900 resultados para Surface morphology
Resumo:
The increasing interest in the interaction of light with electricity and electronically active materials made the materials and techniques for producing semitransparent electrically conducting films particularly attractive. Transparent conductors have found major applications in a number of electronic and optoelectronic devices including resistors, transparent heating elements, antistatic and electromagnetic shield coatings, transparent electrode for solar cells, antireflection coatings, heat reflecting mirrors in glass windows and many other. Tin doped indium oxide (indium tin oxide or ITO) is one of the most commonly used transparent conducting oxides. At present and likely well into the future this material offers best available performance in terms of conductivity and transmittivity combined with excellent environmental stability, reproducibility and good surface morphology. Although partial transparency, with a reduction in conductivity, can be obtained for very thin metallic films, high transparency and simultaneously high conductivity cannot be attained in intrinsic stoichiometric materials. The only way this can be achieved is by creating electron degeneracy in a wide bandgap (Eg > 3eV or more for visible radiation) material by controllably introducing non-stoichiometry and/or appropriate dopants. These conditions can be conveniently met for ITO as well as a number of other materials like Zinc oxide, Cadmium oxide etc. ITO shows interesting and technologically important combination of properties viz high luminous transmittance, high IR reflectance, good electrical conductivity, excellent substrate adherence and chemical inertness. ITO is a key part of solar cells, window coatings, energy efficient buildings, and flat panel displays. In solar cells, ITO can be the transparent, conducting top layer that lets light into the cell to shine the junction and lets electricity flow out. Improving the ITO layer can help improve the solar cell efficiency. A transparent ii conducting oxide is a material with high transparency in a derived part of the spectrum and high electrical conductivity. Beyond these key properties of transparent conducting oxides (TCOs), ITO has a number of other key characteristics. The structure of ITO can be amorphous, crystalline, or mixed, depending on the deposition temperature and atmosphere. The electro-optical properties are a function of the crystallinity of the material. In general, ITO deposited at room temperature is amorphous, and ITO deposited at higher temperatures is crystalline. Depositing at high temperatures is more expensive than at room temperature, and this method may not be compatible with the underlying devices. The main objective of this thesis work is to optimise the growth conditions of Indium tin oxide thin films at low processing temperatures. The films are prepared by radio frequency magnetron sputtering under various deposition conditions. The films are also deposited on to flexible substrates by employing bias sputtering technique. The films thus grown were characterised using different tools. A powder x-ray diffractometer was used to analyse the crystalline nature of the films. The energy dispersive x-ray analysis (EDX) and scanning electron microscopy (SEM) were used for evaluating the composition and morphology of the films. Optical properties were investigated using the UVVIS- NIR spectrophotometer by recording the transmission/absorption spectra. The electrical properties were studied using vander Pauw four probe technique. The plasma generated during the sputtering of the ITO target was analysed using Langmuir probe and optical emission spectral studies.
Resumo:
ZnGa2O4:Dy3+ phosphor thin films were deposited on quartz substrates by radio frequency rf magnetron sputtering and the effect of substrate temperature on its structural and luminescent properties was investigated. Polycrystalline film could be deposited even at room temperature. The crystalline behavior, Zn/Ga ratio, and surface morphology of the films were found to be highly sensitive to substrate temperature. Under UV illumination, the as-deposited films at and above 300°C gave white luminescence even without any postdeposition treatments. The photoluminescent PL emission can be attributed to the combined effect of multicolor emissions from the single luminescence center Dy3+ via host-sensitization. Maximum PL emission intensity was observed for the film deposited at 600°C, and the CIE chromaticity coordinates of the emission were determined to be x,y = 0.34, 0.31 .
Resumo:
A series of short-isora-fiber-reinforced natural rubber composites were prepared by the incorporation of fibers of different lengths (6, 10, and 14 mm) at 15 phr loading and at different concentrations (10, 20, 30, and 40 phr) with a 10 mm fiber length. Mixes were also prepared with 10 mm long fibers treated with a 5% NaOH solution. The vulcanization parameters, processability, and stress-strain properties of these composites were analyzed. Properties such as tensile strength, tear strength, and tensile modulus were found to be at maximum for composites containing longitudinally oriented fibers 10 mm in length. Mixes containing fiber loadings of 30 phr with bonding agent (resorcinol-formaldehyde [RF] resin) showed mechanical properties superior to all other composites. Scanning electron microscopy (SEM) studies were carried out to investigate the fiber surface morphology, fiber pullout, and fiber-rubber interface. SEM studies showed that the bonding between the fiber and rubber was improved with treated fibers and with the use of bonding agent.
