945 resultados para Ti-Ni alloys


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ti and its alloys are widely used as biomaterials. Their main properties are excellent corrosion resistance, relatively low elastic modulus, high specific strength, and good biocompatibility. The development of new Ti alloys with properties favorable for use in the human body is desired. To this end, Ti alloys with Mo, Nb, Zr, and Ta are being developed, because these elements do not cause cytotoxicity. The presence of interstitial elements (such as oxygen and nitrogen) induces strong changes in the elastic properties of the material, which leads to hardening or softening of the alloy. By means of anelastic spectroscopy, we are able to obtain information on the diffusion of these interstitial elements present in the crystalline lattice. In this paper, the effect of oxygen on the anelastic properties of some binary Ti-based alloys was analyzed with anelastic spectroscopy. The diffusion coefficients, pre-exponential factors, and activation energies were calculated for oxygen and nitrogen in these alloys.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The superplastic deformation behavior and superplastic forming ability of the Zr41.25Ti13.75Ni10Cu12.5Be22.5 (at.%) bulk metallic glass (BMG) in the supercooled liquid region were investigated. The isothermal tensile results indicate (hat the BMG exhibits a Newtonian behavior at low strain rates but a non-Newtonian behavior at hiqh-strain rates in the initial deformation stage. The maximum elongation reaches as high as 1624% at 656 K. and nanocrystallization was found to occur during the deformation process. Based cm the analysis on tensile deformation. a gear-like micropart is successfully die-forged via a superplastic forgings process. demonstrating that the BMG has excellent workability in the supercooled liquid region. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This work discusses on the preparation of Ni-45Ti-5Mo, Ni-40Ti-10Mo and Ni-46Ti-2Mo-2Zr (at-%) alloys by high-energy ball milling and hot pressing, which are potentially attractive for dental and medical applications. The milling process was performed in stainless steel balls (19mm diameter) and vials (225 mL) using a rotary speed of 300rpm and a ball-to-powder weight ratio of 10:1. Hot pressing under vacuum was performed in a BN-coated graphite crucible at 900 degrees C for 1 h using a load of 20 MPa. The milled and hot-pressed materials were characterized by X-ray diffraction, electron scanning microscopy, and electron dispersive spectrometry. Peaks of B2-NiTi and Ni4Ti3 were identified in XRD patterns of Ni-45Ti-5Mo, Ni-40Ti-10Mo and Ni-46Ti-2Mo-2Zr powders milled for 1h. The NiTi compound dissolved small Mo amounts lower than 4 at%, which were measured by EDS analysis. Moreover, it was identified the existence of an unknown Mo-rich phase in microstructures of the hot-pressed Ni-Ti-Mo alloys.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fe(100-x)Ti(x) alloys (x = 10, 15, 20) were studied with respect to their microstructure and magnetostriction. Depending on heat treatment temperature and composition, the sample retained either the alpha-phase (A2 structure) or the alpha-phase plus the TiFe(2) Laves phase (C14 structure). The saturation magnetostriction measured at 238K is negative, about -11 ppm. However, for fields up to 0.4 T the magnetostriction is barely zero, a very interesting result. High values of magnetostriction are of interest for applications mainly in sensors and actuators, but zero magnetostriction is also a remarkable property, desirable for many applications such as electric transformers and fluxgate sensor cores. Therefore, the Fe(100-x)Ti(x) (x < 20 at%) are an attractive option to be considered for these applications.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Longitudinal and transverse magnetostriction measurements were performed on polycrystalline Fe(100-x)Ti(x) alloys, for a large Ti concentration range, from x = 8.8 to 34.7 at.%. Our results showed that substituting Fe by Ti does not significantly enhance the magnetostriction. For all Ti concentrations in the magnetically saturated state, the longitudinal magnetostriction values vary from -2 x 10(-6) to 6 x 10(-6). On the other hand, Fe(100-x)Ti(x) alloys exhibit a large forced volume magnetostriction, which increases with increasing Ti-concentration. The magnetostriction behavior could be explained considering investigations of the hyteresis loops and the microstructure.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, we report the remarkable agreement of the glass forming ability of binary alloys with a new criterion that combines the topological instability parameter (lambda) and the average electronegativity difference among the elements of an alloy, assuming both exert a synergetic effect. The best glass forming compositions for Zr-Cu and Ti-Ni systems are well predicted by this new approach. Although the new criterion needs further refinement, it is concluded that the proposed approach is a promising and simple tool to guide and reduce the tedious and labour intensive work to find good glass former compositions in metallic systems. (C) 2008 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Titanium alloys normally contain oxygen, nitrogen, or carbon as impurities, and although this concentration is low, these impurities cause changes in the mechanical properties of Ti alloys. Oxygen is a strong alpha-phase stabilizer and its addition causes solid-solution strengthening, shape memory effect, and superelasticity. The most promising alloys are those with Nb, Zr, Ta, and Mo as alloying elements. In this paper, the preparation, processing, and characterization of Ti-Mo alloys (5 and 10 wt%) used as biomaterials are presented, along with the influence of oxygen on their mechanical properties. The addition of oxygen causes an increase in the elasticity modulus of the Ti-5Mo alloy due to an increase in the alpha' phase volume fraction, which possesses a higher modulus than the alpha '' phase. Ti-10Mo possesses a mixture between alpha '' and beta phases, oxygen enters these two structures and causes a dominating effect.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

