710 resultados para Multiphase steels


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The principal aim of this work was to determine the role of non-metallic inclusions in the process of hydrogen stepwise cracking (SWC). Additionally, the influence of inclusions upon the notch ductility of hydrogen charged (HC) and uncharged (UN) tensile specimens was examined. To obtain a basis for experiment a series of low carbon-manganese steels were prepared by induction melting. In order to produce variations in the composition, morphology, volume fraction, size and distribution of the inclusions the steel chemistry was adjusted prior to casting by additions of deoxidiser and Ca-Si injection. Sections of each ingot were hot rolled. Metallography, image analysis, mechanical tests and hydrogen SWC tests were then carried out. The volume fraction, morphology, and shape of inclusions influenced the tensile ductility of the steels. Marked anisotropy was found in the steels containing type II MnS inclusions at all rolling temperatures, whereas the fully Ca treated steel was isotropic. It was found that several inclusion parameters (projected length PL, mean free distance MFD, nearest-neighbour distance NND) correlated with fracture strain. An increase in inclusion volume fraction and/or the dimension of inclusions on a plane parallel to the plane of fracture led to a decrease in fracture strain. The inclusion parameters did not correlate with the fracture strains for the HC tensile specimens. However, large or clusters of inclusions acted as the principal sites for crack initiation. `Fisheyes' or areas of `flat' fracture were often found on these fracture surfaces. The criteria for SWC initiation was found to be either large inclusions or clusters of inclusions. As the PL of inclusions increased the probability of large SWCs occurring increased. SWC initiation at inclusions was believed to occur at a critical concentration of hydrogen. Factors which assisted the concentration of hydrogen at inclusions were discussed. None of the proposed mechanisms of hydrogen embrittlement could be identified as the single cause of SWC.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ion implantation modifies the surface composition and properties of materials by bombardment with high energy ions. The low temperature of the process ensures the avoidance of distortion and degradation of the surface or bulk mechanical properties of components. In the present work nitrogen ion implantation at 90 keV and doses above 1017 ions/cm2 has been carried out on AISI M2, D2 and 420 steels and engineering coatings such as hard chromium, electroless Ni-P and a brush plated Co-W alloy. Evaluation of wear and frictional properties of these materials was performed with a lubricated Falex wear test at high loads up to 900 N and a dry pin-on-disc apparatus at loads up to 40 N. It was found that nitrogen implantation reduced the wear of AISI 420 stainless steel by a factor of 2.5 under high load lubricated conditions and by a factor of 5.5 in low load dry testing. Lower but significant reductions in wear were achieved for AISI M2 and D2 steels. Wear resistance of coating materials was improved by up to 4 times in lubricated wear of hard Cr coatings implanted at the optimum dose but lower improvements were obtained for the Co-W alloy coating. However, hardened electroless Ni-P coatings showed no enhancement in wear properties. The benefits obtained in wear behaviour for the above materials were generally accompanied by a significant decrease in the running-in friction. Nitrogen implantation hardened the surface of steels and Cr and Co-W coatings. An ultra-microhardness technique showed that the true hardness of implanted layers was greater than the values obtained by conventional micro-hardness methods, which often result in penetration below the implanted depth. Scanning electron microscopy revealed that implantation reduced the ploughing effect during wear and a change in wear mechanism from an abrasive-adhesive type to a mild oxidative mode was evident. Retention of nitrogen after implantation was studied by Nuclear Reaction Analysis and Auger Electron Spectroscopy. It was shown that maximum nitrogen retention occurs in hard Cr coatings and AISI 420 stainless steel, which explains the improvements obtained in wear resistance and hardness. X-ray photoelectron spectroscopy on these materials revealed that nitrogen is almost entirely bound to Cr, forming chromium nitrides. It was concluded that nitrogen implantation at 90 keV and doses above 3x1017 ions/cm2 produced the most significant improvements in mechanical properties in materials containing nitride formers by precipitation strengthening, improving the load bearing capacity of the surface and changing the wear mechanism from adhesive-abrasive to oxidative.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High velocity oxyfuel (HVOF) thermal spraying is one of the most significant developments in the thermal spray industry since the development of the original plasma spray technique. The first investigation deals with the combustion and discrete particle models within the general purpose commercial CFD code FLUENT to solve the combustion of kerosene and couple the motion of fuel droplets with the gas flow dynamics in a Lagrangian fashion. The effects of liquid fuel droplets on the thermodynamics of the combusting gas flow are examined thoroughly showing that combustion process of kerosene is independent on the initial fuel droplet sizes. The second analysis copes with the full water cooling numerical model, which can assist on thermal performance optimisation or to determine the best method for heat removal without the cost of building physical prototypes. The numerical results indicate that the water flow rate and direction has noticeable influence on the cooling efficiency but no noticeable effect on the gas flow dynamics within the thermal spraying gun. The third investigation deals with the development and implementation of discrete phase particle models. The results indicate that most powder particles are not melted upon hitting the substrate to be coated. The oxidation model confirms that HVOF guns can produce metallic coating with low oxidation within the typical standing-off distance about 30cm. Physical properties such as porosity, microstructure, surface roughness and adhesion strength of coatings produced by droplet deposition in a thermal spray process are determined to a large extent by the dynamics of deformation and solidification of the particles impinging on the substrate. Therefore, is one of the objectives of this study to present a complete numerical model of droplet impact and solidification. The modelling results show that solidification of droplets is significantly affected by the thermal contact resistance/substrate surface roughness.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The creep rupture properties of cast ½Cr½Mo¼V and 1Cr1Mo¼V alloy steel used in the manufacture of power station steam generating plant. have been investigated. The effects of constraint and geometry on the creep rupture properties are also considered. The validity of various criteria controlling macroscopic creep crack growth in cast CrMoV alloys has been examined. It is found that neither the stress intensity factor nor reference stress correlate satisfactorily the creep crack growth rates at the test temperature of 550°C. Certain minimum displacements must be achieved for crack initiation and propagation. It is found that this displacement as measured by crack opening displacement or crack aspect ratio, is the same in both compact tension and centre-cracked panel geometries, is invariant with crack length and decreases with increasing constraint. The effect of constraint on creep crack growth rate in the two geometries is less conclusive. A new model describing creep crack growth in cast CrMoV alloy steels has been developed. The model is based on the results from a numerical finite element creep analysis of the relaxation and redistribution of stress ahead of an incubating creep crack . It is found that macroscopic creep crack growth in a material undergoing either plane stress or plane strain deformation can be described by a fracture stress which is based on the Von Mises equivalent stress. It has been shown that this model is capable of rationalising all of the experimental crack velocity data from the cast CrMoV alloys. The resultant degree of data correlation is far superior to that obtained when using the stress intensity factor or reference stress. A cumulative damage creep fracture model based upon the results from the numerical analysis has been developed. It is found that the model is capable of predicting the behaviour of propagating creep cracks in cast CrMoV alloys from smooth bar creep rupture data.