Resumo:
Brasses are widely used as constructional materials in marine environment due to their anticorrosive,antifouling and mechanical properties.However, its resistance to corrosion and fouling may vary according to local marine environmental condition and the seasons.The dezincification of brass is one of the forms of selective corrosion which has attracted the attention of researchers for the last two decades.Many of the dezincification mechanistic studies have been performed in noncomplex media and hence their conclusions cannot be extended to esturine water,which is of great significance since brass is extensively used in marine environment.Inhibited α brasses are largely immune to dezincication and the effect of tin and arsenic addition to α/beta brasses is not so reliable in controlling the dezincification. There have been many cases of dezincification in duplex brasses in both freshwater and seawater.Though there is some protection methods such as inhibitors,electro deposition and electro polymerization,there is no reliable method of inhibiting the dezincification of two-phase brass.Organic coatings are effectively used for the protection metals due to their capacity to act a physical barrieer between the metal surface and corrosive environment.Hence,pure epoxy coating is selected for this as it has antocorrosiion effect on brass.The dezincification behaviour of brass of the present study has been highlighted in terms of corrosion rate,weight gain/loss,corrosion current and polarization resistence,open circuit potential,dezincification factor. The marine fouling as biomass on brass was assessed and presented in this thesis, The physicochemical properties of estuarine water were correlated with corrosion behaviour of brass.The deterioration of the brass subjected to the effect of estuarine water was also investigated as a measure of loss in mechanical properties such as tensile strength,yield strength,percntage elongation and percentage reduction in area.To validate dezincification data,visual observation,spot analysis,surface morphology before and after removal of corrosion products and corrosion product analysis were performed.The dezincification behavior of epoxy coated brass of the present study has beenhighlighted in terms of corrosion rate ,weight gain/loss,corrosion current and polarization resistance,open circuit potential.dezincification factor.The marine fouling as biomass on epoxy coated brass subjeted to the effect of estuarine water was also investigated as ameasure of loss in mechanical properties such as tensile strength,percentage elongation and percentage reduction in area.The results of dezincification behavior of brass and epoxy coated brass in Cochin estuary water has been presented and discussed.Attempt has been made to correlate the dezincification behavior of brass with epoxy coated brass.
Resumo:
The acoustic signals generated in solids due to interaction with pulsed laser beam is used to determine the ablation threshold of bulk polymer samples of teflon (polytetrafluoroethylene) and nylon under the irradiation from a Q-switched Nd:YAG laser at 1.06µm wavelength. A suitably designed piezoelectric transducer is employed for the detection of photoacoustic (PA) signals generated in this process. It has been observed that an abrupt increase in the amplitude of the PA signal occurs at the ablation threshold. Also there exist distinct values for the threshold corresponding to different mechanisms operative in producing damages like surface morphology, bond breaking and melting processes at different laser energy densities.
Resumo:
The main objective of this thesis work is to optimize the growth conditions for obtaining crystalline and conducting Lao.5Sro.5Co03 (LSCO) and Lao.5Sro.5Coo.5.5Nio.5O3 (LSCNO) thin films at low processing temperatures. The films are prepared by radio frequency magnetron sputtering under various deposition conditions. The thin films were used as electrodes for the fabrication of ferroelectric capacitors using BaO.7SrO.3 Ti03 (BST) and PbZro.52 Tio.4803 (PZT). The structural and transport properties of the La1_xSrxCo03 and Lao.5Sro.5Co1_xNix03 are also investigated. The characterization of the bulk and the thin films were performed using different tools. A powder X-ray diffractometer was used to analyze the crystalline nature of the material. The transport properties were investigated by measuring the temperature dependence of resistivity using a four probe technique. The magnetoresistance and thermoelectric power were also used to investigate the transport properties. Atomic force microscope was used to study the surface morphology and thin film roughness. The ferroelectric properties of the capacitors were investigated using RT66A ferroelectric tester.
