900 resultados para Ceramic coatings


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent glass ceramics have been obtained by nucleation and growth of Y2Te6O15 or Er2Te5O13 cubic phase in a new Er3+-doped oxyfluoride tellurite glass. Effect of beat treatment on absorption spectra, luminescence and up-conversion properties in the oxyfluoride tellurite glass has been investigated. With heat treatment the ultraviolet absorption edge red shifted evidently for the oxyfluoride telluride glass. The near infrared emission that corresponds to Er3+:I-4(13/2)-> I-4(15/2) can be significantly enhanced after heat treatment. Under 980 nm LD pumping, red and green up-conversion intensity of Er3+ in the glass ceramic can be observed much stronger than that in the base glass. (C) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We demonstrate broadband optical amplification at 1.3 mu m in silicate glass-ceramics containing beta-Ga2O3:Ni2+ nanocrystals with 980 nm excitation for the first time. The optical gain efficiency is calculated to be about 0.283 cm(-1) when the excitation power is 1.12 W. The optical gain shows similar wavelength dependence to luminescence properties. (C) 2007 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent polycrystalline Nd:YAG ceramics were fabricated by solid-state reactive sintering a mixture of commercial Al2O3,Y2O3, and Nd2O3 powders. The powders were mixed in ethanol and doped with 0.5 wt% tetraethoxysilane, dried, and pressed. Pressed samples were sintered at 1750 degrees C in vacuum. Transparent fully dense samples with average grain sizes of 10 mu m were obtained. The 1 at.% Nd:YAG ceramic was used to research passively Q-switched laser output with a Cr4+:YAG crystal as a saturable absorber. An average output power of 94 mW with a pulse width of 50 ns was obtained when the incident pump power was 750 mW. The slope efficiency was 13%. The pulse energy is 5 mu J, and the peak power is about 100 W.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent polycrystalline Yb:YAG ceramics were fabricated by solid-state reactive sintering a mixture of commercial Al2O3, Y2O3, and Yb2O3 powders. The powders were mixed in ethanol and doped with 0.5 wt% tetraethoxysilane, dried, and pressed. Pressed samples were sintered at 1730 degrees C in vacuum. Transparent fully dense samples with grain sizes of several micrometers were obtained. The phase from 1500 degrees to 1700 degrees C was important for the grain growth, in which the grains grew quickly and a mass of pores were eliminated from the body of the sample. Annealing was an important step to remove the vacancies of oxygen and transform Yb2+ to Yb3+. The 1 at.% Yb:YAG ceramic sample was pumped by a diode laser to study the laser properties. The maximum output power of 1.02 W was obtained with a slope efficiency of 25% at 1030 nm. The size of the lasering sample was 4 mm x 4 mm x 3 mm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The novel nano-ultrafine powders for the preparation of CaCu3Ti4O12 ceramic were prepared by the sol-gel method and citrate auto-ignition method. The obtained precursor powders were pressed, sintered at 1000 degrees C to fabricate microcrystal CaCu3Ti4O12 ceramic. The microcrystalline phase of CaCu3Ti4O12 was confirmed by X-ray powder diffraction (XRD). The morphology and size of the grains of the powders and ceramics under different heat treatments were observed using scanning electron microscopy (SEM). The relative dielectric constant of the ceramic sintered at 1000 degrees C was measured with a magnitude of more than 10(4) at room temperature, which was approaching to those of Pb-containing complex perovskite ceramics, and the loss tangent was less than 0.20 in a broad frequency region. The relative dielectric constant and loss tangent were also compared with that of CaCu3Ti4O12 ceramic prepared by other reported methods. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Spectroscopic properties of (Y0.9-xLa0.1Ybx)(2)O-3 transparent ceramic were studied. Two main absorption peaks of the specimen are centered at 940 and 970 nm, which are suitable for InGaAs laser diode pumping. The main emission peaks were located at 1032 and 1075 nm with larger emission cross-section and longer fluorescence lifetime than those of Yb:Y2O3. These properties of (Y0.9-xLa0.1Ybx)(2)O-3 transparent ceramic are favorable to achieve high efficiency and high power laser output. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The up-conversion luminescence of Yb3+-doped yttriurn lanthanum oxide transparent ceramic was investigated. It was ascribed to cooperative luminescence originated from the coupled states of the Yb3+ ion pairs. The proper doping of La2O3 can remove the cooperative luminescence of Yb3+ ion. But excessive La2O3 (at least 10 at.