907 resultados para AL-W ALLOYS
Resumo:
Aluminum alloyed with small atomic fractions of Sc, Zr, and Hf has been shown to exhibit high temperature microstructural stability that may improve high temperature mechanical behavior. These quaternary alloys were designed using thermodynamic modeling to increase the volume fraction of precipitated tri-aluminide phases to improve thermal stability. When aged during a multi-step, isochronal heat treatment, two compositions showed a secondary room-temperature hardness peak up to 700 MPa at 450°C. Elevated temperature hardness profiles also indicated an increase in hardness from 200-300°C, attributed to the precipitation of Al3Sc, however, no secondary hardness response was observed from the Al3Zr or Al3Hf phases in this alloy.
Resumo:
Bettini et al (2006 Nat. Nanotechnol. 1 182-5) reported the first experimental realization of linear atomic chains (LACs) composed of different atoms (Au and Ag). The different contents of Au and Ag were observed in the chains from what was found in the bulk alloys, which raises the question of what the wire composition is, if it is in equilibrium with a bulk alloy. In this work we address the thermodynamic driving force for species fractionation in LACs under tension, and we present the density-functional theory results for Ag-Au chain alloys. A pronounced stabilization of the wires with an alternating Ag-Au sequence is observed, which could be behind the experimentally observed Au enrichment in LACs from alloys with high Ag content.
Resumo:
It is well known that striation spacing may be related to the crack growth rate, da/dN, through Paris equation, as well as the maximum and minimum loads under service loading conditions. These loads define the load ratio, R, and are considered impossible to be evaluated from the inter-spacing striations analysis. In this way, this study discusses the methodology proposed by Furukawa to evaluate the maximum and minimum loads based on the experimental fact that the relative height of a striation, H, and the striation spacing, s, are strongly influenced by the load ratio, R. Fatigue tests in C(T) specimens were conducted on SAE 7475-T7351 Al alloy plates at room temperature and the results showed a straightforward correlation between the parameters H, s, and R. Measurements of striation height, H, were performed using scanning electron microscopy and field emission gun (FEG) after sectioning the specimen at a large inclined angle to amplify the height of the striations. The results showed that for increasing R the values of H/s tend to increase. Striation height, striation spacing, and load ratio correlations were obtained, which allows one to estimate service loadings from fatigue fracture surface survey.
Resumo:
Background: It has been speculated that the biostimulatory effect of Low Level Laser Therapy could cause undesirable enhancement of tumor growth in neoplastic diseases. The aim of the present study is to analyze the behavior of melanoma cells (B16F10) in vitro and the in vivo development of melanoma in mice after laser irradiation. Methods: We performed a controlled in vitro study on B16F10 melanoma cells to investigate cell viability and cell cycle changes by the Tripan Blue, MTT and cell quest histogram tests at 24, 48 and 72 h post irradiation. The in vivo mouse model (male Balb C, n = 21) of melanoma was used to analyze tumor volume and histological characteristics. Laser irradiation was performed three times (once a day for three consecutive days) with a 660 nm 50 mW CW laser, beam spot size 2 mm(2), irradiance 2.5 W/cm(2) and irradiation times of 60s (dose 150 J/cm(2)) and 420s (dose 1050 J/cm(2)) respectively. Results: There were no statistically significant differences between the in vitro groups, except for an increase in the hypodiploid melanoma cells (8.48 +/- 1.40% and 4.26 +/- 0.60%) at 72 h postirradiation. This cancer-protective effect was not reproduced in the in vivo experiment where outcome measures for the 150 J/cm(2) dose group were not significantly different from controls. For the 1050 J/cm(2) dose group, there were significant increases in tumor volume, blood vessels and cell abnormalities compared to the other groups. Conclusion: LLLT Irradiation should be avoided over melanomas as the combination of high irradiance (2.5 W/cm(2)) and high dose (1050 J/cm(2)) significantly increases melanoma tumor growth in vivo.
Resumo:
Large parity-violating longitudinal single-spin asymmetries A(L)(e+) = 0.86(-0.14)(+0.30) and Ae(L)(e-) = 0.88(-0.71)(+0.12) are observed for inclusive high transverse momentum electrons and positrons in polarized p + p collisions at a center-of-mass energy of root s = 500 GeV with the PHENIX detector at RHIC. These e(+/-) come mainly from the decay of W(+/-) and Z(0) bosons, and their asymmetries directly demonstrate parity violation in the couplings of the W(+/-) to the light quarks. The observed electron and positron yields were used to estimate W(+/-) boson production cross sections for the e(+/-) channels of sigma(pp -> W(+)X) X BR(W(+) -> e(+) nu(e)) = 144.1 +/- 21.2(stat)(-10.3)(+3.4)(syst) +/- 21.6(norm) pb, and sigma(pp -> W(-)X) X BR(W(-) -> e(-) (nu) over bar (e)) = 3.17 +/- 12.1(stat)(-8.2)(+10.1)(syst) +/- 4.8(norm) pb.