Resumo:
Co–Fe–Si based films exhibit high magnetic moments and are highly sought after for applications like soft under layer sinper pendicular recording mediatomagneto-electro-mechanical sensor applications.In this workt he effect of annealing on s tructural,morphologicaland magnetic propertiesofco–Fe–Si thin films wasinvestigated.compositional analysis using x-rayphotoelectron spectroscopy and secondary ion massspectroscopyrevealedanativeoxidesurfacelayerconsistingofoxidesofco,feandsionthe surface. The morphology of theas deposited films shows mound like structures conformingtothe Volmer–Webergrowthmodel.Nanocrystallisationofamorphous films upon annealing was observed by glancing anglex-raydiffraction and transmission electron microscopy.Theevolutionofmagnetic properties with annealing is explained using the Herzermodel.Vibrating sample magnetometry measurements carried out at various angles from01 to 901 to the applied magnetic field were employed to study the angula rvariation of coercivity.The angular variation fits the modified Kondorsky model. Interestingly,the coercivity evolution with annealing deduced frommagneto-opticalKerreffectstudies indicates areversetrendcomparedtomagetisationobservedinthebulk.Thiscanbeattributedtoa domain wallpinningatnativeoxidelayeronthesurfaceofthin films. Theevolutionofsurfacemagnetic properties iscorrelatedwithmorphologyevolutionprobedusingatomicforcemicroscopy.The morphology aswellasthepresenceofthenativeoxidelayerdictatesthesurfacemagneticproperties and this is corroborated by the apparent difference in the bulk and surface magnetic properties
Resumo:
Ultra thin films based on CoFe were prepared from a composite target employing thermal evaporation. The microstructure of the films was modified by thermal annealing. The relationship between microstructure and magnetic properties of the films was investigated using techniques like glancing angle X-ray diffraction (GXRD), transmission electron microscopy (TEM) and vibrating sample magnetometry (VSM). The GXRD and TEM investigations showed an onset of crystallization of CoFe at around 373 K. The magnetic softness of the films improved with thermal annealing but at higher annealing temperature it is found to be deteriorating. Annealing inducedmodification of surface morphology of the alloy thin filmswas probed by atomic force microscopy (AFM). Surface smoothening was observed with thermal annealing and the observed magnetic properties correlate well with surface modifications induced by thermal annealing
Resumo:
ZnO nanoflowers were synthesized by the hydrothermal process at an optimized growth temperature of 200 ◦C and a growth/reaction time of 3 h. As-prepared ZnO nanoflowers were characterized by x-ray diffraction, scanning electron microscopy, UV–visible and Raman spectroscopy. X-ray diffraction and Raman studies reveal that the as-synthesized flower-like ZnO nanostructures are highly crystalline with a hexagonal wurtzite phase preferentially oriented along the (1 0 1 1) plane. The average length (234–347 nm) and diameter (77–106 nm) of the nanorods constituting the flower-like structure are estimated using scanning electron microscopy studies. The band gap of ZnO nanoflowers is estimated as 3.23 eV, the lowering of band gap is attributed to the flower-like surface morphology and microstructure of ZnO. Room temperature photoluminescence spectrum shows a strong UV emission peak at 392 nm, with a suppressed visible emission related to the defect states, indicating the defect free formation of ZnO nanoflowers that can be potentially used for UV light-emitting devices. The suppressed Raman bands at 541 and 583 cm−1 related to defect states in ZnO confirms that the ZnO nanoflowers here obtained have a reduced presence of defects
Resumo:
