Resumo:
Fruit purees, combined or not with polysaccharides, have been used in some studies to elaborate edible films. The present study was conducted to evaluate tensile properties and water vapor barrier of alginate-acerola puree films plasticized with corn syrup, and to study the influence of cellulose whiskers from different origins (cotton fiber or coconut husk fiber, the latter submitted to one- or multi-stage bleaching) on the film properties. The whiskers improved the overall tensile properties (except by elongation) and the water vapor barrier of the films. The films with coconut whiskers, even those submitted only to a one-stage bleaching, presented similar properties to those of films with cotton whiskers, despite the low compatibility between the matrix and the remaining lignin in coconut whiskers. This was probably ascribed to a counterbalancing effect of the higher aspect ratios of the coconut whiskers. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
Organic-inorganic composite membranes were prepared from membranes of the bio-polymer bacterial cellulose (BC) and organic-inorganic sal composed of nanoparticulate boehmite and epoxi modified siloxane. Bacterial cellulose membranes are obtained in a highly hydrated state (1% cellulose and 99% cellulose) from cultures of Gluconacetobacter xylinus and could be used in the never-dried or in the dried state. Depending on the use of dried or never-dried BC membranes two main kinds of composites were obtained. In the first one dried BC membranes coated with the hybrid sol have lead to transparent membranes displaying a hi-phase structure where the two components could be easily distinguished, with individual structures preserved. A decrease was observed for tensile strength (50.5 MPa) and Young's Modulus (2.8 GPa) when compared to pure BC membrane (112.5 MPa and 12.7 GPa). Elongation at break was observed to increase (2.5% against 1.5% observed for BC). When never-dried BC membranes were used transparent membranes were also obtained, however an improvement was observed for mechanical properties (tensile strength - 116 MPa and Young's Modulus - 13.7 GPa). A lower value was obtained for the elongation at break (1.3%). In the last case the interaction between the two-phases lead to changes in the cellulose crystallinity as shown by X rays diffraction results. Multifunctional transparent membranes displaying the cellulose structure in one side and the boehmite-siloxane structure at the opposite face could find special applications in opto-electronics or biomedical areas taking advantage of the different chemical nature of the two components. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
Films of cellulose acetate butyrate (CAB) and carboxymethylcellulose acetate butyrate (CMCAB) were deposited from ethyl acetate solutions onto bare silicon wafers (Si/SiO2) or amino-terminated surfaces (APS) by means of equilibrium adsorption. All surfaces were characterized by means of ellipsometry, atomic force microscopy (AFM) and contact angle measurements. The presence of amino groups on the support surface favored the adsorption of CAB and CMCAB, inducing the orientation almost polar groups to the surface and the exposition of alkyl group to the air. Such molecular orientation caused increase of the dispersive component of surface energy (gamma(d)(s)) and decrease of the polar component of surface energy (gamma(p)(s)) of cellulose esters in comparison to those values determined for films deposited onto bare Si/SiO2 wafers. Adsorption behavior of jacalin or concanavalin A onto CAB and CMCAB films was also investigated. The adsorbed amounts of lectins were more pronounced on cellulose esters with high (gamma(p)(s)) and total surface energy (gamma(t)(s)) values. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Cellulase, an enzymatic complex that synergically promotes the degradation of cellulose to glucose and cellobiose, free or adsorbed onto Si/SiO(2) wafers at 60 degrees C has been employed as catalyst in the hydrolysis of microcrystalline cellulose (Avicel), microcrystalline cellulose pre-treated with hot phosphoric acid (CP), cotton cellulose (CC) and eucalyptus cellulose (EC). The physical characteristics such as index of crystallinity (I(C)), degree of polymerization (DP) and water sorption values were determined for all samples. The largest conversion rates of cellulose into the above-mentioned products using free cellulase were observed for samples with the largest water sorption values; conversion rates showed no correlation with either IC or DP of the biopolymer. Cellulose with large water sorption value possesses large pore volumes, hence higher accessibility. The catalytic efficiency of immobilized cellulase could not be correlated with the physical characteristics of cellulose samples. The hydrolysis rates of the same cellulose samples with immobilized cellulase were lower than those by the free enzyme, due to the diffusion barrier (biopolymer chains approaching to the immobilized enzyme) and less effective contact between the enzyme active site and its substrate. Immobilized cellulase, unlike its free counterpart, can be recycled at least six times without loss of catalytic activity, leading to higher overall cellulose conversion. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The kinetics of sugar cane bagasse cellulose saccharification and the decomposition of glucose under extremely low acid (ELA) conditions, (0.07%), 0.14%, and 0.28% H2SO4, and at high temperatures were investigated using batch reactors. The first-order rate constants were obtained by weight loss, remaining glucose, and fitting glucose concentration profiles determined with HPLC using the Saeman model. The maximum glucose yields reached 67.6% (200 degrees C, 0.07% H2SO4, 30 min), 69.8% (210 degrees C, 0.14% H2SO4, 10 min), and 67.3% (210 degrees C, 0.28% H2SO4, 6 min). ELA conditions produced remarkable glucose yields when applied to bagasse cellulose. The first-order rate constants were used to calculate activation energies and extrathermodynamic parameters to elucidate the reaction mechanism under ELA conditions. The effect of acid concentration on cellulose hydrolysis and glucose decomposition was also investigated. The observed activation energies and reaction orders with respect to hydronium ion for cellulose hydrolysis and glucose decomposition were 184.9 and 124.5 kJ/mol and 1.27 and 0.75, respectively.
