611 resultados para Rheology


Relevância:

10.00% 10.00%

Publicador:

Resumo:

The construction of wells is one of the most important activities of the oil industry. The drilling process is the set of activities and operations to design, program and perform the opening thereof. During this process, the cuttings are removed by the drilling fluid, or mud, and carted to the surface. This fluid is injected into the drill string and returns to the surface through the annular space between the well walls and the drill string. After the descent of the column casing, the annular space between the casing string and the walls of the borehole is filled with cement so as to secure the spine and prevent any migration of fluids between the various permeable zones traversed by the well behind of the coating. To ensure the good quality of the cementation scrubbers are used mattresses which are pumped ahead of the cement slurry so as to avoid contamination of the drilling fluid paste, or vice versa, and assist in the removal of plaster, formed by drilling fluid of the borehole walls, thus enabling a better cement bond to the well. Within this context, this work aims to evaluate the efficiency of mattresses scrubbers, the basis of ionic and nonionic surfactants, on the removal of nonaqueous drilling fluid, based on n-paraffin in oil wells, and the compatibility between the Mattress relations washer / drilling fluid bed scrubber / cement paste mattress washer / cement slurry / drilling fluid and the drilling fluid / cement slurry using laboratory tests rheology, thickening time and compressive strength. Also technique was performed X-ray diffraction (XRD) for a more detailed analysis of these mixtures with hydrated cement paste. In compatibility tests the conditions of temperature and pressure used in the same laboratory procedure simulating the conditions of oil wells, the well is considered the depth of 800 m. The results showed that the compositions of the mattress washer nonionic, KMS obtained a 100% efficient in removing the non-aqueous drilling fluid, and the best formulation showed good results with respect to compliance testing

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Surfactant-polymer interactions are widely used when required rheological properties for specific applications, such as the production of fluids for oil exploration. Studies of the interactions of chitosan with cationic surfactants has attracted attention by being able to cause changes in rheological parameters of the systems making room for new applications. The commercial chitosan represents an interesting alternative to these systems, since it is obtained from partial deacetylation of chitin: the residues sites acetylated can then be used for the polymer-surfactant interactions. Alkyl ethoxylated surfactants can be used in this system, since these non-ionic surfactants can interact with hydrophobic sites of chitosan, modifying the rheology of solutions or emulsions resultants, which depends on the relaxation phenomenon occurring in these systems. In this work, first, inverse emulsions were prepared from chitosan solution as the dispersed phase and cyclohexane as the continuous phase were, using CTAB as a surfactant. The rheological analysis of these emulsions showed pronounced pseudoplastic behavior. This behavior was attributed to interaction of "loops" of chitosan chains. Creep tests were also performed and gave further support to these discussions. Subsequently, in order to obtain more information about the interaction of chitosan with non-ionic surfactants, solutions of chitosan were mixed with C12E8 and and carried out rheological analysis and dynamic light scattering. The systems showed marked pseudoplastic behavior, which became less evident when the concentration of surfactant was increased. Arrhenius and KWW equations were used to obtain parameters of the apparent activation energy and relaxation rate distribution, respectively, to which were connected to the content of surfactant and temperature used in this work