Increasing amounts of plastic waste in the environment have become a problem of gigantic proportions. The case of linear low-density polyethylene (LLDPE) is especially significant as it is widely used for packaging and other applications. This synthetic polymer is normally not biodegradable until it is degraded into low molecular mass fragments that can be assimilated by microorganisms. Blends of nonbiodegradable polymers and biodegradable commercial polymers such as poly (vinyl alcohol) (PVA) can facilitate a reduction in the volume of plastic waste when they undergo partial degradation. Further, the remaining fragments stand a greater chance of undergoing biodegradation in a much shorter span of time. In this investigation, LLDPE was blended with different proportions of PVA (5–30%) in a torque rheometer. Mechanical, thermal, and biodegradation studies were carried out on the blends. The biodegradability of LLDPE/PVA blends has been studied in two environments: (1) in a culture medium containing Vibrio sp. and (2) soil environment, both over a period of 15 weeks. Blends exposed to culture medium degraded more than that exposed to soil environment. Changes in various properties of LLDPE/PVA blends before and after degradation were monitored using Fourier transform infrared spectroscopy, a differential scanning calorimeter (DSC) for crystallinity, and scanning electron microscope (SEM) for surface morphology among other things. Percentage crystallinity decreased as the PVA content increased and biodegradation resulted in an increase of crystallinity in LLDPE/PVA blends. The results prove that partial biodegradation of the blends has occurred holding promise for an eventual biodegradable product
Amphiphile Verbindungen der 14. Gruppe - Synthese, Eigenschaften und Anwendungen von Organosilanolen
Resumo:
Im Rahmen dieser Dissertation wurde an der Darstellung stabiler, amphiphiler Silantriole gearbeitet. Es ist gelungen eine kontinuierliche Reihe sukzessive um CH2-Einheiten verlängerter Silantriole des Typs H3C(CH2)nC(CH3)2Si(OH)3 (n = 1-5) durch eine vierstufige Synthesesequenz ausgehend von n-Alkylbromiden herzustellen und zum Teil röntgenographisch zu untersuchen. Ihre oberflächenaktiven Eigenschaften in wässrigen Lösungen konnten erstmals mittels Oberflächenspannungsmessungen belegt werden. Durch gezielte Kondensationsreaktionen mit Trifluoressigsäure wurden ausgehend von den oben beschriebenen Silantriolen selektiv die entsprechenden Disiloxan-Tetrole erhalten und ebenfalls zum Teil durch Röntgenstrukturanalysen charakterisiert. Als weitere Kondensationsprodukte der Silantriole konnten die ersten Octasilsesquioxane mit tertiären Kohlenstoff-Substituenten durch Umsetzungen mit n-Bu4NF selektiv und in hohen Ausbeuten erhalten und ebenfalls röntgenographisch identifiziert werden. Es wurde an der Darstellung Aryl-substituierter Silantriole RSi(OH)3 (R = Mesityl-, Xylyl- und Tetramethyl-phenyl-) gearbeitet. Diese zeichnen sich jedoch durch ihre hohe Instabilität in Lösung und im Festkörper aus und konnten zum Teil nur zusammen mit ihren primären Kondensationsprodukten erhalten werden. Darüber hinaus wurden stabile Silandiole des Typs R(t-Bu)Si(OH)2 (R = n-Butyl und n-Pentyl) sowie das (o-CF3C6H4)2Si(OH)2 in hohen Ausbeuten und selektiv synthetisiert. Die Festkörpereigenschaften des (o-CF3C6H4)2Si(OH)2 sowie seiner Vorstufe (o-CF3C6H4)2SiCl2 konnten durch Kristallstrukturanalysen genauer untersucht werden. In der Arbeit wurden die ersten Anwendungen von Silanolen als Silan-Kupplungsreagenzien bei der Oberflächenmodifizierung von Glas beschrieben. Im Gegensatz zu gängigen säureassistierten Beschichtungen zeichnen sich diese Silanol-Beschichtungen durch eine deutlich höhere Hydrophobizität aus. Dies konnte durch Kontaktwinkel- und Zeta-Potential-Messungen bestätigt werden. Durch Röntgenreflektivitäts- und Sarfus-Messungen ist die Ausbildung von Monolagen im Falle von t-BuSi(OH)3-beschichteten Oberflächen plausibel. Die Oberflächenmorphologie der Silantriol-Beschichtungen wurde mittels AFM-Messungen untersucht. Die Si(OH)3-Funktion konnte in der vorliegenden Arbeit als ein neues Pharmakophor etabliert werden. Die Silantriole CySi(OH)3, TerSi(OH)3 und CH3CH2C(CH3)2Si(OH)3 (Cy = Cyclohexyl, Ter = Terphenyl) sind in der Lage das Enzym Acetylcholinesterase reversibel zu hemmen. Dabei zeigt das CySi(OH)3 mit 45 % relativ zur Kontrolle die höchste Inhibition.
