Resumo:
This work reports on the preparation of Gd2O3, cubic system, with spherical particles, narrow size distribution, whether or not doped with 1-5 at.% of Eu3+ and the influence of Eu3+ concentration on optical and morphological properties. Average diameter and size distribution particle analyses were performed for all samples from SEM results. Doped samples were also investigated by luminescence spectroscopy and emission kinetic measurements. All oxide samples present a particle average diameter distribution range from 110 to 150 nm and a decrease of particle average diameter with the presence of Eu3+. The particle size decrease is almost the same for all samples with different doping ion concentration. Therefore, the presence of doping ion may be inhibiting particle growth after the nucleation process. From spectroscopic studies, the doping ion distribution in the surface of oxide samples can be considered homogeneous because concentration quenching is not observed, as well as a significant difference among the calculated lifetime for each sample. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
Nanocrystalline Pd-Co alloys were obtained by electrodeposition from an ammoniacal chloride bath. The influence of the crystallite size and the residual stress on the magnetic properties of the alloys was investigated. The residual stress increased as the applied current density was increased. It was associated to the high nucleation rate during electrodeposition and correlated to the lattice strain, estimated from the XRD patterns. Also from the XRD patterns the average crystallite size and the lattice constant were determined by Scherrer's and Rietveld's methods, respectively. Both parameters were directly influenced by the applied current density. Magnetic properties such as coercivity, remanence, saturation magnetization and squareness showed strong dependence on the residual stress and crystallite size. Coercivity higher than 1 kOe was achieved when a high current density was applied. High coercivity was attributed to the presence of residual stress and to the small crystallite size of deposits. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Tungsten carbide, WC, has shown dissimilar thermal behavior when it is heated on changeable heating rate and flow of oxidant atmosphere. The oxidation of WC to WO3 tends to be in a single and slow kinetic step on slow heating rate and/or low flux of air. Kinetic parameters, on non-isothermal condition, could be evaluated to the oxidation of WC to heating rate below 15 degrees C min(-1) or low flow of air (10 mL min(-1)). The reaction is governed by nucleation and growth at 5 to 10 degrees C min(-1) then the tendency is to be autocatalytic, JMA and SB, respectively.
Resumo:
The controlled growth of SnO2 nanoparticles for gas sensor applications is reported by these authors. Nb2O5 additive is used to control nucleation and growth of the SnO2 (see Figure), which is synthesized by the polymeric precursor method. Preliminary gas sensing measurements are performed and it is demonstrated that the response time of the Nb2O5-doped SnO2 is faster than that of the undoped material.
Resumo:
A new synthetic route for producing monodispersed and single crystal acicular goethite particles with small particle size and a high axial ratio adequate for use as a high density magnetic recording media precursor is reported. It essentially consists of the hydrolysis of alkaline Fe-III suspensions in the presence of carbonate by a three-step procedure, the formation of ferrihydrite primary particles, the ferrihydrite dissolution and nucleation of goethite, and the growth of the goethite nuclei. Changing the temperature of heating during ageing achieved a separation of the two last stages. X-Ray diffraction, transmission electron microscopy, infrared spectroscopy and surface area data have been used to determine the mechanism responsible for the formation of goethite particles with controlled size and shape. The best conditions to prepare monodispersed goethite particles have been established. The results show that uniform goethite particles of (a) 60 nm length with an axial ratio of 6 and (b) 230 nm length with a high axial ratio of 10, can be obtained by using an [OH]/[Fe] molar ratio of 0.35 in the initial suspensions with carbonate or sodium hydroxide, respectively. The [OH]/[Fe] molar ratio determines the particle size and elongation by controlling the hydrolysis reaction rate, while the carbonate ions promote a constant [OH] in the solution, keeping the pH around 10 during the entire synthesis process. This procedure, associated with the appropriate temperature control, leads, under certain conditions, to highly homogeneous goethite particles with sizes smaller than those obtained using sodium hydroxide with the same [OH]/[Fe] ratio.
