992 resultados para CERIUM METAL


Relevância:

30.00% 30.00%

Publicador:

Resumo:

The coordination reactions during the solvent extraction of cerium(IV) and fluorine(l) from mixed nitric acid and hydrofluoric acid solutions by di-(2-ethylhexyl)-2-ethylhexylphosphonate, L (DEHEHP) in heptane have been investigated. The extraction data have been analyzed by graphical methods taking into account all plausible species extracted into the organic phase. Different variables influencing the extraction of Ce(IV), such as the concentrations of nitrate ions, hydrofluroric acid, nitric acid, and extractant have been studied. The results demonstrate that DEHEHP can extract not only Ce(NO3)(4) as Ce(NO3)4.2L and HF as HF (.) H2O (.) L, but both together as Ce(HF)(NO3)(4) (.) L. The extraction equilibrium equations are determined according to slope analysis and IR spectra. The equilibrium constants of the extracted complexes have been calculated, taking into account complexation between the metal ion and inorganic ligands in the aqueous phase and all plausible complexes extracted into the organic phase. It is also shown that boric acid, which was added into the mixed solutions to complex with F(I) is not extracted by DEHEHP, and neither does it affect the extraction of cerium(IV) and HF, nor change the extraction mechanism.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Hydrous cerium oxide (HCO) was synthesized by intercalation of solutions of cerium(III) nitrate and sodium hydroxide and evaluated as an adsorbent for the removal of hexavalent chromium from aqueous solutions. Simple batch experiments and a 25 factorial experimental design were employed to screen the variables affecting Cr(VI) removal efficiency. The effects of the process variables; solution pH, initial Cr(VI) concentration, temperature, adsorbent dose and ionic strength were examined. Using the experimental results, a linear mathematical model representing the influence of the different variables and their interactions was obtained. Analysis of variance (ANOVA) demonstrated that Cr(VI) adsorption significantly increases with decreased solution pH, initial concentration and amount of adsorbent used (dose), but slightly decreased with an increase in temperature and ionic strength. The optimization study indicates 99% as the maximum removal at pH 2, 20 °C, 1.923 mM of metal concentration and a sorbent dose of 4 g/dm3. At these optimal conditions, Langmuir, Freundlich and Redlich–Peterson isotherm models were obtained. The maximum adsorption capacity of Cr(VI) adsorbed by HCO was 0.828 mmol/g, calculated by the Langmuir isotherm model. Desorption of chromium indicated that the HCO adsorbent can be regenerated using NaOH solution 0.1 M (up to 85%). The adsorption interactions between the surface sites of HCO and the Cr(VI) ions were found to be a combined effect of both anion exchange and surface complexation with the formation of an inner-sphere complex.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This thesis Entitled INVESTIGATIONS ON THE STRUCTURAL, OPTICAL AND MAGNETIC PROPERTIES OF NANOSTRUCTURED CERIUM OXIDE IN PURE AND DOPED FORMS AND ITS POLYMER NANOCOMPOSITES.Synthesis and processing of nanomatelials and nanostmctures are the essential aspects of nanotechnology. Studies on new physical properties and applications of nanomaterials and nanostructures are possible only when nanostructured materials are made available with desired size, morphology,crystal structure and chemical composition.Recently, several methods have been developed to prepare pure and doped CeO2 powder, including wet chemical synthesis, thermal hydrolysis, flux method, hydrothermal synthesis, gas condensation method, microwave technique etc. In all these, some special reaction conditions, such as high temperature, high pressure, capping agents, expensive or toxic solvents etc. have been involved.Another hi gh-li ght of the present work is room temperature ferromagnetism in cerium oxdie thin films deposited by spray pyrolysis technique.The observation of self trapped exciton mediated PL in ceria nanocrystals is another important outcome of the present study. STE mediated mechanism has been proposed for CeO2 nanocrystals based on the dependence of PL intensity on the annealing temperature. It would be interesting to extent these investigations to the doped forms of cerium oxide and cerium oxide thin films to get deeper Insight into STE mechanism.Due to time constraints detailed investigations could not be canied out on the preparation and properties of free standing films of polymer/ceria nanocomposites. It has been observed that good quality free standing films of PVDF/ceria, PS/C61‘l8, PMMA/ceria can be obtained using solution casting technique. These polymer nanocomposite films show high dielectric constant around 20 and offer prospects of applications as gate electrodes in metal-oxide semiconductor devices.