Resumo:
There is growing interest in cellulose nanofibres from renewable sources for several industrial applications. However, there is a lack of information about one of the most abundant cellulose pulps: bleached Eucalyptus kraft pulp. The objective of the present work was to obtain Eucalyptus cellulose micro/nanofibres by three different processes, namely: refining, sonication and acid hydrolysis of the cellulose pulp. The refining was limited by the low efficiency of isolated nanofibrils, while sonication was more effective for this purpose. However, the latter process occurred at the expense of considerable damage to the cellulose structure. The whiskers obtained by acid hydrolysis resulted in nanostructures with lower diameter and length, and high crystallinity. Increasing hydrolysis reaction time led to narrower and shorter whiskers, but increased the crystallinity index. The present work contributes to the different widespread methods used for the production of micro/nanofibres for different applications. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
Self-supported organic-inorganic hybrid transparent films have been prepared from bacterial cellulose and boehmite. SEM results indicate that the BC membranes are covered by Boehmite and XRD patterns suggest structural changes on cellulose due to Boehmite addition. Thermal stability is accessed through TG curves and is dependent on Boehmite content. Transparency, as evaluated by UV-Vis absorption, increases with increasing content of boehmite suggesting application of these materials as transparent substrates for opto-electronic devices.
Resumo:
Thermal behavior of mixtures composed of cellulose acetate butyrate (CAB), carboxymethylcellulose acetate butyrate (CMCAB), or cellulose acetate phthalate (CAPh), and sorbitan-based surfactants was investigated as a function of mixture composition by means of differential scanning calorimetry (DSC). Surfactants with three different alkyl chain lengths, namely, polyoxyethylenesorbitan monolaurate (Tween 20), polyoxyethylenesorbitan monopalmitate (Tween 40), and polyoxyethylene sorbitan monostearate (Tween 60) were chosen. DSC measurements revealed that Tween 20, 40, and 60 act as plasticizers for CAB, CMCAB, and CAPh (except for Tween 60), leading to a dramatic reduction of glass transition temperature (T-g). The dependence of experimental T-g values on the mixture composition was compared with theoretical predictions using the Fox equation. Plasticization was strongly dependent on mixture composition, surfactant hydrophobic chain length, and type of cellulose ester functional group.
Resumo:
A nanocomposite based on bacterial cellulose (BC) and type I collagen (COL) was evaluated for in vitro bone regeneration. BC membranes were modified by glycine esterification followed by cross-linking of type I collagen employing 1-ethyl-3-(3-dimethylaminopropyl)-carbodiimide. Collagen incorporation was studied by spectroscopy analysis. X-Ray diffraction showed changes in the BC crystallinity after collagen incorporation. The elastic modulus and tensile strength for BC-COL decreased, while the strain at failure showed a slight increase, even after sterilization, as compared to pristine BC. Swelling tests and contact angle measurements were also performed. Cell culture experiments performed with osteogenic cells were obtained by enzymatic digestion of newborn rat calvarium revealed similar features of cell morphology for cultures grown on both membranes. Cell viability/proliferation was not different between BC and BC-COL membranes at day 10 and 14. The high total protein content and ALP activity at day 17 in cells cultured on BC-COL indicate that this composite allowed the development of the osteoblastic phenotype in vitro. Thus, BC-COL should be considered as alternative biomaterial for bone tissue engineering.
