Resumo:
Some aspects of the pyrolysis of polystyrene peroxide (PSP) have been examined. Low-temperature decomposition studies at 60°C and 70°C have been carried out to elucidate the ageing behaviour of PSP. The exothermic decomposition was found to be complete in 44 h at 70°C suggesting that all peroxide bonds have broken. Enthalpy measurements of the aged samples were carried out as a function of storage time. Ageing was also followed by infrared spectroscopy, and the intensity of the peroxide absorption around 1050 cm−1 was found to decrease with ageing time. Benzaldehyde formed as a result of PSP pyrolysis is readily converted into benzoic acid, which crystallizes during the ageing process. Pyrolysis—gas chromatographic studies have shown that up to 450°C the basic decomposition mechanism (i.e., the formation of benzaldehyde and formaldehyde as the major products) does not change. No effect of pressure on the decomposition exotherm in differential thermal analysis was observed, suggesting that peroxide composition involves only condensed phase reactions. Hydroquinone, p-aminophenol and cadmium sulphide were found to retard the thermal decomposition of PSP, suggesting that these compounds would be potential antioxidants for polymers.
Resumo:
Physicochemical characterization of freshwater samples from Finland, Sweden, the Netherlands, and Spain revealed that water hardness and pH decreased and the quantity and quality of humic substances changed considerably in this geographical series from south to north. Since the ambient water chemistry may affect the availability of chemicals, the total aqueous concentration of a chemical may be insufficient to predict the bioconcentration, subsequent biological response, and thus risk. In addition, organisms could be affected directly by water quality characteristics. In this context the main objective of this thesis was to investigate the bioavailability of selected ecotoxicologically relevant chemicals (cadmium, benzo(a)pyrene, and pyrene) in various European surface waters and to show the importance of certain water chemistry characteristics in interpreting the bioavailability and toxicity results. The bioavailability of cadmium to Daphnia magna was examined in very soft humic lake water. Humic substances as natural ligands decreased the free and bioavailable proportion of cadmium in soft lake water. As a consequence the uptake rate and the acute toxicity decreased compared with the humic-free reference. When the hardness of humic lake water was artificially elevated, the acute toxicity of cadmium decreased, although the proportion of free cadmium increased. The decreased bioavailability of cadmium in hard water was a result of effective competition for uptake by the hardness cations, especially calcium ions. The protective role of humic substances and water hardness against cadmium toxicity was also observed in Lumbriculus variegatus, although D. magna was more sensitive to cadmium. The bioavailability of two polycyclic aromatic hydrocarbons (PAHs), pyrene and benzo(a)pyrene, was studied in European surface waters of varying water chemistry. Humic substances acted as complexing ligands with both PAHs, but the bioavailability of the more lipophilic benzo(a)pyrene to D. magna was affected more by humic substances than that of pyrene. In addition, not only the quantity of humic substances, but also their quality affected the bioavailability of benzo(a)pyrene. Nevertheless, the humic substances played a protective role in the photo-enhanced toxicity of pyrene under UV-B radiation. Water hardness had no effect on pyrene toxicity. Results indicate that the typical physicochemical characteristics of boreal freshwaters should be considered carefully in local and regional risk assessment of chemicals concerning the Fennoscandian region.
Resumo:
Hybrid semiconductor-metal nanoparticles monolayer of Cadmium Sclenide and gold nanoparticles has been prepared, using Langmuir – Blodgett technique. The near field photoluminescence spectra from such monolayer films, shows red shift similar to 75 meV with respect to CdSe QDs monolayer film and splitting similar to 57 meV. The composite spectra are much broader similar to 330 meV compared to the corresponding emission spectra of CdSe monolayer similar to 165 meV. The possible explanation for the observed features are provided in terms of exciton - Plasmon interaction.
Resumo:
Magnetotransport measurements in pulsed fields up to 15 T have been performed on mercury cadmium telluride (Hg1-xCdxTe, x similar to 0.2) bulk as well as liquid phase epitaxially grown samples to obtain the resistivity and conductivity tensors in the temperature range 220-300 K. Mobilities and densities of various carriers participating in conduction have been extracted using both conventional multicarrier fitting (MCF) and mobility spectrum analysis. The fits to experimental data, particularly at the highest magnetic fields, were substantially improved when MCF is applied to minimize errors simultaneously on both resistivity and conductivity tensors. The semiclassical Boltzmann transport equation has been solved without using adjustable parameters by incorporating the following scattering mechanisms to fit the mobility: ionized impurity, polar and nonpolar optical phonons, acoustic deformation potential, and alloy disorder. Compared to previous estimates based on the relaxation time approximation with outscattering only, polar optical scattering and ionized impurity scattering limited mobilities are shown to be larger due to the correct incorporation of the inscattering term taking into account the overlap integrals in the valence band.