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Chitosan is a biopolymer derived from the shells of crustaceans, biodegradable, inexpensive and renewable with important physical and chemical properties. Moreover, the different modifications possible in its chemical structure generate new properties, making it an attractive polysaccharide owing to its range of potential applications. Polymers have been used in oil production operations. However, growing concern over environmental constraints has prompted oil industry to search for environmentally sustainable materials. As such, this study sought to obtain chitosan derivatives grafted with hydrophilic (poly(ethylene glycol), mPEG) and/or hydrophobic groups (n-dodecyl) via a simple (one-pot) method and evaluate their physicochemical properties as a function of varying pH using rheology, small-angle Xray scattering (SAXS), dynamic light scattering (DLS) and zeta potential. The chitosan derivatives were prepared using reductive alkylation under mild reaction conditions and the chemical structure of the polymers was characterized by nuclear magnetic resonance (1H NMR) and CHN elemental analysis. Considering a constant mPEG/Chitosan molar ratio on modification of chitosan, the solubility of the polymer across a wide pH range (acidic, neutral and basic) could only be improved when some of the amino groups were submitted to reacetylation using the one-pot method. Under these conditions, solubility is maintained even with the simultaneous insertion of n-dodecyl. On the other hand, the solubility of derivatives obtained only through mPEG incorporation using the traditional methodology, or with the ndodecyl group, was similar to that of its precursor. The hydrophilic group promoted decreased viscosity of the polymer solutions at 10 g/L in acid medium. However, at basic pH, both viscosity and thermal stability increased, as well as exhibited a pronounced pseudoplastic behavior, suggesting strong intermolecular associations in the alkaline medium. The SAXS results showed a polyelectrolyte behavior with the decrease in pH for the polymer systems. DLS analyses revealed that although the dilute polymer solutions at 1 g/L and pH 3 exhibited a high density of protonated amino groups along the polymer chain, the high degree of charge contributed significantly to aggregation, promoting increased particle size with the decrease in pH. Furthermore, the hydrophobic group also contributed to increasing the size of aggregates in solution at pH 3, whereas the hydrophilic group helped reduce their size across the entire pH range. Nevertheless, the nature of aggregation was dependent on the pH of the medium. Zeta potential results indicated that its values do not depend solely on the surface charge of the particle, but are also dependent on the net charge of the medium. In this study, water soluble associative polymers exhibit properties that can be of great interest in the petroleum industry

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Sustainable development is a major challenge in the oil industry and has aroused growing interest in research to obtain materials from renewable sources. Carboxymethylcellulose (CMC) is a polysaccharide derived from cellulose and becomes attractive because it is water-soluble, renewable, biodegradable and inexpensive, as well as may be chemically modified to gain new properties. Among the derivatives of carboxymethylcellulose, systems have been developed to induce stimuli-responsive properties and extend the applicability of multiple-responsive materials. Although these new materials have been the subject of study, understanding of their physicochemical properties, such as viscosity, solubility and particle size as a function of pH and temperature, is still very limited. This study describes systems of physical blends and copolymers based on carboxymethylcellulose and poly (N-isopropylacrylamide) (PNIPAM), with different feed percentage compositions of the reaction (25CMC, 50CMC e 75CMC), in aqueous solution. The chemical structure of the polymers was investigated by infrared and CHN elementary analysis. The physical blends were analyzed by rheology and the copolymers by UV-visible spectroscopy, small-angle X-ray scattering (SAXS), dynamic light scattering (DLS) and zeta potential. CMC and copolymer were assessed as scale inhibitors of calcium carbonate (CaCO3) using dynamic tube blocking tests and chemical compatibility tests, as well as scanning electron microscopy (SEM). Thermothickening behavior was observed for the 50 % CMC_50 % PNIPAM and 25 % CMC_75 % PNIPAM physical blends in aqueous solution at concentrations of 6 and 2 g/L, respectively, depending on polymer concentration and composition. For the copolymers, the increase in temperature and amount of PNIPAM favored polymer-polymer interactions through hydrophobic groups, resulting in increased turbidity of polymer solutions. Particle size decreased with the rise in copolymer PNIPAM content as a function of pH (3-12), at 25 °C. Larger amounts of CMC result in a stronger effect of pH on particle size, indicating pH-responsive behavior. Thus, 25CMC was not affected by the change in pH, exhibiting similar behavior to PNIPAM. In addition, the presence of acidic or basic additives influenced particle size, which was smaller in the presence of the additives than in distilled water. The results of zeta potential also showed greater variation for polymers in distilled water than in the presence of acids and bases. The lower critical solution temperature (LCST) of PNIPAM determined by DLS corroborated the value obtained by UV-visible spectroscopy. SAXS data for PNIPAM and 50CMC indicated phase transition when the temperature increased from 32 to 34 °C. A reduction in or absence of electrostatic properties was observed as a function of increased PNIPAM in copolymer composition. Assessment of samples as scale inhibitors showed that CMC performed better than the copolymers. This was attributed to the higher charge density present in CMC. The SEM micrographs confirmed morphological changes in the CaCO3 crystals, demonstrating the scale inhibiting potential of these polymers

