Polymer films synthesized from plasmas of a tetramethylsilane - Ar mixture were modified by irradiation with 170 keV He ions at fluences ranging from 1 x 10(14) to 1 x 10(16) cm(-2). As revealed by infrared spectroscopy, the ion beam produced intense bond rearrangements, such as the depletion of bonding groups (C-H and Si-H), and induced the formation of new ones, such as O-H and Si-O. From the nanoindentation measurements, a remarkable increase in the surface hardness of the films was observed as the ion fluence was increased. The increases in hardness were accompanied by an increase in the film compaction as shown by using a combination of RBS and film thickness measurements. From both hardness and infrared measurements A was concluded that, under the He ion bombardment, the polymer structure is transformed into a silicon oxycarbide network.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper describes a technique for extending the force range of thin conductive polymer force sensors used for measuring contact force. These sensors are conventionally used for measuring force by changing electrical resistance when they are compressed. The new method involves measuring change in electrical resistance when the flexible sensor, which is sensitive to both compression and bending, is sandwiched between two layers of spring steel, and the structure is supported on a thin metal ring. When external force is applied, the stiffened sensor inside the spring steel is deformed within the annular center of the ring, causing the sensor to bend in proportion to the applied force. This method effectively increases the usable force range, while adding little in the way of thickness and weight. Average error for loads between 10 N and 100 N was 2.2 N (SD = 1.7) for a conventional conductive polymer sensor, and 0.9 N (SD = 0.4) using the new approach. Although this method permits measurement of greater loads with an error less than 1 N, it is limited since the modified sensor is insensitive to loads less than 5 N. These modified sensors are nevertheless useful for directly measuring normal force applied against handles and tools and other situations involving forceful manual work activities, such as grasp, push, pull, or press that could not otherwise be measured in actual work situations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mixtures of C6H6 and SF6 were polymerized in an r.f. discharge. Actinometry (quantitative optical emission spectroscopy) was used to determine trends in the plasma concentrations of the species F, H and CH as a function of the proportion of SF6 in the feed. Infrared spectroscopy and electron spectroscopy for chemical analysis were employed to characterize the deposited material. Increasing proportions of SF, in the feed produced increased fragmentation of the benzene molecules and greater fluorination of the deposited material. The deposition rate, as determined by optical interferometry, was found to be enhanced about 4 times by the presence of 10-20% SF6 in the feed. At 50% SF6 in the feed, deposition rates were greater than in pure C6H6 plasmas despite the (probably large) etching effect of atomic fluorine from the discharge. Relationships between the plasma composition, electron density and temperature, film composition and growth rate are discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High density poly(ethylene) has been submitted to thermal degradation alone, and in the presence of silicoaluminophosphate SAPO-37. The processes were carried out in a reactor connected on line to a gas chromatograph/mass spectrometer in order to analyze the evolved products. Polymer degradation was also evaluated by thermogravimetry, from room temperature until 800 degreesC, under nitrogen dynamic atmosphere, with multiple heating rates. From TG curves, the activation energy related to degradation process was calculated using the Flynn and Wall multiple heating rate kinetic model for pure polymer (PE) and for polymer in the presence of catalyst (PE/S37). SAPO-37 showed good selectivity for low molecular mass hydrocarbons in PE catalytic degradation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Significant progress is being made in the photovoltaic energy conversion using organic semiconducting materials. One of the focuses of attention is the morphology of the donor-acceptor heterojunction at the nanometer scale, to ensure efficient charge generation and loss-free charge transport at the same time. Here, we present a method for the controlled, sequential design of a bilayer polymer cell architecture that consists of a large interface area with connecting paths to the respective electrodes for both materials. We used the surface-directed demixing of a donor conjugated/guest polymer blend during spin coating to produce a nanostructured interface, which was, after removal of the guest with a selective solvent, covered with an acceptor layer. With use of a donor poly(p-phenylenevinylene) derivative and the acceptor C-60 fullerene, this resulted in much-improved device performance, with external power efficiencies more than 3 times higher than those reported for that particular material combination so far.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work describes the influence of the ion bombardment on the electrical, optical and mechanical properties of polymer films deposited from radio-frequency plasmas of benzene. Irradiations were conducted using N+ at 5 x 10(19) ions/m(2), varying the ion energy, E-0, from 0 to 150 keV. Film elemental composition was determined by Rutherford backscattering spectroscopy. Electrical resistivity and hardness were obtained by the two-point probe and nanoindentation technique, respectively. Ultraviolet-visible spectroscopy was employed to investigate the optical constants of the samples. Etching rate was determined by exposure of the films to reactive oxygen plasmas. Ion bombardment induced gradual loss of H and increase in C and O concentrations with Eo. As a consequence the electrical, optical and mechanical properties were drastically affected. Interpretation of these results is proposed in terms of chain cross-linking and unsaturation. (C) 2001 Elsevier B.V. B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The polymer surface degradation and/or modification evolution of Teflon FEP and Mylar C films caused by a low energy electron beam were analyzed using a new method that consists in measuring the second crossover energy shift in the electronic emission curve. Upon prolonged irradiation, the second crossover energy shifts irreversibly to lower values in Teflon FEP but to higher values in Mylar C, indicating distinct mechanisms of surface degradation for the two polymers. The method represents a relatively inexpensive way to monitor early stages of surface degradation since the secondary electron emission comes from a maximum depth below the geometric surface of 100 mn in insulators. (C) 2001 Elsevier B.V. Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the present paper, the ionic conductivity and the dielectric relaxation properties on the poly(vinyl alcohol)-CF(3)COONH(4) polymer system have been investigated by means of impedance spectroscopy measurements over wide ranges of frequencies and temperatures. The electrolyte samples were prepared by solution casting technique. The temperature dependence of the sample's conductivity was modeled by Arrhenius and Vogel-Tammann-Fulcher (VTF) equations. The highest conductivity of the electrolyte of 3.41x10 (-aEuro parts per thousand 3) (Omega cm) (-aEuro parts per thousand 1) was obtained at 423 K. For these polymer system two relaxation processes are revealed in the frequency range and temperature interval of the measurements. One is the glass transition relaxation (alpha-relaxation) of the amorphous region at about 353 K and the other is the relaxation associated with the crystalline region at about 423 K. Dielectric relaxation has been studied using the complex electric modulus formalism. It has been observed that the conductivity relaxation in this polymer system is highly non-exponential. From the electric modulus formalism, it is concluded that the electrical relaxation mechanism is independent of temperature for the two relaxation processes, but is dependent on composition.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

PANI films were deposited on glass substrates by in-situ polymerization and characterized by UV-VIS spectroscopy and atomic force microscopy. A method is developed to accurately analyze ellipsometric data obtained for transparent glass substrates before and after modification with absorbing polymer films. Surface modification was made with an overlayer such as polyaniline ( PANI), which exhibits different optical properties by varying its oxidation state. First, the issue of using transparent substrates for ellipsometry studies was examined and then, spectroscopic ellipsometry was used to characterize absorbing overlayers on transparent glasses. The same methodologies of data analysis can be also applied to other absorbing films on transparent substrates, and deposited by different techniques.