Resumo:
Four crossbred geldings were used in a randomized blocks experimental design. The objective was to study the use of the internal markers indigestible cellulose (iCEL) and indigestible lignin (iLIG), obtained in situ (cattle) or in vivo (equine) to predict nutrient apparent digestibility in horses. Treatments consisted of different methodologies to determine digestibility: direct method with total feces collection (TC), and indirect method using internal markers iCEL and iLIG obtained either by in situ incubation in bovine rumen or in vivo (IV) using the mobile nylon bag (MNB) technique in horses. Feces production was 2.80 kg in DM, and average recovery rate (p > 0.05) was 101%. Nutrient digestibility coefficient (p > 0.05) estimates were adequately predicted by iCEL and iLIG, obtained in situ or in vivo, with average values of 52.63, 54.17, 64.90, 43.73 and 98.28% for dry matter, organic matter, crude protein, neutral detergent fiber and starch, respectively. It can be concluded that iCEL and iLIG may be obtained in vivo by MNB in horses consuming a forage-concentrate diet, to predict nutrient digestibility coefficients.
Resumo:
The separator membrane in batteries and fuel cells is of crucial importance for the function of these devices. In lithium ion batteries the separator membrane as well as the polymer matrix of the electrodes consists of polymer electrolytes which are lithium ion conductors. To overcome the disadvantage of currently used polymer electrolytes which are highly swollen with liquids and thus mechanically and electrochemically unstable, the goal of this work is a new generation of solid polymer electrolytes with a rigid backbone and a soft side chain structure. Moreover the novel material should be based on cheap substrates and its synthesis should not be complicated aiming at low overall costs. The new materials are based on hydroxypropylcellulose and oligoethyleneoxide derivatives as starting materials. The grafting of the oligoethyleneoxide side chains onto the cellulose was carried out following two synthetic methods. One is based on a bromide derivative and another based on p-toluolsulfonyl as a leaving group. The side chain reagents were prepared form tri(ethylene glycol) monoethyl ether. In order to improve the mechanical properties the materials were crosslinked. Two different conceptions have been engaged based on either urethane chemistry or photosensitive dimethyl-maleinimide derivatives. PEO - graft - cellulose derivatives with a high degree of substitution between 2,9 and 3,0 were blended with lithium trifluoromethane-sulfonate, lithium bis(trifluorosulfone)imide and lithium tetrafluoroborate. The molar ratios were in the range from 0,02 to 0,2 [Li]/[O]. The products have been characterized with nuclear magnetic resonance (NMR), gel permeation chromatography (GPC) and laserlight scattering (LS) with respect to their degree of substitution and molecular weight. The effect of salt concentration on ionic conductivity, thermal behaviour and morphology has been investiga-ted with impedance spectroscopy, differential scanning calorimetry (DSC) and thermal gravimetric analysis (TGA). The crosslinking reactions were controlled with dynamic mechanical analysis (DMS). The degree of substitution of our products is varying between 2,8 and 3,0 as determined by NMR. PEO - graft - cellulose derivatives are highly viscous liquids at room temperature with glass transition temperatures around 215 K. The glass transition temperature for the Lithium salt complexes of PEO - graft - cellulose deri-vatives increase with increasing salt content. The maximum conductivity at room temperature is about 10-4 and at 100°C around 10-3 Scm-1. The presence of lithium salt decreases the thermal stability of the complexes in comparison to pure PEO - graft - cellulose derivatives. Complexes heated over 140 – 150°C completely lose their ionic conductivity. The temperature dependence of the conductivity presented as Arrhenius-type plots for all samples is similar in shape and follows a VTF behaviour. This proofs that the ionic transport is closely related to the segmental motions of the polymer chains. Novel cellulose derivatives with grafted oligoethylen-oxide side chains with well-defined chemical structure and high side chain grafting density have been synthesized. Cellulose was chosen as stiff, rod like macromolecule for the backbone while oligoethylen-oxides are chosen as flexible side chains. A maximum grafting density of 3.0 have been obtained. The best conductivity reaches 10-3 Scm-1 at 100°C for a Li-triflate salt complex with a [Li]/[O] ratio of 0.8. The cross-linked complexes containing the lithium salts form elastomeric films with convenient mechanical stability. Our method of cellulose modification is based on relatively cheap and commercially available substrates and as such appears to be a promising alternative for industrial applications.
