered models. The theoretical calculations and experimental measurements of Ultraviolet-visible absorption spectroscopy indicate that the presence of intermediary energy levels in the band gap is favorable for the intense and broad PL emission at room temperature in disordered BZT powders. The PL behavior is probably due the existence of a charge gradient on the disordered structure, denoted by means of a charge transfer process from [TiO5]-[ZrO6] or [TiO6]-[ZrO5] clusters to [TiO6]-[ZrO6] clusters. (C) 2008 Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work, a SiO2 spherical were prepared by the Stober Method and then recovered with a single layer of Eu2O3 oxide (SiO2@Eu2O3) obtained by the Polymeric Precursor Method. The SiO2@Eu2O3 powder was heated treated at 100, 300, 400, 500 and 800 A degrees C. The samples were characterized by the Scanning Electonic Microscopy (SEM), Thermal Analysis (TGA/DTA), and the luminescent properties of the SiO2@Eu2O3 powders were studied by their emission and excitation spectra as well as by the lifetime measurements of the Eu3+ D-5(0) -> aEuro parts per thousand F-7(2) transition. The SEM analysis shows that the silica prepared by the Stober Method is spherical with a particle size of 460 nm. The emission spectra of the SiO2@Eu2O3 powders presented the Eu3+ characteristics bands related to the D-5(0) -> aEuro parts per thousand F-7(J) (J = 0, 1, 2, 3, 4) transitions at 577, 591, 616, 649 and 695 nm, respectively. The band related to the D-5(0) -> aEuro parts per thousand F-7(2) transition is the most intense in the spectra, and its intensity decreases with the temperature enhancement. The decay curves of the SiO2@Eu2O3 samples presented monoexponential features, and the obtained lifetime values were higher than the Eu2O3 oxide. It was possible to conclude that the D-5(0) -> aEuro parts per thousand F-7(2) hypersensitive transition is strongly dependent on the Eu3+ surrounding.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Organic-inorganic hybrids formed by polyether-based chains grafted to both ends to a siliceous backbone through urea cross-linkages (-NHC=O)NH-), named di-ureasil, have been used as host for incorporation of Eu3+ in the form of EuCl3. The bulks and the thin films, both optically transparent, were characterized by excitation, absorption and emission spectroscopy. Photoluminescence results point out that the Eu3+ ions occupy, at least, two distinct local environments. Besides, the processing method (thin films or bulks) has influence on the energy levels of the hybrid host probably due to the lower degree of organization of the thin films structure. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)