New titanium alloys have been developed with the aim of utilizing materials with better properties for application as biomaterials, and Ti-Zr system alloys are among the more promising of these. In this paper, the influence of zirconium concentrations on the structure, microstructure, and selected mechanical properties of Ti-Zr alloys is analyzed. After melting and swaging, the samples were characterized through chemical analysis, density measurements, X-ray diffraction, optical microscopy, Vickers microhardness, and elasticity modulus. In-vitro cytotoxicity tests were performed on cultured osteogenic cells. The results showed the formation essentially of the α′ phase (with hcp structure) and microhardness values greater than cp-Ti. The elasticity modulus of the alloys was sensitive to the zirconium concentrations while remaining within the range of values of conventional titanium alloys. The alloys presented no cytotoxic effects on osteoblastic cells in the studied conditions. © 2013 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Titanium alloys are widely used in the manufacture of biomedical implants because they possess an excellent combination of physical properties and outstanding biocompatibility. Today, the most widely used alloy is Ti-6Al-4V, but some studies have reported adverse effects with the long-term presence of Al and V in the body, without mentioning that the elasticity modulus value of this alloy is far superior to the bone. Thus, there is a need to develop new Ti-based alloys without Al and V that have a lower modulus, greater biocompatibility, and similar mechanical strength. In this paper, we investigated the effect of Nb as a substitutional solute on the mechanical properties of Ti-Nb alloys, prepared in an arc-melting furnace and characterized by density, X-ray diffraction, optical microscopy, hardness and elasticity modulus measurements. The X-ray and microscopy measurements show a predominance of the α phase. The microhardness values showed a tendency to increase with the concentration of niobium in the alloy. Regarding the elasticity modulus, it was observed a nonlinear behavior with respect to the concentration of niobium. This behavior is associated with the presence of the α phase.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

With the increase in life expectancy, biomaterials have become an increasingly important focus of research because they are used to replace parts and functions of the human body, thus contributing to improved quality of life. In the development of new biomaterials, the Ti-15Mo alloy is particularly significant. In this study, the Ti-15Mo alloy was produced using an arc-melting furnace and then characterized by density, X-ray diffraction, optical microscopy, hardness and dynamic elasticity modulus measurements, and cytotoxicity tests. The microstructure was obtained with β predominance. Microhardness, elasticity modulus, and cytotoxicity testing results showed that this material has great potential for use as biomaterial, mainly in orthopedic applications.