Resumo:
In this thesis cholesteric films made of liquid crystalline cellulose derivatives with improved optical properties were prepared. The choice of the solvent, hydrogen bond influencing additives, the synthetic realization of a very high degree of substitution on the cellulosic polymer and the use of mechanical stirring at the upper concentration limit of the liquid crystalline range were the basis for an improved alignment of the applied cellulose tricarbamates. In combination with a tuned substrate treatment and film preparation method, cholesteric films were obtained, with optical properties that were theoretically predicted and only known from low molecular weight liquid crystals so far. Subsequent polymerization allowed a permanent fixing of the alignment and the fabrication of free standing and insensitive films.rnThe incorporation of inorganic nanorods into the cholesteric host material was mediated with tailored block copolymers, available via controlled radical polymerization methods. In addition to the shape match between the rodlike mesogens of the host and the nanorods it was possible to increase the miscibility of both materials. Nevertheless, the size of the nanorods, in comparison to the mesogens, in these densely packed liquid crystalline phases as well as their long equilibration times were the reasons for phase separation. Nanorods are, in principle, valuable substitutes for organics, but their utilization in cellulosic CLC was not to be combined with a high quality alignment of the cholesteric structure.rnA swelling process of polymerized films in a dye solution or dissolving dyes in non-polymerized CLC was used for incorporation of the organic chromophores. With the first method the CLC could be aligned and polymerized without any disturbance due to dye molecules. The optical properties of dye and CLC were matched, with regard to mirrorless lasing devices. The dye was optically excited and laser emission supported by the cholesteric cavity was obtained. The polarization and wavelength of the emitted radiation as well as its bandwidth, the obtained interference pattern and threshold behavior of the emission proofed the feedback mechanism that was not believed to be realizable in liquid crystalline polymers. rnUtilization of a microfluidic co-flow injection device enabled us to transfer the properties of cellulosic CLC from the planar film shape to spherical micrometer sized particles. The pure material yielded particles with distorted mesogen alignment similar to films prepared by capillary flow. Dilution of the CLC with a solvent that migrated into the carrier phase during particle preparation provided the basis for particles with well ordered areas. rnAlthough cellulose derivatives were known for their liquid crystalline behavior for decades and synthesized in mass production, their application as feedback material was affected by bad optical properties. In comparison to low molar mass compounds, the low degree of order in the CLC phase was the cause. With the improved material, defined lasing emission was shown and characterized. Derivatives of cellulose are desirable materials, because, as a renewable resource, they are available in large amounts for a low price and need only simple derivatization reactions. The fabrication of CLC films with tunable lasing emission, for which this thesis can provide a starting point, is in good agreement with today's requirements of modern technology and its miniaturization.rn
Resumo:
In this study a novel method MicroJet reactor technology was developed to enable the custom preparation of nanoparticles. rnDanazol/HPMCP HP50 and Gliclazide/Eudragit S100 nanoparticles were used as model systems for the investigation of effects of process parameters and microjet reactor setup on the nanoparticle properties during the microjet reactor construction. rnFollowing the feasibility study of the microjet reactor system, three different nanoparticle formulations were prepared using fenofibrate as model drug. Fenofibrate nanoparticles stabilized with poloxamer 407 (FN), fenofibrate nanoparticles in hydroxypropyl methyl cellulose phthalate (HPMCP) matrix (FHN) and fenofibrate nanoparticles in HPMCP and chitosan matrix (FHCN) were prepared under controlled precipitation using MicroJet reactor technology. Particle sizes of all the nanoparticle formulations were adjusted to 200-250 nm. rnThe changes in the experimental parameters altered the system thermodynamics resulting in the production of nanoparticles between 20-1000 nm (PDI<0.2) with high drug loading efficiencies (96.5% in 20:1 polymer:drug ratio).rnDrug releases from all nanoparticle formulations were fast and complete after 15 minutes both in FaSSIF and FeSSIF medium whereas in mucodhesiveness tests, only FHCN formulation was found to be mucoadhesive. Results of the Caco-2 studies revealed that % dose absorbed values were significantly higher (p<0.01) for FHCN in both cases where FaSSIF and FeSSIF were used as transport buffer.rn
Resumo:
Cellulose nanofibers are an attractive component of a broad range of nanomaterials. Their intriguing mechanical properties and low cost, as well as the renewable nature of cellulose make them an appealing alternative to carbon nanotubes (CNTs), which may pose a considerable health risk when inhaled. Little is known, however, concerning the potential toxicity of aerosolized cellulose nanofibers. Using a 3D in vitro triple cell coculture model of the human epithelial airway barrier, it was observed that cellulose nanofibers isolated from cotton (CCN) elicited a significantly (p < 0.05) lower cytotoxicity and (pro-)inflammatory response than multiwalled CNTs (MWCNTs) and crocidolite asbestos fibers (CAFs). Electron tomography analysis also revealed that the intracellular localization of CCNs is different from that of both MWCNTs and CAFs, indicating fundamental differences between each different nanofibre type in their interaction with the human lung cell coculture. Thus, the data shown in the present study highlights that not only the length and stiffness determine the potential detrimental (biological) effects of any nanofiber, but that the material used can significantly affect nanofiber-cell interactions.