948 resultados para Polymeric precursor


Relevância:

60.00% 60.00%

Publicador:

Resumo:

Lead zirconate titanate (PZT) was synthesized at the ratio of Zr/Ti=52/48 using two synthesis methods: the polymeric precursor method (PPM) and the microwave-assisted hydrothermal method (MAHM). The synthesized materials were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), particle size distribution by sedimentation, hysteresis measurements and photoluminescence (PL). The results showed that PZT powders are composed of tetragonal and rhombohedral phases. Different particle sizes and morphologies were obtained depending upon the synthesis method. From the hysteresis loop verified that PZT powders synthesized by the PPM have a typical loop of ferroelectric material and are more influenced by spatial charges while particles synthesized by the MAHM have a hysteresis loop similar to paraelectric material and are less influenced by spatial charges. Both samples showed PL behavior in the green region (525 nm) whereas the sample synthesized by the PPM showed higher intensity in spectra. © 2013 Elsevier Ltd and Techna Group S.r.l.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This work describes the influence of the preparation method and the carbon support using a low contentof cerium oxide nanoparticles (CeO2/C 4%) on H2O2electrogeneration via the oxygen reduction reac-tion (ORR). For this purpose, the polymeric precursor (PPM) and sol-gel (SGM) methods with Vulcan XC72R (V) and Printex L6 (P) supports were employed. The materials were characterized by X-ray diffrac-tion (XRD), X-ray photoelectron spectroscopy (XPS) and transmission electron microscopy (TEM). TheXRD analysis identified two phases comprising CeO2and CeO 2-x. The smallest mean crystallite size wasexhibited for the 4% CeO2/C PPM P material, which was estimated using the Debye-Scherrer equation tobe 6 nm and 4 nm for the CeO2and the CeO 2-xphases, respectively, and was determined by TEM to be5.9 nm. XPS analysis was utilized to compare the oxygen content of the 4% CeO2/C PPM P to Printex L6.The electrochemical analysis was accomplished using a rotating ring-disk electrode. The results showedthat the 4% CeO2/C specimen, prepared by PPM and supported on Printex L6, was the best electrocatalystfor H2O2production in 1 mol L -1NaOH. This material showed the highest ring current, producing 88%H2O2and transferring 2.2 electrons per O 2molecule via the ORR at the lowest onset potential. Addition-ally, the ring-current of the 4% CeO2/C PPM P material was higher than that of Vulcan XC 72R and PrintexL6, the reference materials for H2O 2production, indicating the highest electrocatalytic activity for the 4%CeO2/C PPM P material. © 2013 Elsevier Ltd. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A comparative study using different mass proportions of WO3/C (1%, 5%, 10% and 15%) for H2O2 electrogeneration and subsequent phenol degradation was performed. To include the influence of the carbon substrate and the preparation methods, all synthesis parameters were evaluated. The WO3/C materials were prepared by a modified polymeric precursor method (PPM) and the sol-gel method (SGM) on Vulcan XC 72R and Printex L6 carbon supports, verifying the most efficient metal/carbon proportion. The materials were physically characterized by X-ray diffraction (XRD) and by X-ray photoelectron spectroscopy (XPS) techniques. The XRD and the XPS techniques identified just one phase containing WO3 and elevated oxygen concentration on carbon with the presence of WO3. The oxygen reduction reaction (ORR), studied by the rotating ring-disk electrode technique, showed that WO3/C material with the lowest tungsten content (1% WO3/C), supported on Vulcan XC 72R and prepared by SGM, was the most promising electrocatalyst for H2O2 electrogeneration. This material was then analyzed using a gas diffusion electrode (GDE) and 585mgL-1 of H2O2 was produced in acid media. This GDE was employed as a working electrode in an electrochemical cell to promote phenol degradation by an advanced oxidative process. The most efficient method applied was the photo-electro-Fenton; this method allowed for 65% degradation and 11% mineralization of phenol during a 2-h period. Following 12h of exhaustive electrolysis using the photo-electro-Fenton method, the total degradation of phenol was observed after 4h and the mineralization of phenol approached 75% after 12h. © 2013 Elsevier B.V.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

CCTO thin films were deposited on Pt(1 1 1)/Ti/SiO2/Si substrates using a chemical (polymeric precursor) and pressure method. Pressure effects on CCTO thin films were evaluated by X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM) and optical properties which revealed that a pressure film (PF) is denser and more homogeneous than a chemical film (CF). Pressure also causes a decrease in the band gap and an increase in the photoluminescence (PL) emission of CCTO films which suggests that the pressure facilitates the displacement of Ti in the titanate clusters and the charge transference from TiO6 to [TiO5V0z], [TiO5V0z] to [CaO11V0z] and [TiO5V0z] to [CuO4]x. © 2013 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Tungsten oxide/titania (WO3/TiO2) nanopowders were synthesized by the polymeric precursor method which varied the WO3 content between 0 and 10 mol%. The powders were thermally treated in a conventional furnace and their structural, microstructural and electric properties were evaluated by X-ray diffraction (XRD), Raman spectrometry, N 2 physisorption, NH3 chemisorption, temperature-programmed reduction (TPR), X-ray absorption near-edge spectroscopy (XANES) in situ XANES and extended X-ray absorption fine structure spectroscopy (EXAFS) and transmission electron microscopy (TEM). XRD and Raman spectrometry confirmed the homogeneous distribution of an amorphous WO3 phase in the TiO 2 matrix which stabilized the anatase phase through the generation of [TiO5·V0] or [TiO5·V 0] complex sites. Conventional TPR-H2 (temperature programmed reduction) along with XANES TPR-H2 and XANES TPR-EtOH showed that WO3/TiO2 sample reduction occurs through the formation of these complex clusters. Moreover, the addition of WO3 promoted an increase in the surface acidity of doped samples as revealed by NH3 chemisorption. The WO3/TiO2 bulk-ceramic samples were further used to estimate their potential application in a humidity sensor in the range of 15-85% relative humidity. Probable reasons that lead to the different humidity sensor responses of samples were given based on the structural and surface characterizations. Correlation between the sensing performance of the sensor and its structural features are also discussed. Although all samples responded as a humidity sensor, the W2T sample (2 mol% added WO3) excelled for sensitivity due to the increase in acid sites, optimum mean pore size and pore size distribution. © 2013 Elsevier B.V.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pós-graduação em Química - IQ

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Pós-graduação em Ciência e Tecnologia de Materiais - FC

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)