Resumo:
Examples of 3D cadmium thiosulfate based inorganic-organic hybrid compounds have been shown to be active photocatalysts using sunlight.
Resumo:
In this paper, we study the thermoelectric power under strong magnetic field (TPSM) in quantum dots (QDs) of nonlinear optical, III-V, II-VI, GaP, Ge, Te, Graphite, PtSb2, zerogap, Lead Germanium Telluride, GaSb, stressed materials, Bismuth, IV-VI, II-V, Zinc and Cadmium diphosphides, Bi2Te3 and Antimony respectively. The TPSM in III-V, II-VI, IV-VI, HgTe/CdTe quantum well superlattices with graded interfaces and effective mass superlattices of the same materials together with the quantum dots of aforementioned superlattices have also been investigated in this context on the basis of respective carrier dispersion laws. It has been found that the TPSM for the said quantum dots oscillates with increasing thickness and decreases with increasing electron concentration in various manners and oscillates with film thickness, inverse quantizing magnetic field and impurity concentration for all types of superlattices with two entirely different signatures of quantization as appropriate in respective cases of the aforementioned quantized structures. The well known expression of the TPSM for wide-gap materials has been obtained as special case for our generalized analysis under certain limiting condition, and this compatibility is an indirect test of our generalized formalism. Besides, we have suggested the experimental method of determining the carrier contribution to elastic constants for nanostructured materials having arbitrary dispersion laws.
Resumo:
We have studied the as grown and annealed CdZnTe (Zn similar to 4 %) crystals for the assessment of their crystalline quality. As grown crystals suffer from tellurium precipitates and cadmium vacancies, which are inherent, due to retrograde solid solubility curve in the phase diagram. This is reflected in the Fourier transform infrared (FTIR) spectra over the 400 - 4500 cm(-1) range by a strong absorption around 2661 cm(-1) which corresponds to the band gap of tellurium confirming their presence, where-as a monotonic decrease in the transmission with the decrease in wave number indicates the presence of cadmium vacancies. Obviously the presence of Cd vacancies lead to the formation of tellurium precipitates confirming their presence. Annealed samples under cadmium + zinc ambient at 650 degrees C for 6 hours show an improvement in the transmission over the same range. This can be attributed to thermo-migration of tellurium precipitates and hence bonding with Cd or Zn to form CdZnTe. This is further supported by the reduced full width at half maximum in the X-ray diffraction rocking curve of these CdZnTe crystals. Cadmium annealing although can passivate Cd vacancy related defects and reduce the Te precipitates, as is observed in our low temperature Photoluminescence (PL) spectra, alone may not be sufficient possibly due to the loss of Zn. Vacuum annealing at 650 degrees C for 6 hours further deteriorated the material quality as is reflected in the low temperature PL spectra by the introduction of a new defect band around 0.85 eV and reduced IR transmission.
Resumo:
Dielectric measurements have been made on a number of molecular complexes of beryllium, zinc, cadmium and mercuric halides. The polarizations observed have been interpreted in terms of a tetrahedral configuration for the undissociated beryllium, zinc and cadmium halide complexes. In other cases the observed polarization has been shown to be due to the dissociation of the complex in solution.
Resumo:
Using the pulse method in the range of 2 to 26Mc's the ultrasonic absorption, velocity and the adiabatic compressibility have been studied in eleven aqueous acetate solutions up to a concentration of 1 mole/litre. The substances studied are the acetates of lithium, sodium, potassium, ammonium, magnesium, calcium, strontium, barium, zinc, cadmium and lead. Absorption in mercuric acetate has been studied only at 2 and 6 Mc/s. Two regions of relaxation are noticed, one below 10 Mc/s and the other between 10 and 26 Mc/s. The first relaxation is ascribed to the dissociation reaction of the salt and the second one to the monomerdimer reaction of the acetic acid formed by the hydrolysis of the salt in water.
Resumo:
The study of proteins involved in de novo biosynthesis of purine nucleotides is central in the development of antibiotics and anticancer drugs. In view of this, a protein from the hyperthermophile Pyrococcus horikoshii OT3 was isolated, purified and crystallized using the microbatch method. Its primary structure was found to be similar to that of SAICAR synthetase, which catalyses the seventh step of de novo purine biosynthesis. A diffraction-quality crystal was obtained using Hampton Research Crystal Screen II condition No. 34, consisting of 0.05 M cadmium sulfate hydrate, 0.1 M HEPES buffer pH 7.5 and 1.0 M sodium acetate trihydrate, with 40%(v/v) 1,4-butanediol as an additive. The crystal belonged to space group P3(1), with unit-cell parameters a = b = 95.62, c = 149.13 angstrom. Assuming the presence of a hexamer in the asymmetric unit resulted in a Matthews coefficient (V-M) of 2.3 angstrom(3) Da(-1), corresponding to a solvent content of about 46%. A detailed study of this protein will yield insights into structural stability at high temperatures and should be highly relevant to the development of antibiotics and anticancer drugs targeting the biosynthesis of purine nucleotides.