Resumo:
Results of differential scanning calometry (DSC), x-ray diffraction (XRD), and F-19 nuclear magnetic resonance (NMR) of InF3-based glasses, treated at different temperatures, ranging from glass transition temperature (T-g) to crystallization temperature (T-c), are reported. The main features of the experimental results are as follows. DSC analysis emphasizes several steps in the crystallization process. Heat treatment at temperatures above T-g enhances the nucleation of the first growing phases but has little influence on the following ones. XRD results show that several crystalline phases are formed, with solid state transitions when heated above 680 K, the F-19 NMR results show that the spin-lattice relaxation, for the glass samples heat treated above 638 K, is described by two time constants. For samples treated below this temperature a single time constant T-1 was observed. Measurements of the F-19 spin-lattice relaxation time (T-1), as a function of temperature,made possible the identification of the mobile fluoride ions. The activation energy, for the ionic motion, in samples treated at crystallization temperature was found to be 0.18 +/- 0.01 eV. (C) 1998 American Institute of Physics.
Resumo:
Stoichiometric CaWO4 and SrWO4 thin films were synthesized using a chemical solution processing, the so-called polymeric precursor method. In this soft chemical method, soluble precursors such as strontium carbonate, calcium carbonate and tungstic acid, as starting materials, were mixed in an aqueous solution. The thin films were deposited on glass substrates by means of the spinning technique. The surface morphology and crystal structure of the thin films were investigated using X-ray diffraction (XRD), scanning electron microscopy (SEM), and atomic force microscopy (AFM). Nucleation stages and surface morphology evolution of the thin films on glass substrates were studied by atomic force microscopy. The films nucleate at 300 degreesC, after the coalescence of small nuclei into larger grains yielding a homogeneous dense surface. XRD characterization of these films showed that the CaWO4 and SrWO4 phases crystallize at 400 degreesC from an inorganic amorphous phase. No intermediate crystalline phase was identified. The optical properties were also studied. It was found that CaWO4 and SrWO4 thin films have an optical band gap, E-gap=5.27 and 5.78 eV, respectively, of a direct transition nature. The excellent microstructural quality and chemical homogeneity confirmed that this soft solution processing provides an inexpensive and environmentally friendly route for the preparation of CaWO4 and SrWO4 thin films. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
The adsorption process in layer-by-layer (LBL) films of poly(o-methoxyaniline) alternated with poly(vinyl sulfonic acid) is explained using the Avrami equation. This equation was used due to its mathematical simplicity and adequate description of experimental data in real polymer systems. The Avrami parameters are a convenient means to represent empirical data of crystallization, and if microscopic knowledge is available these parameters can also be associated with adsorption mechanisms. The growth of spherulites in the LBL films was studied as a function of time using atomic force microscopy and the data were used to estimate the number and radii of aggregates, from which the Avrami parameters were determined. We find that the adsorption mechanism may correspond to a tri dimensional, diffusion-controlled growth, with increasing nucleation rate, consistent with results from kinetics of adsorption.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Buried two-dimensional arrays of InP dots were used as a template for the lateral ordering of self-assembled quantum dots. The template strain field can laterally organize compressive (InAs) as well as tensile (GaP) self-assembled nanostructures in a highly ordered square lattice. High-resolution transmission electron microscopy measurements show that the InAs dots are vertically correlated to the InP template, while the GaP dots are vertically anti-correlated, nucleating in the position between two buried InP dots. Finite InP dot size effects are observed to originate InAs clustering but do not affect GaP dot nucleation. The possibility of bilayer formation with different vertical correlations suggests a new path for obtaining three-dimensional pseudocrystals.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
The preparation of nanometer-sized structures of zinc oxide (ZnO) from zinc acetate and urea as raw materials was performed using conventional water bath heating and a microwave hydrothermal (MH) method in an aqueous solution. The oxide formation is controlled by decomposition of the added urea in the sealed autoclave. The influence of urea and the synthesis method on the final product formation are discussed. Broadband photoluminescence (PL) behavior in visible-range spectra was observed with a maximum peak centered in the green region which was attributed to different defects and the structural changes involved with ZnO crystals which were produced during the nucleation process.