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The present article describes the preparation and characterization A anionic Collagen gels obtained from porcine intestinal submucosa after 72 h of alkaline treatment and in the form of rhamsan composites to develop injectable biomaterials for plastic for construction. All materials were characterized by SDS/polyacrylamide gel electrophoresis, infrared spectroscopy, thermal stability, potentiometric titration, rheological properties, and fluidity tests. Biocompatibility was appraised after the injection of anionic collagen:rhamsan composites at 2.5% in 60 North Folk rabbits. Independently of processing, the Collagen's secondary structure was preserved in all cases, and after 72 h of hydrolysis the Collagen was characterized by a carboxyl group content of 346 :L 9, which, at physiological pH, corresponds to an increase of 106 17 negative charges, in comparison to native Collagen, due to the selective hydrolysis of asparagine and glutamine carboxyamide side chain. Rheological studies of composites at pH 7.4 in concentrations of 2, 4, and 6% (in proportions of 75:1 and 50:1) showed a viscoelastic behavior dependent on the frequency, which is independent of concentration and proportion. In both, the concentration of the storage modulus always predominated over the loss modulus (G' > G and delta < 45 degrees). The results from creep experiments confirmed this behavior and showed that anionic collagen:rhamsan composites at pH 7.4 in the proportion of 50:1 are less elastic and more susceptible to deformation in comparison to gels in the proportion of 75:1, independent of concentration. This was further confirmed by flow experiments, indicating that the necessary force for the extrusion of anionic collagen:rhamsan composites, in comparison to anionic Collagen, was significantly smaller and with a smooth flow. Biocompatibility studies showed that the tissue reaction of anionic collagen:rhamsan composites at 2.5% in the proportion of 75:1 was compatible with the application of these gels in plastic reconstruction. These results suggest that the association of Collagen with rhamsan may be a good alternative in the replacement of glutaraidehyde to stabilize the microfibril assembly of commercial Collagen gel preparations. (c) 2005 Wiley Periodicals, Inc.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Partial pseudoternary phase diagrams were constructed for soy bean oil (SBO)/surfactant/NaCl aqueous solution systems, at 25 degrees C, using the anionic sodium bis(2-ethylhexyl) sulfosuccinate (ACT) and zwiterionic phosphatidylcholine (PC) or mixtures of these surfactants. The isotropic single phase of water-in-oil (W/O) microemulsions (MEs) is shown in the phase diagram and their viscosity reported. ME samples containing small amount of surfactant exhibit slightly higher viscosity than pure SBO, and were used in the solubilization of small water soluble molecules. NaCl enhances the area of the ME phase and MEs with different surfactant composition exhibit different induction time as obtained from tests of oxidative stability, and so are the MEs enriched with ascorbic acid, folic acid and FeSO4, with the latter exhibiting lower stability. The so prepared enriched soy bean oil has potential application in food industry since the surfactants are food grade. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Este estudo surgiu da necessidade das indústrias cerâmicas do pólo de Santa Gertrudes (SP) se adaptarem às mudanças do comportamento do mercado e às exigências dos órgãos ambientais em relação aos riscos causados pela geração de poeira na fase de preparação da massa. Assim, o processo de preparação de massa via úmida pode ser uma alternativa para esta substituição, sendo necessária a obtenção de uma barbotina que apresente um comportamento reológico adequado ao processo e ao consumo de energia. Foram feitas medidas de viscosidade, tensão de cisalhamento e taxa de cisalhamento com viscosímetro rotacional, tendo como parâmetros de controle, o teor de sólidos da barbotina e a granulometria. Desta forma, foram verificadas variações das suspensões, como o comportamento pseudoplástico e a tixotropia. Também foi analisada a dependência do comportamento reológico com a mineralogia das argilas, obtida por difração de raios X. Os resultados das curvas reológicas mostraram-se muito coerentes com a mineralogia determinada, indicando uma piora do comportamento reológico no sentido da base para o topo da Formação Corumbataí, devido à alteração supérgena e presença de esmectitas.