Resumo:
LiCoO₂thin films have been grown by pulsed laser deposition on stainless steel and SiO₂/Si substrates. The film deposited at 600°C in an oxygen partial pressure of 100mTorr shows an excellent crystallinity, stoichiometry and no impurity phase present. Microstructure and surface morphology of thin films were examined using a scanning electron microscope. The electrochemical properties of the thin films were studied with cyclic voltammetry and galvanostatic charge-discharge techniques in the potential range 3.0-4.2 V. The initial discharge capacity of the LiCoO2 thin films deposited on the stainless steel and SiO₂/Si substrates reached 23 and 27 µAh/cm², respectively.
Resumo:
The morphology in the solid state of a series of triblock copolymers comprising a poly(ethylene glycol) (PEG) midblock and symmetric poly(gamma-benzyl-L-glutamate) (PBLG) end blocks has been studied using X-ray scattering and microscopy techniques. Transmission electron microscopy (TEM) on samples selectively stained with uranyl acetate provided clear assignment of morphologies for as-cast and annealed samples. The thickness of both PEG and PBLG domains was in good agreement with calculations based on the conformations of the respective chains, allowing for the crystal or amorphous state of PEG and the a-helical or P-sheet structure of the PBLG. Atomic force microscopy provided complementary information on surface morphology for several samples that was in good agreement with the structure observed by TEM. A morphology diagram was constructed. Cylindrical structures were observed for ordered samples with low f(PBLG), whereas at higher f(PLBG) there was evidence for broken lamellar and "hockey puck" nanostructures. Regular lamellae were observed for intermediate compositions.
Resumo:
Practically all extant work on flows over obstacle arrays, whether laboratory experiments or numerical modelling, is for cases where the oncoming wind is normal to salient faces of the obstacles. In the field, however, this is rarely the case. Here, simulations of flows at various directions over arrays of cubes representing typical urban canopy regions are presented and discussed. The computations are of both direct numerical simulation and large-eddy simulation type. Attention is concentrated on the differences in the mean flow within the canopy region arising from the different wind directions and the consequent effects on global properties such as the total surface drag, which can change very significantly—by up to a factor of three in some circumstances. It is shown that for a given Reynolds number the typical viscous forces are generally a rather larger fraction of the pressure forces (principally the drag) for non-normal than for normal wind directions and that, dependent on the surface morphology, the average flow direction deep within the canopy can be largely independent of the oncoming wind direction. Even for regular arrays of regular obstacles, a wind direction not normal to the obstacle faces can in general generate a lateral lift force (in the direction normal to the oncoming flow). The results demonstrate this and it is shown how computations in a finite domain with the oncoming flow generated by an appropriate forcing term (e.g. a pressure gradient) then lead inevitably to an oncoming wind direction aloft that is not aligned with the forcing term vector.
Resumo:
The aim of this study was to assess in vitro the influence of Er:YAG laser irradiation distance on the shear strength of the bond between an adhesive restorative system and primary dentin. A total of 60 crowns of primary molars were embedded in acrylic resin and mechanically ground to expose a flat dentin surface and were randomly assigned to six groups (n = 10). The control group was etched with 37% phosphoric acid. The remaining five groups were irradiated (80 mJ, 2 Hz) at different irradiation distances (11, 12, 16, 17 and 20 mm), followed by acid etching. An adhesive agent (Single Bond) was applied to the bonding sites, and resin cylinders (Filtek Z250) were prepared. The shear bond strength tests were performed in a universal testing machine (0.5 mm/min). Data were submitted to statistical analysis using one-way ANOVA and the Kruskal-Wallis test (p < 0.05). The mean shear bond strengths were: 7.32 +/- 3.83, 5.07 +/- 2.62, 6.49 +/- 1.64, 7.71 +/- 0.66, 7.33 +/- 0.02, and 9.65 +/- 2.41 MPa in the control group and the groups irradiated at 11, 12, 16, 17, and 20 mm, respectively. The differences between the bond strengths in groups II and IV and between the bond strengths in groups II and VI were statistically significant (p < 0.05). Increasing the laser irradiation distance resulted in increasing shear strength of the bond to primary dentin.