Resumo:
The synthesis of manganese(II), cobalt(II), nickel(II), copper(II), zinc(II) and cadmium(II) complexes of a new ligand 2-thiophene-2-yl-3(thiophene-2-carboxylidene-amino)-1,2-dihydroquinazolin-4(3H)-one (TTCADQ) is described. The ligand and metal complexes were characterized by elemental analysis, conductivity measurements, spectral (u.v.-vis., i.r., 1D n.m.r., 2D hetcor and e.p.r.) and thermal studies. The formation of 1,2-dihydroquinazolin-4(3H)-one rather than hydrazone, in the reaction of aromatic aldehyde and o-aminobenzoylhydrazide is proved by single crystal X-ray diffraction and 2D hetcor n.m.r. studies. On the basis of elemental analysis, u.v.-vis.spectroscopy and magnetic moment studies, six coordinate geometry for all the complexes was proposed. The i.r. spectral studies reveal the bidentate behaviour of the ligand.
Resumo:
Thin films of hybrid arrays of cadmium selenide quantum dots and polymer grafted gold nanoparticles have been prepared using a BCP template. Controlling the dispersion and location of the respective nanoparticles allows us to tune the exciton-plasmon interaction in such hybrid arrays and hence control their optical properties. The observed photoluminescence of the hybrid array films is interpreted in terms of the dispersion and location of the gold nanoparticles and quantum dots in the block copolymer matrix.
Resumo:
Ionic conductivity measurements have been made on pure, copper-doped and cadmium-doped single crystals. Dielectric measurements in the frequency range 30Hz–100Hz showed that there was no anomalously to be (0.64 ± 0.02) eV and migration energies for silver ion intersitials and vacancies in the c direction to be (0.41 ± 0.02) eV and (0.50 ± 0.02) eV respectively. ESR measurements have shown that copper exists as Cu+ in these crystals. Dielectric measurements in the frequency range (OHz–100KHz showed that there was no anomalously high value for ε as reported earlier.
Resumo:
Excitation spectra and transient and steady-state photoconductivity have been studied in undoped and 0.8-mole% Cu-doped single-crystal β-AgI between 150 and 260°K. A single peak in the spectral response was found to occur in each case, at 2.88 eV for undoped and at 2.81 eV for copper-doped specimens at 260 K, the difference being due to a decrease in band gap. The anisotropy due to polarization of incident radiation parallel or perpendicular to the c direction, which is a measure of the energy difference between the Γ9 and Γ7 levels in the valence band, was found to be 0.010 eV. Transient-photoconductivity experiments showed that the hole lifetime was 6 μ sec at 300°K, an order of magnitude larger than the electron lifetime. The hole drift mobility was found to be 12±2 cm2/ V sec at 300°K and limited by traps at a depth of 0.51±0.01 eV with concentration (3-5)×109/cm3 and capture cross section 10-11 cm2. The study of photoconductivity decay versus temperature revealed the presence of shallow hole traps at 0.14±0.02 eV with concentration greater than 1016/cm3 and capture cross section 10-19 cm2. The steady-state photoconductivity was determined by the deep hole traps at 0.51 eV, and showed the presence of shallow electron traps at a depth of 0.28 eV. The trap distribution was found to be substantially the same in pure and copper-doped specimens, indicating the monovalent substitutional role of copper. The effects of iodine annealing, cadmium doping, and heating above the transition temperature were also studied. The possible nature of the traps is discussed.
Resumo:
A review of the research work that has been carried out thus far relating the casting and heat treatment variables to the structure and mechanical properties of Al–7Si–Mg (wt-%) is presented here. Although specifications recommend a wide range of magnesium contents and a fairly high content of iron, a narrow range of magnesium contents, closer to either the upper or lower specified limits depending on the properties desired, and a low iron content will have to be maintained to obtain optimum and consistent mechanical properties. A few studies have revealed that the modification of eutectic silicon slightly increases ductility and fracture toughness and also that the effect of modification is predominant at low iron content. Generally, higher solidification rates give superior mechanical properties. Delayed aging (the time elapsed between quenching and artificial aging during precipitation hardening) severely affects the strength of the alloy. The mechanism of delayed aging can be explained on the basis of Pashley's kinetic model. It has been reported that certain trace additions (cadmium, indium, tin, etc.) neutralise the detrimental effect of delayed aging. In particular, it should be noted that delayed aging is not mentioned in any of the specifications. With reference to the mechanism by which trace additions neutralise the detrimental effect of delayed aging, various hypotheses have been postulated, of which impurity–vacancy interaction appears to be the most widely accepted.