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The physicochemical (pH, fat and total solids content), sensory (appearance, consistency and taste), and rheological characteristics of five different commercial brands of lactic beverages were determined. Rheological measurements were obtained at 5 degreesC and 25 degreesC using a Brookfield rheometer. The experimental data were described by the power law and Herschel-Bulkley models. The ANOVA of the results were conducted using an incomplete block design, and using Tukey test. Samples showed a significant difference (P less than or equal to 0.05%) for fat content and pH. There was a significant difference in total solids content only among Nestle (A), Batavo (C), and Parmalat (D) samples. Sensory evaluation showed more global acceptability for Nestle; however, Nestle and Vigor (E) lactic beverages obtained better results for appearance than for consistency and taste. Batavo obtained the best score for taste. All test samples exhibited non-Newtonian behavior, with thixotropy. Upward curves showed pseudoplastic behavior, while downward curves showed dilatant behavior with the exception of the Nestle sample, at 25 degreesC. Lactic beverages from all brands analyzed showed similar rheological behavior. (C) 2001 Elsevier B.V. Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Hybrid siloxane-polymethylmethacrylate (PMMA) nanocomposites with covalent bonds between the inorganic (siloxane) and organic (polymer) phases were prepared by the sot gel process through hydrolysis and polycondensation of 3-(trimethoxysilyl)propylmethacrylate (TMSM) and polymerization of methylmethacrylate (MMA) using benzoyl peroxide (BPO) as initiator. The effect of MMA, BPO and water contents on the viscoelastic behaviour of these materials was analysed during gelation by dynamic rheological measurements. The changes in storage (G') and loss moduli (G), complex viscosity (eta*) and phase angle (6) were measured as a function of the reaction time showing the viscous character of the sot in the initial step of gelation and its progressive transformation to an elastic gel. This study was complemented by Si-29 and C-13 solid-state nuclear magnetic resonance (NMR/MAS) measurements of dried gel. The analysis of the experimental results shows that linear chains are formed in the initial step of the gelation followed by a growth of branched structures and formation of a three-dimensional network. Near the gel point this hybrid material demonstrates the typical scaling behaviour expected from percolation theory.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The thermoreversible sol-gel transition is well-known in biological and organic polymeric systems but has not been reported for inorganic systems. In this paper we put in evidence a thermoreversible sol-gel transition for zirconyl chloride aqueous solutions modified by sulfuric acid in the ratio 3:1 Zr:SO4. The synthesis conditions are detailed and a variety of experimental techniques (turbidimetry, dynamic rheology, and EXAFS) have been employed for investigating the thermal reversibility and the chemical structure of this new material. Turbidimetric measurements performed for solutions containing different concentrations of precursor have evidenced that the sol-gel transformation temperature increases from 50 to 80 degrees C as the concentration of zirconyl chloride decreases from 0.22 to 0.018 mol L-1. A more detailed study has been done for the sample with [Zr] = 0.156 mol L-1, in which the sol-gel-sol transformation has been repeated several times by a cyclic variation of the temperature. The mechanical properties of this sample, evaluated by measuring the storage and the loss moduli, show a change from liquid like to viscoelastic to elastic behavior during the sol-gel transition and vice versa during the gel-sol one. In situ EXAFS measurements performed at the Zr K-edge show that no change of the local order around Zr occurs during the sol-gel-sol transition, in agreement with the concept of physical gel formation. We have proposed for the structure of the precursor an inner core made of hydroxyl and oxo groups bridging together zirconium atoms surrounded in surface by complexing sulfate ligands, the sulfate groups act as a protective layer, playing a key role in the linking propagation among primary particles during sol-gel-sol transition.