953 resultados para P-TYPE ZNO
Resumo:
Sensors to detect toxic and harmful gases are usually based on metal oxides that are operated at elevated temperature. However, enabling gas detection at room temperature (RT) is a significant ongoing challenge. Here, we address this issue by demonstrating that microrods of semiconducting CuTCNQ (TCNQ=7,7,8,8-tetracyanoquinodimethane) with nanostructured features can be employed as conductometric gas sensors operating at 50°C for detection of oxidizing and reducing gases such as NO2 and NH3. The sensor is evaluated at RT and up to 200°C. It was found that CuTCNQ is transformed into a N-doped CuO material with p-type conductivity when annealed at the maximum temperature. This is the first time that such a transformation, from a semiconducting charge transfer material into a N-doped metal oxide is detected. It is shown here that both the surface chemistry and the type of majority charge carrier within the sensing layer is critically important for the type of response towards oxidizing and reducing gases. A detailed physical description of NO2 and NH3 sensing mechanism at CuTCNQ and N-doped CuO is provided to explain the difference in the response. For the N-doped CuO sensor, a detection limit of 1 ppm for NO2 and 10 ppm for NH3 are achieved.
Resumo:
The recombination properties of cobalt centers in p-type germanium containing cobalt in the concentration range 1014 to 1016 atoms/cm3 have been investigated. The measurement of lifetime has been carried out by steady-state photoconductivity and photo-magneto-electric methods in the temperature range 145 to 300°K. The cross-sections Sno (electron capture cross-section at neutral centers). Sn- (electron capture cross-section at singly negatively charged centers) and their temperature variations have been estimated by the analysis of the lifetime data on the basis of Sah-Shockley's multi-level formula. The value of Sno is (15±5).10-16 cm2 and is temperature independent. The value of Sn- is ≈4·10-16 cm2 around 225°K and it increases with increase of temperature. The possible mechanisms for capture at neutral and repulsive centers are discussed and a summary of the capture cross-sections for cobalt centers is given. A comparison of the cross-section values of cobalt and their temperature variations with those of the related impurities-manganese, iron and nickel-in germanium has been made.
Resumo:
Dimethylzine (DMZn) was used as a p-type dopant in GaAs grown by low pressure metalorganic vapor phase epitaxy using trimethylgallium and arsine (AsH3) as source materials, The hole carrier concentrations and zinc (Zn) incorporation efficiency are studied by using the Hall effect, electrochemical capacitance voltage profiler and photoluminescence (PL) spectroscopy, The influence of growth parameters such as DMZn mole fraction, growth temperature, and AsH, mole fraction on the Zn incorporation have been studied. The hole concentration increases with increasing DMZn and AsH3 mole fraction and decreases with increasing growth temperature. This can be explained by vacancy control model. The PL experiments were carried out as a function of hole concentration (10(17)-1.5 x 10(20) cm(-3)). The main peak shifted to lower energy and the full width at half maximum (FWHM) increases with increasing hole concentrations. We have obtained an empirical relation for FWHM of PL, Delta E(p)(eV) = 1.15 x 10(-8)p(1/3). We also obtained an empirical relation for the band gap shrinkage, Delta E-g in Zn doped GaAs as a function of hole concentration. The value of Delta E-g(eV) = -2.75 x 10(-8)p(1/3), indicates a significant band gap shrinkage at high doping levels, These relations are considered to provide a useful tool to determine the hole concentration in Zn doped GaAs by low temperature PL measurement. The hole concentration increases with increasing AsH3 mole fraction and the main peak is shifted to a lower energy side. This can be explained also by the vacancy control model. As the hole concentration is increased above 3.8 x 10(18) cm(-3), a shoulder peak separated from the main peak was observed in the PL spectra and disappears at higher concentrations. (C) 1997 American Institute of Physics.