%) the cooperative up-conversion of Yb3+:Y2O3 is obtained again, and the intensity of up-conversion luminescence strengthens with the increase of La2O3 content. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Considering the interface absorption in optical coatings, we propose a model to simulate interface absorption. Calculations are made and the temperature field of several kinds of thin film multilayers, including those of partial reflectivity, high-reflectivity, and antireflectivity coatings are analyzed. The interface absorption is found to greatly influence the temperature distribution within multilayer coatings and to weaken the laser damage resistance of the samples. The real-time results of the photothermal deflection technique for laser induced damage to samples supports the model. (C) 1997 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The laser-induced damage threshold (LIDT) and damage morphology of antireflection (AR) coatings on quartz and sapphire are investigated. A very interesting phenomena is found in the measurement. In the case of a single pulse laser, the LIDT of the AIR coatings on quartz is higher than that of sapphire. On the contrary, for a free-pulse laser, the LIDT of AIR coatings on sapphire is higher than that of quartz. (C) 2004 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coatings with layer structures of Ag/glass, Ag/Cr/glass, and Ag/Cr-Ag/Cr/glass deposited with magnetron sputtering are investigated. The results indicate that the performance for reflectance, hardness, adherence, and humidity durability of the silver coatings with Ag/Cr/glass and Ag/Cr-Ag/Cr/glass structures are better than pure silver film. In addition, the silver coatings with an Ag/Cr-Ag/glass structure present more advantages than that of the Ag/Cr/glass. Reasons are analyzed accordingly. (C) 2004 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Laser conditioning effects of the HfO2/SiO2 antireflective (AR) coatings at 1064 nm and the accumulation effects of multishot laser radiation were investigated. The HfO2/SiO2 AR coatings were prepared by E-beam evaporation (EBE). The singleshot and multi-shot laser induced damage threshold was detected following ISO standard 11254-1.2, and the laser conditioning was conducted by three-step raster scanning method. It was found that the single-shot LIDT and multi-shot LIDT was almost the same. The damage mostly > 80% occurred in the first shot under multi-shot laser radiation, and after that the damage occurring probability plummeted to < 5%. There was no obvious enhancement of the laser damage resistance for both the single-shot and multi-shot laser radiation of the AR coatings after laser conditioning. A Nomarski microscope was employed to map the damage morphology, and it found that the damage behavior is defect-initiated for both unconditioned and conditioned samples. © 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Y2O3/SiO2 coatings were deposited on fused silica by electron beam evaporation. A continuous wave CO2 laser was used to condition parts of the prepared samples at different scanning speeds in the air. LAMBDA 900 spectrometer was used to investigate the changes of the transmittance and residual reflection spectrum. A Nomarski microscope under dark field was used to examine the changes of the micro defect density. The changes of the surface roughness and the microstructure of the film before and after conditioning were investigated by AFM and X-ray diffraction, respectively. We found that laser-induced damage threshold (LIDT) of the films conditioning at 30 mm/s scanning speed was increased by more than a factor of 3 over the thresholds of the as-deposited films. The conditioning effect was correlated with an irradiation-induced decrease of the defect density and absorption of the films. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZrO2 coatings were deposited on different substrates of Yb:YAG and fused silica by electron beam evaporation. After annealed for 12 h at 673 and 1073 K, respectively, weak absorption of coatings was measured by surface thermal lensing (STL) technique, and then laser-induced damage threshold (LIDT) was determined also. The crystalline phase of ZrO2 coatings and the size of the crystal grain were investigated by X-ray diffraction. It was found that microstructure of ZrO2 coatings was dependent on both annealing temperature and substrate structure, and coatings containing monoclinic phases had higher damage threshold than others. Due to the strong absorption of Yb:YAG, damage threshold of coatings on Yb:YAG was much less than that on fused silica. (C) 2004 Elsevier B.V. All rights reserved.