834 resultados para UFG titanium
Resumo:
Thin films of titanium dioxide and titanium dioxide with incorporated gold and silver nanoparticles were deposited onto glass microscope slides, steel and titanium foil coupons by two sol-gel dip-coating methods. The film's photocatalytic activity and ability to evolve oxygen in a sacrificial solution were assessed. It was found that photocatalytic activity increased with film thickness (from 50 to 500 nm thick samples) for the photocatalytic degradation of methylene blue in solution and resazurin redox dye in an intelligent ink dye deposited on the surface. Contrastingly, an optimum film thickness of similar to 200 nm for both composite and pure films of titanium dioxide was found for water oxidation, using persulfate (S2O82-) as a sacrificial electron acceptor. The nanoparticle composite films showed significantly higher activity in oxygen evolution studies compared with plain TiO2 films.
Resumo:
Twenty eight films of titanium dioxide of varying thickness were synthesised by using atmospheric pressure chemical vapour deposition (CVD) of titanium(IV) chloride and ethyl acetate onto glass and titanium substrates. Fixed reaction conditions at a substrate temperature of 660 degrees C were used for all depositions, with varying deposition times of 5-60 seconds used to control the thickness of the samples. A sacrificial electron acceptor system composed of alkaline sodium persulfate was used to determine the rate at which these films could photo-oxidise water in the presence of 365 nm light. The results of this work showed that the optimum thickness for CVD films on titanium substrates for the purposes of water oxidation was approximate to 200 nm, and that a platinum coating on the reverse of such samples leads to a five-fold increase in the observed rate of water oxidation.
Resumo:
Thick paste TiO2 films are prepared and tested for photocatalytic and photoinduced superhydrophilic (PSH) activity. The films are effective photocatalysts for the destruction of stearic acid using near or far UV and all the sol-gel films tested exhibited a quantum yield for this process of typically 0.15 %. These quantum yields are significantly greater (4-8-fold) than those for titania films produced by an APCVD technique, including the commercial self-cleaning glass product Activ(TM). The films are mechanically robust and optically clear and, as photocatalysts for stearic acid removal, are photochemically stable and reproducible. The kinetics of stearic acid photomineralisation are zero order with an activation energy of ca. 2.5 Kj mol(-1). All titania films tested, including those produced by APCVD, exhibit PSH. The light-induced fall, and dark recovery, in the water droplet contact angle made with titania paste films are similar in profile shape to those described by others for thin titania films produced by a traditional sol-gel route. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
High levels of ozone (typically 850 ppm) are readily decomposed by semiconductor photocatalysis, using a thin film of the semiconductor titanium dioxide (Degussa P25 TiO2) cast on a glass tube, and UVA light, i.e. light of energy greater than that of the bandgap of the semiconductor (ultra-bandgap light); in the absence of this light the thermal decomposition of ozone is relatively slow. The semiconductor films show no evidence of chemical or photochemical wear with repeated use. At high levels of ozone, i.e. 100 ppm less than or equal to [O-3] less than or equal to 1400 ppm, the initial rate of ozone decomposition by semiconductor photocatalysis is independent of [O-3], whereas, at lower ozone concentrations, i.e. 5 ppm less than or equal to [O-3] less than or equal to 100 ppm, the initial rate of ozone photodestruction decreases in a smooth, but non-linear, manner with decreasing [O-3]. The kinetics of ozone photodecomposition fit a Langmuir-Hinshelwood type kinetic equation and the possible mechanistic implications of these results are briefly discussed. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Thin (50-500 nm) films of TiO2 may be deposited on glass substrates by the atmospheric pressure chemical vapor deposition (APCVD) reaction of TiCl4 with ethyl acetate at 400600 C. The TiO2 films are exclusively in the form of anatase, as established by Raman microscopy and glancing angle X-ray diffraction. X-ray photoelectron spectroscopy gave a 1:2 Ti:O ratio with Ti 2P(3/2) at 458.6 eV and O 1s is at 530.6 eV. The water droplet contact angle drops from 60degrees to
Resumo:
Atmospheric pressure chemical vapour deposition of titanium dioxide coatings on glass substrates was achieved by the reaction of TiCl4 and a co-oxygen source (MeOH, EtOH, (PrOH)-Pr-i or H2O) at 500-650degreesC. The coatings show excellent uniformity, surface coverage and adherence. Growth rates were of the order of 0.3 mum min(-1) at 500degreesC. All films are crystalline and single phase with XRD showing the anatase TiO2 diffraction pattern; a = 3.78(1), c = 9.51(1) Angstrom. Optically, the films show minimal reflectivity from 300-1600 nm and 50-80% total transmission from 300-800 nm. Contact angles are in the range 20-40degrees for as-prepared films and 1-10degrees after 30 min irradiation at 254 nm. All of the films show significant photocatalyic activity as regards the destruction of an overlayer of stearic acid.