Resumo:
The ethanol sensing properties of porous Cr2O3 thin films deposited by the ultrasonic nebulized spray pyrolysis of an aqueous combustion mixture is reported. The impact of the precursor selection and various deposition parameters on the film crystallinity, surface morphology and stoichiometry are studied using thermo-gravimetric analysis, X-ray diffraction, scanning electron microscopy, transmission electron microscopy, X-ray photoelectron spectroscopy and atomic force microscopy techniques. The film morphology exhibits a highly porous nature, as a result of the exothermic combustion reaction during film deposition. The gas sensing properties of these films are investigated in the temperature range of 200-375 degrees C for ethanol. The films show two different regions of response for ethanol above and below 300 degrees C. A good relationship between the response and the ethanol concentration is observed, and is modeled using an empirical relation. The possible mechanism and the surface chemical reactions of ethanol over the chromium oxide surface are discussed.
Resumo:
We report on the realization of ZnO homojunction light-emitting diodes (LEDs) fabricated by metalorganic chemical vapor deposition on (0001) ZnO bulk substrate. The p-type ZnO epilayer was formed by nitrogen incorporation using N2O gas as oxidizing and doping sources. Distinct electroluminescence (EL) emissions in the blue and yellow regions were observed at room temperature by the naked eye under forward bias. The EL peak energy coincided with the photoluminescence peak energy of the ZnO epilayer, suggesting that the EL emissions emerge from the ZnO epilayer. In addition, the current-voltage and light output-voltage characteristics of ZnO homojunction LEDs have also been studied. (c) 2006 American Institute of Physics.
Photoresponse characteristics of n-type tetrahedral amorphous carbon/p-type Si heterojunction diodes
Resumo:
A new method to test the hole concentration of p-type GaN is proposed, which is carried out by analyzing the spectral response of p-n(+) structure GaN ultraviolet photodetector. It is shown that the spectral response of the photodetector changes considerably with reversed bias. It is found that the difference between photodetector's quantum efficiency at two wavelengths, i.e. 250 and 361 nm, varies remarkably with increasing reversed bias. According to the simulation calculation, the most characteristic change occurs at a reversed voltage under which the p-GaN layer starts to be completely depleted. Based on this effect the carrier concentration of p-GaN can be derived.
Resumo:
It is revealed from first-principles calculations that polarization-induced asymmetric distribution of oxygen vacancies plays an important role in the insulating behavior at p-type LaAlO3/SrTiO3 interface. The formation energy of the oxygen vacancy (V-O) is much smaller than that at the surface of the LaAlO3 overlayer, causing all the carriers to be compensated by the spontaneously formed V-O's at the interface. In contrast, at an n-type interface, the formation energy of V-O is much higher than that at the surface, and the V-O's formed at the surface enhance the carrier density at the interface. This explains the puzzling behavior of why the p-type interface is always insulating but the n-type interface can be conducting.
Resumo:
Using first-principles methods we have calculated electronic structures, optical properties, and hole conductivities of CuXO2 (X=Y, Sc, and Al). We show that the direct optical band gaps of CuYO2 and CuScO2 are approximately equal to their fundamental band gaps and the conduction bands of them are localized. The direct optical band gaps of CuXO2 (X=Y, Sc, and Al) are 3.3, 3.6, and 3.2 eV, respectively, which are consistent with experimental values of 3.5, 3.7, and 3.5 eV. We find that the hole mobility along long lattice c is higher than that along other directions through calculating effective masses of the three oxides. By analyzing band offset we find that CuScO2 has the highest valence band maximum (VBM) among CuXO2 (X=Y, Sc, and Al). In addition, the approximate transitivity of band offset suggests that CuScO2 has a higher VBM than CuGaO2 and CuInO2 [Phys. Rev. Lett. 88, 066405 (2002)]. We conclude that CuScO2 has a higher p-type doping ability in terms of the doping limit rule. (C) 2008 American Institute of Physics. [DOI: 10.1063/1.2991157]