880 resultados para SILICA-COATED CDTE


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Arrays of vertically well-aligned ZnO nanorod-nanowall junctions have been synthesized on an undoped ZnO-coated silicon substrate by a carbothermal reduction and vapour phase transport method. X-ray diffraction (XRD) and scanning electron microscopy (SEM) show that the nanostructures are well-oriented with the c-axis perpendicular to the substrate. The room temperature photoluminescence (PL) spectrum of the as-prepared ZnO nanostructure reveals a dominant near-band-edge (NBE) emission peak and a weak deep level (DL) emission, which demonstrates its good optical properties. Temperature-dependent PL spectra show that both the intensity of NBE and DL emissions increased with decreasing temperature. The NBE emission at 3.27 eV is identified to originate from the radiative free exciton recombination. The possible growth mechanism of ZnO nanorod-nanowall junctions is also proposed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Er-Si-O (Er2SiO5) crystalline films are fabricated by the spin-coating and subsequent annealing process. The fraction of erbium is estimated to be 21.5 at% based on Rutherford backscattering measurement. X-ray diffraction pattern indicates that the Er-Si-O films are similar to Er2SiO5 compound in the crystal structure. The fine structure of room-temperature photoluminescence of Er3+-related transitions suggests that Er has a local environment similar to the Er-O-6 octahedron. Our preliminary results show that the intensity of 1.53 mu m emission is enhanced by a factor of seven after nitrogen plasma treatment by NH3 gas with subsequent post-annealing. The full-width at half-maximum of 1.53 pm emission peak increases from 7.5 to 12.9 nm compared with that of the untreated one. Nitrogen plasma treatment is assumed to tailor Er3+ local environment, increasing the oscillator strength of transitions and thus the excitation/emission cross-section. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The GaSb and Ga0.62In0.38Sb nanocrystals were embedded in the SiO2 films by radio-frequency magnetron co-sputtering and were grown on GaSb and Si substrates at different temperatures. We present results on the 10K excitonic photoluminescence (PL) properties of nanocrystalline GaSb and Ga0.62In0.38Sb as a function of their size. The measurements show that the PL of the GaSb and Ga0.62In0.38Sb nanocrystallites follows the quantum confinement model very closely. By using deconvolution of PL spectra, origins of structures in PL were identified. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Cyclotron resonance in CdTe/CdMgTe quantum wells (QWs) was studied. Due to the polaron effect the zero-field effective mass is strongly influenced by the QW width. The experimental data have been described theoretically by taking into account electron-phonon coupling and the nonparabolicity of the conduction band. The subband structure was calculated self-consistently. The best fit was obtained for an electron-phonon coupling constant alpha = 0.3 and bare electron mass of m(b) = 0.092m(0).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this study, we first present the process of the melt epitaxial (ME) growth method, and the improvement of low-temperature electron mobility of the long-wavelength InAsSb epilayers grown by ME in a fused silica boat. The electrical properties were investigated by van der Pauw measurement at 300 and 77 K. It is seen that the electron mobility of the InAsSb samples grown by graphite boat decreased from 55,700 to 26,600 cm(2)/V s when the temperature was reduced from 300 to 77 K, while for the samples grown by fused silica boat, the electron mobility increased from 52,600 at 300 K to 54,400 cm(2)/V s at 77 K. The electron mobility of 54,400cm(2)/Vs is the best result, so far, for the InAsSb materials with cutoff wavelength of 8-12 mum at 77 K. This may be attributed to the reduction of the carbon contamination by using a fused silica boat instead of a graphite boat. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The circular polarization of excitonic luminescence is studied in CdTe/Cd1-xMgxTe quantum wells with excess electrons of low density in an external magnetic field. It is observed that the circular polarization of X and X- emissions has opposite signs and is influenced by the excess electron density. If the electron density is relatively high so that the emission intensity of the negatively charged excitons X- is much stronger than that of the neutral excitons X, a stronger circular polarization degree of both X and X- emissions is observed. We find that the circular polarization of both X- and X emissions is caused by the spin polarization of the excess electrons due to the electron-spin-dependent nature of the formation of X-. If the electron density is relatively low and the emission intensity of X- is comparable to that of X, the circular polarization degree of X and X- emissions is considerably smaller. This fact is interpreted as due to a depolarization of the excess electron spins, which is induced by the spin relaxation of X-.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Single crystal GaN films have been grown on to an Al2O3 coated (001)Si substrate in a horizontal-type low-pressure MOVPE system. A thin Al2O3 layer is an intermediate layer for the growth of single crystal GaN on to Si although it is only an oriented polycrystal him as shown by reflection high electron diffraction. Moreover, the oxide was not yet converted to a fully single crystal film, even at the stage of high temperature for the GaN overlayer as studied by transmission electron microscopy. Double crystal X-ray diffraction showed that the linewidth of (0002) peak of the X-ray rocking curve of the 1.3 mu m sample was 54 arcmin and the films had heavy mosaic structures. A near band edge peaking at 3.4 eV at room temperature was observed by photoluminescence spectroscopy. (C) 1998 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new-style silica planar lightwave circuit (PLC) hybrid integrated triplexer, which can demultiplex 1490-nm download data and 1550-nm download analog signals, as well as transmit 1310-nm upload data, is presented. It combines SiO2 arrayed waveguide gratings (AWGs) with integrated photodetectors (PDs) and a high performance laser diode (LD). The SiO2 AWGs realize the three-wavelength coarse wavelength-division multiplexing (CWDM). The crosstalk is less than 40 dB between the 1490- and 1550-nm channels, and less than 45 dB between 1310- and 1490- or 1550-nm channels. For the static performances of the integrated triplexer, its upload output power is 0.4 mW, and the download output photo-generated current is 76 A. In the small-signal measurement, the upstream 3-dB bandwidth of the triplexer is 4 GHz, while the downstream 3-dB bandwidths of both the analog and digital sections reach 1.9 GHz.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The characteristic features of the absorption and photoluminescence spectra of ZnSe quantum dots (QDs) inside a silica matrix derived from a sol-gel method were studied at room temperature. Compared with the bulk materials, the absorption edges of ZnSe QDs in silica gel glass were shifted to higher energies and the spectra exhibited the discrete excitonic features due to the quantum confinement effects. Besides the band-edge emission, photoluminescence at ultraviolet excitation also showed the emissions related to the higher excitonic states. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Micro Fabry-Perot (F-P) interferometers (MFPIs) are machined in a single-mode fiber (SMF) and a photonic crystal fiber (PCF) by using a near-infrared femtosecond laser, respectively. The strain and temperature characteristics of the two MFPIs with an identical cavity length are investigated and the experimental results show that the strain sensitivity of the PCF-based MFPI is smaller than that of the SMF-based MFPI due to their different waveguide structures, while the two MFPIs have close temperature sensitivities which are much smaller than that of an in-line SMF etalon sensor reported previously. These MFPIs in silica fibers are compact, stable, inexpensive, capable for mass-production and easy fabrication, offering great potentials for wide sensing applications. (c) 2007 Optical Society of America.