Resumo:
The results of a kinetic study of the bleaching of the photostable dye rhodamine 6G by dissolved oxygen, photosensitized by TiO2, are reported. The observed variations in the initial rate of dye photobleaching as a function of the O2 percentage, temperature, incident light intensity and concentrations of rhodamine 6G and sacrificial electron donor are described and the results are rationalized using a proposed photochemical reaction scheme. The photosensitized bleaching of rhodamine 6G dye by TiO2 has a formal quantum yield of 2.65 X 10(-3), but the rate of complete photomineralization is about twofold slower. The overall activation energy for the semiconductor-sensitized dye photobleaching process is 15.0 +/- 1.5 kJ mol-1.
Resumo:
The results of a study of the variation in photocatalytic activity of TiO2, as measured by its ability to photomineralise 4-chlorophenol, as a function of temperature used to anneal the TiO2, are reported. Heat treatment of the TiO2 leads to a marked decrease in its photocatalytic activity at annealing temperatures above 600-degrees-C. This decrease is associated with a concomitant drop in the specific surface area of the TiO2, owing to particle sintering, rather than the anatase to rutile transformation, which occurs largely at temperatures above 700-degrees-C. There is a reasonable correlation between photocatalytic activity and the surface area of the aggregate particles in the dispersions of the different heat-treated TiO2 samples.
Resumo:
The kinetics of photomineralization of 4-chlorophenol (4-CP) sensitized by Degussa P25 TiO2 in O2-saturated solution is studied as a function of the following different experimental parameters: pH, [TiO2], percentage O2 [O2], [4-CP], T, I, lambda and [KNO3]. At pH 2 and T=30-degrees-C the initial relative rate of CO2 photogeneration R(CO2) conforms to a Langmuir-Hinshelwood-type kinetic scheme and the relationship between R(CO2) and the various experimental parameters may be summarized as follows: R(CO2) = gammaK(O2)[O2](I(a))(theta)K(4-CP]0/(1 + K(O2])(1 + K(4-CP)[4-CP]0) where gamma is a proportionality constant, K(O2) = 0.044 +/- 0.005[O2]-1, theta = 0.74 +/- 0.05 and K(4-CP) = (29 +/- 3) x 10(3) dm3 mol-1. The overall activation energy for this photosystem was determined as 16 +/- 2 kJ mol-1. This work forms part of an overall characterization study in which it is proposed that the 4-CP-TiO2-O2 photosystem is adopted as a standard test system for incorporation into all future semiconductor-sensitized photomineralization studies in order to facilitate comparisons between the results of the different studies.
Resumo:
The photomineralisation of 4-chlorophenol (4-CP) sensitised by Degussa P25 TiO2 in O2-saturated solution represents a possible standard test system in semiconductor-sensitised photomineralisation studies. As part of a detailed examination of this photosystem, the results of the temporal variations in the concentrations of 4-CP, CO2, Cl- and the major organic intermediates, namely, 4-chlorocatechol (4-CC), hydroquinone (HQ), benzoquinone and 4-chlororesorcinol, are reported. The observed variations in [4-CP], [4-CC], [HQ] and [CO2] fit those predicted by a kinetic model which utilises kinetic equations with a Langmuir-Hinshelwood form and assumes that there are three major possible routes in which the photogenerated hydroxyl radicals can react with 4-CP, ie. 4-CP --> 4-CC, 4-CP --> HQ and 4-CP --> (unstable intermediate) --> CO2 and that these routes have the following probabilities of occurring: 48%, 10% and 42%.