Resumo:
The development of Nb(3)Al and Nb(3)Sn superconductors is of great interest for the applied superconductivity area. These intermetallics composites are obtained normally by heat treatment reactions at high temperature. Processes that allow formation of the superconducting phases at lower temperatures (<1000 degrees C), particularly for Nb(3)Al, are of great interest. The present work studies phase formation and stability of Nb(3)Al and Nb(3)Sn superconducting phases using mechanical alloying (high energy ball milling). Our main objective was to form composites near stoichiometry, which could be transformed into the superconducting phases using low-temperature heat treatments. High purity Nb-Sn and Nb-Al powders were mixed to generate the required superconducting phases (Nb-25at.%Sn and Nb-25at.%Al) in an argon atmosphere glove-box. After milling in a Fritsch mill, the samples were compressed in a hydraulic uniaxial press and encapsulated in evacuated quartz tubes for heat treatment. The compressed and heat treated samples were characterized using X-ray diffractometry. Microstructure and chemical analysis were accomplished using scanning electron microscopy and energy dispersive spectrometry. Nb(3)Al XRD peaks were observed after the sintering at 800 degrees C for the sample milled for 30 h. Nb(3)Sn XRD peaks could be observed even before the heat treatment. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Multilayer CVD coatings for high speed cutting applications were designed to achieve high wear and heat resistance during machining of steel alloys. In this work the microstructure and cutting performance of these novel multilayer CVD coatings are investigated and compared with standard CVD multilayer coatings. 3D-FIB tomography is used to characterize the microstructure of the layers, especially the transition between the Ti(C,N) and the Al(2)O(3) layer. The 3D reconstruction of the surface of the Ti(C,N) layer shows the formation of protruded Ti(C,N) grains with a very particular architecture, which penetrate into the Al(2)O(3) top-layer, providing a mechanical anchoring between both layers. Cemented carbides coated with the novel CVD multilayer present reduced crater and flank wear as well as improved adherence between the Al(2)O(3) top-layer and the Ti(C,N) layer leading to a dramatic improvement of cutting performance.
Resumo:
This work evaluates the glass formation of selected alloys based on the Ti-Zr-Fe-Co system, assuming the synergy of two distinct criteria: minimum topological instability and average electronegativity plots. Combining the minimum topological instability and the average electronegativity values result in a plot in which the most probable good glass former compositions are identified Ti-Zr rich alloys with Fe and Co additions were produced, compared against the final plot, and the best glass forming alloy composition was found to be very close the theoretically predicted ones on the Ti-Zr rich side, for both Ti-Zr-Fe and Ti-Zr-Co systems. (C) 2009 Elsevier B V All rights reserved
Resumo:
In this paper, we report the remarkable agreement of the glass forming ability of binary alloys with a new criterion that combines the topological instability parameter (lambda) and the average electronegativity difference among the elements of an alloy, assuming both exert a synergetic effect. The best glass forming compositions for Zr-Cu and Ti-Ni systems are well predicted by this new approach. Although the new criterion needs further refinement, it is concluded that the proposed approach is a promising and simple tool to guide and reduce the tedious and labour intensive work to find good glass former compositions in metallic systems. (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
The glass-forming ability (GFA) of metallic alloys is associated with a topological instability criterion combined with a new parameter based on the average electronegativity difference of an element and its surrounding neighbours. In this model, we assume that during solidification the glassy phase competes directly with the supersaturated solid solution having the lowest topological instability factor for a given composition. This criterion is combined with the average electronegativity difference among the elements in the alloy, which reflects the strength of the liquid. The GFA is successfully correlated with this combined criterion in several binary glass-forming systems.
Resumo:
Ti(6)Al(4)V thin films were grown by magnetron sputtering on a conventional austenitic stainless steel. Five deposition conditions varying both the deposition chamber pressure and the plasma power were studied. Highly textured thin films were obtained, their crystallite size (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
In the last few years great efforts have been made in order to find and to develop environmentally friendly substitutes for Cr6+ pre-treatments applied on aluminium alloys used in the aircraft industry. Among the potential substitutes, silane layers have attracted considerable interest from researchers and from the industry. The present work investigates the anti-corrosion behaviour of (bis-1, 2-(triethoxysilyl) ethane (BTSE)) silane layers modified with Ce ions and/or silica nanoparticles applied on Al alloy 2024-T3 substrates. The corrosion behaviour was investigated in 0.1 M NaCl solution via d.c. polarization and electrochemical impedance spectroscopy (EIS). Contact angle measurements and XPS were used to assess information on the chemistry of the silane pre-treated surfaces. The results have shown that the introduction of additives improves the corrosion protection properties of the silane layer. (c) 2008 Elsevier Ltd. All rights reserved.
Resumo:
A new assessment of the aluminum corner of the quaternary Al-Fe-Mn-Si system has been made that extends beyond the COST-507 database. This assessment makes use of a recent, improved description of the ternary Al-Fe-Si system. In the present work, modeling of the Al-rich corner of the quaternary Al-Fe-Mn-Si system has been carried out by introducing Fe solubility into the so-called alpha-AlMnSi and beta-AlMnSi phases of the Al-Mn-Si system. A critical review of the data available on the quaternary system is presented and used for the extension of the description of these ternary phases into the quaternary Al-Fe-Mn-Si.
Resumo:
The stress corrosion cracking (SCC) behavior and pre-exposure embrittlement of AZ31 magnesium alloy have been studied by slow strain rate tensile (SSRT) tests in this paper. It is showed that AZ31 sheet material is susceptible to SCC in distilled water, ASTM D1.387 solution, 0.01 M NaCl and 0.1 M NaCl solution. The AZ31 magnesium alloy also becomes embrittled if pre-exposed to 0.01 M NaCl solution prior to tensile testing. The degree of embrittlement increased with increasing the pre-exposure time, It is proposed that both the pre-exposure embrittlement and SCC were due to hydrogen which reduces the cohesive strength. i,e,. hydrogen embrittlement, (c) 2005 Elsevier B.V. All rights reserved.