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The bifunctional carbamoyl methyl sulfoxide ligands, PhCH2SOCH2CONHPh (L-1), PhCH2SOCH2CONHCH2Ph (L-2), (PhSOCH2CONPr2)-Pr-i (L-3), PhSOCH2CONBu2 (L-4), (PhSOCH2CONBu2)-Bu-i (L-5) and PhSOCH2CON(C8H17)(2) (L-6) have been synthesized and characterized by spectroscopic methods. The selected coordination chemistry of L-1, L-3, L-4 and L-5 with [UO2(NO3)(2)] and [Ce(NO3)(3)] has been evaluated. The structures of the compounds [UO2(NO3)(2)((PhSOCH2CONBu2)-Bu-i)] (10) and [Ce(NO3)(3)(PhSOCH2CONBu2)(2)] (12) have been determined by single crystal X-ray diffraction methods. Preliminary extraction studies of ligand L-6 with U(VI), Pu(IV) and Am(III) in tracer level showed an appreciable extraction for U(VI) and Pu(IV) in up to 10 M HNO3 but not for Am(III). Thermal studies on compounds 8 and 10 in air revealed that the ligands can be destroyed completely on incineration. The electron spray mass spectra of compounds 8 and 10 in acetone show that extensive ligand distribution reactions occur in solution to give a mixture of products with ligand to metal ratios of 1 : 1 and 2 : 1. However, 10 retains its solid state structure in CH2Cl2.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Tinplate is one of the most widely used food canning materials, however, there are significant problems related to the use of tinplate cans, such as alterations in sensory features affecting food quality and corrosion phenomena of the canning material. To avoid corrosion problems different methods have been used for the passivation of tinplate such protective lacquers or different kinds of corrosion inhibitors (chromate and dichromate). However, chromates and dichromates are extremely harmful to the environment and can cause carcinogenic tumors to humans. An option, protective coatings obtained by the sol-gel process, act as a physical barrier, which isolates the surface of metal protecting from the corrosive agents. The aim of this work is to study the influence of addition of cerium (IV) ions in the inorganic and organic part of sol-gel processing in the formation of hybrid coatings based on siloxane-PMMA on tin plate. The coatings were obtained by dip-coating technique and evaluated by open circuit and impedance measurements, linear polarization and polarization curves obtained in 3.5% NaCl solution. The results have clearly shown the improvement on the protective properties of the Ce 4+ modified film when added into the organic phase, which can be due to the formation of a more uniform and densely reticulated siloxane-PMMA film. © 2009 by NACE International.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The interface formed between the metal and the porcelain of laser-welded Ni-Cr-Mo alloy was studied on a metallurgical basis. The characterization was carried out by using optical microscope, electron scan microscopy and X-ray dispersive spectroscopy techniques and mechanical three-point flexion tests, in the laser-welded region, with and without porcelain. The union of the porcelain with the alloy is possible only after the oxidation of the metallic surface and the subsequent application of a bonding agent known as opaque. The porcelain applied to the base metal and weld bead showed different behaviours - after the flexion test, the base metal showed cracks, while that in the weld bead broke away completely. It was noted that the region subjected to laser welding had lower adherence to the porcelain than the base metal region, due to microstructural refinement of the weld bead. These results can be shown by the X-ray dispersive spectroscopy carried out on the regions studied. The flexion tests demonstrated that the Ni-Cr-Mo alloy subject to laser welding had significant alterations in its mechanical properties after application of the porcelain.